• Title/Summary/Keyword: 미소체적

Search Result 41, Processing Time 0.032 seconds

$M\"{o}ssbsuer$ Effect Study of Nanocrystalline $Fe_{73.5}Cu_{1}Nb_{3}Si_{16.5}B_{6}$ Alloy (초미세결정립 $Fe_{73.5}Cu_{1}Nb_{3}Si_{16.5}B_{6}$ 합금의 뫼스바우어 효과 연구)

  • 김재경;신영남;양재석
    • Journal of the Korean Magnetics Society
    • /
    • v.5 no.5
    • /
    • pp.864-873
    • /
    • 1995
  • Amorphous $Fe_{73.5}Cu_{1}Nb_{3}Si_{16.5}B_{6}$ ribbons were annealed for different time at $500^{\circ}C$ and $552^{\circ}C$, just before and after the exothermic reaction in DSC curve. The development of nanocrystalline phase was investigated by means of $M\"{o}ssbsuer$ spectroscopy. The crystalline phase consists mainly of $DO_{3}Fe-Si$. Though slight in amount (5%), another ferromagnetic phase which could be presumed $t-Fe_{3}B$ was detected Si content of $DO_{3}Fe-Si$, Si/(Fe+Si), was 0.218 under the heat treatment at $500^{\circ}C$ for 60 min and 0.222 at $552^{\circ}C$ for 10 min. Since then both of those values decreased with time until 120 min and finally these two values remained constant at 0.210. The variation in Si content with annealing time results in the variation in the hyperfine field and the isomer shift. The increase in the mean hyperfine fields and the decrease in the mean isomer shifts of Fe-Si are caused by the increase in Si content. The volume fractions of residual amorphous phase rapidly decrease during the early stage of annealing and come nearer to saturation after 120 min both at $500^{\circ}C$ and $552^{\circ}C$. The decrease in the mean hyperfine field of residual amorphous. in spite of slight changes in the volume fractions of Fe-Si and of residual amorphous after 120 min. is caused by the increase in the content of Nb and B in residual amorphous phase. The saturated volume fraction of the crystalline phase was 81% for $500^{\circ}C$ (180 min) and 77% for $552^{\circ}C$ (960 min), different from expectation.

  • PDF

Hysteresis of the Suction Stress in Unsaturated Weathered Mudstone Soils (불포화 이암풍화토에서의 흡입응력 이력현상)

  • Song, Young-Suk;Choi, Jin-Su
    • Journal of the Korean Geotechnical Society
    • /
    • v.28 no.3
    • /
    • pp.55-66
    • /
    • 2012
  • To investigate the hysteresis of the suction stress in unsaturated weathered mudstone soils (CL), matric suction and volumetric water content were measured in both drying and wetting processes using Automated Soil-Water Characteristics Curve Apparatus. The drying and wetting processes in unsaturated soils were reproduced in the test; the drying process means to load matric suction to spill pore water from the soils, and the wetting process means to unload matric suction to inject pore water into the soils. Based on the measured result, Soil Water Characteristic Curve(SWCC)s were estimated by van Genuchten model (1980). SWCCs have nonlinear relationship between effective degree of saturation and matric suction. The hysteresis in SWCCs between drying and wetting processes occurred. As a result of estimating Suction Stress Characteristic Curve(SSCC) using Lu and Likos model (2006), the suction stress rapidly increased in the low level of matric suction and then increased slightly. Also, the hysteresis in SSCCs between drying and wetting processes occurred. In order to design geo-structures and check its stability considering unsaturated soil mechanics, therefore, it is more reasonable that the SSCC of drying process should be applied in the condition of rainfall infiltration and the SSCC of wetting process in the condition of evaporation or drainage.

