• Title/Summary/Keyword: 산화내구성

Search Result 176, Processing Time 0.027 seconds

A Study of Combustion Reaction of Methane by Pd Catalyst - Effects of Support Size & Calcination Temperature - (팔라듐 촉매의 메탄의 연소반응에 관한 연구 -담체의 크기와 소성온도에 따른 효과-)

  • Lee Taeck Hong
    • Journal of the Korean Institute of Gas
    • /
    • v.8 no.3 s.24
    • /
    • pp.52-56
    • /
    • 2004
  • Pd catalyst have been used in hydrogenation, oxidation, and low temperature combustion reaction. Recently, it is candidated as a possible reagents in the partial oxidation of methanol reformers of the fuel cell. Pd catalysts, even though it is very precious and expensive, catalytic functioning is good, but it still need to be improved in the matter of durability and low catalytic activity after calcination. In this study, we synthesize the improved Pd catalyst and study their chemical functioning.

  • PDF

A Study on the Electrode Properties of $CaNi_5$ Hydrogen Storage Alloy by F-Treatment (불화처리에 의한 $CaNi_5$ 수소저장합금의 전극 특성에 관한 연구)

  • 오세진;강성군
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 1998.11a
    • /
    • pp.92-92
    • /
    • 1998
  • 반도체 기술의 경이적인 발전에 힘입이 최근 휴대용 이동통신기기, 노트북 컴퓨터 등 무선전자제품의 폭발적인 수요와 함께 이들의 소형화, 경량화가 요구되어 전원인 2차전지의 경량화, 고용량화, 장수명화의 필요성이 절실해졌다. Ni-MH 전지는 Ni-Cd전지에 비해 에너지밀도가 1.5~2배에 이르고 충방전 cycle이 길며 오염물질이 없어 환경 친화적이라는 장점이 었다. Ni-MH 전지의 성능은 음극재료인 수소저장합금에 의해 좌우되므로 수소저장능력이 크고 내식 성이 우수한 합금개발이 중요하다. $CaNi_5$는 수소저장능력이 크고 매장량이 많아 값이 싸다는 장점이 있지만 KOH 용액에서 내구성이 떨어진다는 단점이 있어 주로 Heat Pump 재료에만 사용이 제한되어왔다. 본 실험에서는 결정 구조의 nanocrystalline 및 amorphous화함으로써 해리압의 변화, 방전용량의 변화 등 새로운 전극 특성을 나타낸다고 보고되고 있는 MG (Mechanical Grinding)방법을 통해 CaNis 합금의 전극특성의 변화를 살펴보았고, 아울러 고상-기상반응에서 표면에 형성된 산화피막을 제거하여 안정한 불화물을 표면에 형성시킴으로써 불순물 가스에 대한 내구성을 높이고 활성화특성을 향상 시킨다고 보고되고있는 불화처리 방법을 이용하여 불화처리 시간을 달리하면서 용액 속에서의 pH의 변화, ICP분석, 전극의 성능 및 표면 특성변화를 충방전 test, SEM 등을 통해 고찰하였다.

  • PDF

Acid Based Gel Compound의 녹제거 효과

  • 강영구;김정훈
    • Proceedings of the Korean Institute of Industrial Safety Conference
    • /
    • 2003.10a
    • /
    • pp.184-187
    • /
    • 2003
  • 다양한 부식 형태 준 금속부식은 대기중, 수중, 지중, 화학약품 등의 부식환경에 의해 영향을 받는다. 특히 금속 표면의 산화 반응에 의해 생성되는 녹(Rust)은 iron, steel, bronze, aluminium 등의 대상소재를 사용하는 일반 가전제품, 산업공정설비 및 각종 구조물 등에 작용하여 원재료 손상, 내구수명 저하, 구조물 붕괴, 화재 및 폭발위험성 등 대부분 안전사고로 직결되는 것이 일반적이다.(중략)

  • PDF

Compaction of Soft Magnetic Composites via Silica Sol-Gel Process (실리카 졸-겔 공정에 의한 연자성 복합체 분말 성형)

  • Kim, Ho-Hyeong;Gwak, Jeong-Geun;Lee, Heung-Ryeol
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2015.11a
    • /
    • pp.263-263
    • /
    • 2015
  • 절연층이 코팅된 연자성복합체(Soft magnetic composites) 분말 성형 시 발생하는 밀도와 강도 저하의 문제를 개선하기 위해 금속산화물 전구체로 표면 개질된 자성분말을 성형 후 경화시키는 방법으로 분말 자심을 제조하였다. 이를 통해 공정이 단순화 되면서 자심의 물리적 내구성을 향상시킬 수 있음을 확인하였다.

