Microstructure and Wear Characteristics of TiC-SKD11 Composite Fabricated by Liquid Pressing Infiltration Process (용융가압함침 공정으로 제조한 TiC-SKD11 복합재료의 미세조직 및 내마모 특성)

  • Cho, Seungchan;Jo, Ilguk;Lee, Sang-Kwan;Lee, Sang-Bok
    • Composites Research
    • /
    • v.30 no.3
    • /
    • pp.209-214
    • /
    • 2017
  • Titanium carbide (TiC) reinforced SKD11 matrix composites were successfully fabricated by a novel liquid pressing infiltration process. Microstructure, mechanical properties, and wear characteristics of the fabricated 60 vol% TiC-SKD11 composite are analyzed. The composite exhibits superior mechanical properties, such as hardness and compressive strength with 24% lower density as compared with SKD11. Improved wear resistance of the TiC-SKD11 composite originates from uniformly reinforced TiC having strong interfacial bonding strength between TiC/SKD11 interface.

Improvement of Electrical Conductivity of Carbon-Fiber Reinforced Plastics by Nano-particles Coating (나노입자 코팅 탄소섬유 강화 복합재료의 전기전도도 향상)

  • Seo, Seong-Wook;Ha, Min-Seok;Kwon, Oh-Yang;Cho, Heung-Soap
    • Composites Research
    • /
    • v.23 no.6
    • /
    • pp.1-6
    • /
    • 2010
  • The electrical conductivity of carbon-fiber reinforced plastics (CFRP's) has been improved by indium-tin oxide (ITO) nano-particle coating on carbon fibers for the purpose of lightning strike protection of composite fuselage skins. ITO nano-particles were coated on the surface of carbon fibers by spraying the colloidal suspension with 10~40% ITO content. The electrical conductivity of the CFRP has been increased more than three times after ITO coating, comparable to or higher than that of B-787 composite fuselage skins with metal wire-meshes on the outer surface, without sacrificing the tensile property due to the existence of nano-particles at fiber-matrix interface. The damage area by the simulated lightning strike was also verified for different materials and conditions by using ultrasonic C-scan image. As the electrical conductivity of 40% nano-ITO coated sample surpass that of the B-787 sample, the damage area by lightning strike also appeared comparable to that of the materials currently employed for composite fuselage construction.