Temperature Sensitivity Analysis of TDR Moisture Content Sensor for Road Pavement (도로하부 함수비 계측을 위한 TDR 방식 함수비 센서 온도 민감도 분석)

  • Cho, Myunghwan;Lee, Yoonhan;Kim, Nakseok;Jee, Keehwan
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.33 no.1
    • /
    • pp.329-336
    • /
    • 2013
  • The infrastructure of flexible pavement is composed of aggregate subbase, anti-frost layer, and subgrade. In particular, the subgrade performance is affected by climates such as frost action and precipitation. The method of TDR(Time Domain Reflectometry) sensors to measure moisture contents in subgrade layer has been used in the research. Due to the TDR method using dielectric permitivity of soil and water, the sensors can be affected by the low subgrade temperatures. The air temperatures frequently drops below $-20^{\circ}C$ in the winter in Korea. As a result, it is necessary to estimate the accuracy of the TDR moisture sensors in the range of below zero temperatures. In this study, the subgrade temperatures of lower than $-2^{\circ}C$ were extended to evaluate temperature sensitivity of the TDR moisture sensors. The test results revealed that the moisture contents around the sensors were reduced while those of the upper part of specimen showed a tendency to increase as the specimen surface temperature drops below zero under the volumetric moisture contents(VMC) of 20% and 30%. However, the impact of temperature on the function of the sensor at lower water contents was found to be negligible if any.

Life Prediction of Composite Pressure Vessels Using Multi-Scale Approach (멀티 스케일 접근법을 이용한 복합재 압력용기의 수명 예측)

  • Jin, Kyo-Kook;Ha, Sung-Kyu;Kim, Jae-Hyuk;Han, Hoon-Hee;Kim, Seong-Jong
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.11 no.9
    • /
    • pp.3176-3183
    • /
    • 2010
  • A multi-scale fatigue life prediction methodology of composite pressure vessels subjected to multi-axial loading has been proposed in this paper. The multi-scale approach starts from the constituents, fiber, matrix and interface, leading to predict behavior of ply, laminates and eventually the composite structures. The multi-scale fatigue life prediction methodology is composed of two steps: macro stress analysis and micro mechanics of failure based on fatigue analysis. In the macro stress analysis, multi-axial fatigue loading acting at laminate is determined from finite element analysis of composite pressure vessel, and ply stresses are computed using a classical laminate theory. The micro stresses are calculated in each constituent from ply stresses using a micromechanical model. Three methods are employed in predicting fatigue life of each constituent, i.e. a maximum stress method for fiber, an equivalent stress method for multi-axially loaded matrix, and a critical plane method for the interface. A modified Goodman diagram is used to take into account the generic mean stresses. Damages from each loading cycle are accumulated using Miner's rule. Monte Carlo simulation has been performed to predict the overall fatigue life of a composite pressure vessel considering statistical distribution of material properties of each constituent, fiber volume fraction and manufacturing winding angle.

A Study on Electrolysis of Heavy Water and Interaction of Hydrogen with Lattice Defects in Palladium Electrodes (팔라디움전극에서 중수소의 전기분해와 수소와 격자결함의 반응에 관한 연구)

  • Ko, Won-Il;Yoon, Young-Ku;Park, Yong-Ki
    • Nuclear Engineering and Technology
    • /
    • v.24 no.2
    • /
    • pp.141-153
    • /
    • 1992
  • Excess tritium analysis was peformed to verify whether or not cold fusion occurs during electrolysis of heavy water in the current density range of 83~600 mA/$\textrm{cm}^2$ for a period of 24 ~ 48 hours with use of palladium electrodes of seven different processing treatments and geometries. The extent of recombination of D$_2$ and $O_2$gases in the electrolytic cell was measured for the calculation of accurate enthaplpy values. The behavior and interaction of hydrogen atoms with defects in Pd electrodes were examined using the Sieverts gas charging and the positron annihilation(PA) method. Slight enrichment of tritium observed was attributed to electrolytic enrichment but not to the formation of a by-product of cold fusion. The extent of recombination of D$_2$and $O_2$gases was 32%. Hence the excess heat measured during the electrolysis was considered to be due to the exothermic reaction of recombination but not to nuclear fusion. Lifetime results from the PA measurements on the Pd electrodes indicated that hydrogen atoms could be trapped at dislocations and vacancies in the electrodes and that dislocations were slightly more preferred sites than vacancies. It was also inferred from R parameters that the formation of hydrides was accompanied by generation of mostly dislocations. Doppler broadening results of the Pd electrodes indicated that lattiec defect sites where positrons were trapped first increased and then decreased, and this cycle was repeated as electrolysis continued. It can be inferred from PA measurements on the cold-rolled Pd and the isochronally annealed Pd hydride specimens that microvoid-type defects existed in the hydrogen-charged electrode specimen.

