  • In this study, in order to develop the composition ceramics for low loss and low temperature sintering multilayer piezoelectric actuator, PMN-PZN-PZT ceramics were fabricated using two stage calcination method and $Li_2CO_3$, $Bi_2O_3$ and CuO as sintering aids and their piezoelectric characteristics were investigated according to the 2nd calcination and sintering temperature. At the calcination temperature of $750^{\circ}C$ and sintering temperature of $930^{\circ}C$, density, electromechanical coupling factor ($k_p$), mechanical quality factor ($Q_m$), Dielectric constant (${\varepsilon}_r$) and piezoelectric constant ($d_{33}$) of specimen showed the optimum value of $7.94g/cm^2$ 0.581, 1554, 1555 and 356pC/N, respectively for multilayer piezoelectric actuator application.

  • PDF

하소온도의 변화에 따른 $Ba(Mg_{1/3}Ta_{2/3})O_3$계 세라믹스의 소결 거동과 마이크로파 유전특성 (Effect of Calcining Temperature on the Sintering Behaviors and Microwave Dielectric Properties of $Ba(Mg_{1/3}Ta_{2/3})O_3$ Ceramics)

  • 이정아;김정주;이희영;김태홍;최태구
    • 한국세라믹학회지
    • /
    • 제31권12호
    • /
    • pp.1561-1569
    • /
    • 1994
  • Effect of calcining temperature on the sintering behaviors and microwave dielectric properties of BMT[Ba(Mg1/3Ta2/3)O3] ceramics was studied. The calcining temperatures were varied from 80$0^{\circ}C$ to 130$0^{\circ}C$, respectively. It was found that, as calcining temperature lowered below 125$0^{\circ}C$, second phase such as Ba5Ta4O15 phases started to appear in calcined powder with unreacted powders. After sintering, exaggerately grown Ba5TaO3 phase could be found amang the uniform BMT grains in sintered body. Basis on the infiltration experiment, Ba0.05TaO3 phase should be formed by reaction of BMT grain and BaO-MgO eutectic liquid. But increase of calcining temperature above 125$0^{\circ}C$, there was not any second phase or unreated component in calcined powder and sintered body. As result, low calcining temperature led to precipitation of second phase in specimen and resulted decrease of Q value of BMT ceramics.

  • PDF

(Pr, Co, Cr, La)-doped ZnO 바리스터의 전기적 특성에 미치는 소결온도효과 (Effects Sintering Temperature on Electrical Properties of (Pr, Co, Cr, La)-doped ZnO Varistors)

  • 남춘우
    • 한국전기전자재료학회논문지
    • /
    • 제19권12호
    • /
    • pp.1085-1091
    • /
    • 2006
  • The microstructure, electrical properties, and its stability of (Pr, Co, Cr, La)-doped ZnO varistors were investigated at different sintering temperatures in the range of $1230{\sim}1300^{\circ}C$. As the sintering temperature increased, the sintered density increased from 5.50 to $5.77g/cm^3$, the varistor voltage decreased from 777.9 to 108.0 V/mm, the nonlinear coefficient decreased from 77.0 to 7.1, and the leakage current increased from $0.4{\mu}A\;to\;50.6{\mu}A$. On the other hand, the donor concentration increased from $0.90{\times}10^{18}\;to\;2.59{\times}10^{18}/cm^3$ and the barrier height decreased from 1.89 to 0.69 eV with increasing temperature. The stability of nonlinear electrical properties was obtained from sintering temperature of $1260^{\circ}C$. The varistors sintered at $1260^{\circ}C$ marked the high electrical stability, with $%{\Delta}V_{1mA}=+1.9%,\;%{\Delta}a=10.6%,\;and\;%{\Delta}I_L=+20%$ for DC accelerated aging stress state of $0.95V_{1mA}/150^{\circ}C/24h$.