FeO, $TiH_2$, Carbon 원료분말을 이용한 Fe-TiC 나노 복합분말 제조 및 소결

  • An, Gi-Bong;Kim, Ji-Sun
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.10a
    • /
    • pp.26-26
    • /
    • 2011
  • Fe계 TiC 합금은 미량의 합금원소를 첨가시켜 경화능, 내식성, 내마모성 성질을 개선한 특수 공구용 재료로서 현재 절삭, 내마모성, 광산, 금형재료 등의 분야에 널리 사용되고 있다. 금속과 세라믹의 복합재료인 초경합금은 비열처리용 공구강으로 WC, TiC 등의 4, 5, 6족 금속탄화물에 Co, Ni, Fe등의 철족이 결합금속으로 소결한 복합재료로 WC-Co계 초경합금이 주종을 이루고 있으나, 전략 소재로서 고가인 Co 원료를 대체하기 위한 재료로서 초경재료의 고경도와 공구강의 경제성 및 가공성의 장점을 이용한 Fe-TiC계 초경합금의 연구가 다양하게 진행되고 있다. 본 연구에서는 Fe기지에 서브마이크론 크기의 미세한 TiC 입자가 균일하게 분산된 Fe-TiC 복합분말을 경제적으로 제조하기 위해 순수한 Fe, Ti 원료분말에 비해 단가가 낮고 미세 분쇄가 용이한 FeO, $TiH_2$ 분말을 고에너지 밀링 후 반응 열처리 시키는 유사 기계화학적 공정을 시도하였다. 조성비 Fe-30wt%TiC 복합분말을 제조하기위해 마이크론(micron) 크기의 FeO, $TiH_2$, C 분말을 사용하였고, 1단계로 FeO와 C을 고에너지 밀링으로 혼합 후 반응시켜 환원시키는 공정과 2단계로 이렇게 환원된 분말과 TiH2를 고에너지 밀링으로 다시 혼합, 분쇄한 후 반응열처리 하는 두 단계 공정을 사용하였다. FeO의 환원 단계에서는 $700{\sim}1,000^{\circ}C$ 온도 범위에서 1시간 유지하였고, 고에너지 밀링 시 밀링시간, 회전속도를 변수로 두고 실험하였다. 환원된 분말은 수평관상로를 이용해 아르곤분위기에서 $1,000{\sim}1300^{\circ}C$까지 1시간 유지하여 반응열처리시켜 Fe-TiC 복합분말을 제조하였다. 준비된 복합분말을 XRD와 FE-SEM, EDS, 입도분석기 (LPSA) 등을 이용해 분말의 형태와 특성, 상, 조성, 입도, 분산도 등을 조사하였다. 제조된 Fe-TiC 나노복합분말을 방전플라즈마소결(SPS) 과 상압소결 실험을 진행하였다. Fe-TiC 복합분말 제조공정의 첫 번째 단계인 FeO의 환원반응은 $800^{\circ}C$이상의 온도에서 Fe로 환원이 진행됨을 확인하였다. 두 번째 단계인 반응열처리공정에서는 $1,000^{\circ}C$ 이상에서 TiC가 형성됨을 XRD 상분석을 통해 확인할 수 있었고, $1,100^{\circ}C$ 이상의 온도에서 반응열처리를 했을 때 XRD 분석결과와 산소 조성 분석 결과로부터 반응의 완결성과 순도에서 최적 온도 조건임을 확인하였다. 온도를 $1,300^{\circ}C$로 증가시킬 경우 반응의 완결성에 큰 변화가 없는 반면 분말입자간의 목형성이 일어나 가소결 되는 것을 FE-SEM을 통해 관찰하였다. 또한 최적조건으로 제조된 Fe-TiC 복합분말의 입도분석과 FE-SEM/EDS 관찰/분석을 시행한 결과 평균 입도 0.6 ${\mu}m$의 미세한 Fe-TiC 복합분말 내에 Fe분말 주변과 내부에 나노크기의 TiC입자가 균일하게 분산되어 존재하는 것을 확인하였다.

  • PDF

Wetting improvement of SiC/Al Metal Matrix Composite by Cu Surface Treatment (보강재에 도금된 Cu층이 Al/SiC복합재료의 젖음성에 미치는 영향)

  • Lee, Gyeong-Gu;Jo, Gyu-Jong;Lee, Do-Jae
    • Korean Journal of Materials Research
    • /
    • v.11 no.5
    • /
    • pp.398-404
    • /
    • 2001
  • Effects of coating treatment of metallic Cu film on SiC for Al/SiC composite were studied. The Copper was deposited on SiC by electroless plating method. Al/sic composite was fabricated at temperature range of $670^{\circ}C$ to 90$0^{\circ}C$ under vacuum atmosphere. The wetting behavior of Al/SiC composite were analysed by SEM and XRD. The coating treatment on SiC improved wettability of Al melt on SiC considerably comparing to the non coated SiC. This improved wettability seems strongly concerned to the increase of chemical reactivity between coated layer and Al matrix. The improvement of wettability of Al melt on the Cu coated SiC was closely related to in the initial stage of reaction. The metallic film played an important role in reducing the interfacial free energy and breaking down the aluminum oxide film through the reaction with Al melt. The wetting behavior of the as-received SiC with Al melt was not uniform, indicated by the contact angles from less than $97^{\circ}$to more than $97^{\circ}$.

