Limitation of Nitrogen ion Implantation and Ionplating Techniques Applied for Improvement of Wear Resistance of Metallic Implant Materials (금속 임플란트 소재의 내마모성 향상을 위하여 적용되는 질소 이온주입 및 이온도금법의 한계)

  • 김철생
    • Journal of Biomedical Engineering Research
    • /
    • v.25 no.2
    • /
    • pp.157-163
    • /
    • 2004
  • Nitrogen ion implantation and ion plating techniques were applied for improvement of the wear resistance of metallic implant materials. In this work, the wear dissolution behaviour of a nitrogen ion implanted super stainless steel (S.S.S, 22Cr-20Ni-6Mo-0.25N) was compared with those of S.S.S, 316L SS and TiN coated 316L SS. The amounts of Cr and Ni ions worn-out from the specimens were Investigated using an electrothermal atomic absorption spectrometry. Furthermore, the Ti(Grade 2) disks were coated with TiN, ZrN and TiCN by use of low temperature arc vapor deposition and the wear resistance of the coating layers was compared with that of titanium. The chemical compositions of the nitrogen ion implanted and nitride coated layers were examined with a scanting auger electron spectroscopy. It wat observed that the metal ions released from the nitrogen ion implanted S.S.S surface were significantly reduced. From the results obtained, it was shown that the nitrogen ion implanted zone obtained with 100 KeV ion energy was easily removed within 200,000 revolutions from a wear dissolution testing under a similar load condition when applied to artificial hip joint. The remarkable improvement in wear resistance weir confirmed by the nitrides coated Ti materials and the wear properties differ greatly according to the chemical composition of the coating layers. for specimens with the same coating thickness of about 3$\mu\textrm{m}$, TiCN coated Ti showed the highest wear resistance. However, after removing the coating layers, the wear rates of all nitrides coated Ti reverted to their normal rates of below 10,000 revolutions from Ti-disk-on-disk wear testing under the same load condition. From the results obtained, it is suggested that the insufficient depth of the 100 Kel N$\^$+/ ion implanted zone and of the nitrides coated layers of 3$\mu\textrm{m}$ are subject to restriction when used as frictional parts of load bearing implants.

Relationship between Violent Criminal Behavior and Imbalance of Scalp Hair Minerals in Man (두발중 미량 중금속과 필수금속의 과다 또는 과소의 불균형과 폭력범죄 행동과의 관련성 연구)

  • Kim, Doo-Hie;Jang, Bon-Ki;Lee, Duk-Hee;Hong, Sung-Chul;Kim, Byung-Hie
    • Journal of Preventive Medicine and Public Health
    • /
    • v.27 no.1 s.45
    • /
    • pp.25-43
    • /
    • 1994
  • To estimate the factors to the inclination of the criminal violence, the content of trace minerals and toxic metals in the scalp hair were measured during the period from May 1992 to October 1992. One hundred eleven violent and 89 nonviolent criminal inmates of Taegu Correctional Institute were selected. The inmates of violent criminals were imprisoned by murder, robber, rape, injury and violent acts. Those of nonviolent criminals were swindle, larceny, and adultery and had no history of institutional violence. The contents of two toxic metals (cadmium, lead) and five trace minerals (Cu, Fe, Zn, Mg, Na) were determined by an atomic absorption spectrophotometer (IL. 551). The contents of cadmium and lead in hair of violent criminals were significantly higher as $0.56{\pm}0.14ppm,\;11.53{\pm}3.32ppm$, respectively, than $0.42{\pm}0.20ppm,\;9.63{\pm}4.31ppm$ of nonviolent group (p<0.01). But the level of copper was significantly lower than nonviolent group (p<0.05). The factors that had a significant correlation with the inclination of violence in multiple logistic regression analysis were cadmium (odds ratio=98.09), unmarried (odds ratio=0.39), many times of criminal history(odds ratio=1.57) and residence of rural area (odds ratio=0.44). The results suggest that the sub-toxic contents of cadmium and lead in the hair may be of potential effect on behavior, and the mineral analysis may be an important adjunctive diagnostic procedure. Further studies into this problem are necessary.