소결온도에 따른 ZnO 바리스터의 내환경 특성 (Environmental Properties of ZnO Varistors with Variation of Sintering Temperature)

  • 이성갑;조현무;이종덕;박상만
    • 한국전기전자재료학회논문지
    • /
    • 제18권12호
    • /
    • pp.1111-1116
    • /
    • 2005
  • ZnO varistor ceramics added a glass-frit 0.03 $wt\%$ were fabricated with variation of sintering temperature. The sintering temperature and time were $1125^{\circ}C\~1200^{\circ}C$ and 2 h. The average grain sizes increased and the varistor voltage decreased with increasing the sintering temperature. The values of the specimen sintered at $1200^{\circ}C$ were $23.7\;{\mu}m$ and 329 V, respectively. The leakage current of all specimens was less than $1\;{\mu}A$ at DC $82\%$ of varistor voltage. The clamping voltage ratio of the specimen sintered at $1175^{\circ}C$ was 1.37. The endurance of surge current and the deviation of varistor voltage of the specimen sintered at $1175^{\circ}C$ were 6400 $A/cm^2$ and ${\Delta}-2.81\%$, respectively. After the High Temperature Load Test(HTLT) at $85^{\circ}C$ for 1000 h, the specimen sintered at $1175^{\circ}C$ showed the lowest deviation of varistor voltage of ${\Delta}-1.92\%$.

소결온도에 따른 BMCT 세라믹스의 구조적 특성 (Structural Properties of BMCT Ceramics with Sintering Temperature)

  • 이문기;임성수;김강;정장호;박인길;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2001년도 하계학술대회 논문집 C
    • /
    • pp.1421-1423
    • /
    • 2001
  • $Ba(Mg_{1-x}Co_x)TaO_3$[BMCT] ceramics were prepared by the conventional mixed oxide method. The ceramics were sintered at the temperature of 1525 $\sim$ 1625$^{\circ}C$ for 5hr. in air. The crystal structure of BMCT ceramics was investigated by the XRD. The microstructure of the specimens were observed by SEM. The structural properties of BMCT specimens were investigated as a function of composition and sintering temperature. All BMCT ceramics sintered over 1575$^{\circ}C$ were showed a polycrystalline complex perovskite structure without second phases and any unreacted materials. The density of BMCT (90/10) specimen sintered at 1575$^{\circ}C$ was 7.75g/$cm^2$. As the Co contents decreased, the ordering parameter of B-site in BMCT increased. The ordering parameter of BMCT(90/10) specimen sintered at 1575$^{\circ}C$ was 0.98.

  • PDF

소결온도에 따른 (Ba,Sr)(Nb,Ti)$O_3$ 세라믹스의 구조적 특성 (The structural properties of (Ba,Sr)(Nb,Ti)$O_3$ ceramics with sintering temperature)

  • 박보근;김지헌;이문기;류기원;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2001년도 하계학술대회 논문집 C
    • /
    • pp.1411-1413
    • /
    • 2001
  • The $(Ba_{0.5}Sr_{0.5})(Nb_{0.5}Ti_{0.5})O_3$ [BSNT] ceramics were prepared by conventional mixed oxide method. The structural properties of the BSNT ceramics with sintering temperature were investigated by XRD, SEM, EDS. Increasing the sintering temperature, diffraction intensity of the BST(110) peak was increased. The average grain size of BSNT ceramics were increased with sintering temperature. In the case of BSNT ceramics sintered at 1550$^{\circ}C$, the grain was uniform and the pore was not existed. Increasing the sintering temperature from 1400$^{\circ}C$ to 1500$^{\circ}C$, the amount of Nb and Sr were decreased. The density of BSNT ceramics sintered at 1550$^{\circ}C$ was $1.125g/cm^2$.

  • PDF

소결온도에 따른 0.96$MgTiO_3$-0.04$BaTiO_3$ 세라믹스의 마이크로파 유전특성 (Microwave Dielectric Properties of the 0.96$MgTiO_3$-0.04$BaTiO_3$ Ceramics with Sintering Temperature)

  • 최의선;이상철;이성갑;배선기;이영희
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2001년도 하계학술대회 논문집 C
    • /
    • pp.1408-1410
    • /
    • 2001
  • The 0.96$MgTiO_3$-0.04$BaTiO_3$ ceramics were prepared by the conventional mixed oxide method. The structural properties were investigated with sintering temperature and composition ratio by XRD, SEM and EDS. According to the X-ray diffraction patterns of the 0.96$MgTiO_3$-0.04$BaTiO_3$ ceramics, the hexagonal $BaMg_6Ti_6O_{19}$ and ilmenite $MgTiO_3$ structures were coexisted. In the case of the 0.96$MgTiO_3$-0.04$BaTiO_3$ ceramics sintered at 1325$^{\circ}C$, dielectric constant, quality factor and temperature coefficient of resonant frequency were 23.95, 70,200, -55.8ppm/$^{\circ}C$, respectively.

