• Title/Summary/Keyword: 관통속도

Search Result 98, Processing Time 0.024 seconds

High-Velocity Impact Experiment on Impact Resistance of Steel Fiber-Reinforced Concrete Panels with Wire Mesh (와이어매쉬와 강섬유로 보강된 콘크리트 패널의 내충격성 규명을 위한 고속충격실험)

  • Kim, Sang-Hee;Hong, Sung-Gul;Yun, Hyun-Do;Kim, Gyu-Yong;Kang, Thomas H.K.
    • Journal of the Korea Concrete Institute
    • /
    • v.27 no.2
    • /
    • pp.103-113
    • /
    • 2015
  • This paper studies impact performance of wire-mesh and steel fiber-reinforced concrete based on high-velocity impact experiments using hard spherical balls. In this experimental study, panel specimens were tested with various parameters such as steel fiber volume fraction, presence/absence of wire mesh, panel thickness, impact velocity, and aggregate size for the comparison of impact resistance performance for each specimen. While improvement of the impact resistance for reducing the penetration depth is barely affected with steel fiber volume fraction, the impact resistance to scabbing and perforation is improved substantially. This was due to the fact that the steel fiber had bridging effects in concrete matrix. The wire mesh helped minimizing the crater diameter of front and back face and enhanced the impact resistance to scabbing and perforation; however, the wire mesh did not affect the penetration depth. The wire mesh also reduced the bending deformation of the specimen with wire mesh, though some specimens had splitting bond failure on the rear face. Additionally, use of 20 mm aggregates is superior to 8 mm aggregates in terms of penetration depth, but for reducing the crater diameter on front and back faces, the use of 8 mm aggregates would be more efficient.

Mass transfer Characteristic during Osmotic Dehydration of Ginger and Its Effect on Quality (생강 삼투압 건조 시 물질이동 특성과 품질에 미치는 효과)

  • Kim, Myung-Hwan
    • Applied Biological Chemistry
    • /
    • v.41 no.5
    • /
    • pp.372-376
    • /
    • 1998
  • Internal mass transfer during osmotic dehydration of gingers in sugar solution was examined as a function of concentration, temperature and immersion time of those solutions using moisture loss, sugar gain, molality and rate parameter. Influence of osmotic dehydration on browning reaction and texture properties of air dried rehydrated was also evaluated. Increasing the concentration and temperature of sugar solutions increased moisture loss, sugar gain, molality and rate parameter. Water loss and sugar gain were rapid in the first 3 min and then changed gentle slope. Moisture loss during osmotic dehydration using a sugar solution $(60\;Brix,\;80^{\circ}C)$ with 18 min immersion time was 40.05 g moisture/100 g wet ginger which was 52% reduction of initial moisture content in ginger (83.02%, wet basis). The changes of rate parameter were more affected by temperature than by concentration of sugar solution. Minimum browning degree (O.D.=0.027) was carried out by osmotic dehydration in sugar solution $(40\;or\;50\;Brix,\;80^{\circ}C)$ with 15 min immersion time compared to control (O.D.=0.132). Influence of osmotic dehydration on puncture forces of 3 min rehydrated ginger in boiling water were $22{\sim}34%$ of reduction, while blanching treatment had not affected compared to those of control.

  • PDF

Ballistic Protection Effectiveness Analysis of Armor Plates with Various Incident angles using Small Caliber Live Fire Test (소화기 실사격 실험 기반의 장갑 재질에 따른 입사각도별 방호성능 효과분석)

  • Lee, Gun-woo;Baek, Jang-Woon;Lee, Byoung-hwak;Kim, Jin-young;Kim, Jong-Hwan
    • Journal of the Korea Society for Simulation
    • /
    • v.30 no.1
    • /
    • pp.55-63
    • /
    • 2021
  • As a study on ballistic protection performance of a weapon system that is used in combat simulation, this paper aims to propose an improvement effect of the ballistic protection performance varying with incident angle of a bullet. For this, live-fire ballistic tests were performed to determine either complete penetration(CP) and partial penetration(PP) of three types of general armor plates made of uniformly rolled steel plates against a small caliber threat using 5.45 mm bullets with various speed. The major test parameter was the material of the weapon system and incident angle of the bullet with the target. Further, to quantitatively analyze the ballistic protection performance, three existing measurement methods were used for ballistic limit velocity. The test results showed that the ballistic protection performance with the incident angle of 30 degrees was 4% to 14% varying with the material of the armor plates greater than that of 0 degrees, which was approximately 1.1 times the performance improvement on average when compared to the conventional angle of incidence of the 0 degree. Those test results are expected to contribute to developing a more realistic combat simulation addressing the parameter improving the ballistic protection performance of an armor plate.