  • PDF

Mercury Contents of Scalp Hair by Consumption Pattern of Fishes, Shellfishes and its Products (어패류와 그 제품 섭취양상에 따른 두발중 총수은 및 유기수은 함량)

  • Lee, Won-Shik;Kim, Doo-Hie
    • Journal of Preventive Medicine and Public Health
    • /
    • v.27 no.1 s.45
    • /
    • pp.44-58
    • /
    • 1994
  • This study was conducted to examine the levels of total and organic mercury in the scalp hair of the elementary school children and adults, and their relationship with the consumption pattern of fishes and shellfishes. The scalp hair samples were collected from the occipital part of 115 children and 131 adults in costal, urban and rural areas of Kyungpook province from June to August 1991. The mercury content was analysed by the atomic absorption spectrophotometer (model IL. 555) with atomic vapor accessory (model IL. 440). The total and organic mercury contents of hair were significantly higher (p<0.01) among the children who prefer fish and/or shellfish (7.728 ppm, 6.610 ppm), and canned fish and/or fish pastes (6.969 ppm, 5.885 ppm) than those who prefer meat (4.822 ppm, 3.905 ppm) and vegetables (3.974 ppm, 3.224 ppm). The children who prefer to eat the canned fish without cooking showed a higher mercury content than the children who prefer to eat it as stew or mixed with vegetables (p<0.01). There was a dose-response relationship between the intake frequency of canned fish, raw fish and cooked fish and the content of total and organic mercury of hair, the children who eat fish almost everyday showed 2 times higher than those who eat rarely (p<0.01). The mercury content in the hair of the children who eat raw fish was significantly higher than that of the children who eat boiled or broiled fish (p<0.01). The total and organic mercury contents of adult scalp hair increased with age up to the forties and slightly decreased in the fifties. The mercury contents of those who were engaged in the fishery and raw fish restaurant were 2 times higher than those of the farmers. The mercury content of the persons who were favorite dishes of fish and shellfish were most high, and who prefer raw fish were 2 times higher than those of the persons who prefer vegetables and broiled fish. The contents of total and organic mercury in adult scalp hair showed also a increasing tendency with the intake frequency of raw and cooked fish.

  • PDF

The study of nondestructive method for measuring the acidity of the recent record paper in Hanji by using FT-NIR spectroscopy and Integrating sphere (푸리에 변환 근적외선 분광분석기(FT-NIR)와 적분구를 이용한 근대 한지 기록물의 산성도 비파괴 평가방법에 대한 연구)

  • Shin, Yong-Min;Park, Soung-Be;Kim, Chan-Bong;Lee, Seong-Uk;Cho, Won-Bo;Kim, Hyo-Jin
    • Proceedings of the Korea Technical Association of the Pulp and Paper Industry Conference
    • /
    • 2011.10a
    • /
    • pp.255-269
    • /
    • 2011
  • The purpose of study has to analyze with non destructive method for researching the tool that could be measured with the status of record written on Hanji speedily. Because the original record should be destructed for analyzing with previous method in the case of the paper record, it was to develop the tool based on non destructive method for overcoming such limit. The study was used with FT NIR (Fourier transform NIR) for analyzing the Hanji for being written and preserved. The FT NIR spectrometer that of NIR spectrometer has the better performance of precision and accuracy than dispersive NIR spectrometer was used. Also the wavelength of FT-NIR was measured with 12,500 to 4,000 $cm^{-1}$, and the integrating sphere as diffuse reflectance type was used for analyzing Hanji. The moisture and acidity (pH) of chemical factors as quality evaluated factor of Hanji was studied for the correlation of NIR spectrum. And then The NIR spectrum was pretreated for showing the coefficients of optimum correlation. MSC and First derivative of Savitzky - Golay was used as pretreated method, and the coefficients of optimum correlation were shown by PLSR(Partial least square regression). And the coefficients of optimum correlation were calculated by PLSR(Partial least square regression). The correlation coefficients of acidity had 0.92 on NIR spectra without pretreatment. Also the SEP of acidity was 0.24. And then The NIR spectra with pretreatment would have more good correlation coefficients ($R^2=0.98$) and more good SEP(=019) on acidity. Therefore the data of correlation coefficients ($R^2$) and SEP with pretreatment was shown to be superior. And NIR spectra data of first derivative had best linearity on the correlation coefficients ($R^2=0.99$) and also SEP(=0.45) was superior. Therefore the correlation coefficients and SEP of first derivative had better than those of NIR spectra of no pretreatment. As such result, it was possible to evaluate the record status of Hanji speedily with integrated sphere and NIR analyzer as non destructive method.

