Lightweight foamed concrete is a concrete which is lighter than conventional concree by
mixing ptetoamed foam in cement slurry. The objectives of this study are to develop
optimal prefoarneti lightweight foamed concrete with high lightness. high flowability and
enough strength fol special use of structural application by using the polymer foam agent.
By mixing the admixtures such as silica-fume and fly-ash and the industrial by-product
such as styrofoam for the purpose of practical use of industrial waste, lightweight foamed concrete shich has better lightness. flowability and strength than the conventional prefoamed lightweight foamed concrete is developed. This paper presents extensive data on characteristics of compressive strength and flowability of the concrete manufactured with the different factors in mix design and also presents optimum mix proportion.
경량기포콘크리트란 시멘트슬러리 속에 미리 생성된 기포를 혼합시켜 양생시킴으써 동일한 체적의 보통콘크리트보다 가볍게 만든 콘크리트를 의미한다. 따라서 경량기포콘크리트는시멘트풀 결합재내에 기포가 무작위로 분포된 복합재료이다. 본 연구의 목적은 이러한경량기포콘크리트의 탄성계수 추정식을 미시역학적 이론을 바탕으로 추정하는데 있다. 이르 위해 본 논문에서는 미시역학적인 미분법에 Hansen의 수정기법을 적용한 수정미분법을 사용하여 경량기포콘크리트의 탄성계수 추정식을 제안하였다. 제안된 추정식을 사용하여 얻어진 결과는 실험결과와 잘 일치하였고 기존의 어떤 추정식보다도 우수한 결과를 보였다.
Foamed concrete for cast-in-site, which shows excellent lightweight, thermal insulation, noise insulation, constructability and cost efficiency, has been applied as thermal insulation or filling material for On-dol. However, the technology is too insufficient to obtain the high level of quality, and serious problems often occur in quality control at sites. It, thus, is necessary to establish the proper and reasonable quality control method for ensuring the required quality, based on the investigation on the physical properties and their reciprocal relation. This study aims to settle the quality control method in case of applying FA foamed concrete replacing 40% by weight with fly-ash as the filling material for On-dol. The results of the study include the correlation among flow, as-placed density and foam ratio of fresh foamed concrete, the correlation between physical properties before hardening and after 28-day, provision of an equation to estimate 28-day compressive strength early with 7-day compressive strength, and suggestion of quality criteria for the revision of KS on foamed concrete for cast-in-site.
본 연구는 폐수처리공정에서 경량기포콘크리트를 이용하여 폐수 중에 존재하는 음이온계면 활성제와 총인 그리고 총질소성분을 제거하기 위하여 실시되었다. 경량기포콘크리트는 폐수 처리공정에서 반응기에 충진하여 사용하였으며, 이때 사용된 폐수는 인공폐수(음이온계면활성제 : 10-31 mg/L, 총인 : 66-73 mg/L 그리고 총질소 : 56-163 mg/L)를 사용하였다. 실험결과 경량기포콘크리트를 사용하여 폐수를 처리한 결과 음이온계면활성제의 85-95 %, 총인성분의 92 %, 그리고 총질소 성분의 90 % 정도가 제거되었다.
The objective of this study is to obtain the mechanical characteristics of prefoarmed lightweight foamed concrete using the polymer ham agent which has high lightness. flowability and strength. For this purpose, the prefoarmed lightweight foamed concrete which was developed to have flow value over 180mm. unit weight between 0.38t/$m^3$ and 0.64t/$m^3$, and compressive strength about 30kg/$cm^2$ was used. This paper presents extensive test data on Young's modulus. Poisson's ratio, stress-strain curve, the characteristics of strength of the foamed concrete and also presents the mechanical characteristics of the foamed concrete with different foam sizes. It is expected that this study provides an importance guide to design and manufacture lightweight foam concrete, so that it helps to expand its structural use.
Proceedings of the Korea Concrete Institute Conference
/
2009.05a
/
pp.357-358
/
2009
Expanded vermiculite and Al powder can produce lightweight porous concrete with excellent insulation performance. From the results, we could find out the possibility to develop environmental-friendly interior materials.
Kim, Jae-Kyung;Ahn, Jung-Hyun;Lee, Sang-An;Kim, Wha-Jung
Proceedings of the Korea Concrete Institute Conference
/
2010.05a
/
pp.297-298
/
2010
This study was investigates to the lightweight foamed concrete are uses by foamed agent to hydrogen peroxide($H_2O_2$). and then, lightweight foamed to improve the physical characteristics were mixed. mixes to type of admixture/level by changes/character to investigates, It is a purpose to look up admixture and mix proportion to be suitable in order to improve lightweight foamed concrete.
Journal of the Korean Recycled Construction Resources Institute
/
v.6
no.4
/
pp.304-310
/
2018
The aim of the research is to provide possibility of quality controlling by rheological properties for lightweight foamed concrete. The lightweight foamed concrete achieves its low density by containing air bubbles (foam) produced during the mixing process. Therefore, containing foamed volume during setting period is critical for the securing the performance as an insulating material. In this research, regarding foam collapse during the setting period, rheolgocial properties of fresh state lightweight foamed concrete were assessed to get its relationship with volume stability, or foam stability. For the experiment regarding foaming factors including mixing time, mix design of contents for materials, rheological properties of fresh state lightweight foamed concrete were tested with its density and settling depth. Based on the settling depth with various factors, relationship with rheological properties was analyzed, and especially, close relationship of plastic viscosity and settling depth was found. Therefore, from the results of this research, it is considered to contribute on suggesting a new approach of quality controlling for lightweight foamed concrete using rheological test method.
Journal of the Korea Institute of Building Construction
/
v.9
no.4
/
pp.63-73
/
2009
Recently, the use of lightweight panels in building structures has been increasing. Of the various lightweight panel types, styrofoam sandwich panels are inexpensive and are excellent in terms of their insulation capacity and their constructability. However, sandwich panels that include organic material are quite vulnerable to fire, and thus can numerous casualties in the event of a fire due to the lack of time to vacate and their emission of poisonous gas. On the other hand, lightweight foamed concrete is excellent, both in terms of its insulation ability and its fire resistance, due to its Inner pores. The properties of lightweight concrete is influenced by foaming agent type. Accordingly, this study investigates the insulation properties by foaming agent type, to evaluate the possibility of using light-weight foamed concrete instead of styrene foam. Our research found thatnon-heating zone temperature of lightweight foamed concrete using AP (Aluminum Powder) and FP (animal protein foaming agent) are lower than that of light-weight foamed concrete using AES (alkyl ether lactic acid ester). Lightweight foamed concrete using AES and FP satisfied fire performance requirements of two hours at a foam ratio 50, 100. Lightweight foamed concrete using AP satisfied fire performance requirements of two hours at AP ratio 0.1, 0.15. The insulation properties were better in closed pore foamed concrete by made AP, FP than with open pore foamed concrete made using AES.
Shrinkage may cause cracking in concrete. In practice such cracking must be considered in most concrete applications because, under normal conditions, drying of the concrete is unavoidable, and when drying takes place shrinkage occurs. Cracked concrete is an inferior concrete because it is weaker, more permeable, and more susceptible to chemical attack. The development of the strength of LAC with aging depends on a few factors such as type of the cement, W/C ratio, curing conditions and periods. The higher the strength of LAC, the lower the possibility of shrinkage cracking. Hence, the strength of LAC in the hypocaust system depends to a large extent on the effect of cracking decrease of the antifoaming rate to drying shrinkage in cement.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.