• Title/Summary/Keyword: 고압축비

Search Result 506, Processing Time 0.025 seconds

An Experimental Study on Structural Behavior of High-strength Concrete Members with Compressive Strength of 80 MPa Subjected to Flexure (휨을 받는 압축강도 80 MPa 수준의 고강도 콘크리트 부재의 구조거동 실험 연구)

  • Yang, In-Hwan;Hwang, Chul-Sung;Kim, Kyoung-Chul;Joh, Chang-Bin
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.21 no.4
    • /
    • pp.1-12
    • /
    • 2017
  • This paper concerns the structural behavior of high-strength concrete beams with compressive strength of 80 MPa subjected to flexure. Main test variables were nominal yielding strength of longitudinal rebar including normal strength rebar(SD 400) and high strength rebar(SD 600), reinforcement ratio from 0.98 to 1.58% and beam section size with $200{\times}250$, $200{\times}300mm$. The nine beams were cast and tested under flexure. The study investigated ultimate flexural strength, load-deflection relationship, crack patterns, failure patterns and ductility of the test beams. Test results indicate that when rebar ratio increased flexural strength increased and ductility decreased. In addition, the number of cracks increased and the crack width decreased as the reinforcement ratio increased. The yield strength of rebar did not affect significantly load-crack width relationship. Nonlinear analysis of test beams was performed and then test results and analytical results of ultimate load were compared. Analytical results of high-strength concrete beams overall underestimated flexural strength of test beams.

Flexural-Shear Behavior of Beam Members according to the Spacing of Stirrups and Tension Steel Ratio (스터럽간격과 인장철근비에 따른 고강도 콘크리트 보의 파괴거동)

  • Park, Hoon-Gyu;An, Young-Ki;Jang, Il-Young;Choi, Goh-Il
    • Journal of the Korea Concrete Institute
    • /
    • v.15 no.4
    • /
    • pp.513-521
    • /
    • 2003
  • Existing tests results have shown that confining the concrete compression region with closed stirrups improves the ductility and load-carrying capacity of beams. However, only few researchers have attempted to utilize the beneficial effects of the presence of these stirrups in design. This paper presents the result of experimental studies on the load-deflection behavior and the strengthening effect of laterally confined structural high-strength concrete beam members in which confinement stirrups have been introduced into the compression regions. Fifteen tests were conducted on full-scale beam specimens having concrete compressive strength of 41 MPa and 61 MPa. Different spacing of stirrups(0.25∼1.0d) and amount of tension steel($0.55{\sim}0.7{\rho}_b$) as major variables were investigated. And also, this study present an appropriate shear equation for decision of ultimate failure modes of high-strength concrete beams according to stirrup spacing. The equation is based on interaction between shear strength and displacement ductility. Prediction of failure mode from presented method and comparison with test results are also presenteded

New high-efficient universal code(BL-beta) proposal for com pressed data transferring of real-time IoT sensing or financia l transaction data (IoT 및 금융 거래 실시간 데이터 정보의 압축 전송을 위한 새로운 고효율 유니버설 코드(BL-beta) 제안)

  • Kim, Jung-Hoon
    • The Journal of Korea Institute of Information, Electronics, and Communication Technology
    • /
    • v.11 no.4
    • /
    • pp.421-429
    • /
    • 2018
  • While IoT device sensing data or financial transaction data is transmitted in real time, huge data traffic is generated in processing it. This huge data can be effectively compressed or transmitted using universal code, which is a real-time lossless compressor. In this paper, we propose our BL-beta code, which is newly developed universal code for compressing stock trading data, which the maximum range of measured values is difficult to predict and is generated within a relatively constant range over a very short period of time. For compressing real-time stock trading data, Compared with the fixed length bit transmission, the compression efficiency is at least 49.5% higher than that of the fixed length bit transmission, and the compression transmission performance is 16.6% better than the Exponential Golomb code.

