Creep Life Prediction of Friction Welded Joints (Cu-Alloy/STS316L) for Nuclear Power Plant (원자력 발전소용 마찰용접재 (Cu합금/STS316L)의 크리프 수명예측)

  • 유인종;공유식;오세규;김선진
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2001.10a
    • /
    • pp.258-263
    • /
    • 2001
  • In this paper, the real-time prediction of high temperature creep life was carried out for the friction welded joints of dissimilar heat resistintg steels (CulCr0.5Zr-STS316L). Various life prediction methods such as LMP (Larson-Miller Parameter) and ISM (initial strain method) were applied. The creep behaviors of those steels and the welds under static load were examined by ISM combined with LMP at 300, 400 and 50$0^{\circ}C$, and the relationship between these two methods was investigated. A real-time creep life (tsub/r/, hr) prediction equation by initial strain ($\varepsilon_0$, %) under any creep stress ($\sigma$, MP$\alpha$) at any high temperature (T, K) was developed

  • PDF

Tensile Properties and Creep Rupture Characteristics of Cu-1Cr-0.5Zr/STS316L Friction Welded Joints at Elevated Temperature (Cu-1Cr-0.5Zr 합금과 STS316L강의 마찰용접재의 고온 인장 성질과 크리프 파단 특성)

  • Yoo, I.J.;Kong, Y.S.;Kim, S.J.
    • Journal of Power System Engineering
    • /
    • v.6 no.4
    • /
    • pp.49-55
    • /
    • 2002
  • In this paper, the elevated temperature tensile properties and short-time creep rupture characteristics were investigated for the friction welded joints of dissimilar materials, Cu-1%Cr-0.5%Zr and STS316L. The joining tests on Cu-1%Cr-0.5%Zr/STS316L by friction welding were performed, and optimum joining conditions of the friction welded joints were determined. The characteristics of the elevated temperature tensile strength, hardness, fractographs were examined, and the creep rupture characteristics for the optimum welded joints were investigated under uniaxal static load at 300, 400 and $500^{\circ}C$.

  • PDF

The Effect of Aging Treatment on the High Temperature Fatigue Fracture Behavior of Friction Welded Domestic Heat Resisting Steels (SUH3-SUS 303) (마찰용접된 국산내열 강 (SUH3-SUS303 )의 시효열처리가 고온피로강도 및 파괴거동에 미치는 영향에 관한 연구)

  • Lee, Kyu-Yong;Oh, Sae-Kyoo
    • Journal of the Korean Society of Fisheries and Ocean Technology
    • /
    • v.17 no.2
    • /
    • pp.93-103
    • /
    • 1981
  • It is well-known that nowadays heat resisting and anti-corrosive materials have been widely used as the components materials of gas turbines, nuclear power plants and engines etc. In the fields of machine production industry. And materials for engine components, like as the exhaust valve of internal combustion engine, have been required to operate under the high temperature range of $700^{\circ}C$-$800^{\circ}C$ and high pressured gas with repeated mechanical load for the high performance of engines. For these components, friction welding for bonding of dissimilar steels can be applied for in order to obtain process shortening, production cost reduction and excellent bonding quality. And age hardening recently has been noticed to the heat resisting materials for further strengthening of high temperature strength, especially high temperature fatigue strength. However, it is difficult to find out any report concerning the effects of age hardening for strengthening high temperature fatigue strength to the Friction welded heat resisting and anti-corrosive materials. In this study the experiment was carried out as the high temperature rotary bending fatigue testing under the condition of $700^{\circ}C$ high temperature to the friction welded domestic heat resisting steels, SUH3-SUS303, which were 10hr., 100hr. aging heat treated at $700^{\circ}C$ after solution treatment 1hr. at $1, 060^{\circ}C$ for the purpose of observing the effects of the high temperature fatigue strength and fatigue fracture behaviors as well as with various mechanical properties of welded joints. The results obtained are summarized as follows: 1) Through mechanical tests and micro-structural examinations, the determined optimum welding conditions, rotating speed 2420 rpm, heating pressure 8kg/mm super(2), upsetting pressure 22kg/mm super(2), the amount of total upset 7mm (heating time 3 sec and upsetting time 2 sec) were satisfied. 2) The solution treated material SUH 3, SUS 303, have the highest inclination gradient on S-N curve due to the high temperature fatigue testing for long time at $700^{\circ}C$. 3) The optimum aging time of friction welded SUH3-SUS 303, has been recognized near the 10hr. at $700^{\circ}C$ after the solution treatment of 1hr. at $1, 060^{\circ}C$. 4) The high temperature fatigue limits of aging treated materials were compared with those of raw material according to the extender of aging time, on 10hr. aging, fatigue limits were increased by SUH 3 75.4%, SUS 303 28.5%, friction welded joints SUH 3-SUS 303 44.2% and 100hr. aging the rates were 64.9%, 30.4% and 36.6% respectively. 5) The fatigue fractures occurred at the side of the base matal SUS303 of the friction welded joints SUH 3-SUS 303 and it is difficult to find out fractures at the friction welding interfaces. 6) The cracking mode of SUS 303, SUH 3-303 is intergranular in any case, but SUH 3 is fractured by transgranular cracking.

