Effects of KNbO3-Substitution on the Dielectric and Piezoelectric Properties of (Li,Na,K)(Nb,Sb,Ta)O3 System Ceramics (KNbO3 치환이 (Li,Na,K)(Nb,Sb,Ta)O3계 세라믹스의 유전 및 압전 특성에 미치는 영향)

  • Noh, Jungrae;Yoo, Ju-Hyun;Lee, Sang-Don
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.26 no.3
    • /
    • pp.204-208
    • /
    • 2013
  • In this study, $KNbO_3$-substituted (Li,Na,K)(Nb,Sb,Ta)$O_3$ ceramics were investigated to develop Pb-free composition ceramics for multilayer actuator and energy harvester applications. The X-ray diffraction analysis indicated that all samples were pure perovskite phase and no secondary phase was found. A tetragonality as a function of $KNbO_3$ substitution showed the maximum value at 1.5 mol% $KNbO_3$ and then decreased. The SEM image analysis showed the maximum grain size of $3.14{\mu}m$ at 1.5mol% $KNbO_3$. In the composition ceramics with 1.5 mol% $KNbO_3$ sintered at $1,100^{\circ}C$, excellent properties of density= 4.75 $g/cm^3$, electromechanical coupling factor ($k_p$)= 0.50 and piezoelectric constant($d_{33}$)= 290 pC/N were obtained, respectively, suitable for piezoelectric actuator and energy harvester applications.

Dielectric and Piezoelectric Properties of (Na0.5K0.5)0.97NbO3 Ceramics Substituted with CeMnO3 (CeMnO3 치환된 (Na0.5K0.5)0.97NbO3 세라믹스의 유전 및 압전 특성)

  • Oh, Young-Kwang;Yoo, Ju-Hyun;Mah, Suk-Burm;Jeong, Yeong-Ho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.24 no.3
    • /
    • pp.194-199
    • /
    • 2011
  • In this study, non-stoichiometric 1-x$[(K_{0.5}Na_{0.5})_{0.97}(Nb_{0.96}Sb_{0.04})O_3]$ + x $CeMnO_3$ + 0.8 mol%CuO + 0.2 wt% $Ag_2O$ (x=0, 0.005) ceramics were prepared by a conventional mixed oxide and carbonate method, their dielectric and piezoelectric properties were investigated with the variations of sintering temperature. As $CeMnO_3$ substitution incereased, the density, piezoelectric constant($d_{33}$) and dielectric constant($\varepsilon_r$) were increased and the mechanical quality factor(Qm) was decreased. At the sintering temperature of $1100^{\circ}C$, the density, electromechanical coupling factor($k_p$), dielectric constant($\varepsilon_r$) and piezoelectric constant($d_{33}$) of 0.5mol% $CeMnO_3$ specimen showed the optimun values of 4.475 $g/cm^2$, 0.437, 552 and 166 pC/N, respectively. However, the mechanical quality factor($Q_m$) showed the minimum value of 380.

Dielectric and Piezoelectric Properties of 0.95(K0.5Na0.5)NbO3-0.05Li(Sb0.8Nb0.2)O3 Ceramics according to the Amount of CuO Addition (CuO첨가에 따른 0.95(K0.5Na0.5)NbO3-0.05Li(Sb0.8Nb0.2)O3 세라믹스의 유전 및 압전특성)

  • Lee, Yu-Hyung;Kim, Do-Hyung;Yoo, Ju-Hyun;Kim, In-Sung;Song, Jae-Sung;Hong, Jae-Il
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.22 no.6
    • /
    • pp.489-494
    • /
    • 2009
  • In this study, In order to improve dielectric and piezoelectric properties of Lead-free piezoelectric ceramics, $0.95(K_{0.5}Na_{0.5})NbO_3-0.05Li(Sb_{0.8}Nb_{0.2})O_3+0.2\;wt%Ag_2O+0.4\;wt%MnO_2+Xwt%CuO$ were investigated as a function of the amount of CuO addition. With increasing the amount of CuO addition, density was increased up to 0.4 wt.% CuO and then decreased above. And also, electro mechanical coupling factor ($k_p$) was decreased. At the 0.4 wt% CuO added specimen sintered at $1020^{\circ}C$, $k_p$, Qm, density, dielectric constant (${\varepsilon}_r$) and $d_{33}$[pC/N] showed the optimal value of $4.37\;g/cm^3$, 0.354, 305, 645, and 144 pC/N respectively.