Characteristics Strength of Silicasol-cement Grout Material for Ground Reinforcement (지반보강용 실리카졸 약액의 강도특성에 대한 연구)

  • Kim, Hyunki;Kim, Younghun;Chun, Byungsik
    • Journal of the Korean GEO-environmental Society
    • /
    • v.11 no.9
    • /
    • pp.47-53
    • /
    • 2010
  • This study was made on the fact that the compressive strength characteristic of the recently developed alkali silica-sol chemical grout material was examined, whose grout material used for this study was designed to understand its strength property through the uniaxial compressive strength test(homo-gel, sand-gel), permeability test, deflection strength test, etc. In order to compare with the engineering characteristics regarding alkali silica-sol grout material and sodium silicate grout material. The uniaxial compressive strength of silica-sol grout material was identified to be increased more than 3~5 times than sodium silicate grout material at the early stage(within 72 hours). When comparing with the uniaxial compressive strengths of Sand-gel and Homo-gel at the material age of 28 days in case of silica-sol grouting material the strength of Sand-gel was measured to be about 1.3 times higher than Homo-gel. In case of silica-sol, it is assumed to have the property to exert high strength when it is actually grouted into the ground. As a result of permeability test it is judged that it is possible to apply the silica-sol to the site in the place requiring the water cut-off as the silica-sol. As a result of testing the strength at the material age of 28 days of grouting-use silica-sol showed more than 3 times' difference than the sodium silicate grouting material.

Introduction of Numerical Simulation Techniques for High-Frequency Combustion Instabilities (고주파 연소불안정 예측을 위한 해석기술 개발 사례)

  • Kim, Seong-Ku;Joh, Miok;Han, Sanghoon;Choi, Hwan-Seok
    • Proceedings of the Korean Society of Propulsion Engineers Conference
    • /
    • 2017.05a
    • /
    • pp.68-77
    • /
    • 2017
  • High-frequency combustion instability results from a feedback coupling between the unsteady heat release rate and the acoustic waves formed resonantly in the combustion chamber. It can be modeled as thermoacoustic problems with various degrees of the assumptions and simplifications. This paper presents numerical analysis of self-excited combustion instabilities in a variable-length lean-premixed combustor and designs of passive control devices such as baffle and acoustic resonators in a framework of 3-D FEM Helmholtz solver. Nonlinear behaviors such as steep-fronted shock waves and a finite amplitude limit cycle are also investigated with a compressible flow simulation technique.

  • PDF

A Study on Isolation Performance of High Damping Rubber Bearing Through Shaking Table Test and Analysis (진동대 실험 및 해석을 통한 고감쇠 고무받침의 면진성능 연구)

  • Kim, Hu-Seung;Oh, Ju
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.17 no.5
    • /
    • pp.601-611
    • /
    • 2016
  • The research, development and use of seismic isolation systems have been increasing with the gradual development of structure safety assurance methods for earthquakes. The High Damping Rubber Bearing (HDRB), one type of seismic isolation system, is a Laminated Rubber Bearing using special High Damping Rubber. However, as its damping function is slightly lower than that of the Lead Rubber Bearing, a similar seismic isolation system, its utilization has not been high. However, the HDRB has a superior damping force to the Natural Rubber Bearing, which has similar materials and shapes, and the existing Lead Rubber Bearing has a maleficence problem in that it contains lead. Thus, studies on HDRBs that do not use lead have increased. In this study, a test targeting the HDRB was done to examine its various dependence properties, such as its compressive stress, frequency and repeated loading. To evaluate the HDRB's seismic performance in response to several earthquake waves, the shaking table test was performed and the results analyzed. The test used the downscaled bridge model and the HDRB was divided into seismic and non-seismic isolation. Consequently, when the HDRB was applied, the damping effect was higher in the non-seismic case. However, its responses on weak foundations, such as in Mexico City, represented increased shapes. Thus, its seismic isolator.

