Development of Nanomodified Snow-Melting Concrete Using Low-Temperature Phase-Change Material Impregnated Lightweight Aggregate (저온 상변화 물질 함침 경량골재를 이용한 나노 개질 융설 콘크리트 개발)

  • Kyoung, Joo-Hyun;Kim, Sean-Mi;Hu, Jong-Wan
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.42 no.6
    • /
    • pp.787-792
    • /
    • 2022
  • In winter, the excessive use of deicing salt deteriorates concrete pavement durability. To reduce the amount of deicing salt used, phase-change materials (PCMs) potentially offer an alternative way to melt snow through their latent heat storage characteristics. In this research, thermal energy storage concrete was developed by using PCM-impregnated expanded clay as 50 % replacement to normal aggregate by volume. In addition, to improve the thermal efficiency of PCM lightweight aggregate (PCM-LWA)-incorporated concrete, multi-walled carbon nanotubes (MWCNTs) were incorporated in proportions of 0.10 %, 0.15 %, and 0.20 % by binder weight. Compressive strength testing and programmed thermal cycling were performed to evaluate the mechanical and thermal responses of the PCM-LWA concrete. Results showed a significant strength reduction of 54 % due to the PCM-LWA; however, the thermal performance of the PCM-LWA concrete was greatly improved with the addition of MWCNTs. Thermal test results showed that 0.10 % MWCNT-incorporated concrete had high thermal fatigue resistance as well as uniform heat flow, whereas specimens with 0.15 % and 0.20 % MWCNT content had a reduced thermal response due to supercooling when the ambient temperature was varied between -5℃ and 10℃.

Heavy Metals of Landfilled Biomass and Their Environmental Standard, Including CCA-treated Wood for Eco-housing Materials (방부처리 목재를 포함한 토양매립 바이오메스의 중금속 함량과 안전성 문제)

  • Lim, Kie-Pyo;Lee, Jong-Tak;Bum, Jung-Won
    • Journal of the Korean Wood Science and Technology
    • /
    • v.34 no.4
    • /
    • pp.37-45
    • /
    • 2006
  • Recently, wood-framed houses has been built in the Korea for pension. Wood is good material for human healthy, while the construction lumbers are treated with preservative such as CCA (chromated copper arsenate), which contain some toxic elements for human body. However, if the waste woody biomass treated with various heavy metals, which has been collected from house construction or demolition, was fired in the field, and incinerated or landfilled after mass collection, such components will result in the toxic air pollutants in the burning or land fills, and spreaded into other areas. So the careful selection of wood and chemicals are required in advance for house construction, in particular, for environment-friendly housings. Therefore, this study was carried out to determine the content of toxic heavy metals in woody materials such as domestic hinoki and imported hemlock treated with CCA for housing materials, and the post-treated wood components such as organic fertilizer, sludge, dry-distilled charcoal and carbonized charcoal, to be returned finally into soil. The results are as follows. 1) The chemical analysis of toxic trace elements in various solid biomass required accurate control and management of laboratory environment, and reagents and water used, because of the error of data due to various foreign substances added in various processing and transporting steps. So a systematic analyzers was necessary to monitor the toxic pollutants of construction materials. 2) In particular, the biomass treated with industrial biological or thermal conditions such as sludge or charcoals was not fully dissolvable after third addition of $HNO_3$ and HF. 3) The natural woody materials such as organic fertilizer, sludge. and charcoals without any treatment of preservatives or heavy metal components were nontoxic in landfill because of the standard of organic fertilizers, even after thermal or biological treatments. 4) The CC A-treated wood for making the construction wood durable should not be landfilled, because of its higher contents of toxic metals than the criterion of organic fertilizer for agriculture or of natural environment. So the demolished waste should be treated separately from municipal wastes.