Effects of Al2O3 on the Piezoelectric Properties of Pb(Mn1/3Nb2/3)O3-PbZrO3-PbTiO3 Ceramics (Pb(Mn1/3Nb2/3)O3-PbZrO3-PbTiO3 세라믹스의 압전특성에 미치는 Al2O3의 영향)

  • Kim Mi-Jung;Kim Jae-Chang;Kim Young-Min;Ur Soon-Chul;Kim Il-Ho
    • Korean Journal of Materials Research
    • /
    • v.15 no.7
    • /
    • pp.453-457
    • /
    • 2005
  • Piezoelectric properties of $Pb(Mn_{1/3}Nb_{2/3})O_3-PbZrO_3-PbTiO_3$ ceramics were investigated with $Al_2O_3$ content $(0.0-1.0 wt\%)$. The constituent phases, microstructure, electromechanical coupling factor, dielectric constant, piezoelectric charge and voltage constants were analyzed. Diffraction peaks for (002) and (200) planes were identified by X-ray diffractometer for all the specimens doped with $Al_2O_3$, indicating the MPB (morphotropic phase boundary) composition of tetragonal structures. The highest sintered density of $7.8 g/cm^3$ was obtained for $0.2wt\%\;Al_2O_3-doped$ specimen. Grain size increased by doping $Al_2O_3$ up to $0.3 wt\%$, and it decreased by more doping. Electromechanical coupling factor, dielectric constant, piezoelectric charge and voltage constants increased by doping $Al_2O_3$ up to $0.2wt\%$, and it decreased by more doping. This might result from the formation of oxygen vacancies due to defects in $O^{2-}$ ion sites and the substitution of $Al^{3+}$ ions.

Piezoelectric and Dielectric Characteristics of Low Temperature Sintering PNW-PMN-PZT Ceramics with the Amount of $CaCO_3$ Addition ($CaCO_3$ 첨가에 따른 저온소결 PNW-PMN-PZT 세라믹스의 압전 및 유전 특성)

  • Lee, Sang-Ho;Lee, Chang-Bae;Chung, Kwang-Hyur;Yoo, Ju-Hyun;Park, Chang-Yub;Jeong, Yeong-Ho
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.11a
    • /
    • pp.421-424
    • /
    • 2004
  • In this study, in order to develop low temperature sintering ceramics for ultrasonic vibrator, PNW-PMN-PZT system ceramics were manufactured with the amount of $CaCO_3$ addition and their piezoelectric, dielectric and microstructural characteristics were investigated. $CaCO_3$ addition to PNW-PMN-PZT basic composition was proved to be capable of sintering the ceramics at temperature below $1000^{\circ}C$ due to the effect of $Li_2CO_3-CaCO_3$ liquid phase. However, with increasing the amount of $CaCO_3$ addition, the second phase was appeared. As the results, electromechanical coupling coefficient (kp) and dielectric constant $(\epsilon_r)$ decreased. Taking into consideration electromechanical coupling coefficient (kp) of 0.49, mechanical quality factor (Qm) of 1396, dielectric constant $(\epsilon_r)$ of 1300 and density of $7.78[g/cm^2]$, it was concluded that the 0.25wt% $CaCO_3$ addition composition ceramics sintered at $920^{\circ}C$ was suitable for ultrasonic vibrator application.

  • PDF

Effects of the Mixing Method and Sintering Temperature on the Characteristics of PZNN-PZT Piezoelectric Ceramic Materials (합성방법과 소결 온도가 PZNN-PZT 압전 세라믹스 소재특성에 미치는 영향)

  • Kim, So Won;Jeong, Yong Jeong;Lee, Hee Chul
    • Journal of Powder Materials
    • /
    • v.25 no.6
    • /
    • pp.487-493
    • /
    • 2018
  • The impact of different mixing methods and sintering temperatures on the microstructure and piezoelectric properties of PZNN-PZT ceramics is investigated. To improve the sinterability and piezoelectric properties of these ceramics, the composition of $0.13Pb((Zn_{0.8}Ni_{0.2})_{1/3}Nb_{2/3})O_3-0.87Pb(Zr_{0.5}Ti_{0.5})O_3$ (PZNN-PZT) containing a Pb-based relaxor component is selected. Two methods are used to create the powder for the PZNN-PZT ceramics. The first involves blending all source powders at once, followed by calcination. The second involves the preferential creation of columbite as a precursor, by reacting NiO with $Nb_2O_5$ powder. Subsequently, PZNN-PZT powder can be prepared by mixing the columbite powder, PbO, and other components, followed by an additional calcination step. All the PZNN-PZT powder samples in this study show a nearly-pure perovskite phase. High-density PZNN-PZT ceramics can be fabricated using powders prepared by a two-step calcination process, with the addition of 0.3 wt% MnO2 at even relatively low sintering temperatures from $800^{\circ}C$ to $1000^{\circ}C$. The grain size of the ceramics at sintering temperatures above $900^{\circ}C$ is increased to approximately $3{\mu}m$. The optimized PZNN-PZT piezoelectric ceramics show a piezoelectric constant ($d_{33}$) of 360 pC/N, an electromechanical coupling factor ($k_p$) of 0.61, and a quality factor ($Q_m$) of 275.