Experimental Study on the Properties of Strength of the No-Fines Concrete (No-Fines Concrete의 강도특성(强度特性)에 관(關)한 실험적(實驗的) 연구(硏究))

  • Kim, Seong Wan;Sung, Chan Yong;Min, Jeong Kie
    • Korean Journal of Agricultural Science
    • /
    • v.14 no.2
    • /
    • pp.373-383
    • /
    • 1987
  • No-fines concrete is concrete from which the fine aggregate fraction has been omitted. The concrete so formed, consisting only of coarse aggregate, cement, and water, has large voids uniformly distributed through its mass. This study was performed to obtain the basic data which can be applied to the use of no-fines concrete. The data was based on the properties of no-fines concrete depending upon various mixing ratios. The results obtained were summarized as follows. 1. Test result of the consistency, suitable water-cement ratio was increased with the increasing of mixing ratio. 2. At the suitable water-cement ratio, the highest strengths were showed. But it gradually was decreased with the increasing of mixing ratio and strengths are considerably lower than that of conventional portland cement concrete. 3. The relations between compressive and tensile strength were highly singnificant as a straight line shaped. The strength ratio was decreased with the increasing of mixing ratio and considerably lower than of conventional portland cement concrete. 4. Bulk density was decreased with the increasing of the mixing ratio, and was similar to that of the conventional portland cement concrete at mixing ratio 1:4. 5. The relations between strength and bulk density were highly significant as a straight line shaped. The decreasing ratio of strengths was higher than that of bulk density.

  • PDF

Experimental Study on the Evaluation of frost-Resistance of High-Strength Concrete Damaged by frost at Early Age in Cold Climates (동절기 초기재령에서 동해를 받은 고강도콘크리트의 내동해성 평가에 관한 실험적 연구)

  • 권영진
    • Journal of the Korea Concrete Institute
    • /
    • v.13 no.2
    • /
    • pp.139-145
    • /
    • 2001
  • One of ways to make high-strength concrete is for the mix contain particles graded down to the finest size : this is achieved by the use of fly ash, silica fume which fills the spaces between the cement particle and between the aggregate and the cement particles. And, the mix needs a sufficient workability. This is achieved by the use of a superplasticizer. This study is to investigate frost resistance of high-strength concrete at early age, with ratio of tensile strength and recovery of compressive strength, when high-strength concrete is placed in cold climates. According to this study, it is necessary to ensure 4 % of air content, 5 kgf/$\textrm{cm}^2$ of tensile strength, at least, for frost resistance of high-strength concrete at early age.

광미를 이용한 인공경량골재의 제조와 물리화학적 특성

  • 이종석;이현구;박영훈;김상중
    • Proceedings of the KSEEG Conference
    • /
    • 2003.04a
    • /
    • pp.169-171
    • /
    • 2003
  • 최근 환경문제가 대두됨에 따라 산업폐기물의 처리문제에 많은 관심과 연구가 진행되고 있다. 또한 현대의 콘크리트 구조물은 거대화, 고층화되어 그 중량이 계속 커지고 있으므로 구조물을 경량화 하려는 노력과 개발이 계속 진행되어 왔다. 구조물의 주재료로 사용되고 있는 콘크리트는 강도 및 내구성에 비해 비중이 크다는 결점을 가지고 있으므로 강하고 가벼운 고강도의 경량골재 콘크리트 개발이 행해져 왔다. (중략)

  • PDF

An Experimental Study on the Properties of Compressive Strength of Fly Ash Replaced Antiwash out Underwater Concrete Considering Marine Environment (해양환경을 고려한 플라이애쉬${\cdot}$수중 불분리 콘크리트의 압축강도에 관한 실험적 연구)

  • Kwon, Joong-Hyen;Jung, Hee-Hyo;Moon, Je-Kil
    • Magazine of the Korea Concrete Institute
    • /
    • v.11 no.2
    • /
    • pp.231-239
    • /
    • 1999
  • When the concrete is cast at the sea, there are lots of restrictions in the working process being different from in land, and the concrete is suffered from the physical and chemical action in terms of marine environment. The compressive strength was measured after antiwash out underwater concrete mixed with fly ash had been cast and cured in order to produce the endurable high performance concrete, and then its characteristic was discussed by comparing one cured in air with in fresh water, and the effect of fly ash usage under the properly controled sea water temperature of $15{\pm}3^{\circ}C$ was also covered. The present work showed that the proper usage of fly ash was obtained at the condition of around 10% of substituted binder weight under the structure required the early age strength, and at the condition of over 40% if considering its durability and economy.