태양광 고효율 저가화 기술동향

  • Gil, Jong-Seok
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2015.08a
    • /
    • pp.85-85
    • /
    • 2015
  • 현재 태양광에너지 시장은 해마다 빠른 속도로 성장하는 추세이며 50 GWp/년 이상의 시장으로 변화하였고 앞으로도 전체적인 성장세는 지속 유지될 것으로 판단된다. 하지만 이와 아울러 각 Value chain 별로 많은 기업들이 생겨나게되어 각각의 기업들이 제품을 고효율 저가화 함으로서 경쟁력을 확보하기 위해 많은 노력들이 기울이고 있으며 본 강연에서는 이러한 측면에서 태양광 에너지의 분야별 고효율/저가화를 위한 기술동향을 살펴보고자 한다. 태양광 산업은 아직은 다소 높은 발전단가로 인해 일부 정부의 지원이나 정책에 의해 산업의 규모가 결정되게 되는데 주요한 지원제도는 RPS 제도와 FIT 제도가 있으며 우리나라는 초기 FIT 제도로 국가에서 태양광에서 생산된 전기를 높은 가격에 사주었으나 근래에들어 RPS 제도를 운영하게 되었으며 매전을 하면서 SMP에 준하는 수익을 창출하고 이와 아울러 REC 를 확보하여 확보된 REC 단가에 의해 추가적인 수익을 창출하는 구조의 발전사업이 진행되고 있다. 그리고 RPS나 FIT와 같은 정부의 지원없이도 발전단가의 경쟁력을 확보하는 시점을 그리드패러티라고 하며 이는 매우 중요한 의미를 갖는다. 태양광의 저가화는 그리드패러티 달성을 확보하기 위해 필수적으로 필요한 사안이며 앞으로도 이러한 저가화 / 고효율화 기술노력은 계속 진행될 것으로 판단된다. 우선 소재의 가격을 줄이기 위해 웨이퍼의 두께가 점점 박형화 되어가고 박형화 되면서도 안정적인 공정수율 및 효율을 향상시키기 위한 기술개발이 진행되고 있으며 Cell 분야에 있어서도 고효율을 위한 다양한 Texturing 기술 및 패시베이션 기술의 개발이 이루어 지고 있으며 고효율 컨셉의 MRT cell, Back contact cell 등 고효율 구조의 cell의 양산을 진행하고 있는 등 최근 n-type 기반의 고효율 cell 기술이 활발하게 양산화 검토가 이루어 지고 있다. 모듈 분야에 있어서는 저가/고효율화와 아울러 제품의 신뢰성 확보가 무엇보다도 중요하게 다루어 지고 있으며 이는 모듈이 최소 25년 이상 Field 에서 운용되어 수익창출이 가능해야 하므로 가장 중요한 요소중에 하나라고 할 수 있다. 신뢰성 측면에서 중요하게 다루어 지고 있는 것 중 하나가 PID 저감을 위한 노력이며 이와 관련된 각 소재의 개발이 가장 활발하게 진행되고 있으며 이와 아울러 장수명을 보장하기 위한 내구성이 겸비된 봉지재의 개발 또한 많은 관심을 불러 일으키고 있다. 저가/고효율화를 위해 CTM loss를 줄이기 위한 다양한 시도가 이루어지고 있으며 특수 형태의 리본으로 빛의 흡수를 증가시키거나 컨택저항을 최소화 하기위한 소재의 개발이 이루어 지고 있다. 태양광 시스템 분야의 경우 발전량과 수익창출에 있어 직접적인 영향을 미치는 분야로서 전체 시스템의 loss 를 줄이고 최적의 환경에서 최대한의 발전량을 확보하기 위한 array 설계 및 운용기술이 활발하게 개발되고 있으며 시스템에서의 loss를 줄여줄수 있는 마이크로 인버터나 multi string 인버터의 적용도 이루어 지고 있으나 저가화를 위한 추가적인 노력이 필요한 상황이다. 본 강연의 마지막으로 이러한 노력들의 산물인 특수 태양광 제품 및 시스템의 기술동향에 대해 살펴하고자 한다. 사막은 전체면적의 1/3을 차지할 정도로 넓은 면적을 자랑하지만 밤과 낮의 기온차 그리고 계통 선로의 부재 등 적용하기 어려운 환경적인 제약도 함께 존재하며 이러한 문제를 해결하기 위한 방안에 대해 살펴보고 최근 Hot issue 중의 하나인 수상 태양광 시스템의 장, 단점과 기술적 특성 등을 살펴보고자 한다.