  • PDF

A Study on Dimethacryloyloxy Alkane Derivatives Having an Anti-wear Performance as Lubricating Oil Additives (윤활유첨가제로써 마모억제 성능을 갖는 Dimethacryloyloxy Alkane 유도체에 관한 연구)

  • Han, Hye-Rim;Cho, Jung-Eun;Sim, Dae-Seon;Kang, Chung-Ho;Kim, Young-Wun;Jeong, Noh-Hee;Kang, Ho-Cheol
    • Applied Chemistry for Engineering
    • /
    • v.27 no.6
    • /
    • pp.583-589
    • /
    • 2016
  • Lubricant additives including zinc dialkyldithiophosphate (ZDDP) containing metal have been widely used due to the advantage of very low cost, but they can generate impurities such as ash. In this work, ZDDP containing metals was partially replaced with bis[3-(dialkyloxyphosphorothionyl) thio-2-methylpropanyloxy] butane (BAP4s) which was synthesized conveniently and effectively from alkanediol without any metal components. Also, the wear resistance property of synthesized BAP4s were studied. Wear scar diameter (WSD) values of BAP4s with butyl, octyl, decyl, dodecyl or tetradecyl groups were also measured by four-ball test. As the length of the alkyl group increased from 4 to 8, the WSD value of BAP4s decreased rapidly from 0.59 to 0.45 mm, but from 8 to 14, the value increased very slowly from 0.45 to 0.50 mm. Thus, among all BAP4s, B8P4 having BAP4 with the octyl group, showed the lowest WSD value. Furthermore, the WSD values were measured in a lubricant base oil mixed with a 0.50 percent concentration (w/w) of either BAP4 or ZDDP. The former was 0.55 mm, and the latter was 0.45 mm. The thermal stability and tribofilm formation peroperty were also measured by thermogravimetric analyzer (TGA) and energy-dispersive X-rays spectroscopy (EDS), respectively.

Radium Isotope Ratio as a Tracer for Estimating the Influence of Changjiang Outflow to the Northern Part of the East China Sea (라듐 동위원소 방사능비를 추적자로 사용한 동중국해 북부 해역에서 장강 유출수의 영향 추정)

  • Kim, Kee-Hyun;Kim, Seung-Soo
    • Journal of the Korean Society for Marine Environment & Energy
    • /
    • v.12 no.3
    • /
    • pp.133-142
    • /
    • 2009
  • In order to understand the present environmental condition and future impingement of Changjiang(Yangtze River) outflow upon the adjacent seas after the scheduled completion of the Sanxia (Three Gorges) Dam in 2009, we tried to estimate the mixing ratios among surface waters of three end-members: Changjiang Water (CW), Kuroshio Water (KW), and East China Sea Water (ECSW) using $^{228}Ra/^{226}Ra$ activity ratio and salinity as tracers. Water samples were collected from 32 stations in November 2005 (R/V Tamgu 3), from 20 stations in July 2006 (R/V Ocean 2000) and from 17 stations in August 2006 (R/V Ieodo) in the northern part of the East China Sea. Radium isotopes in ~300 liters of surface seawater were extracted onboard by filtering through manganese impregnated acrylic fibers and following coprecipitation as $Ba(Ra)SO_4$. Activities of radium isotopes were determined by a high purity germanium detector. Results show that the fraction of CW was in the range of 1-23% in the study area, while KW was in the range of 0-30 % and ECSW 58-100 %. The eastward plume of Changjiang outflow, commonly observed in satellite images during summer and also displayed by the eastward-decreasing CW fraction in this study, could be attributed to Ekman transport caused by the SE monsoon prevailing in this region during summer. Results of this study showed that in the drought season, there was a little or no fraction of CW in the study area. Concentration of dissolved inorganic nitrogen (DIN) showed strong positive relationship with the fraction of CW, suggesting Changjiang as the major source of nitrogen. The mixing curve of DIN indicates the removal of nitrate by biological uptake during the mixing of CW with ambient seawater in the study area.

