• Title/Summary/Keyword: 분극성

Search Result 390, Processing Time 0.028 seconds

Effective material properties of radially poled piezoelectric ring transducer for analysis of tangentially poled piezoelectric ring (원주 분극 압전 링 트랜스듀서 해석을 위한 방사 분극 링 유효 물성 도출)

  • Lee, Haksue;Cho, Cheeyoung;Park, Seongcheol;Cho, Yo-Han;Lee, Jeong-min
    • The Journal of the Acoustical Society of Korea
    • /
    • v.38 no.2
    • /
    • pp.184-192
    • /
    • 2019
  • Compared to 31-mode rings, 33-mode rings are highly utilized as wide bandwidth underwater acoustic transducers because the electro-mechanical coupling and piezoelectric constant d are high. On the other hand, the 31-mode ring is an axial symmetry structure, so it is possible to model it as a simple two-dimensional asymmetrical model for numerical analysis, but the 33-mode ring requires a three-dimensional numerical analysis. That is, a lot of computing resources and computation time are required. In this study, the effective material properties of an equivalent 31-mode ring were derived to simulate the electro-mechano-acoustical responses of the 33-mode ring transducer. Using the effective material properties derived from this study, a numerical analysis of rings in vacuum, air backed rings in water, and FFR (Free Flooded Ring) transducers were performed to compare the responses of 33-mode rings.

Electrochemical Behavior of Tin and Silver during the Electrorecycling of Pb-free Solder (Sn-Ag-Cu) Waste (폐무연솔더(Sn-Ag-Cu)의 전해재활용 시 주석과 은의 전기화학적 거동 연구)

  • Kim, Min-seuk;Lee, Jae-chun;Kim, Rina;Chung, Kyeong-woo
    • Resources Recycling
    • /
    • v.31 no.3
    • /
    • pp.61-72
    • /
    • 2022
  • We investigated the electrochemical behavior of Sn (93.0 %)-Ag (4.06 %)-Cu (0.89 %) during electrolysis of Pb-free solder waste to recover tin and silver. A thin strip of the solder waste produced by high-temperature melting and casting was used as a working electrode to perform electrochemical analysis. During anodic polarization, the current peak of an active region decreased with an increase in the concentration of sulfuric acid used as an electrolyte. This resulted in the electro-dissolution of the working electrode in the electrolyte (1.0 molL-1 sulfuric acid) for a constant current study. The study revealed that the thickening of an anode slime layer at the working surface continuously increased the electrode potential of the working electrode. At 10 mAcm-2, the dissolution reaction continued for 25 h. By contrast, at 50 mAcm-2, a sharp increase in the electrode potential stopped the dissolution in 2.5 h. During dissolution, silver enrichment in the anode slime reached 94.3% in the 1 molL-1 sulfuric acid electrolyte containing a 0.3 molL-1 chlorine ion, which was 12.7% higher than that without chlorine addition. Moreover, the chlorine enhanced the stability of the dissolved tin ions in the electrolyte as well as the current efficiency of tin electro-deposition at the counter electrode.

Durability of MEA Using sPEEK Membrane Reinforced with Poly Imide in PEMFC (고분자전해질연료전지에서 폴리이미드 강화 sPEEK막 MEA의 내구성)

  • Lee, Hye-Ri;Na, Il-Chai;Oh, Sung-Jun;Park, Kwon-Pil
    • Korean Chemical Engineering Research
    • /
    • v.55 no.3
    • /
    • pp.296-301
    • /
    • 2017
  • Recently, there are many efforts focused on development of more economical non-fluorinated membranes for PEMFCs (Proton Exchange Membrane Fuel Cells). In this study, sulfonated poly (ether ether ketone) (sPEEK) membrane reinforced with poly imide was made to enhance of membrane durability. In order to test durability of single (un-reinforced) membrane and reinforced membrane MEA (Membrane and Electrode Assembly), degradation accelerated stress test was used. Before and after degradation, I-V polarization curve, hydrogen crossover current, electrochemical surface area, membrane resistance and charge transfer resistance were measured. As a result of experiments, hydrogen crossover current of reinforced MEA was lower than that of single MEA, therefor durability of reinforced MEA was higher than that of single MEA. There was not especially short phenomena in reinforced MEA after degradation accelerated stress test.