Piezoelectric Characteristics of Lead-Free 0.74(Bi0.5Na0.5)TiO3-0.26SrTiO3 Ceramics According to Calcination Temperature (무연 0.74(Bi0.5Na0.5)TiO3-0.26SrTiO3 압전 세라믹스의 하소온도 변화에 따른 전기적 특성 변화)

  • Kim, Seong-Hyun;Lee, Sang-Hun;Han, Hyoung-Su;Lee, Jae-Shin
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.32 no.1
    • /
    • pp.35-39
    • /
    • 2019
  • In this study, we investigated the optimum calcination temperature of lead-free $0.74(Bi_{0.5}Na_{0.5})TiO_3-0.26SrTiO_3$(BNST) piezoelectric ceramics by analyzing the crystal structure, dielectric properties, and electric field-induced strain behavior. BNST ceramics prepared by conventional solid-state reaction methods at various calcination temperatures according to the industrial standard. All samples of BNST ceramics were subsequently sintered at $1,175^{\circ}C$ for 2 h. Crystal structure classification of the ceramics showed a single perovskite phase, with no second phase detectable for the samples calcined at $750^{\circ}C$ or higher. BNST samples calcined at $850^{\circ}C$ exhibited the most optimal values for itsand the common physical parameters of $density=5.518g/cm^3$, ${\varepsilon}=1,871.837$, $tan{\delta}=0.047$, and ${d_{33}}^*=874pm/V$.

Optimization Study for Material Properties of Piezoelectric Material Using Parameter Estimation Method: Part I. Polycrystal PZT Ceramics (매개변수 평가법을 이용한 압전재료의 재료물성 최적화 연구 Part I. 다결정 PZT 세라믹스)

  • Shin, Ho-Yong;Lee, Ho-Yong;Hong, Il-Gok;Kim, Jong-Ho;Im, Jong-In
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.35 no.5
    • /
    • pp.471-479
    • /
    • 2022
  • Recently, piezoelectric devices, such as ultrasonic surgery, ultrasonic atomizer, and ultrasonic speaker, are analyzed and designed by finite element simulation methods. However, the discrepancy between the design and the experiment results of the device typically occurs due to the inaccuracy of the piezoelectric material properties. To improve the simulation accuracy, the material properties of the PZT ceramics were better refined using parameter estimation method. The material parameters are elastic stiffness cEij and piezoelectric constant eij of PZT ceramics. The impedance curve characteristics for the LTE mode of PZT ceramics were calculated. The mismatch between the simulation and the experimental data were compared and minimized by a least square method. Finally, the simulated impedance data were compared with the experimental data for the various vibration modes of PZT ceramics and the optimized material properties of PZT ceramics were verified. To further verify the accuracy, this method was also applied to piezoelectric PMN-PT single crystals.

Electrical Properties and Phase Transition Behavior of Lead-Free BaTiO3-Modified Bi1/2Na1/2TiO3-SrTiO3 Piezoelectric Ceramics (BaTiO3 첨가에 따른 Bi1/2Na1/2TiO3-SrTiO3 무연 압전 세라믹스의 전기적 특성 및 상전이 거동 연구)

  • Kang, Yubin;Park, Jae Young;Devita, Mukhllishah Aisyah;Duong, Trang An;Ahn, Chang Won;Kim, Byeong Woo;Han, Hyoung-Su;Lee, Jae-Shin
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.35 no.5
    • /
    • pp.516-521
    • /
    • 2022
  • We investigated the microstructure, crystal structure, dielectric, and elecromechanical strain properties of lead-free BaTiO3 (BT)-modified (Bi1/2Na1/2)TiO3-SrTiO3 (BNT-ST) piezoelectric ceramics. Samples were prepared by a conventional ceramic processing route. Temperature dependent dielectric properties confirmed that a phase transition from a nonergodic relaxor to an ergodic relaxor was induced when the BT concentration reached 1.5 mol%, interestingly, where the average grain size reached a maximum value of 4.5 ㎛. At the same time, enhanced electromechanical strain (Smax/Emax = 600 pm/V) was obtained. It is suggested that the induced ferroelectric-relaxor phase transition by the BT modification is responsible for the enhancement of electromechanical strain in 1.5 mol% BT-modified BNT-ST ceramics.

Effect of Li2CO3 Doping on Phase Transition and Piezoelectric Properties of 0.96K0.5Na0.5NbO3-0.04SrTiO3 Ceramics (0.96K0.5Na0.5NbO3-0.04SrTiO3 세라믹스의 상전이와 압전 특성에 대한 Li2CO3 도핑 효과)

  • Jae Young Park;Trang An Duong;Sang Sub Lee;Chang Won Ahn;Byeong Woo Kim;Hyoung-Su Han;Jae-Shin Lee
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.36 no.5
    • /
    • pp.513-519
    • /
    • 2023
  • It was reported that a tetragonal phase can be stabilized with maintaining good piezoelectric properties when Na0.5K0.5NbO3 (KNN) is modified with 0.06 mol SrTiO3. However, such a high amount of SrTiO3 leads not only to poor sinterability but low Curie temperature (TC). To maintain high TC with good piezoelectric properties in KNN-based lead-free piezoelectric ceramics, this study investigates the effect of Li-doping on the dielectric and piezoelectric properties of 0.96Na0.5K0.5NbO3-0.04SrTiO3 (KNN-4ST) ceramics. As a result, the orthorhombic-tetragonal phase transition was observed at 2 mol% Li2CO3 modified KNN-4ST ceramics, whose TC, d33 and kp values are 328℃, 165pC/N and 0.33, respectively.