  • PDF

A Study on Heat Transfer Coefficient of a Perfluorocarbon Heat Pipe (Perfluorocarbon 히트파이프의 열전달 계수에 관한 연구)

  • 강환국;김철주;김재진
    • Journal of Energy Engineering
    • /
    • v.7 no.2
    • /
    • pp.194-201
    • /
    • 1998
  • In electric commuter trains using AC motors, lots of GTO thyristors and diodes are needed for power controls. These semiconductors generate heat about 1~2 kW, and for cooling which perfluorocarbon(PFC) heat pipes have been in use for the last two decades. The present study was investigated on the effects of such important design parameters as structure of internal surface (grooved or smooth), fill charge ratio, and inclinating angle from a vertical on heat transfer coefficients at both evaporators and condensers. To obtain experimental data, several heat pipes of the same geometry of 520 mm long and diameter of 15.88 mm but different in fill charge ratio and internal surface structure were designed and fabricated. For prediction of the heat transfer coefficients, related expressions were examined and the results of calculations were compared with experimental data. Performance tests were conducted while heat pipes operated at mode of thermosyphons. High enhancements of heat transfer coefficient were obtained internal grooves. In these cases, the evaporating heat transfer coefficients distributed in the range of 2~5.5 kW/$m^2$K, with an increase of heat flux from 15~45 kW/$m^2$. These experimental data were in good agreement with Rohsenow's expression based on nucleate boiling when correction factor $C_R$=1.3 was encountered. In addition, the condensation heat transfer coefficients were distributed from 1.5 to 3.5 kW/$m^2$K, and the data were in good agreements with Nusselt's correlation, based on filmwise condensation on vertical plate, when choosing a correction factor $C_N=4$. A fill charge ratio of 40~100% were recommended, and the in clination angle effects were negligible when the angle was higher then 30$^{\circ}$.

  • PDF

Foliar ultrastructure of Korean Orostachys species (한국산(韓國産) 바위솔속(屬) 엽육조직(葉肉組織)의 미세구조(微細構造))

  • Kim, In-Sun;Pak, Jae-Hong;Seo, Bong-Bo;Song, Seung-Dal
    • Applied Microscopy
    • /
    • v.25 no.4
    • /
    • pp.52-61
    • /
    • 1995
  • Ultrastructural characteristics were examined with leaves of three species, O. japonicus A. Berger, O. malacophyllus Fisch., and O. sikokianus Owhi that probably have CAM mode. The mesophyll cells of these Orostachys possessed vacuoles with precipitates, myelin-like figures, and plasmalemmasomes, along with typical chloroplasts, microbodies and darkly stained bodies in their thin peripheral cytoplasm. Separation of the plasmalemma from the cell wall, leaving a space between them, was a common phenomenon in these species. A complex array of small to large vacuoles which contain small, membrane-bounded vesicles or vacuole-like structures were frequently found. A well-developed thylakoid system was observed in the chloroplasts and this indicates that the photosynthetic capacity of these mesophyll cells is probably active. A peculiar configuration of cytoplasm, especially around the chloroplasts, was also encountered. The variety of cytoplasmic constituents and vacuoles suggest the water-storing mesophyll cells may be complex in function. Some cellular features detected in this study strongly suggest the possible occurrence of CAM mode in Orostachys species.

  • PDF

Manufacture of Immobilization Device (Vac-lok) and the Usefulness of Evaluation for Reproducibility of Patients in the Radiotherapy (환자의 재현성을 위한 고정장치(Vac-lok) 제작과 방사선치료에서 유용성 평가)