  • PDF

Si(100) 기판 위에 코팅된 $TiO_2$박막의 결정구조와 초친수 특성 (Crystal Structure and Superhydrophilic Property of $TiO_2$ Thin Film Coated on Si(100) Wafer)

  • 김사라;조운조;박재관;이용철
    • 한국결정학회지
    • /
    • 제12권3호
    • /
    • pp.177-181
    • /
    • 2001
  • TiO₂박막의 초친수성 특성을 열처리에 따른 박막의 결정구조 변화와 연관지어 연구하였다. 박막은 Sol-Gel법을 이용하여 실리콘 (100)웨이퍼 위에 제조하였다. 1차 소결후, 500℃에서 후열처리한 시편은 anatase 상을, 1000℃에서 열처리한 시편은 rutile 상을 가지며 그 중판 온도인 750℃에서 열처리한 경우는 anatase와 rutile상이 혼재 되어 있다. 이 후열 처리한 시편들은 UV를조사하지 않아도 친수성을 보였고, 특히 750℃에서 열처리한 시편은 5°이하의 초친수성을나타내었다. 친수성을 가지는 시편들은 암실처리 중 서서히 퇴화되어 소수성을 띄게되지만, UV를 조사하면 1시간 이내에 급격히 초진수성을 회복하는 우수한 특성을 보였다.

  • PDF

소결온도에 의한 중적외선 투과용 ZnS 세라믹스의 광학적 특성 (Optical Properties of Middle Infrared Transparent ZnS Ceramics at Various Sintering Temperatures)

  • 여서영;권태형;김창일;백종후
    • 센서학회지
    • /
    • 제27권4호
    • /
    • pp.249-253
    • /
    • 2018
  • Infrared transparent ZnS ceramics were synthesized through hydrothermal synthesis ($180^{\circ}C$, 70 h) and sintered using a hot press process at $750^{\circ}C-1000^{\circ}C$. We carried out x-ray diffraction, scanning electron microscopy, and Fourier transform-infrared spectroscopy to confirm the optical properties of the ZnS ceramics after sintering at various temperatures. The phase of ZnS nanopowders was a single phase (cubic) without the hexagonal phase. However, as sintering temperature increased, the formation and increment of hexagonal structures was confirmed. The ZnS ceramic sintered at a temperature of $750^{\circ}C$ showed poor transmittance because it was not completely sintered and because of the pore effect. The ZnS ceramic with the highest transmittance (approximately 69%) was sintered at $800^{\circ}C$. As sintering temperature increased, transmittance gradually decreased owing to the increase in the formation of the hexagonal phase.

세라믹소지에 생성되는 석회에 의한 백화현상분석 (Analysis of Ca-rich efflorescence in ceramic bodies)

  • 이기강
    • 한국결정성장학회지
    • /
    • 제16권3호
    • /
    • pp.127-131
    • /
    • 2006
  • 세라믹소지에 발생하는 온도별 백화생성기구를 백화를 형성하는 양이온과 음이온을 분석하여 규명하였다. 백화가 발생된 세라믹 소지의 표면을 SEM과 EDS 분석을 하여 백화의 주 성분은 Ca와 S임을 확인하였다. 세라믹소지를 pH 7과 pH 10에서 각기 습식혼합 하였으며, 이때 여과된 액을 ICP와 IC 분석을 하여, 양이온 및 음이온 농도분석을 하였다. pH 7에서 제조된 세라믹 소지의 Ca 이온농도는 pH 10에서 제조된 세라믹소지의 Ca 이온농도의 8배 값을 보였으며, pH 10에서 제조된 세라믹소지는 $1100^{\circ}C$ 이상으로 소결된 소지에서도 백화가 발견되지 않았다.