• Title/Summary/Keyword: σ

Search Result 198, Processing Time 0.026 seconds

Effect of reaction temperature on the particle size and crystal shape of precipitated calcium carbonate (반응온도가 침강성탄산칼슘의 입도 및 형상에 미치는 영향)

  • 송영준;박찬훈;조동성
    • Resources Recycling
    • /
    • v.4 no.1
    • /
    • pp.38-45
    • /
    • 1995
  • The objective of this study was to investigate the effect of temperature on the formation of CaCO, polymorphs(i.e.,calcite, aragonite, vaterite) and on the crystal shape of CaCO,.The reaction systems were rnvestigated at the temperature range of 2.0%-85.3r, at the fixed cmditions ofconcentration and pressure, 2X10-' M, atomospheric pressure, respectively.The reaction systems studied include a Ca(HCO.,),-Air bubble, O Ca(OH)s-CO,, @ Ca(OH),-H,CO, ,Ca(OH1,-Na>CO,, O Ca(OH),-K,CO,, @ Ca(OH),-(NH,),CO,, D CaC1,-Na,CO,, CaC1,-K3C03, 8 CaC1,-(NH,,),CO,, 0 Ca(N0,X-Na,CO,, 03 Ca(N0,X-QCO,. 0 Ca(NO,),-(NH,XCO,. The results obtained are summarizedas follows:Calcite is formed at the temperature range of 2t-80"C and the highest calcite yield was obtained at 30%.Aragonite begins to be formed at the temperature range of 41.0%-53.0%. and the higher temperature is thehigher yield is obtained. pH of the reaction system affect the yield of aragonite, and the yield reaches the highestpercentage at the pH range of 10.0-11.0, and at the conditions of pH 12.3 or over, aragonite is scarcely formed.Vaterlle is fnrmed at the temperature range of 40.0% or less, and transites utterly to calcite within 10-60mmutes in the case of bemg residenced in mother liqmd which C1 is not contained, and within 140hours inthe case of containing CI-.s in the case of containing CI-.

  • PDF

A study on the Structural Properties of PZT/BT thick film (PZT/BT 세라믹 후막의 구조적 특성에 관한 연구)

  • Lee, Sang-Heon;Lim, Sung-Soo;Lee, Young-Hie
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.05b
    • /
    • pp.57-59
    • /
    • 2005
  • Ploycrystalline $Pb(Zr_{0.5},Ti_{0.5})O_3$ and $BaTiO_3$ powder were prepared by sol-gel process. The alumina substrate were sintered at $1400^{\circ}C$ with bottom electrode of Pt for 2 hours. The Pb(Zr0.5,Ti0.5)O3 / BaTiO3 multilayered thick films with laminating times were fabricated on alumina substrate by screening printing method. The obtained thick films were sintered at $800^{\circ}C$ with upper electrode of Ag paste for 1 hour. Structural properties of Pb(Zr0.5,Ti0.5)O3 / BaTiO3 multilayered thick films were investigated. As a result of the Differential Thermal Analysis(DTA) of Pb(Zr0.5,Ti0.5)O3, exothermic peak was observed at around $650^{\circ}C$. The X-ray diffraction (XRD) patterns indicated that BaTi03 and Pb(Zr0.5,Ti0.5)O3 phases and porosities were formed in the interface of Pb(Zr0.5,Ti0.5)O3 / BaTiO3 multilayered thick films.

  • PDF

Studies on the Early Growth of Rockfish, Sebastes schlegeli (조피볼락, Sebastes schlegeli의 초기성장에 관한 연구)