  • PDF

Preparation and Application of DTP printable UV curable Ink for Leather (DTP용 자외선 경화형 잉크의 제조와 피혁에의 응용)

  • Park, Soo-Min;Hao, Fei;Lee, Sang-Heon;Lee, Sang-Chul;Kim, Hea-In
    • Proceedings of the Korean Society of Dyers and Finishers Conference
    • /
    • 2012.03a
    • /
    • pp.54-54
    • /
    • 2012
  • 전통 날염방식(Silk Screen)과 디지털날염(Digital Textile Printing)을 비교해보면, 디지털날염은 디자인에서부터 날염까지의 전공정을 완전히 디지털화함으로서 다양하게 디자인할 수 있고 미묘한 색감의 흐름을 표현할 수 있어서 자연스러운 이미지의 표현이 가능하다. 그러나 현재 디지털날염을 피혁이나 직물에 적용하기에는 프린팅속도가 느려서 생산성이 낮고 이미지 내구성(세탁, 승화, 일광, 및 마찰견뢰도)이 낮은 등 많은 단점을 가지고 있다. 또한 신발산업은 현재 중국이나 동남아시아 등 개발도상국의 등장으로 수출의 국제적 경쟁시대에 접어들면서 대량생산이나 획일적인 디자인으로부터 벗어나 고부가가치 상품을 생산해야하는 과제를 안게 되었다. 한편 가죽에 응용가능한 잉크는 크게 수성, 유성, 용제형과 자외선 경화형의 잉크가 있으며 자외선 경화형 잉크는 자외선을 이용하여 기존의 잉크의 단점을 보완한 것이다. 자외선 경화형 잉크는 자외선 램프를 열원으로 하여 이온 또는 라디칼 중합, 광중합을 하며, 에너지 소비가 적어 경제적이며 시스템 가동시 비활성 기체가 필요하지 않다. 또한 자외선 경화형 기술은 상온에서 이용할 수 있으며 잉크의 경우 건조하는 데 걸리는 시간이 필요하지 않다. 또한 시스템을 가동 시키거나 중지 시키는 것이 쉬우며 고속으로 연속적인 일을 처리할 수 있다. 프린터의 크기가 작아 공간 효율이 유리하며 용제나 $CO_2$가 발생하지 않아 친환경적인 기술이라 할 수 있다. 따라서 본 연구에서는 자외선 경화형 시스템을 잉크에 적용하여 피혁 표면에 프린팅한 다음 그 견뢰도를 측정함으로써 그 효과를 알아보았다. 세탁에 의한 Matlab 측정값으로부터 용제형 잉크의 경우는 세탁 전, 후 line width가 큰 차이를 보이나 자외선 경화형 잉크의 경우는 그 차이가 적음으로부터 자외선 경화형 잉크가 용제형에 비해 색상 탈리가 적었음을 말한다. 또한 raggedness값 역시 마찬가지 결과를 보여 안료 색소와 피혁의 접착성이 향상된 것을 알 수 있다. SEM을 이용한 피혁의 표면과 단면 사진을 보면 용제형보다 자외선 경화형 잉크를 사용한 피혁이 좀 더 매끈한 표면을 보이는데 이것은 접착기능을 하는 아크릴레이트에 의해 균일한 날염이 가능하기 때문이라 고 생각된다. 이상의 결과로부터 자외선 경화형 잉크가 세탁, 마찰, 일광 견뢰도가 우수함을 알 수 있었으며 기존의 용제형 잉크를 대체할 수 있는 좋은 재료라고 생각된다.

