• Title/Summary/Keyword: 골재종류

Search Result 266, Processing Time 0.023 seconds

The pH Reduction of the Recycled Aggregate Originated from the Waste Concrete by the scCO2 Treatment (초임계 이산화탄소를 이용한 폐콘크리트 순환골재의 중성화)

  • Chung, Chul-woo;Lee, Minhee;Kim, Seon-ok;Kim, Jihyun
    • Economic and Environmental Geology
    • /
    • v.50 no.4
    • /
    • pp.257-266
    • /
    • 2017
  • Batch experiments were performed to develop the method for the pH reduction of recycled aggregate by using $scCO_2$ (supercritical $CO_2$), maintaining the pH of extraction water below 9.8. Three different aggregate types from a domestic company were used for the $scCO_2$-water-recycled aggregate reaction to investigate the low pH maintenance of aggregate during the reaction. Thirty five gram of recycled aggregate sample was mixed with 70 mL of distilled water in a Teflon beaker, which was fixed in a high pressurized stainless steel cell (150 mL of capacity). The inside of the cell was pressurized to 100 bar and each cell was located in an oven at $50^{\circ}C$ for 50 days and the pH and ion concentrations of water in the cell were measured at a different reaction time interval. The XRD and SEM-EDS analyses for the aggregate before and after the reaction were performed to identify the mineralogical change during the reaction. The extraction experiment for the aggregate was also conducted to investigate the pH change of extracted water by the $scCO_2$ treatment. The pH of the recycled aggregate without the $scCO_2$ treatment maintained over 12, but its pH dramatically decreased to below 7 after 1 hour reaction and maintained below 8 for 50 day reaction. Concentration of $Ca^{2+}$, $Si^{4+}$, $Mg^{2+}$ and $Na^+$ increased in water due to the $scCO_2$-water-recycled aggregate reaction and lots of secondary precipitates such as calcite, amorphous silicate, and hydroxide minerals were found by XRD and SEM-EDS analyses. The pH of extracted water from the recycled aggregates without the $scCO_2$ treatment maintained over 12, but the pH of extracted water with the $scCO_2$ treatment kept below 9 of pH for both of 50 day and 1 day treatment, suggesting that the recycled aggregate with the $scCO_2$ treatment can be reused in real construction sites.

An Experimental Study on the Mechanical Properties of Lightweight Aggregate Concrete subjected to Pre-stressed and Heating (사전재하 및 가열을 받은 경량골재콘크리트의 역학적 특성에 관한 실험적 연구)

  • Lee, Hyoung-Jun;Shin, Kyoung-Su;Lim, Chang-Hyuck;Koo, Kyung-Mo;Kim, Young-Sun;Kim, Gyu-Yong
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2009.05a
    • /
    • pp.361-362
    • /
    • 2009
  • In this study, measured properties(which is compressive strength, elastic modulus) of concrete by conditions(which is aggregate type, pre-stressed level) using normal aggregate and lightweight aggregate.

  • PDF

A Study on Compressive Strength Properties of Mortar Using Ceramic Bid as Fine Aggregate (세라믹비드를 잔골재로 대체한 모르타르의 압축강도 특성)

  • Kim, Ju-Ho;Jeon, Chan-Ki;Park, Jong-Pil;Lee, Jae-Seong;Jeon, In-Kyu
    • Proceedings of the Korean Society of Disaster Information Conference
    • /
    • 2015.11a
    • /
    • pp.132-133
    • /
    • 2015
  • 이 논문은 세라믹 비드를 일반 모르타르의 잔골재로 대체하여 사용했을 경우 모르타르의 압축강도에 변화를 확인하고자 수행하였다. 잔골재를 대체할 세라믹 비드의 입도분포를 확인하였고, 세라믹 비드의 잔골재 대체율을 10%, 20%, 30%로 설정하고 2가지 종류의 세라믹 비드를 이용하여 시험체를 제작하여 7일, 14일 28일의 압축강도를 측정하였다.