  • Hyun Choung-Hun;Rho Sum
    • Journal of Aquaculture
    • /
    • v.9 no.1
    • /
    • pp.25-42
    • /
    • 1996
  • The study has been conducted to know an appropriate feeding strategy and effects of the rearing density on larval growth of the rockfish, Sebastes schlegeli. The results obtained are as fellowed ; 1. Thirty-day-old larvae reached at $25.25{\pm}3.76$ mm in total length and $0.23{\pm}0.07$ g in body weight in experiment A, at which rotifer was provided from the beginning to the end of 30-day experiment, Anemia from 3th to 18th day, and artificial feed from 13th to 30th day after hatching. When rotifer was provided for 30 days, Artemia from 6th to 18th day, and artificial feed from 18th to 30th day after hatching (experiment B), these larvae grew up to $27.52{\pm}2.50$ mm in total length and $0.26{\pm}0.06$ g in body weight. On the other hand, when rotifer and artificial feed were supplied with the same time schedule as shown in experiment B, and Artemia was feed from 6th to 30th day after hatching (experiment C), the total length and body weight of those larvae were $23.22{\pm}3.44$ mm and $0.15{\pm}0.05$ g, respectively. The best result for larval growth was obtained from experiment B. The survival rates estimated were $57.6\%$ in experiment A, $66.4\%$ in experiment B, and $44.4\%$ in experiment C. 2. The growth in total length of the larvae according to their rearing days could be represented by the following equations : Experiment A : Y=4.350+0.116X+$1.887X^2$ (r=0.993) Experiment B : Y=4.500+8.931X+$2.221X^2$ (r=0.994) Experiment C : Y=4.478+5.734X+$1.881X^2$(r=0.990) The average number of Artemia nauplius intaken by the larvae was rapidly increased between 15th and 20th day afer hatching, and 9, 212, 242, 750, and 1,171 nauplius were found in the different sizes of larvae, whose total length were 5.65, 6.81, 9.45, 14.96, and 24.52 mm, respectively. 3. Larval growth in total length and body weight reared at four different densites (A: 1.8 $kg/m^3$, B; 4.0 $kg/m^3$, C; 5.0 $kg/m^3$, D; 6.2 $kg/m^3$) indicated that the best growth was found in experiment A, at which the larval were reared at the lower density and the final survival rates extimated were $92.9\%$ in exp. A, $99.5\%$ in exp. C, $89.0\%$ in exp. B, and $88.2\%$ in exp. D. The amount of production per cubic meter turned out to be 30.45 kg in exp. D, 25.89 kg in exp. C, 20.75 kg in exp. B and 10.48 kg in exp. A. therefore, considering both larval growth and survival rate, higher yields seemed to be attainable at the relatively high-rearing density.

  • PDF

The Particle Size Distribution of $\alpha-Fe_2O_3$from Mossbauer Spectra (${\Alpha}-Fe_2O_3$ 미세입자의 크기분포에 관한 Mossbauer 분광학적 연구)

  • 이민용;김시정;고영복;서정철;이충섭
    • Journal of the Korean Magnetics Society
    • /
    • v.9 no.1
    • /
    • pp.23-28
    • /
    • 1999
  • ${\Alpha}-Fe_2O_3$ was accomplished by chemical method as low temperature as possible and the crystallographic and magnetic properties have been studied by Mossbauer spectroscopy and X-ray diffraction. The sample heated at 15$0^{\circ}C$ is found to have a Corundums symmetry with the hexagonal lattice constant a=8.26$\pm$0.05$\AA$, c=8.75$\pm$0.05$\AA$. The M$\"{o}$ssbauer spectra between the 4.2K and the room temperature show that the ${\Alpha}-Fe_2O_3$ crystallized with a single phase and fine sizes. The particle size distribution has the Gaussian distribution center at 98$\AA$ and the half width of 32$\AA$.TEX>.

  • PDF

Effect of Metal Chloride Coloring Liquids on Color and Strength Changes of Tetragonal Zirconia Polycrystals (금속염화물 착색제 침투가 정방정 지르코니아 다결정체의 색조와 강도 변화에 미치는 영향)

  • Oh, Jong-Jin;Noh, Hyeong-Rok
    • Journal of dental hygiene science
    • /
    • v.15 no.5
    • /
    • pp.577-584
    • /
    • 2015
  • The purpose of this study was to evaluate the effect of metal chloride infiltration treatment on color and strength changes of the yttria-stabilized tetragonal zirconia polycrystals (Y-TZP). Fifty disc specimens were prepared with a Y-TZP powder (ZPEX; Tosoh, Japan). Thirty different metal chloride solutions containing 0.03~0.08 wt% chromium and 0.03~0.07 wt% terbium ions were prepared. Presintered Y-TZP specimens were soaked in metal chloride coloring liquids for 3 minutes and sintered in air at $1,450^{\circ}C$ for 2 hours. The color of the specimens was measured with spectrophotometer and color difference (${\Delta}E^*$) was obtained based on the CIE $L^*$, $a^*$, $b^*$ color coordinate values. To evaluate the effect of metal chloride infiltration strength changes, the biaxial flexural test was performed at crosshead speed 0.5 mm/min. Colors of the sintered Y-TZP showed the colors of Vita shade guide A1, A2 and A3 with the infiltration of chromium and terbium chloride solutions. Density of the sintered Y-TZP increased by the infiltration of chromium and terbium chloride solutions. Bi-axial flexural strength of the sintered Y-TZP did not show statistically significant differences by the infiltration of chromium and terbium chloride solutions (p>0.05). Chromium and terbium chloride did not affect the crystal phase of zirconia, and all specimens showed tetragonal phase. Accordingly, this study suggests that chromium and terbium chlorides can make colored zirconia while adding in a liquid form. The color of colored zirconia differ from that of vita shade guide but it can use all ceramic restoration as substructure in dental clinic.