Characterization on corrosion damage of nickel alloy for nuclear energy instrument by chemical decontamination solution (원전기기용 니켈합금강의 화학제염용액에 따른 부식손상 특성 규명)

  • Park, Il-Cho;Yang, Ye-Jin;Jeong, Gwang-Hu;Lee, Jeong-Hyeong;Han, Min-Su;Kim, Seong-Jong
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2017.05a
    • /
    • pp.135-135
    • /
    • 2017
  • 제염기술은 원자력발전소의 순환계통장치 및 기기류의 방사성 오염물질을 제거하는 기술이다. 현재 국내 원전의 설계 수명 및 유지보수 시기가 도래함에 따라, 작업 전 작업자의 방사선 피사량을 극소화하기 위한 제염 기술이 주목을 받고 있다. 제염 방법에는 크게 기계적 제염과 화학약품을 사용하는 화학제염이 있다. 그 중 화학제염은 복잡한 구조의 제염 대상물에 대한 큰 효과 및 간단한 공정 때문에 주로 사용되고 있다. 제염 시 방사성 산화물과 오염성분을 제거하기 위해 강산 또는 강알칼리의 화학용액이 사용된다. 강한 화학약품을 사용함으로써 큰 제염효과를 얻을 수 있는 반면, 금속 재료의 부식에 대한 구동력도 커지게 된다. 금속 재료의 경우, 강한 부식성 환경에서 공식(pitting corrosion) 및 입계부식(intergranular corrosion)형태의 손상이 크게 발생하기 때문에, 제염공정 시 사용되는 화학용액에 대한 재료의 건전성 검증이 반드시 필요하다. 본 연구에서는 원전기기용 재료인 니켈합금강 Inconel600의 화학제염 시 시험공정 3가지에 대한 부식손상 특성을 규명하였다. 산화공정은 $HMnO_4$ 실험용액을 공통으로 사용하였으며, 산화공정 종료 후 환원공정은 각 시험공정에 따라 환원공정 1은 2000ppm $H_2C_2O_4$, 환원공정 2는 1500ppm $H_2C_2O_4$ + 500ppm $H_8C_6O_7$, 그리고 환원공정 3은 3000ppm $H_2C_2O_4$ 실험용액을 각각 투입하여 수행하였다. 산화, 환원공정을 1Cycle로 하여 온도 $75^{\circ}C$로 유지된 용액에 각 2시간씩 침적하였다. 각 시험공정 별로 총 5Cycle을 실시하였다. 각 시험공정 Cycle종료 후 시험편을 취외하여 무게감량측정, SEM(Scanning electron microscope)분석, 3D현미경분석 그리고 타펠분극 실험을 실시하였다. 각 분석결과를 토대로 하여, 니켈합금 Inconel600에 대한 화학제염 시 시험공정에 따른 부식특성을 규명하였다.

  • PDF

MO Studies on (4 + 2) Cycloadditions of Substituted-Arenediazocyanides and Nitrosobenzenes (치환체-Arendiazocyanide, Nitrosobenzene의 (4 + 2) 고리첨가 반응에 대한 분자궤도론적 연구)

  • Gu Cheun Chung;Seong Kyu Park;Il Doo Kim;Ikchoon Lee
    • Journal of the Korean Chemical Society
    • /
    • v.28 no.5
    • /
    • pp.284-292
    • /
    • 1984
  • This paper aims to predict the substituent and Lewis acid catalysis effect or reactivity on the regioselectivity of (4+2) cycloaddition reaction of the substituted-E-arene-diazocyanides and nitrosobenzenes. Frontier orbital theory (FMO) has been applied to thermal and catalyzed Diels-Alder reaction by means of CNDO/2 and EHT-SPD methods. It has been found that: (1) The above reaction is positive rho(${\rho}$) values in Hammett equation, so it takes normal electron demand reaction, and four-frontier orbitals and Anh methods are identical with experimental major regioisomer.(2) When electron withdrawing radicals are substituted HOMO and LUMO energies of dienophiles are reduced, and the reactivity is increased. (3) The major regioisomer is predicted as B type, as the Lewis acid makes complexes of dienophile, and polaries LUMO coefficients of dienophile in an opposite way. (4) The linear correlation of Hammett is indicated in the graph of stabilized energies(${\Delta}$E) and sigma(${\sigma}$).

  • PDF

티타늄 스크랩을 이용한 분말제조 및 소결 성형체 특성평가

  • Choe, Jeong-Cheol;Jang, Se-Hun;Cha, Yong-Hun;O, Ik-Hyeon
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2009.11a
    • /
    • pp.38.1-38.1
    • /
    • 2009
  • 산업이 발전함에 따라서 특수한 물성을 갖는 재료의 수요가 점점 증가하고 있는데최근 재료의 경량화, 화학적 안정화 등을 이용한 시스템의 효율성 향상, 환경오염방지 등과 같은 목적으로 사용재료의 고급화 추세가 현저해짐에 따라 티타늄 소재에 대한 관심과 수요가 증가하고 있다. 하지만, 국내에서는 티타늄 및 티타늄 합금의 원재료 및 가공제품을 대부분 수입에 의존하는 실정이다. 또한 티타늄 및 티타늄 합금의 스크랩의 경우 재활용률은 50~80%에 달하고 알려져 있으나 국내에는 이들의 재활용처리를 위한 시설이 없으며 폐기 또는 외국으로 저가로방출하고 있는 실정이다. 이에 따라 본 연구에서는 판재, 선재 및 관등의 기계 가공 시 주로 발생하는 티타늄 스크랩을 이용하여 HDH법을 이용하여 티타늄 분말을 제조하였다. 제조된 분말은 $900{\sim}1200^{\circ}C$의 온도범위에서 방전플라즈마소결공법을이용하여 소결체를 제작하였으며, 소결체의 강도, 경도 및미세조직 등을 평가하였다. 내식성향상을 위해 염화팔라듐을 이용하여 티타늄-팔라듐 분말 합금을 제조하여 티타늄 합금 분말의 소결체와 순수티타늄의 소결체와 내식성 비교를 위해 동전위분극시험을 통해 평가하였다.