  • PDF

Characteristics of Electrochemical and Cavitation Damage after Sealing Treatment for Arc Thermal Sprayed Coating Layer (후처리된 아크 용사코팅 층의 전기화학적 및 캐비테이션 손상 특성)

  • Kim, Seong-Jong;Han, Min-Su;Park, Il-Cho
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2014.11a
    • /
    • pp.300-300
    • /
    • 2014
  • 해양환경 하에서 대형 강구조물의 경우 장기간 부식손상을 방지하기 위해 아크 용사코팅 기술이 오래전부터 유용하게 이용되어 왔다. 아크 용사코팅 기술은 타 용사코팅 기술에 비해 경제성과 생산성이 뛰어나 대형 강구조물에 적용되고 있다. 용사재료로는 Al, Zn 또는 그 합금들이 주로 사용되어 강재에 대해 희생양극 방식효과를 나타낸다. 그러나 아크용사에 의해 적층된 코팅 층은 용사공정 중 불가피하게 수많은 기공과 산화물이 포함되어 내식성 및 내구성에 악영향을 미치게 된다. 따라서 본 연구에서는 알루미늄 합금의 용사코팅 층에 대하여 다양한 후처리를 통해 내식성과 더불어 내구성을 향상시키고자 하였다. 용사코팅은 알루미늄 합금 선재(1.6 ${\varnothing}$)를 사용하여 아크용사를 실시하였다. 용사 시 용사거리는 200 mm, 공기압력은 약 $7kg/cm^2$ 정도로 유지하면서 용사코팅을 실시하여 약 $200{\mu}m$ 두께로 코팅 층을 형성시켰다. 이후 용사코팅 층의 표면에 다양한 후처리재를 적용하였으며, 내구성을 평가하기 위하여 후처리 적용 전후 시험편에 대하여 캐비테이션 실험을 실시하였다. 캐비테이션 실험은 ASTM G32-92에 의거하여 주파수 20 kHz의 초음파 진동 장치(ultrasonic vibratory device)를 사용하였다. 그리고 시험편 표면과 발진 혼에 부착된 팁(tip)과의 거리는 1 mm로 일정하게 유지시킨 뒤, 캐비테이션 발생 시간을 변수로 하여 실험을 실시하였다. 손상된 용사코팅 층의 표면은 주사전자현미경과 광학현미경으로 관찰하였으며, 시험편 손상깊이는 3D 현미경으로 비교 분석하였다. 또한 캐비테이션 실험 전후의 무게를 측정하여 무게 감소량을 상호 비교하였다. 그리고 전기화학적 실험은 천연해수 속에서 자체 제작한 홀더(holder)를 이용하여 $0.33183cm^2$의 용사코팅 층만을 노출시켜 실시하였다. 그리고 기준전극은 은/염화은 전극을, 대극은 백금전극을 사용하였다. 분극실험을 통해 후처리 적용에 따른 용사코팅 층의 부식전위 및 부식전류밀도를 비교 평가하였다. 그 결과, 용사코팅 층에 의하여 강재에 대한 희생양극 방식전위가 확보되었으며, 후처리재가 적용된 용사코팅 층에서 내식성 및 캐비테이션 저항성이 향상되었다.