  • PDF

Durability of Mortar Matrix Replaced with Recycled Fine Aggregates (순환골재(循環骨材)를 혼입(混入)한 모르타르 경화체(硬化體)의 내구(耐久) 특성(特性))

  • Kim, Jong-Pil;Lee, Seung-Tae;Jung, Ho-Seop;Park, Kwang-Pil;Kim, Seong-Soo
    • Resources Recycling
    • /
    • v.16 no.6
    • /
    • pp.20-27
    • /
    • 2007
  • This paper presents a detailed experimental study on the durability properties of mortar matrix made with two kind of recycled fine aggregates(RAA, RAB) and five replacement levels (0, 25, 40, 75 and 100) of the recycled fine aggregates as a partial replacement of natural fine aggregate (NA). The durability properties of mortar matrix was evaluated using compressive strength, chloride ion ingress, sulfate attack and carbonation. The test results indicated that the water absorption and Adhered mortar of the recycled fine aggregate was a major factor controlling durability properties. Hereafter, when using built recycled fine aggregate is expected, appropriate removal Adhered mortar and reasonable replacement ratio of recycled fine aggregates was 25% weight of cement are advised to apply to the concrete materials.

Experimental Study on Thermal Conductivity of Concrete (콘크리트의 열전도율에 관한 실험적 연구)

  • 김국한;전상은;방기성;김진근
    • Journal of the Korea Concrete Institute
    • /
    • v.13 no.4
    • /
    • pp.305-313
    • /
    • 2001
  • Conductivity is an important thermal property which governs heat transfer in a solid medium. Generally, the determination of conductivity in concrete is very difficult, because concrete is a heterogeneous material composed of cement, water, aggregate, et cetera and time dependent material of which properties change with curing age. In this study, influencing factors on thermal conductivity of concrete are quantitatively investigated by QTM-D3, a conductivity tester developed in Japan. Then, a prediction equation of thermal conductivity of concrete is suggested from the regression analysis of test results. To consider the factors influencing thermal conductivity of concrete, mortar, and cement paste, seven testing variables (age, amount of cement, types of admixtures, amount of coarse aggregate, fine aggregate ratio, temperature, and humidity condition) of the specimens are used. According to the experimental results, the amount of coarse aggregate and humidity condition of specimen are the main factors affecting the conductivity of concrete. Meanwhile, the conductivity of mortar and cement paste is strongly affected by the amount of cement and types of admixtures. However, the curing age has minor effect on the conductivity variation. Finally, the prediction formula of concrete conductivity as a function of aggregate amount, fine aggregate ratio, specimen temperature, and humidity condition is developed.

A Study on the Nano Silica-Sol Coating for Improving Performance of Recycled Aggregate (순환골재의 성능향상을 위한 나노실리카졸의 코팅에 관한 연구)

  • Kim, Seong-Soo;Lee, Jeong-Bae;Ko, Ji-Soo;Kim, Il-Kon
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.17 no.4
    • /
    • pp.84-90
    • /
    • 2013
  • In this study we propose an effective method, Coating processing methods, which can improve the quality of recycled aggregate relatively easily without new equipment investment and complex treatment process and verify the improved effect using the devised method, Coating processing methods. To attain the research aim we used adequately diluted silicate solution for coating and carried out several property valuation for twelve types of material with different coating method. Also we formed concrete with coated aggregates which showed the best property. In conclusion the aggregates with the method of repeated impregnation in the silicate and drying showed the most excellent quality while other coating methods also resulted in an improvement of aggregate quality but failed to meet the KS Standard. Lastly with the optimal material we could obtain the approved compressive strength from the concrete allowing it to be utilized for road facility of which standard compressive strength of design is under 24MPa.