  • PDF

Friction Stir Welding of 7075-T651 Aluminum Plates and Its Fatigue Crack Growth Property (7075-T651 알루미늄 판재의 마찰교반용접과 피로균열전파 특성)

  • Kim, Chi-Ok;Sohn, Hye-Jeong;Kim, Seon-Jin
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.35 no.10
    • /
    • pp.1347-1353
    • /
    • 2011
  • Friction stir welding (FSW) method has extensively been used in manufacturing methods because of the several advantages over conventional welding methods, such as better mechanical properties, reduced occurrence of joining defects, high material saving, and low production time, etc. The aim of this paper is to review the optimal FSW conditions using the previous experimental results and is to investigate the fatigue crack growth rate in three different zones, WM, HAZ and BM for FSWed Al7075-T651 aluminum plates. As far as our experiments are concerned, the optimal conditions are obtained as rotation speed, 800rpm and travelling speed, 0.5mm/sec. The fatigue crack growth rate showed strong dependency on three different zones WM, HAZ and BM, and crack driving force.

Study on Creep Life Prediction by Initial Strain Method for Friction Welded Joints of Heat Resisting Steels (내열강 마찰용접재의 ISM에 의한 크리프 수명예측에 관한 연구)

  • 김헌경;김일석;이연탁;공유식;오세규
    • Journal of Ocean Engineering and Technology
    • /
    • v.15 no.2
    • /
    • pp.46-52
    • /
    • 2001
  • In this paper, the real-time prediction of high temperature creep life was carried out for the friction welded joints of dissimilar heat resisting steels (SUH3-SUH35). various life prediction method such as LMP (Larson_miller Parameter) and ISM (initial strain method) were applied. The creep behaviors of those steels and the welds under static load were examined by ISM combined with LMP at 500, 600 and $700^{\circ}C$, and the relationship between these two methods was investigated. A real-time creep lie (tr, hr) prediction equation by initial strain (${\varepsilon}_0$, %) under any creep stress ($\sigma$, MPa) at any high temperature (T, K) was developed as follows: $t_r={\alpha}{\varepsilon}_0^{\beta}{\sigma}^{-1}$ where, ${\phi}=16: {\alpha}=10^{51.412-0.104T+5.375{\times}10^5T^2}$, $ {\beta}=-83.989+0.180T-9.957{\times}10^{-5}T^2,{\phi}=20:$ ${\alpha}=10^{69.910-0.146T+7.744{\times}10^{-5}T^2$, ${\beta}=-51.442+0.105T-5.595{\times}10^{-5}T^2$ for SUH3-SUH35 friction weld of =16mm and 20mm, respectively.

  • PDF

Effects of Postweld Aging Treatment on Rotary Bending Fatigue strength of Friction Welded Joints at Elevated Temperature (마찰 용접부의 고온 회전굽힘 피로 강도에 미치는 용접후 시효열처리의 영향에 관한 연구)

  • Oh, Sae Kyoo
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.7 no.2
    • /
    • pp.36-49
    • /
    • 1983
  • 최근 높은 경제성과 용접성의 우수성에 의한 마찰 용접의 응용에 있어서 내열.내식 재료가 개스터어빈, 기관, 핵 발전기등의 기계 부품 생산 공업에 널리 이용되고 있다. 따라서 이종내열 합금강의 마찰 용접된 부품을 이용함에 있어서 내식.내마모 및 용접성 뿐만 아니라 고온 피로 강도와 크리이프 강도 등의 복합 특성에 관한 연구가 요구되고 있다. 본 연구에서는 마르텐사이트계 실크롬 내열강과 오오스테나이트계 닉켈크롬 스테인레스강의 이종 내식.내열 합금강의 최적 용접조건하에서 마찰 용접된 후의 시효 열처리가 용접재의 700 .deg.C 고온 회전 굽힘 피로강도 특성에 미치는 영향에 관하여 실험과 강도해석에 의해 조사되었고 용접후의 용체화 처리와 시효 열처리법에 의한 내열강 마찰 용접강도 개선법을 개발코저한 것이다.