  • PDF

A Study on the Activity of Metal Filter Pt Coated on Soot Oxidation (백금 코팅 메탈필터소재의 Soot 산화반응에 대한 활성 연구)

  • Kim, Sung Su;Lee, Sang Moon;Jang, Du Hun;Bae, Se Hyun;Hong, Sung Chang
    • Applied Chemistry for Engineering
    • /
    • v.22 no.4
    • /
    • pp.400-404
    • /
    • 2011
  • The activity and stability of the metal filter material Pt coated on NOx and soot oxidation were examined. The catalytic reaction test for NOx and soot were also performed independently and simultaneously. As a result, it showed the NO to $NO_2$ shift reaction with 20% conversion, NOx decomposition (about 10%) and perfect soot oxidation on the material Pt coated proceeded. Onset temperature of soot oxidation shift to lower temperature (about $30^{\circ}C$) by generated $NO_2$. The material also was less affected by thermal shock than $Pt/Al_2O_3$ or $Pt/TiO_3$ catalysts due to its stability of surface structure.

Preparation and Characterizations of poly(arylene ether sulfone)/SiO2 Composite Membranes for Polymer Electrolyte Fuel Cell (고분자 전해질 연료전지(PEFC)용 poly(arylene ether sulfone)/SiO2 복합막의 제조 및 특성분석)

  • Shin, Mun-Sik;Kim, Da-Eun;Park, Jin-Soo
    • Membrane Journal
    • /
    • v.27 no.2
    • /
    • pp.182-188
    • /
    • 2017
  • Sulfonated poly(arylene ether sulfone) (SPAES)-3-mercaptopropyl silica gel (3MPTSG) composite membranes with improved oxidative stability were prepared for polymer electrolyte fuel cell application. It has been reported that ether part of main chain of aromatic hydrocarbon based membranes were weak to radical attack to decrease membrane durability. In this study, the hydrophilic inorganic particles were introduced by minimizing a decrease in ion conductivity and increasing an oxidative stability. The composite membranes were investigated in terms of ionic conductivity, ion exchange capacity (IEC), FT-IR, TGA and contact angle, etc. As a result, increasing amount of the 3MPTSG resulted in decrease in proton conductivities and water uptakes at 100% R.H. but enhanced thermal and oxidative stabilities.

Characteristics of green colored opal glass with contents of iron oxide for LED light diffuser (LED diffuser용 green color 유백유리에 있어서 산화철 함량에 따른 특성)

  • Ku, Hyun-Woo;Lim, Tae-Young;Yoo, Seol;Hwang, Jonghee;Kim, Jin-Ho;Lee, Mi-Jai;Shin, Dong Wook
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.24 no.3
    • /
    • pp.120-126
    • /
    • 2014
  • Translucent green colored opal glass was fabricated to substitute polycarbonate diffuser of LED lighting in order to solve the durability problem. Batch materials of green colored opal glass with the composition of calcium phosphate for opacifier and iron oxide for colorant were made and melted at $1550^{\circ}C$. As the results, translucent green colored opal glass was obtaind, which had excellent optical properties compare with nomal color glass for the diffuser of LED lighting, with no dazzling from direct light by high haze value over 90 % and low parallel transmittance value about 1 %. Therefore, it is concluded that this translucent green colored opal glass can be used for the glass diffuser materials of LED lighting with high heat resistance and high durability to substitute polycarbonate diffuser.

The influence of preparation conditions on the electrochemical degradation of tungsten oxide thin films prepared by electron beam deposition (제작조건이 전자비임으로 제작된 텅스텐산화물 박막의 전기화학적 퇴화에 미치는 영향)

  • 이길동
    • Journal of the Korean Vacuum Society
    • /
    • v.7 no.4
    • /
    • pp.306-313
    • /
    • 1998
  • The electrochromic $WO_3$thin films were prepared by using the electron-beam evaporatin technique. Flms prepared at a vacuum pressure of $10^{-4}$ mbar were found to be most stable during repeated potential cycles. The chemical stability of the film in aqueous solutions was also affected by the vacuum pressure during evaporation. The redox current and the optical properties of the degraded films were affected by the thickness of the film. The 5,000$\AA$-thick films were found to be most stable, undergoing the least degradation during the repeated coloring and bleaching cycles. The origin of the mechanism dominating the degradation during the repeated coloring and bleaching cycles was the accumulation of lithium in the film, which results in decreasing redox current. Tungsten oxide films with titanium content of about 10-15 mol% was found to be most stable, undergoing the least degradation during the repeated cycles. The origin of the mechanism dominating the least degradation during the repeated cycles was the reduction of lithium ion trapping sites in the films, which results in a increased durability.

  • PDF