수중불분리성 콘크리트 중의 철근부식 평가 (Estimation on Corrosion of Reinforcing bar in Antiwashout Underwater Concrete)

  • 문한영;김성수;김홍삼;김종필
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회논문집(I)
    • /
    • pp.447-450
    • /
    • 2000
  • Recently, antiwashout underwater concrete has used for underwater structure such as high strength massive concrete structures. When, concrete is placed in seawater the quality and durability of concrete could be doubt to especcially because the amount of cement placed in the concrete can be diminished by flowing seawater. In this study, antiwashout underwater concrete mixed with mineral admixtures for improvement of properties was placed in air, water, and salt water. Half-cell potential and current density was of specimens which made under different conditions measured for estimating corrosion degree. The experimental results demostrate that corrosion resistantce in saltwater was little and mineral admixtures improved properties of concrete.

  • PDF

배합시간과 배합량이 수중불분리성 콘크리트의 특성에 미치는 영향 (An Effect on the Properties of Antiwashout Underwater Concrete by mixing time and mixing quantity)

  • 박세인;김동명;김종수;김명식
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 가을 학술발표회논문집(I)
    • /
    • pp.345-350
    • /
    • 2000
  • The objective of this study makes investigation into the effect on the properties of underwater antiwashout concrete. which is followed by mixing time and mixing quantity. There is an tendency that (the compressive strength of underwater antiwashout concrete made and cured in fresh water or sea water) is increase when dry mixing time, mixing quantity, total mixing time is increase as unit weight grows. The difference of compressive strength (in case of no dry mixing time and 60 second) is averagely 46.8kgf/㎠ in the fresh water and 35.6kgf/㎠ in sea water. it's considered that dry mixing is dispersed by underwater antiwashout admixture.

  • PDF

잔골재의 혼합비율 변화에 따른 수중불분리성 콘크리트의 특성에 관한 연구 (Study on the Properties of Antiwashout Underwater Concrete with Variation of Mixing Proportion of Fine Aggregate Types)

  • 배원만;박세윤;백동일;김명식
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 가을 학술발표회 논문집
    • /
    • pp.533-536
    • /
    • 2003
  • The objective of in this study makes investigation into the characteristics of antiwashout underwater concrete as to mix proportion, casting and curing water through experimental researches. in this study, sea sand is blended with river sand, crushed sand is blended with river sand and sea sand as to investigate the quality change and characteristics of antiwashout underwater concrete with variation of blend ratio of sea sand and crushed sand(0, 20, 40, 60, 80, 100%). Higher compressive strength is measured following the order of river sand, sea sand, crushed sand regardless of age and casting condition. Except for case of using river sand, blended ratio of 40% is appeared on most compressive strength.

  • PDF

양생온도에 따른 수중불분리성 콘크리트의 물리.역학적 특성 (Mechanical and Physical of Antiwashout Underwater Concrete under Different Curing Temperature)

  • 이병덕;원종필;안태송
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1997년도 봄 학술발표회 논문집
    • /
    • pp.301-307
    • /
    • 1997
  • This paper is evaluated for properties of aggregate and antiwashout admixture not only to minimize segregation and water contamination of underwater concrete but also to meet concrete quality required. Two antiwashout admixtures used in this study were available domestically and slump flow, pH, setting time, and filing property of fresh concrete and the compressive strength, flexural strength under water and in the air under 2 different curing conditions ($10^{\cire}C$ and $20^{\cire}C$ ) were measured. Compressive strength ratio of specimens cured in and water temperature $10^{\cire}C$ /$20^{\cire}C$ added HPEC and HPMC was 64% and 89%, respectively. Relative compressive strength of 2 kinds observed higher concrete added HPEC, 3% at $10^{\cire}C$ curing temperature, 34% at $20^{\cire}C$ . The flexural strength of specimens made under water was 1/4~1/6 of compressive strength similar to the existing data in the literature.