  • PDF

CO2 Sequestration and Utilization of Calcium-extracted Slag Using Air-cooled Blast Furnace Slag and Convert Slag (괴재 및 전로슬래그를 이용한 CO2 저감 및 칼슘 추출 후 슬래그 활용)

  • Yoo, Yeongsuk;Choi, Hongbeom;Bang, Jun-Hwan;Chae, Soochun;Kim, Ji-Whan;Kim, Jin-Man;Lee, Seung-Woo
    • Applied Chemistry for Engineering
    • /
    • v.28 no.1
    • /
    • pp.101-111
    • /
    • 2017
  • Mineral carbonation is a technology in which carbonates are synthesized from minerals including serpentine and olivine, and industrial wastes such as slag and cement, of which all contain calcium or magnesium when reacted with carbon dioxide. This study aims to develop the mineral carbonation technology for commercialization, which can reduce environmental burden and process cost through the reduction of carbon dioxide using steel slag and the slag reuse after calcium extraction. Calcium extraction was conducted using NH4Cl solution for air-cooled slag and convert slag, and ${\geq}98%$ purity calcium carbonate was synthesized by reaction with calcium-extracted solution and carbon dioxide. And we conducted experimentally to minimize the quantity of by-product, the slag residue after calcium extraction, which has occupied large amount of weight ratio (about 80-90%) at the point of mineral carbonation process using slag. The slag residue was used to replace silica sand in the manufacture of cement panel, and physical properties including compressive strength and flexible strength of panel using the slag residue and normal cement panel, respectively, were analyzed. The calcium concentration in extraction solution was analyzed by inductively coupled plasma optical emission spectrometer (ICP-OES). Field-emission scanning electron microscope (FE-SEM) was also used to identify the surface morphology of calcium carbonate, and XRD was used to analyze the crystallinity and the quantitative analysis of calcium carbonate. In addition, the cement panel evaluation was carried out according to KS L ISO 679, and the compressive strength and flexural strength of the panels were measured.

Formation and Dissociation Kinetics of Zinc(II) Complexes of Tetraaza-Crown-Alkanoic Acids (Zinc(Ⅱ) Tetraaza-Crown-Allkanoic Acids 착물의 형성 및 해리 반응속도론)

  • Choi, Ki Young;Kim, Dong Won;Kim, Chang Suk;Park, Byung Bin;Choi, Suk Nam;Hong, Choon Pyo;Ryu, Hae Il
    • Journal of the Korean Chemical Society
    • /
    • v.44 no.5
    • /
    • pp.403-409
    • /
    • 2000
  • The formation and dissociation rates of $Zn^{2+}$ Complexes with l,4,7,10-tetraaza-13,16-diox-acyclooctadecane-N,N',N",N'"-tetraacetic acid (1), 1,4,7,10-tetraaza-13,16- dioxacyclooctadecane-N,N',N",N'"-tetramethylacetic acid (2), and 1,4,7,10-tetraaza-13,16- dioxacyclooctadecane-N,N',N",N'"-tetrapropionic acid(3) have been measured by stopped-flow and conventional spectrophotometry. Observations were made at 25.0$\pm$0.1 $^{\circ}C$ and at an ionic strength of 0.10 M NaClO$_4$. The formation reactions of $Zn^{2+}$ ion with 1 and 2 took place by the rapid formation of an intermediate complex (ZnH$_3L^+$) in which the $Zn^{2+}$ ion is incompletely coor-dinated. This might then lead to be a final product in the rate-determining step.ln the pH range 4.76-5.76, the diprotonated (H2L2-) form is the kinetically active species despite of its low concentration. The stability con-stants (log$K_{(ZnH$_3$3$L^+$)}$) and specific water-assisted rate constants (koH) of intermediate complexes have been deter-mined from the kinetic data. The dissociation reactions of $Zn^{2+}$ complexes of 1,2, and 3 were investigated with $Cu^{2+}$ ions as a scavenger in acetate buffer. All complexes exhibit acid-independent and acid-catalyzed con-tributions. The effect of buffer and $Cu^{2+}$ concentration on the dissociation rate has also been investigated. The ligand effect on t dissociation rate of $Zn^{2+}$ complexes is discussed in terms of the side-pendant armsand the chelate ring sizes of the ligands.

