In this study, a method to reduce temperature rise due to hydration in mass concrete is investigated. It is to use retarder (glucose) for reducing heat of hydration and to use calcium silicate hydrate (C-S-H) for compensating the retardation effect due to its role as a nucleation seed. For this purpose, the temperature rise of cement paste due to hydration was measured and the effect of using both C-S-H and glucose on setting and 28-day compressive strength of mortar specimens was investigated. According to the experimental results, using C-S-H and glucose caused the reduction in the maximum temperature but accelerated the time to reach the maximum temperature compared to that of retarded cement paste using glucose. In addition, using C-S-H and glucose did not show significant effect on 28-day compressive strength of mortar specimens, indicating that the method shown in this study can be a successful alternative to control maximum temperature rise in mass concrete.
Kim, Hong-Yeon;Cha, Jae-Hyeok;Youn, Jong-Young;Kim, Sung-Jin;Lee, Donghoon
Journal of the Korea Institute of Building Construction
/
v.23
no.3
/
pp.251-260
/
2023
The construction of free-form structures with intricate curved exteriors necessitates the use of bespoke molds. To fulfill this requirement, a blend of Phase Change Material(PCM) and Ultra-High Performance Concrete(UHPC) is utilized. PCM endows the solution with recyclability, while UHPC facilitates the effortless execution of curvature in the mold fabrication process. However, it's worth mentioning that the melting point of PCM hovers around 58-64℃, and the heat emanating from UHPC's hydration process can potentially jeopardize the integrity of the PCM mold. Hence, experimental validation of the mold shape is a prerequisite. In the conducted experiment, UHPC was poured into two distinct mold types: one that incorporated a 3mm silicone sheet mounted on the fabricated PCM mold(Panel A), and the other devoid of the silicone sheet(Panel B). The experimental outcomes revealed that Panel A possessed a thickness of 3.793mm, while Panel B exhibited a thickness of 5.72mm. This suggests that the mold lacking the silicone sheet(Panel B) was more susceptible to the thermal effects of hydration. These investigations furnish invaluable fundamental data for the manufacturing of ultra-high strength irregular panels and PCM molds. They contribute substantially to the enrichment of comprehension and application of these materials within the realm of construction.
Proceedings of the Korea Concrete Institute Conference
/
2009.05a
/
pp.331-332
/
2009
The purpose of this study was to evaluate the effect of rejct fly-ash and blast-furnace slag on hydration heat and strength development of ternary system cement and concrete. Main experimental variables were performed fly-ash contenes (20%) and rejct fly-ash contents (20%) and slag contents (50%, 55%). The hydration heat and insulation temperature, strength development were measured to analyze the concrete of ternary system cement
Journal of Korean Tunnelling and Underground Space Association
/
v.11
no.1
/
pp.37-45
/
2009
In this study, experiments of development and application of 50 MPa high-performance concrete are performed for large dimensional tunnel linings. In order to produce 50MPa high-performance concrete, eight optimal mixtures replacing with fly ash and ground granulated blast furnace slag up to 50 percent of type I Portland cement were selected then tests for mechanical properties and simple adiabatic temperature rise tests were carried out. And in order to assess the quantitative characteristics of heat of hydrations of developed mixtures, three mixtures that the type I Portland cement (OPC) and each one mixture of binary and ternary mixtures (BS30, F15S35) were reselected, then the adiabatic temperature rise tests and mock-up tests were performed. Consequently, the comparisons between the results of mock-up tests and finite element analysis can be enhanced the reliability of analyzing routines of thermal behaviours of the developed high-performance concrete.
Lee, Jae-Min;Yang, Hee Hun;Jeong, Seoung Hyun;Kim, Seong Kyum;Jang, Il Young
Proceedings of the Korean Society of Disaster Information Conference
/
2022.10a
/
pp.437-438
/
2022
본 논문에서는 상변환 재료를 이용하여 동절기에 발생하는 도로포장의 블랙아이스 현상을 저감시키기 위한 기초연구를 진행하였다. 콘크리트 내에서 누출을 막기 위해 마이크로 캡슐화된 상변환 재료를 이용했으며 초기 개발단계인 만큼 페이스트 단계에서 실험을 진행 하였다. 실험은 초기 수화거동에서의 수화열 발생 경향을 분석하기 위해서 미소수화열 측정 실험과 반복되는 온도변화 환경에서의 상변환재료 캡슐의 안정성을 분석하기 위해 주사전자현미경을 이용하였다. 상변환 재료의 열에너지 저장 및 방출 능력은 시멘트의 미소수화열 발생에 상당한 변화를 주었으며, 온도변화에 의한 상변환 재료 캡슐계면의 이상은 발생하지 않는 것으로 나타났다.