  • PDF

하수관거 보수용 알루미나계 결합재 초속경 모르타르의 내구 특성 (Durability Properties of Ultra Rapid Hardening Mortar Produced with Alumina-based Binder for Repairing Sewage Treatment Pipes)

  • 김은호;이병재;이선목;김윤용
    • 한국건설순환자원학회논문집
    • /
    • 제10권4호
    • /
    • pp.482-488
    • /
    • 2022
  • 이 연구에서는 하수관거에 대한 수중불분리성 보수재료 개발을 위해 결합재 조성에 따른 내구성능을 평가하였다. 배합조건에 따른 모르타르의 내부 구조 분석 결과, CAC 배합의 경우 내식성 문제가 야기될 수 있는 Ca(OH)2를 형성하지 않고 알루미나겔(Al2(OH)3)를 형성 함으로서 내식성이 우수한 것으로 확인되었다. 압축강도 시험결과, OPC가 가장 낮은 강도를 나타내었으며, CAC100 > CAC100P > C12A7 > CSA > CAC80순으로 나타나 기존연구결과와 유사한 경향을 나타내었다. 염소이온침투저항성 및 동결융해시험 결과 동일한 내구성능을 나타내었으며 알루미나시멘트(CAC 및 C12A7의) 계열은 OPC보다 우수한 경향을 나타내었지만 CSA는 내부 팽창균열로 인해 내구성능이 낮은 것으로 판단된다. 화학저항성 시험결과, CAC100P 배합이 가장 우수한 화학저항성을 나타내었다. 이는 보수재 내부에 형성된 알루미나겔과 폴리머 분자가 결합하여 매트릭스가 치밀해졌기 때문으로 판단된다.

수중불분리성 콘크리트의 장기강도 특성에 관한 연구 (Study on the Long age Strength Properties of Antiwashout Underwater Concrete)

  • 박세인;이동화;김종수;김명수
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 봄 학술발표회 논문집
    • /
    • pp.113-117
    • /
    • 2000
  • The objective of this study is to find the long-age strength property and the compressive strength of age which is used as the specified concrete strength. The W/W ratio (45%, 50%, 55%, 60%) fine aggregate of useful river sand or blended sand(river sane : sea sand=1:1) were chosen as the experimental parameters. the experimental results show that pH(it means the material segregation resistance) & suspension were increased larger, so W/C become larger, and slump flow was increased as W/C increased (except W/C=60%), air-contents were decreased as W/C became increase and all of this results are satisfied with the under of 40%. The compressive strength ( a case use only river sand as fine aggregate) is showed less than the case of blended asnd. Because the unit weight of the blended sand is more heavy than the unit weigh of the river sand. The results of the case which haven been used only river sand, and the case have been used blended sand), both case have considered W/C. So it's possible to use the compressive strength of age 28 day like the case of plain concrete.

  • PDF

수중불분리성 콘크리트의 해양공사 적용에 관한 기초적 연구 (A Fundamental Study on the Antiwashout Underwater Concrete for the Underwater Work of Ocean)

  • 김명식;윤재범;박세인
    • 콘크리트학회논문집
    • /
    • 제12권5호
    • /
    • pp.25-34
    • /
    • 2000
  • When concrete is placed underwater, it is diluted with separating cementitious material and as a result the quality of concrete becomes poor. To solve this problem, antiwashout underwater concrete is increasingly used for the construction and repair of the concrete structure underwater. The objective of this study is to investigate the characteristics of antiwashout underwater concrete as to the mix proportion, casting and curing water through experimental researches. The unit weight of water and cement, water-cement ratio, fine aggregate ratio, unit weight of antiwashout underwater agent and superplasticizer, and casting and curing water were chosen to measure the suspended solids, pH, air contents, slump flow, unit weight of hardened concrete, and compressive strength. From this study, the incremental modulus at mix proportion design and unit weight of antiwashout underwater agent were increased more than fresh water, and it is a optimum mix proportion that the unit weight of water(and cement) is 230kg/$\textrm{m}^3$(460kg/$\textrm{m}^3$), waterOcement ratio is 50%, fine aggregate ratio is 40%, unit weight of antiwashout underwater agent is 1.2% of water contents per unit weight of concrete, and unit weight of supeplasticizer is 2.5% of cement contents per unit weight of concrete when the antiwashout underwater concrete is used for the underwater work of ocean.