Experimental Study of Wireless Communication System by Surface wave Communication through Confined Spaces on Vessels (선박 밀폐 공간 무선통신 구현을 위한 표면파 통신의 선박 활용 연구)

  • Jin-Woo Kong;Suk-Gun Song;Hak-Sun Kim;Bu-Young Kim;Woo-Seong Shim
    • Proceedings of the Korean Institute of Navigation and Port Research Conference
    • /
    • 2021.11a
    • /
    • pp.127-128
    • /
    • 2021
  • This study suggests surface wave communication, which uses a metal surface as a medium, to provide wireless communication in the extreme environment due to surrounding metal materials on vessels. The test was conducted on a G/T 265 tons tug boat, and to confirm the possibility of surface wave communication between a bridge and each designated space in the boat. As a result, the transmission speed was 13Mbps in average. For the test case between the bridge and the engine room, transmission speed was 4.3Mbps while the engine was on, and 1.2Mbps during sailing. It was able to be overcome by partially changing the equipment installation location. Surface wave communication in a bow storage, a fully enclosed space, had 8Mbps better transmission speed than wireless communication; this confirmed the superiority of surface wave communication in confined spaces on a vessel. Additional surface wave generators were designed and applied to resolve the paint issue. It is expected to apply surface wave communication to implement the new wireless solution on vessels.

  • PDF

Development of Eddy Current Testing System using Magnetic Saturation in ferromagnetic Materials (자기포화를 이용한 강자성체의 와전류검사장비 개발)

  • Sung, Je-Joong;Shin, Young-Hoon;Um, Tae-Gun;Kang, Seok-Chul;Kweon, Young-Ho;Suh, Dong-Man
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.23 no.4
    • /
    • pp.356-363
    • /
    • 2003
  • An eddy current testing system was developed for detection of flaws in the ferromagnetic steel tubes. Because the eddy current signals from the ferromagnetic steel tubes could be distorted easily due to an irregularity of magnetic permeability, magnetic saturation is required to suppress this variation of magnetic fields. A magnetic saturation probe with the Hemholtz coil was designed for the inspection of the steel tubes. The bandwidth pass filters were adapted to minimize the noise from the DC magnetization. When using the designed test probe, the flaw signals could be discriminated from the noise. The system was tested at the production line and showed a capability of detecting flaws, like a drilled hole of the diameter of 2.0mm at the moving speed of 1m/sec.

An Investigation on the Spray Characteristics of DME with Variation of Nozzle Holes Diameter using the Common Rail Fuel Injection System (인젝터 노즐 홀 직경의 변화에 따른 DME 커먼레일 연료 분사 시스템의 분무 특성에 관한 연구 II)

  • Lee, Sejun;Lim, Ocktaeck
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.21 no.4
    • /
    • pp.1-7
    • /
    • 2013
  • DME spray characteristics were investigated about varied ambient pressure and fuel injection pressure using the DME common rail fuel injection system when the nozzle holes diameter is varied. The common rail fuel injection system with DME cooling system was used since DME has properties of compressibility and vaporization in atmospheric temperature. The fuel injection quantity and spray characteristics were measured. The spray analysis parameters were spray shape, penetration length, and spray angle at six nozzle holes. Three types of injector were used, the nozzle holes diameter were 0.166 mm (Injector 1), 0.250 mm (Injector 2), and 0.250 mm with enlargement of orifice hole from 0.6 mm to 1.0 mm (Injector 3). The fuel injection pressure was varied by 5MPa from 35 to 70MPa when the ambient pressure was varied 0, 2.5, and 5MPa. When using Injector 3 in comparison to the others, the DME injection quantity was increased 1.69 ~ 2.02 times. Through this, it had the similar low heat value with diesel which was injected Injector 1. Among three types of injector, Injector 3 had the fastest development velocity of penetration length. In case of spray angle, Injector 2 had the largest spray angle. Through these results, only the way enlargement the nozzle holes diameter is not the solution of DME low heat value problem.

Cu Filling process of Through-Si-Via(TSV) with Single Additive (단일 첨가액을 이용한 Cu Through-Si-Via(TSV) 충진 공정 연구)