  • PDF

Microstructure and Mechanical Properties of Amorphous Matrix Composite Reinforced with Tungsten Porous Foam (텅스텐 다공성폼 강화 Zr계 비정질 기지 복합재료의 미세조직과 기계적 성질)

  • Son, Chang-Young;Lee, Sang-Bok;Lee, Sang-Kwan;Kim, Choongnyun Paul;Lee, Sunghak
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.2
    • /
    • pp.109-115
    • /
    • 2010
  • In the present study, a Zr-based amorphous alloy matrix composite reinforced with tungsten porous foam was fabricated without pores or defects by liquid pressing process, and its microstructures and mechanical properties were investigated. About 69 vol.% of tungsten foam was homogeneously distributed inside the amorphous matrix, although the matrix of the composite contained a small amount of crystalline phases. The compressive test results indicate that the composite was not fractured at one time after reaching the maximum compressive strength, but showed considerable plastic strain as the compressive load was sustained by tungsten foam. The tungsten foam greatly improved the strength (2764 MPa) and ductility (39.4%) of the composite by homogeneously dispersing the stress applied to the matrix. This was because the tungsten foam and matrix were simultaneously deformed without showing anisotropic deformation due to the excellent bonding of tungsten/matrix interfaces. These findings suggest that the liquid pressing process is useful for the development of amorphous matrix composites with improved strength and ductility.

Preparation of Nanocomposite Metal Powders in Metal-Carbon System by Mechanical Alloying Process (기계적 합금화 방법에 의한 금속-카본계에서의 나노복합금속분말의 제조)

  • Kim, Hyun-Seung;Lee, Kwang-Min
    • Korean Journal of Materials Research
    • /
    • v.8 no.4
    • /
    • pp.328-336
    • /
    • 1998
  • In metal-carbon system with no mutual solubility between matrix and alloying elements as solid or liquid phases, Cu-C-X nanocomposite metal powders were prepared by high energy ball milling for solid-lubricating bronze bearings. Elemental powder mixtures of Cu-lOwt.%C- 5wt. %Fe and Cu- lOwt. %C- 5wt. %Al were mechanically alloyed with an attritor in an argon atmosphere, and then microstructural evolution of the Cu-C-X nanocomposite metal powders was examined. It has been found that after 10 hours of MA, the approximately 10$\mu\textrm{m}$ sized Cu-C- X nanocomposite metal powders can be produced in both compositions. Morphological characteristics and microstructural evolution of the Cu-C-X powders have shown a similar MA procedure compared to those of metal-metal system. As a result of X - ray diffraction analysis, diffraction peaks of Cu and C were broaden and peak intensities were decreased as a function of MA time. Especially, the gradual disappearance of C peaks in the X- ray spectra is proved to be due to the lower atomic scattering factor of C. The calculated Cu crystallite sizes in Cu- C- X nanocomposite metal powders by Williamson- Hall equation were about lOnm size, on the other hand, the observed ones by TEM were in the range of 10 to 30nm.

  • PDF

A Study on Microstructure and Mechanical Properties of TiC/Steel Composites Fabricated by Powder Metallurgy Process (분말야금공정으로 제조된 TiC/steel 금속복합재료의 미세조직 및 기계적 물성 연구)

  • Lee, Jihye;Cho, Seungchan;Kwon, Hansang;Lee, Sang-Kwan;Lee, Sang-Bok;Kim, Daeha;Kim, Junghwan
    • Composites Research
    • /
    • v.34 no.5
    • /
    • pp.311-316
    • /
    • 2021
  • In this study, TiC/steel metal matrix composites were fabricated by powder metallurgy process using Fealloy powders with 3 wt.% Cr and 10 wt.% Cr, respectively, as matrix material. Subsequently, the composite samples were heat treated by the annealing and quenching-tempering(Q-T), respectively, to understand the effect of heat treatment on the mechanical properties of the composites. The correlation between microstructure and structural strength depending on the chromium content and the heat treatment conditions was studied through tensile, compressive, and transverse rupture test and microstructural analysis. In the case of TiC/steel composite containing 10 wt.% Cr, the tensile strength and transverse rupture strength at room temperature were significantly lowered by the influence of coarse chromium carbide formed at the TiC/steel interface. On the other hand, both TiC/steel composites containing 3 wt.% Cr and 10 wt.% Cr showed much higher compressive strength of about 4 GP after quenching-tempering compared to the annealed specimens regardless of the presence of the chromium carbide.