  • PDF

A Study on the Rupture and Crack Propagation Dharacteristics in the Material Friction-Welded with Hetrogeneous Steels of SM40C and STS304 (SM40C와 STS304 이종재료 마찰용접재의 파단특성 및 크랙전파특성의 연구)

  • 오세욱;허정원;유재환;김재철
    • Journal of Welding and Joining
    • /
    • v.10 no.4
    • /
    • pp.230-239
    • /
    • 1992
  • The specimens of two base metals and material friction-welded with hetrogeneous steels of SM40C and STS304 have been prepared and the characteristics of rupture and crack propagation of them have been examined. In the friction-welded material, the width of HAZ is 3.0mm for STS304 and 3.4mm for SM40C. The hardness distribution in HAZ of SM40C is decreased gradually as being getting off interface, but that in HAZ of STS304 is decreased remarkedly and the value of hardness becomes a little lower than that of the base metal in region of 1mm from interface and becomes a little higher than that of the base metal. The tensile strength of the friction-welded material appeared a little lower than that of the base metal and rupture by tensile load is developed in HAZ of STS304 and the position of rupture is at region of low hardness(1mm from interface). The crack propagation rates(da/dN) in both HAZ of the friction-welded material are a little higher than those in both base metals, but the difference are less except for the case of SM45C in low .DELTA. K value. It has been ascertained that the crack in the interface propagates selectively along the HAZ of SM40C and consequently the crack propagation rate is almost similar to that in the HAZ of SM40C.

  • PDF

Spatial Randomness of Fatigue Crack Growth Rate in Friction Stir Welded 7075-T651 Aluminum Alloy Welded Joints (Case of LT Orientation Specimen) (마찰교반용접된 7075-T651 알루미늄 합금 용접부의 피로균열전파율의 공간적 불규칙성 (LT 방향의 시험편에 대하여))

  • Jeong, Yeui Han;Kim, Seon Jin
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.37 no.9
    • /
    • pp.1109-1116
    • /
    • 2013
  • This study aims to investigate the spatial randomness of fatigue crack growth rate for the friction stir welded (FSWed) 7075-T651 aluminum alloy joints. Our previous fatigue crack growth test data are adopted in this investigation. To clearly understand the spatial randomness of fatigue crack growth rate, fatigue crack growth tests were conducted under constant stress intensity factor range (SIFR) control testing. The experimental data were analyzed for two different materials-base metal (BM) and weld metal (WM)-to investigate the effects of spatial randomness of fatigue crack growth rate and material properties, the friction stir welded (FSWed) 7075-T651 aluminum alloy joints, namely weld metal (WM) and base metal (BM). The results showed that the variability, as evaluated by Weibull statistical analysis, of the WM is higher than that of the BM.

Mechanical Properties and Microstructure on Dissimilar Friction-Stir-Weld of Aluminium Alloys (FSW된 이종알루미늄합금의 접합 특성 및 미세 조직)

  • Han, Min-Su;Jang, Seok-Ki
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.35 no.1
    • /
    • pp.75-81
    • /
    • 2011
  • Dissimilar joining of aluminum 6061-T6 alloy to aluminum 5083-O alloy was performed using friction-stir welding technique. The mechanical properties, hardness, macro- and micro-structure on dissimilar friction-stir-weld aluminium alloy were investigated. Mechanical properties of the weld mainly depend on which Al alloy is placed at the retreating sides of the rotating tool respectively during dissimilar friction-stir weld because the microstructure of stir zone was mainly composed of welded Al alloys of the retreating side. Onion ring pattern was observed like lamella structure stacked by each Al alloy in turn. It apparently results in defect-free weld zone that traverse speed was changed to 124 mm/min under conditions of tool rotation speed like 1250 rpm with 5 mm of tool's prove diameter, 4.5 mm of prove length, 20 mm of shoulder diameter, and $2^{\circ}$ of tilting angle. The 231 MPa of ultimate stress and the 121 MPa of yield point are obtained about the friction-stir-welded Al 6061-T6(AS) to Al 5083-O(RS).

Strength Evaluation of Friction Welded SUH35/SUB3 Considering Stress Singularity (응력특이성을 고려한 SUH35/SUH3 마찰용접재의 강도평가)

  • Chung, Nam-Yong;Park, Chul-Hee
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.14 no.4
    • /
    • pp.59-67
    • /
    • 2006
  • Recently, application of friction welded SUH35/SUH3 is increasing in the manufacturing process of automotive engine valves For securing its reliability and a reasonable strength evaluation method, it is necessary to assess stress singularity under the residual stress condition on the friction welded interface between dissimilar materials. In this paper, strength evaluation method of friction welded materials was investigated by boundary element method and static tensile testing. An advanced method of quantitative strength evaluation for SUH35/SUH3 friction welded material is to be suggested by establishing fracture criterion by using stress singularity factors.