  • PDF

The Study on the Wear Corrosion Behavior of Induction Hardening High Strength Cast Iron in the pH Environments (고주파 열처리한 강인주철재의 마멸부식거동에 관한 연구)

  • Park, Yun-Sik;Lim, Uh-Joh;Park, Dong-Gi
    • Journal of the Korean Institute of Gas
    • /
    • v.12 no.4
    • /
    • pp.52-57
    • /
    • 2008
  • This paper studies on the wear corrosion behavior of induction hardening high strength cast iron in the acidic environments. In a variety of pH solutions, wear corrosion behavior of GC 300 with a variety of contact pressures was investigated, and corrosion wear behavior after immersion test was considered. Also, electrochemical polarization test for GC 300 was carried out in various pH solutions. The main results are as following: In the strong acidic environment, wear corrosion rate of GC 300 appears highly and in the neutral environment is stable. Also, graphitic corrosion in the strong acidic environment occurs. The corrosion current density of GC 300 becomes high in a order of pH 1 > pH 2 > pH 4 > pH 6.5.

  • PDF

Intrinsic Flux Inequality in Forward Osmosis (FO) and Pressure-Retarded Osmosis (PRO) Processes (수학적 귀납법을 이용한 정삼투 및 압력지연삼투 공정의 투과율 불균형 해석)

  • Kim, Albert S.;Lee, Seung-won
    • Membrane Journal
    • /
    • v.25 no.4
    • /
    • pp.367-372
    • /
    • 2015
  • In pressure-retarded osmosis (PRO) and forward osmosis (FO) processes, solvent (permeate) flux depends on which surface the draw solution faces. There are two operation modes. PRO mode indicates that the active layer faces the draw solution, and FO mode means that the porous substrate fronts the draw stream. It is often observed that the PRO mode produces higher flux than that of FO under the same operating conditions. The current work uses the method of proof by contradiction, and mathematically proves the intrinsic flux inequality between the two modes.

The Study on the Corrosion Behavior of STS 304 for Gas Boiler in the Condensed Water (응축수 중에서 가스보일러용 STS 304의 부식거동에 관한 연구)

  • Du Yun Byoung;Lim Uh Joh;Jeong Ki Cheol
    • Journal of the Korean Institute of Gas
    • /
    • v.9 no.1 s.26
    • /
    • pp.21-25
    • /
    • 2005
  • This paper was studied on the corrosion behavior of STS 304 for gas boiler in the condensed water, the electrochemical polarization test of STS 304 for gas boiler in the condensed water was carried out. And the corrosion behavior of STS 304 was considered. The main results are as following: 1) As corrosion environment is acidified from neutrality, the polarization resistance of STS 304 decreases and the corrosion potential is less noble. 2) The corrosion reaction mechanism of STS 304 is cathodic control. 3) As corrosion environment is acidified, the passive potential range of STS 304 decreases. Also, the passive current density of STS 304 increases.

  • PDF

A Estimation of Ionic Space Charge Polarization in Polyimide by TSC (폴리이미드에서 TSC에 의한 이온성 공간전하분극의 평가)

  • Lee, Won-Jae;Lee, Sung-Il;Lee, Ho-Sik;Jang, Kyung-Uk;Choi, Myong-Kyu;Kim, Tae-Wan;Kang, Dou-Yol
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.10a
    • /
    • pp.15-20
    • /
    • 2000
  • In this paper. Thermally Stimulated Current spectra have been measured in the Polypy - romellitimide (polyimide). As a result of the investigation. three peaks have been observed: $A(50^{\circ}C)$, $B(120^{\circ}C)$, $C(200^{\circ}C)$. Among three peaks, C peak has been observed in detail. The C peak is shown to be created due to the polarization of ionic space charge from the experimental results which were measured as a function of forming time, forming temperature. forming voltage and collecting voltage. As a result, we have measured the TSC in ion ($Na^+$) implanted - Polyimide, also found the peak at $215^{\circ}C$. Therefore, TSC characteristics in the C peak is probably caused by residual impurity. And The activation energy caculated by means of initial rising method 1.8eV, hopping distance. $90{\AA}$. and the mobility. $2.88{\times}10^{-11}cm^2/v.s$

  • PDF