  • Purpose. The purpose of this study was to evaluate the effect of surface treatments on the shear bond strength of two types of zirconia (3-TZP and 5Y-PSZ) with resin cement. Materials and methods. Two different types of zirconia specimens with a fully sintered size of 14.0×14.0×2.0 mm3 were prepared, polished with 400, 600, and 800 grit silicon carbide paper, and buried in epoxy resin. They were classified into four groups each control, sandblasting, primer, and sandblasting & primer. Cylindrical resin adhered to the surface-treated zirconia with resin cement. It was stored in distilled water (37℃) for 24 hours, and a shear bond strength test was performed. The normality of the experimental group was confirmed with the Kolmogorov-Smirnov & Shapiro-Wilk test. The interaction and statistical difference were analyzed using a two-way ANOVA. A post-hoc analysis was performed using Dunnett T3. Results. As a result of two-way ANOVA, there was no significant difference in shear bonding strength between zirconia types (P > .05), but there was a significant correlation in the sandblasting, primer, and alumina sandblasting & primer group (P < .05). Dunnett T3 post-test showed that, regardless of the type of zirconia, shear bonding strength was sandblasting & primer > Primer > sandblasting > control group (P < .05). Conclusion. There was no difference in shear bond strength between the types of zirconia. The highest shear bond strength was shown when the mechanical and chemical treatments of the zirconia surface was performed simultaneously.

The effect of different bonding systems on shear bond strength of repaired composite resin (접착 시스템이 수리된 복합 레진의 전단 결합 강도에 미치는 영향)

  • Seon, Eun-Mi;Kim, Hyeon-Cheol;Hur, Bock;Park, Jeong-Kil
    • Restorative Dentistry and Endodontics
    • /
    • v.33 no.2
    • /
    • pp.125-132
    • /
    • 2008
  • The purpose of this study is to compare the shear bond strength of repaired composite resin with different bonding agents and evaluate the effect of bonding agents on composite repair strength. Forty composite specimens (Z-250) were prepared and aged for 1 week by thermo cycling between 5 and $55^{\circ}C$ with a dwell time of 30s. After air abrasion with $50\;{\mu}m$ aluminum oxide, following different bonding agents were applied (n = 10); SB group: Scotchbond multipurpose adhesive (3 step Total-Etch system); XE group: Clearfil SE bond (2 step Self-Etch system); XP group: XP bond (2 step Total-Etch system); XE group: Xeno III (1 step Self-Etch system). After bonding procedure was completed, new composite resin (Z-250) was applied to the mold and cured. For control group. 10 specimens were prepared. Seven days after repair, shear bond strength was measured. Data was statistically analyzed using one-way ANOVA and Tukey's test (p<0.05). The means and standard deviations of shear bond strength (MPa ${\pm}$ S.D.) per group were as follows: SB group: 17.06; SE group: 19.10; XP group: 14.44; XE group: 13.57; Control Group: 19.40. No significant difference found in each group. Within the limit of this study, it was concluded that the different type of bonding system was not affect on the shear bond strength of repaired composite resin.

The Effect of Pre-Treatment Methods for the Life Time of the Insoluble Electrodes (불용성 전극의 전처리 방법이 전극의 수명에 미치는 영향)

  • Park, Mi-Jung;Lee, Taek-Soon;Kang, Meea;Han, Chi-Bok
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.38 no.6
    • /
    • pp.291-298
    • /
    • 2016
  • Electrochemical water treatment process as a useful treatment method for the removal of non-degradable matter has been consistently studied for several decades. Key process of electrochemical water treatment are oxidation reaction from an anode and reduction from a cathode. In this study, the effect of pre-treatment methods in the insoluble electrode manufacturing process for the water treatment has been evaluated for the life time of electrode The results of this study showed that pre-treatment methods of a base metal such as surface roughness, clean method and interlayer formation influenced to life time of electrode when the same condition (catalyst electrode layer coating method and material system) was applied for pre-treatment methods. This study was conducted by using $IrO_2/Ti$ electrode In the test of sand-blasting process, an electrode manufactured by using sanding media of different sizes resulted in the most effective electrode life time when the size of alumina was used for $212{\sim}180{\mu}m$ praticle size (#80). The most effective method was considered using arc plasma in the additional roughness control and cleaning process, sputtering method to form Ta type interlayer formation process.