  • PDF

A Making of Aesthetic Dental restorations with Nano Hybrid Ceramic material by CAD/CAM System (치과 CAD/CAM용 Nano Hybrid Ceranic 소재를 이용한 심미 치과보철물의 제작)

  • Choi, Beom-jin
    • Journal of the Korean Academy of Esthetic Dentistry
    • /
    • v.25 no.2
    • /
    • pp.98-108
    • /
    • 2016
  • In recent days, perhaps the biggest driver in new material development is the desire to improve restorations esthetics compared to the traditional metal substructure based ceramics or all-ceramic restorations. Each material type performs differently regarding strength, toughness, effectiveness of machining and the final preparation of the material prior to placement. For example, glass ceramics are typically weaker materials which limits its use to single-unit restorations. On the other hand, zirconia has a high fracture toughness which enables multi-unit restorations. This material requires a long time sintering procedure which excludes its use for fast chair side production. Hybrid ceramic material developed for CAD/CAM system is contained improved nano ceramic elements. This new material, called a Resin Nano Hybrid Ceramic is unique in durability of function and aesthetic base compositions. The new nano-hybrid ceramic material is not a composite resin. It is also not a pure ceramic. The material is a mixture of both and consists of nano-ceramic fillers. Like a composite, the material is not brittle and is fracture resistant. Like a glass ceramic, the material has excellent polish retention for lasting esthetics. The material is easily machined by chair side or in a dental lab side, could be an useful restorative option.

Reaction Characteristics of Combined Steam and Carbon Dioxide Reforming of Methane Reaction Using Pd-Ni-YSZ Catalyst (Pd-Ni-YSZ 촉매를 이용한 수증기-이산화탄소 복합개질 반응 특성)

  • Kim, Sung Su
    • Applied Chemistry for Engineering
    • /
    • v.29 no.4
    • /
    • pp.382-387
    • /
    • 2018
  • In this study, the reaction characteristics of combined steam and carbon dioxide reforming of methane (CSCRM) reaction using Pd-Ni-YSZ catalyst were investigated according to types of catalysts and gas compositions. Catalysts were prepared in the form of powder and porous disk. The injected gases were supplied at different ratios of $CH_4/CO_2/H_2O$. As a result, the conversion of $CH_4$ and $CO_2$ was improved as a result of using the porous disc type catalyst as compared with that of the powder type catalyst. When the $CH_4/CO_2/H_2O$ ratio of the feed gas was 1 : 0.5 : 0.5, the $H_2/CO$ ratio was adjusted close to 2. However, after 6 hours of the reaction, $CH_4$ conversion was partially reduced by the carbon deposition and the pressure drop increased from 0.1 to 0.8. This issue was then solved by optimizing the water content. As a result, it was confirmed that the durability was secured by preventing the carbon deposition when the gas was supplied at a $CH_4/CO_2/H_2O$ ratio of 1 : 0.5 : 1, and the conversion rate was maintained at a relatively high level.

Basic Study on Development of Eco-Friendly Vegetation-Block (친환경 식생블록 개발을 위한 기초연구)

  • Heo, Yol;Oh, Sewook;Bang, Seongtaek
    • Journal of the Korean GEO-environmental Society
    • /
    • v.15 no.4
    • /
    • pp.61-67
    • /
    • 2014
  • With a view to resolving environmental problems of hazardous cement, this study seeks to identify the unconfined compressive strength and bending strength of the vegetation block designed herein by utilizing high-strength natural soil stabilizer instead of cement. Soil stabilizer is mainly made of mixture of short fiber extracted from natural fiber and lime, etc. Soil stabilizer reinforces the shearing strength of soil to improve block supportive power and durability while preventing flood and frost damages. For the unconfined compressive strength test, test pieces were prepared by mixing soil stabilizer and weathered soil in different ratios of 6 %, 12 % and 18 %. Experiments were carried out according to curing periods of 5th, 7th, 14th and 28th of the day. For bending strength test, blocks were made in the same mixture ratios as for the unconfined compressive test and tested for each stage. Also, to evaluate for the field applicability, proposed optimum water content considering the characteristics of the soil stabilizer. Permeability test result for the vegetation block, satisfied by the KS F 4419 quality standards.