수중 불분리성 콘크리트의 부착 강도 특성에 관한 연구 (Bond Strength Properties of Antiwashout Underwater Concrete)

  • 김명식;김기동;윤재범
    • 콘크리트학회논문집
    • /
    • 제12권1호
    • /
    • pp.89-99
    • /
    • 2000
  • The objective of this study is to investigate the bond strength properties of antiwashout underwater concrete. The arrangement of bars (vertical bar, horizontal upper bar, horizontal lower bar), condition of casting and curing (fresh water, sea water), type of fine aggregate (river sand, blended sand(river sand : sea sand = 1:1), and proportioning strength of concrete (210, 240, 270, 300, 330kgf/$\textrm{cm}^2$)are chosen as the experimental parameters. The test results(ultimate bond stress) are compared with bond and development provisions of the ACI Building Code(ACI 318-89) and proposed equations from previous research(which was proposed by Orangun et. al). The experimental results show that ultimate bond stress of antiwashout underwater concrete which arranged bar on the horizontal lower, used the blend sand, and was cast and cured in the fresh water are higher that other conditions. The ultimate bond stress were increased in proportion to {{{{( SQRT {fcu }) }}3 2. From this study, rational analytic formula for the ultimate bond stress are to be from compressive strength of concrete.

고강도 수중불분리성콘크리트의 기초물성에 대한 연구 (Fundamental Properties High-Strength Antiwashout Underwater Concrete)

  • 문한영;김성수;송용규;전중규
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2000년도 봄 학술발표회 논문집
    • /
    • pp.195-198
    • /
    • 2000
  • Recently, the anriwashout underwater concrete has been increasingly used for underwater structures such as vary high diaphrame walls of high strength massive concrete structures. In this study, experiments were made on the fundamental properties of antiwashout underwater concrete replaced with Fly Ash from 10% to 30% to improve its properties. Resultant to the test, we got the results as follows; the value of slump flow wasi ncreased, the setting, time was very delayed, and the heat evolution amount decreased, whereas the amount of suspended solids became high, and pH value became low as to increasing the replacement ratio of Fly Ash. Also the ratios of compressive strength (in water compared to in air) at 28day were obtained over 90%, and these values were satisfied with 70% of a criterion.

  • PDF

지반함몰 저감을 위한 속경형 하수관거 뒤채움재료 개발 (Development of Rapid Hardening Backfill Material for Reducing Ground Subsidence)

  • 유용선;한진규;채우리;구자술;이대영
    • 한국지반신소재학회논문집
    • /
    • 제14권3호
    • /
    • pp.13-20
    • /
    • 2015
  • 하수관거 시공시 부적절한 뒤채움재 및 다짐불량으로 인해 하수관로 파손 및 지반침하 현상이 발생한다. 최근들어 이러한 문제점을 해결하기 위해 유동성 채움재에 대한 관심이 증가하고 있다. 본 연구에서는 속경성, 가소성, 유동성, 수중불분리성을 갖춘 뒤채움재의 최적배합 도출과 뒤채움재의 경제성 향상을 위한 기초 연구를 수행하였다. 속경성 결합재의 최적배합 도출 실험 결과를 통해 뒤채움재의 최적 배합의 특성을 평가하였다. 시험결과, 속경성 결합재 페이스트의 W/M을 100%까지 증가시켜도 가소제 첨가량을 적절히 조절하여 사용하면 요구 성능을 만족시킴과 동시에 경제성 또한 확보 할 수 있을 것으로 사료된다.