  • Jin, Sang-Hyeon;Lee, Jin-Hyeon;Yu, Bong-Yeong
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2016.11a
    • /
    • pp.128-128
    • /
    • 2016
  • Cu 배선폭 미세화 기술은 반도체 디바이스의 성능 향상을 위한 핵심 기술이다. 현재 배선 기술은 lithography, deposition, planarization등 종합적인 공정 기술의 발전에 따라 10x nm scale까지 감소하였다. 하지만 지속적인 feature size 감소를 위하여 요구되는 높은 공정 기술 및 비용과 배선폭 미세화로 인한 재료의 물리적 한계로 인하여 배선폭 미세화를 통한 성능의 향상에는 한계가 있다. 배선폭 미세화를 통한 2차원적인 집적도 향상과는 별개로 chip들의 3차원 적층을 통하여 반도체 디바이스의 성능 향상이 가능하다. 칩들의 3차원 적층을 위해서는 별도의 3차원 배선 기술이 요구되는데, TSV(through-Si-via)방식은 Si기판을 관통하는 via를 통하여 chip간의 전기신호 교환이 최단거리에서 이루어지는 가장 진보된 형태의 3차원 배선 기술이다. Si 기판에 $50{\mu}m$이상 깊이의 via 및 seed layer를 형성 한 후 습식전해증착법을 이용하여 Cu 배선이 이루어지는데, via 내부 Cu ion 공급 한계로 인하여 일반적인 공정으로는 void와 같은 defect가 형성되어 배선 신뢰성에 문제를 발생시킨다. 이를 해결하기 위해 각종 유기 첨가제가 사용되는데, suppressor를 사용하여 Si 기판 상층부와 via 측면벽의 Cu 증착을 억제하고, accelerator를 사용하여 via 바닥면의 Cu 성장속도를 증가시켜 bottom-up TSV filling을 유도하는 방식이 일반적이다. 이론적으로, Bottom-up TSV filling은 sample 전체에서 Cu 성장을 억제하는 suppressor가 via bottom의 강한 potential로 인하여 국부적 탈착되고 via bottom에서만 Cu가 증착되어 되어 이루어지므로, accelerator가 없이도 void-free TSV filling이 가능하다. Accelerator가 Suppressor를 치환하여 오히려 bottom-up TSV filling을 방해한다는 보고도 있었다. 본 연구에서는 유기 첨가제의 치환으로 인한 TSV filling performance 저하를 방지하고, 유기 첨가제 조성을 단순화하여 용액 관리가 용이하도록 하기 위하여 suppressor만을 이용한 TSV filling 연구를 진행하였다. 먼저, suppressor의 흡착, 탈착 특성을 이해하기 위한 연구가 진행되었고, 이를 바탕으로 suppressor만을 이용한 bottom-up Cu TSV filling이 진행되었다. 최종적으로 $60{\mu}m$ 깊이의 TSV를 1000초 내에 void-free filling하였다.

  • PDF

Evaluation of Ballistic Performance of Ceramic-Tile-Inserted Metal Block (세라믹 타일이 삽입된 금속 블록의 최적 방호구조 연구)

  • Lee, Seunghwan;Lee, Minhyung
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.40 no.3
    • /
    • pp.297-304
    • /
    • 2016
  • A numerical simulation has been performed for the penetration of a long-rod penetrator into a metal block (ceramic-tile-inserted 4340-steel plate). The impact velocity is 1.5km/s at a normal incidence angle. The first two validations are conducted for a semi-infinite block measuring the depth of penetration (DOP). The material model of ceramic is the JH-2 (Johnson-Holmquist) model. The predicted DOP values are in close agreement with the experimental data. Then, the primary simulation is performed by varying the position of the confined ceramic tile for three types of thickness of ceramic tile. The residual velocity, residual mass and residual kinetic energy of the long-rod are obtained from the simulation. Based on these predicted values, the trend of the ballistic performance of the protective structure is estimated. In addition, the mass efficiency is calculated in order to determine the performance of the ceramic-tile-inserted metal block. Finally, the optimum protective structure is identified.

Butt Weldability for SS400 Using Laser-Arc Hybrid Welding (레이저-아크 하이브리드 용접을 이용한 SS400의 맞대기 용접 특성)

  • Kim, Jong Do;Myoung, Gi Hoon;Park, In Duck
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.40 no.7
    • /
    • pp.667-672
    • /
    • 2016
  • This study presents results of an experimental investigation of the laser-arc, hybrid, butt welding process of SS400 structural steel. Welding parameters including laser power, welding current and speed were varied in order to obtain one-pass, full-penetration welds without defects. The conditions that resulted in optimal beads were identified. After welding, hardness measurements and microstructure observations were carried out in order to study weld properties. The mechanical properties of both the base material and welded specimen were compared based on the results of tensile strength measurements. The yield and tensile strengths were found to be similar.

Interfacial Reaction of Ag Bump/Cu Land Interface for B2it Flash Memory Card Substrate (B2it 플래시 메모리 카드용 기판의 Ag 범프/Cu 랜드 접합 계면반응)

  • Hong, Won-Sik;Cha, Sang-Suk
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.19 no.1
    • /
    • pp.67-73
    • /
    • 2012
  • After flash memory card(FMC) was manufactured by $B^2it$ process, interfacial reaction of silver bump with thermal stress was studied. To investigate bonding reliability of Ag bump, thermal shock and thermal stress tests were conducted and then examined on the crack between Cu land and Ag bump interface. Diffusion reaction of Ag bump/Cu land interface was analyzed using SEM, EDS and FIB. The Ag-Cu alloy layer due to the interfacial reaction was formed at the Ag/Cu interface. As the diffusivity of Ag ${\rightarrow}$ Cu is faster than Cu ${\rightarrow}$ Ag, a lot of (Cu, Ag) alloy layers were observed at the Cu layer than Ag. These alloy layers contributed to increase the Cu-Ag bonding strength and its reliability.