Journal of the Korea institute for structural maintenance and inspection
/
v.5
no.4
/
pp.227-233
/
2001
최근 비약적인 경제발전에 힘입어 장대교량, 항만, 댐, 도로, 원자력 발전소 등과 같은 대규모 기간구조물의 건설이 증가하고 있으며, 구조물은 대형화 혹은 고강도화되는 추세에 있다. 특히, 전술한 구조물을 매스콘크리트로 가설하게 되면 초기재령시에 수화열로 인한 균열이 발생할 가능성이 매우 높기 때문에 효율적인 매스콘크리트의 개발과 매스콘크리트 구조물의 설계기술 및 시공방법이 중요한 연구대상으로 등장하게 된다. 본 논문에서는 가로 52.6m, 세로 14.4m, 높이 8.5m의 기계기초 매스콘크리트의 시공에 적합한 온도관리기법을 다음과 같은 단계로 제안하고자 한다. 먼저 온도상승요인을 최소화하는 콘크리트의 배합비를 산정한다. 산정된 콘크리트의 열특성을 측정하기 위해 단열온도실험을 수행하여 각종 열특성상수와 단열온도 상승곡선식을 도출한다. 이와 같은 열특성치를 콘크리트 구조체에 적용하여 열응력해석을 수행한다. 이와 같은 열응력해석을 통하여 구조물의 분할타설높이에 따라 온도균열이 발생하지 않는 콘크리트 내외부의 온도차를 결정한다. 이때 열응력해석에 범용 유한요소 프로그램인 Diana을 사용한다. 콘크리트의 타설은 현장조건과 타설시점을 최대로 고려하고 양생방법으로 콘크리트 내외부의 온도차를 최소화하기 위해 이중단열효과가 있는 거푸집과 가열장비을 사용한다. 또한 콘크리트의 온도관리를 위하여 구조물 내외부에 온도게이지를 매립하고 30분마다 계측을 수행하면서 콘크리트 내외부 온도차가 허용 해석범위를 유지하도록 한다. 양생기간은 7-10일 정도를 유지한다. 전술한 온도관리기법을 통하여 완공후 수평정밀도가 기초의 허용침하량으로 환산하여 $1{\mu}m$ 인 고정밀도의 기계기초는 완벽하게 시공되었다. 따라서 매스콘크리트의 온도균열을 제어할 수 있는 시공방법으로 제안한다. 또한 매스콘크리트의 내외부 온도차를 단열온도실험과 온도해석으로부터 정한 값이내로 제어하고 충분한 양생관리를 병행하면 수화열에 의한 콘크리트의 온도균열을 최소화할 수 있을 것으로 기대한다.
Proceedings of the Korean Society for Agricultural Machinery Conference
/
2003.02a
/
pp.434-439
/
2003
20세기 후반부에 이르러 초음파는 과학 및 산업분야 전반에 걸쳐 다각도로 활용 및 응용되고 있다. 본 연구는 초음파를 이용한 분무입경의 미세화 및 균일입경의 분무를 위한 초음파 응용기기의 설계를 위한 선행연구로서 초음파 에너지에 의한 고형성분의 파쇄여부를 측정하였다. 초음파 에너지를 부가한 후, 즉 초음파 처리된 상태에서의 수화제의 물리적인 파쇄특성을 광학현미경과 SEM을 이용하여 관찰하였다. (중략)
Purpose: The purpose of the study is to help economic and safe construction by accurately predicting the initial strength of high-strength concrete (70MPa) for each type of cement, securing reliability of concrete quality, and drawing accurately the timing of form deformed, tensioning time of PS concrete, and openning of traffic after road repair with maturity. Method: Calculate the maturity by measuring the hydration heat with cement type for each age, and measure the strength of concrete with age to predict the strength corresponding to the any maturity. Result: In estimating the time required for traffic opening in road repair, ASTM C1074 was theoretically estimated at 16.4 hours for high-strength concrete, but in this study, maturity was calculated at 307, 14.4 hours for OPC and maturity at 2700, 34 hours for LHPC and maturity 200, 8 hours for ESPC. Conclusion: The timing of form deformed of structures using high-strength concrete and the opening of traffic of road repair may be much faster than in the case of concrete using OPC below the design basis strength 40MPa applied by ACI Committee 347.
Setting time of cement-based materials can represent a developing strength in early-age mixture, and it can be used a significant parameter of high-performance concrete having various mix-proportions. Generally, initial and final setting time of concrete is measured by penetration resistance method that used a wet-sieving mortar mixture, therefore, it hardly represents the setting time of sound concrete including coarse aggregate. Recently, several nondestructive methods, such as ultrasonic velocity and impendence measurement, are proposed to evaluate the setting time of fresh concrete. This study attempts to measure an electrical resistivity using four-electrode method for evaluation of setting time in early-age cement-based materials. For this purpose, total 10 mixtures are prepared as different mix-proportions including chemical admixture. Based on the experimental results, two electrical parameters, such as initial electrical resistivity and rising time, are proposed to reflect a microstructure development by hydration of cement-based materials. As a result, proposed parameter is also discussed with the measured setting time by penetration resistance method.
Concrete has excellent mechanical properties, high durability, and economical advantages over other construction materials. Nevertheless, it is not an easy task to apply concrete to long span bridges. That's because concrete has a low strength to weight ratio. Ultra high performance concrete (UHPC) has a very high strength and hence it allows use of relatively small section for the same design load. Thus UHPC is a promising material to be utilized in the construction of long span bridges. However, there is a possibility of crack generation during the curing process due to the high binder ratio of UHPC and a consequent large amount of hydration heat. In this study, adiabatic temperature rise and mechanical properties were modeled for the stress analysis due to hydration heat. Adiabatic temperature rise curve of UHPC was modeled superposing 2-parameter model and S-shaped function, and the Arrhenius constant was determined using the concept of equivalent time. The results are verified by the mock-up test measuring the temperature development due to the hydration of UHPC. In addition, models for mechanical properties such as elastic modulus, tensile strength and compressive strength were developed based on the test results from conventional load test and ultrasonic pulse velocity measurement.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.