Analysis of 2019 Domestic Aggregate Production in Korea (I) (2019년도 국내 골재 수급 분석 (I))

  • Hong, Sei Sun;Lee, Jin Young
    • Economic and Environmental Geology
    • /
    • v.53 no.6
    • /
    • pp.755-769
    • /
    • 2020
  • In 2019, about 134 million ㎥ of aggregate was produced in an estimated 880 quarries and pits in 17 metropolitan governments. Leading producing metropolitan cities were Gyeonggi-do, Gyeongsangnam-do, Chungcheongbuk-do, Gangwon-do, Gyeongsangbuk- do, Chungcheongnam-do, in order decreasing volume, which together accounted for about 71% of total product. Of the total domestic aggregates produced in 2019, about 31 % was sand and about 69% was gravel. It estimated that of the 134 million ㎥ of aggregates in Korea in 2019, about 50.3% was produced by screening crushed aggregate by 41.4% by forest aggregate, 3.3% by land aggregate, 1.7% by sea aggregate and 1.7% by washing each other, and 0.7% by river aggregate. This indicates that screening crushed aggregate and forest aggregate are the main producers of domestic aggregates. The most crushed and forest aggregate was extracted at the Gyeonggi-do and Gyeongsangnam-do, respectively. Land aggregate was mainly extracted at Gyeongsangbuk-do and Gangwon-do. Therefore, in the future supply and demand of aggregate resources, it is judged that there should be a primary policy direction for screening crushed and forest aggregate.

A Comparative Study on the Quality of Recycled Aggregate for Concrete by Crushing Method (파쇄 방법에 따른 콘크리트용 순환골재의 품질 비교 연구)

  • Choi, Won-Young;Lee, Sae-Hyun;Kim, Seoung-Hwan
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.2
    • /
    • pp.121-129
    • /
    • 2017
  • In this study, the quality of recycled aggregate for concrete was investigated as the number of recycled aggregate crushing cycles, grinder and crusher, peeling and crushing. First, the quality of density, absorption ratio and solid content was improved as the separation distance decreased and the number of crushing increased, depending on the number of crushing of recycled aggregate and the distance between mantle and cone cave. The quality of density, absorption ratio and solid content was improved as the wire mesh used in striking plate and the number of hammers increased, depending on the type of striking plate and the number of hammers.

Properties of Concrete using Surface Treatment Recycled Aggregates and Steel Fibers (강섬유보강(鋼纖維補强) 표면처리(表面處理) 순환골재(循環骨材)콘크리트의 특성(特性))

  • Bae, Ju-Seong;Kim, Nam-Wook
    • Resources Recycling
    • /
    • v.20 no.1
    • /
    • pp.46-53
    • /
    • 2011
  • The recycled aggregate produced from the waste concrete have the disadvantages in the quality for the natural aggregate. Therefore, in order to reuse the recycled aggregate widely it is a previous subject to improve the quality of recycled aggregate. We deduced the more effective surface treatment method using the colloidal silica solution for quality improvement of recycled aggregate. This study aimed to verify the influences of the deduced surface treatment method and the reinforcement of steel fiber to the properties of concrete. For this object, we inquired into the results of the strengths and the flexural failure tests for the five kinds of concrete specimens.

Properties of Fresh Concrete with Recycled Coarse and Fine Aggregates (순환(循環)굵은/잔골재(骨材)를 사용한 굳지 않은 콘크리트의 특성(特性))

  • Choi, Ki-Sun;You, Young-Chan;Kim, Keung-Hwan;Lee, Do-Heun
    • Resources Recycling
    • /
    • v.18 no.3
    • /
    • pp.20-26
    • /
    • 2009
  • The objective of this study is to investigate the properties of fresh concrete with recycled coarse and fine aggregates. Four different kinds of aggregate with natural, recycled aggregates were prepared. The concrete mixtures were produced with test parameters of replacement ratio of recycled aggregate. The properties of the fresh concrete were measured by means of slump and air content according to elapsed time. Quality control method to maintain the constant total mixing water for recycled aggregate concrete was suggested. The all concrete mixtures were produced with approximately the same slump on the job site after an hour. Test results indicated that compressive strength of concrete with constant slump is not affected by the replacement ratio of recycled aggregate. Also the practical way for the quality control of recycled aggregate concrete is to maintain the constant total mixing water.