Evaluation of flexural performance of high performance fiber reinforced cementitious composites according to fiber shape, aspect ratio and volume fraction (강섬유의 형상, 길이 및 혼입율에 따른 고성능 섬유보강 시멘트 복합체의 휨 특성 평가)

  • Park, Gi-Joon;Park, Jung-Jun;Kim, Sung-Wook;Lee, Jang-Hwa
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.18 no.12
    • /
    • pp.697-704
    • /
    • 2017
  • High-Performance Fiber-Reinforced Cement Composites (HPFRCC) has outstanding durability, and has attracted interest because of its ductility and development of strength, which allows a reduction of the self-weight of a structural member by substantially decreasing the cross section. Therefore, the present study aimed to improve the economic efficiency of HPFRCC by examining experimentally the flexural performance considering various characteristics of the steel fiber. To find an efficient fiber reinforcement method, the flexural performance was evaluated for different shapes, aspect ratios, and volume ratios of the steel fiber. Straight, hooked, and twisted fiber configurations were considered by adopting a fiber length longer than the usual 13 mm. The test results showed that HPFRCC reinforced by 19.5 nun-long straight fibers with a volume fraction of 1.5% shows better flexural performance than that reinforced by 13 mm-long straight fibers with a volume fraction of 2.0%. Consequently, HPFRCC with enhanced economic efficiency can be produced by adopting a reduced amount of steel fiber.

Evaluation on the Mechanical Performance of Concrete Using Entanglement Polyamide Fiber (다발형 폴리아미드섬유 보강 콘크리트의 역학적 성능평가)

  • Jeon, Joong Kyu;Kim, Gyu Yong;Jeon, Chan Ki;Lee, Soo Choul
    • Journal of the Society of Disaster Information
    • /
    • v.8 no.3
    • /
    • pp.223-233
    • /
    • 2012
  • Steel fiber is high stiffness and large weight. So, Pumping hose to rupture of the safety management is difficult. Steel fiber caused by corrosion of the deterioration of durability and high-rebound losses are needed for the improvements. Thus, the revised regulations in 2009 by a steel fiber to reinforce other materials is possible. Variety of fiber reinforcement material for concrete review of applicability is needed. Steel fiber strength than the other fibers is large and by the geometry of the fibers are attached to improve performance. However, compared to steel fiber organic fibers and low modulus of elasticity and tensile strength of fiber and agglomeration occurs in the concrete to be used as reinforcement material is difficult. In this regard, the present study as a single object in the micro-fiber bouquet sharp entanglement through make muck attach surface area, distributed fibers from surfactant of the surface enhanced polyamide fibers, steel fiber and PP fiber reinforced concrete by comparing the scene to provide a basis for the use.

Fundamental Properties of Fly ash Concrete Containing Lightly Burnt MgO Powder (저온 소성한 MgO 분말을 함유한 플라이애시 콘크리트의 기본 물성)

  • Choi, Seul-Woo;Jang, Bong-Seok;Lee, Kwang-Myong
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.33 no.2
    • /
    • pp.475-481
    • /
    • 2013
  • Although the lightly burnt MgO at $850{\sim}1000^{\circ}C$ has expansibility, it does not lead to unsound concrete. The expansion of MgO could compensate for shrinkage of concrete for a long-term, because the hydration of MgO occurs at a slow pace. Recently, the study and application of mineral admixture such as fly ash and blast furnace slag have increased for the hydration heat reduction, durability improvement, and reducing $CO_2$ emission in the construction industry. Thus, it is necessary to research on the concrete that contains both a mineral admixture and MgO as an expansion agent. This study investigates fundamental properties of fly ash concrete with lightly burnt MgO through various experiments. The adiabatic temperature test results showed that the fly ash concrete with MgO of the 5% replacement ratio had the slower pace of the temperature rise and the lower final temperature than the fly ash concrete. The influences of MgO on long-term compressive strength varied depending on water-binder ratio, and the long-term length change test results indicated the expansion effects of the FA concrete containing MgO.