  • Lee, Jae-Seung;Kim, Gyoung-Hee;Jeong, Kyu-Hwan;Kweon, Dae-Cheol;Goo, Eun-Hoe;Park, Cheol-Woo;Im, In-Chul;Dong, Kyung-Rae;Chung, Woon-Kwan
    • Journal of Radiation Protection and Research
    • /
    • v.36 no.1
    • /
    • pp.8-16
    • /
    • 2011
  • We manufactured the Vac-lok that can be applied to patient of special body shape and need to special set-up position and evaluated the usefulness in the radiation therapy. The manufacture Vac-lok, It was used EVA resin and biobeadform of a diameter 1.5 mm. carried out the test of functionality, structural and analyzed the relative reproducibility of phantoms and patients. During the total period of radiation therapy, Vacuum pressure bring variety to a very small amount in the test of functionality of the manufacture Vac-lok. But It was a negligible quantity. The manufacture Vac-lok improved the relative reproducibility of phantoms than the existing Vac-lok and tolerance has a confidence less than 4% error. Also, relative reproducibility of patient increased error than phantom in the antero-posterior and lateral plan. However, the maximum set-up error was less than ${\pm}\;2.3$ mm. In conclusion, If tolerance set-up error of radiotherapy is less than ${\pm}\;3$ mm, the manufacture Vac-lok was enough possible to use and improvement of reproducibility, considering supply with the Vac-lok made to measure of special patient that produced at a low price and without delay.

Effects of Heat Treatment Conditions on the Interfacial Reactions and Crack Propagation Behaviors in Electroless Ni/electroplated Cr Coatings (열처리 조건에 따른 무전해 Ni/전해 Cr 이중도금의 계면반응 및 균열성장거동 분석)

  • Son, Kirak;Choi, Myung-Hee;Lee, Kyu Hawn;Byon, Eungsun;Rhee, Byong-Ho;Park, Young-Bae
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.23 no.3
    • /
    • pp.69-75
    • /
    • 2016
  • This study investigated the effect of heat treatment conditions not only on the Cr surface crack propagation behaviors but also on the Ni/Cr interfacial reaction characteristics in electroless Ni/electroplated Cr double coating layers on Cu substrate. Clear band layer of Ni-Cr solid solutions were developed at Ni/Cr interface after heat treatment at $750^{\circ}C$ for 6 h. Channeling cracks formed in Cr layer after 1 step heat treatment, that is, heat treatment after Ni/Cr plating, while little channeling cracks formed after 2 step heat treatment, that is, same heat treatments after Ni and Cr plating, respectively, due to residual stress relaxation due to crystallization of Ni layer before Cr plating.

$M\""{o}ssbauer$ Effet Studies on Nanocrystalline $Fe_{73.5}Cu_{1}Nb_{3}Si_{16.5}B_6$ Alloy (초미세결정립 $ Fe_{73.5}Cu_{1}Nb_{3}Si_{16.5}B_6$ 합금의 $M\""{o}ssbauer$ 효과 연구)

  • 신영남;김재경;양재석;조익한;강신규
    • Journal of the Korean Magnetics Society
    • /
    • v.4 no.1
    • /
    • pp.12-19
    • /
    • 1994
  • The crystallization behavior of the amorphous $Fe_{73.5}Cu_{1}Nb_{3}Si_{16.5}B_{6}$ alloy with isothermal annealing at $552^{\circ}C$ was studied by $M\"{o}ssbauer$ spectroscopy. The amorphous phase was revealed to coexist together with $Do_{3}-FeSi$ nanocrystalline and Cu-duster in annealed alloys by $M\"{o}ssbauer$ spectrum analysis. At the early stage of crystallization, Si content of FeSi is high due to the creation of Cu-cluster, and decreases with annealing until 60 minutes, which results in the increase in the mean hyperfine field of FeSi, and thereafter keeps constant. After 60 minutes, the decrease in the mean hyperfine field of the residual armrphous, in spite of a slight change in the volume fraction of the FeSi and the residual armrphous, is caused by the increase in the content of Nb and B in residual amorphous phase. Both directions of the hyperfine field, those of the FeSi and the residual amorphous, become randomly oriented in about 60 minutes. For FeSi and Cu-duster, the Avrami exponents are 0.51 and O.65, the activation energies are 2.35 eV and 2.44 eV, and the incubation times are 2.4 minutes and 0.8 minutes respectively. Earlier formation of Cu-duster than that of FeSi is coincidence with the fact that Cu atom promotes the nucleation of the FeSi.