  • PDF

Radiotherapy of Supratentorial Primitive Neuroectodermal Tumor (천막상부 원시신경외배엽 종양의 방사선요법)

  • Kim Il Han;Yoo Hyung Jun;Cho Young Kan;Kim Dae Yong
    • Radiation Oncology Journal
    • /
    • v.15 no.1
    • /
    • pp.11-18
    • /
    • 1997
  • Purpose : To evaluate the efficacy of combined treatment of surgery and chemoradiotherapy for supratentorial primitive neuroectodermal tumors (SPNET) and obtain the Prognostic factors and complications Materials and Methods .The a9e of 18 patients ranged from 1 to 27 years (median=5 years). There were 12 males and 6 females The extents of surgery were gross total (n:9), subtotal (n:8), biopsy only (n: 1). Craniospinal radiotherapy was delivered to all the patients except 2 patients who were treated only with the whole brain and primary lesion. Radiation dose were 3120-5800cGy (median=5460) to primary mass, 1500-4200cGy (median=3600cGy) to the whole brain and 1320-3600cGy (median= 2400 cGy) to the spinal axis. Chemotherapy was done in 13 patients. Median follow-up period was 45 months ranged from 1 to 89 months. Results : Patterns of failure were as follows; local recurrence (1), multiple intracranial recurrence (2), spinal seeding (3), craniospinal seeding (2) and multiple bone metastasis (1). Two of two patients who did not received craniospinal radiotherapy failed at spinal area. All the relapsed cases died at 1 to 13 months after diagnosis of progression. The 2- and 5-rear overall survival rates were $61\%\;and\;49\%$, respectively The a9e, sex, tumor location did not influence the survival but aggressive resection with combined chemotherapy showed better outcome. Among 9 survivors, complications were detected as radiation necrosis (n=1), hypopituitarism (n=2), cognitive defect(n=1), memory deficit (n=1), growth retardation (n=1). Conclusion : To improve the results of treatment of SPNET, maximal surgical resection followed by radiation therapy and chemotherapy is necessary. The extended radiation field including craniospinal axis may reduce the recurrence in spinal axis.

  • PDF

Crystal Growth of $Cr:Al_2O_3$ and $Ti:Al_2O_3$ by Czochralski Technique (용액인상법에 의한 $Cr:Al_2O_3$$Ti:Al_2O_3$ 단결정 육성)

  • Yu, Yeong-Mun;Lee, Yeong-Guk;Park, Ro-Hak
    • Korean Journal of Crystallography
    • /
    • v.6 no.1
    • /
    • pp.1-13
    • /
    • 1995
  • Cr:A12O3 and Ti:A12O3 single crystals were grown by Czochralski method, and the effects of crystal growth parameters such as pulling rate, rotation rate, dopant and growth atmosphere on crystal quality were investigated. And spectroscopic properties including lasing efficiency were also measured. Single crystals, sized of 20mm in diameter and 100-135mm in length, were successfully grown from the seed of <001> direction. With the doping level of 0.5w/o Cr2O3, pulling rate 2.0mm/hr, rotation rate of 30rpm and inert atmosphere by nitrogen gas, high quality crystals of Cr:A12O3 were grown. While in case of Ti:A12O3 crystals, high quality crystals were grown under the conditions of the doping level of 0.25w/o TiO2, pulling rate of 1.5mm/hr, rotation rate of 30rpm and reducing atmosphere by hydrogen - nitrogen mixed gas. It was confirmed that Cr3+ ion which maintains its ionoc valence during growth easily de-bubbled than Ti4+ ion which changes its valence, Fe3+ ion also has do-bubbling effect to Ti:A12O3 crystal and the reducing atmosphere by 90% N2 - 10% H2 mixed gas gave effective result on the changing of Ti4+ to Ti3+ and de-bubbling. As a result of spectroscopic measurements of Cr:A12O3 crystal, 4A2 →4F2 and 4F1 absorption transitions and E →4A2(R1) and 2A →4A2(R2) fluorenscence transitions were confirmed. And it was measured that wavelengths of laser R1 and R2 transitions were 696±5nm and 692±5nm respectively, line width of these transitions were 12A, and life-time of fluorenscence was 152μsec. In case of Ti:A12O3 crystals, it was confirmed that absortion transition of 4T2→4E and fluorescence transition of 4E→4T2 with wide range of 650-1050nm was occured. And 147μsec of life-time of fluorescence, 125.4 of figure of merit and 9% of laser efficience were also measured.

  • PDF