Influence of sandblasting and primer on shear bond strength of resin cement to zirconia (샌드블라스팅과 프라이머가 지르코니아와 레진시멘트의 전단결합강도에 미치는 영향)

  • Lee, Jung-Haeng;Kim, Hyeong-Seob;Pae, Ah-Ran;Woo, Yi-Hyung
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.49 no.1
    • /
    • pp.49-56
    • /
    • 2011
  • Purpose: The aim of this study was to evaluate the effect of mechanical, chemical surface treatments on the zirconia-to-resin cement shear bond strength (SBS). Materials and methods: Eighty zirconia discs (Lava, 3M ESPE) and eighty zirconia/alumina composite (Zirace, Acucera) were embedded in an epoxy resin base. Zirconia discs were randomly divided in to four treatment groups(10 for each manufacturer): $50\;{\mu}m$ $Al_2O_3$ sandblasting (S50), $110\;{\mu}m$ $Al_2O_3$ sandblasting (S110), $50\;{\mu}m$ $Al_2O_3$ and primer (Z-Prime Plus, Bisco Inc) (S50z) and $110\;{\mu}m$ $Al_2O_3$ and primer (Z-Prime Plus) (S110z). Two resin-based luting cements (Calibra, Panavia F) were used to build 2 mm diameter cylinders onto the zirconia. After 24 h of storage in water, SBS testing was evaluate using a universal testing machine. Bond strength data were analyzed with one-way ANOVA, two-way ANOVA test and post hoc comparison was done using Tukey test (${\alpha}$ = .05). Results: Groups using primer showed the high shear bond strength. The groups that did not use primer presented lower shear bond strengths. Conclusion: The use of primer (Z-Prime Plus, Bisco) had significantly higher shear bond strengths.

Osseointegration of zirconia implant in the tibia of pigs (돼지의 경골에 식립된 지르코니아 임플란트의 골유착에 관한 연구)

  • Kim, Lee-Kyoung;Cho, In-Ho
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.51 no.3
    • /
    • pp.190-198
    • /
    • 2013
  • Purpose: The purposes of this study were to investigate osseointegration around zirconia implants which had machined or alumina sandblasted surface, and to compare the results with titanium implants. Materials and methods: The study was performed on the tibia of 6 pigs. Three types of implants were investigated: group T-titanium implant, group Z-machined zirconia implant, group ZS-alumina sandblasting treated zirconia implant. Zirconia implants were manufactured from yttria-stabilized tetragonal zirconia polycrystalline (Acucera Inc., Pocheon, Korea). A total of 36 implants were installed in pigs' tibias. After 1, 4 and 12 weeks of healing period, the periotest and the histomorphometric analysis were performed. The data were analyzed using one-way ANOVA and significance was assessed by the Scheffe test (${\alpha}=.05$). Results: In the measurement of surface roughness, highest Ra value was measured in group T with significant difference. No significant differences were found among groups regarding Periotest values. After 1 week, in comparison of bone to implant contact (BIC), group Z showed higher value with significant difference. In comparison of bone area (BA), group T and group Z showed higher value with significant difference than group ZS. After 4 weeks, in comparison of BIC, group T showed higher value with significant difference. Comparison of BA showed no significant difference among each implant. After 12 weeks, the highest mean BIC values were found in group T with significant difference. Group ZS showed higher BIC value with significant difference than group Z. In comparison of BA, group T and group ZS showed higher value with significant difference than group Z. Conclusion: Zirconia implant showed low levels of osseointegration in this experiment. Modification of surface structure should be taken into consideration in designing zirconia implants to improve the success rate.