Fabrication and Fracture Properties of Alumina Matrix Composites Reinforced with Carbon Nanotubes (Carbon Nanotube로 강화된 알루미나 기지 복합재료의 제조 및 파괴특성)

  • Kim, Sung Wan;Chung, Won Sub;Sohn, Kee-Sun;Son, Chang-Young;Lee, Sunghak
    • Korean Journal of Metals and Materials
    • /
    • v.47 no.1
    • /
    • pp.50-58
    • /
    • 2009
  • In this study, alumina matrix composites reinforced with carbon nanotubes (CNTs) were fabricated by ultrasonic dispersion, ball milling, mixing, compaction, and sintering processes, and their relative density, electrical resistance, hardness, flexure strength, and fracture toughness were evaluated. 0~3 vol.% of CNTs were relatively homogeneously dispersed in the composites in spite of the existence of some pores. The three-point bending test results indicated that the flexure strength increased with increasing volume fraction of CNTs, and reached the maximum when the CNT fraction was 1.5 vol.%. The fracture toughness increased as the CNT fraction increased, and the fracture toughness of the composite containing 3 vol.% of CNTs was higher by 40% than that of the monolithic alumina. According to observation of the crack propagation path after the indentation fracture test, a new toughening mechanism of grain interface bridging-induced CNT bridging was suggested to explain the improvement of fracture toughness in the alumina matrix composites reinforced with CNTs.

A Study on Bonding Process for Improvement of Adhesion Properties Between CFRP-Metal Dual Materials (CFRP/금속간 접합력 강화를 위한 접합공정 연구)

  • Kwon, Dong-Jun;Park, Sung-Min;Park, Joung-Man;Kwon, Il-Jun
    • Composites Research
    • /
    • v.30 no.6
    • /
    • pp.416-421
    • /
    • 2017
  • The structural adhesive have been manufactured for improvement of bonding process between CFRP and metal. The optimal condition for bonding process were investigated by evaluating the lap shear strength with amount of adhesive and curing time and the surface treatment of the CFRP. To confirm proper adhesion conditions, the fracture sections between CFRP and metal was observed using reflection microscope. Not only the improvement of the adhesion condition was important, but surface treatment on CFRP was also important. The optimal curing temperature was at $180^{\circ}C$ for 20 minutes. The improvement for adhesive property was confirmed After surface treatment on CFRP. The optimal amount of structural adhesive for bonding between CFRP and metal was $1.5{\times}10^{-3}g/mm^2$. Through the optimization of bonding process, the improvement of mechanical property over 10% is confirmed in comparison with existing adhesive.

Manufacture and Mechanical Properties of $ABO_w/AC4CH$ Composite Material ($ABO_w/AC4CH$복합재료의 제조 및 기계적 특성)

  • 허선철;박원조;허정원
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.9 no.5
    • /
    • pp.188-194
    • /
    • 2001
  • Metal matrix composites with whisker reinforcements have significant potential for demanding mechanical applications including defense, aerospace, and automotive industries. Especially, metal matrix composites, which are reinforced with aluminum borate whisker, have been used for the part of piston head in automobile because of good specific strength and wear resistance. Aluminum alloy-based metal matrix composites with whisker reinforcements have been produced using squeeze casting method, which is kind of an infiltration method. In this study, AC4CH-based metal matrix composites with $Al_{18}B$_4$O_{33}$ reinforcement have been produced using squeeze casting method, after T6 heat treatment, we evaluated mechanical properties of matrix and MMC composite were evaluated.