Radiation exposure to the eyes and thyroid during C-arm fluoroscopy-guided cervical epidural injections is far below the safety limit

  • Choi, Eun Joo;Go, Gwangcheol;Han, Woong Ki;Lee, Pyung-Bok
    • The Korean Journal of Pain
    • /
    • v.33 no.1
    • /
    • pp.73-80
    • /
    • 2020
  • Background: The aim of this study was to evaluate radiation exposure to the eye and thyroid in pain physicians during the fluoroscopy-guided cervical epidural block (CEB). Methods: Two pain physicians (a fellow and a professor) who regularly performed C-arm fluoroscopy-guided CEBs were included. Seven dosimeters were used to measure radiation exposure, five of which were placed on the physician (forehead, inside and outside of the thyroid protector, and inside and outside of the lead apron) and two were used as controls. Patient age, sex, height, and weight were noted, as were radiation exposure time, absorbed radiation dose, and distance from the X-ray field center to the physician. Results: One hundred CEB procedures using C-arm fluoroscopy were performed on comparable patients. Only the distance from the X-ray field center to the physician was significantly different between the two physicians (fellow: 37.5 ± 2.1 cm, professor: 41.2 ± 3.6 cm, P = 0.03). The use of lead-based protection effectively decreased the absorbed radiation dose by up to 35%. Conclusions: Although there was no difference in radiation exposure between the professor and the fellow, there was a difference in the distance from the X-ray field during the CEBs. Further, radiation exposure can be minimized if proper protection (thyroid protector, leaded apron, and eyewear) is used, even if the distance between the X-ray beam and the pain physician is small. Damage from frequent, low-dose radiation exposure is not yet fully understood. Therefore, safety measures, including lead-based protection, should always be enforced.

Synthesis and Formation Mechanism of ZrTiO4 Gray Pigment (ZrTiO4계 Gray 안료 합성과 형성기구)

  • Hwang, Dong-Ha;Lee, Byung-Ha
    • Journal of the Korean Ceramic Society
    • /
    • v.49 no.1
    • /
    • pp.84-89
    • /
    • 2012
  • Attempts were made to develop a stable gray pigment at reducing atmosphere, substituting Ti in $ZrTiO_4$ with Mn, Fe, Co and Cu The pigment synthesized at $1300~1500^{\circ}C$ by solid state method with the composition of $ZrTi_{1-x-y}A_xB_yO_4$ (x = y = 0.005, 0.015, 0.035, 0.055, 0.075, 0.095, 0.115, 0.135, 0.155, 0.175 and 0.195 mole, A = Mn(III), Fe(III), Co(II, III) and Cu(II) (chromophores), B = Sb (counterion). The pigments were fired at $1400^{\circ}C$ for 3 h with substitute amount changes of Mn, Fe, Co and Cu to $ZrTiO_4$ crystals, and analyzed by Raman spectroscopy to figure out substitute limits. Results indicated 0.035 mole for Mn, 0.115 mole for Fe, 0.015 mole for Co and 0.015 mole for Cu as substitute limits, respectively. Figs. 1, 2, 3, and 4 represent each substitute pigments of Mn, Fe, Co and Cu. Synthesized pigment was applied to a lime and a lime-magnesia glaze at 7 wt% each, and fired at reducing atmosphere of $1240^{\circ}C$, soaking time 1h. Gray color was obtained with CIE-$L^*a^*b^*$ values at 44.55, -0.65, 1.19(Mn), 40.36, -0.90, 0.30(Fe), 42.63, -0.03, -1.49(Cu) and -40.79, -0.28, -0.91(Co), respectively.

The Surface Properties and Wear Resistance of Cr-Mo-V Steel by Salt bath Process after Pseudo-electrolysis (의(擬)전기분해식 염욕질화처리를 통한 Cr-Mo-V강의 내마모와 표면성질에 관한 연구)

  • Jung, Gil Bong;Yoon, Jae Hong;Hur, Sung Kang
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.3
    • /
    • pp.225-234
    • /
    • 2010
  • Salt bath nitriding, which has been developed recently by domestic company, is an emerging ecofriendly surface treatment. The salt bath nitriding is accompanied by the electrolysis process in the pretreatment step, and this whole processis called Pseudo-Electrolysised Salt bath Nitriding (PESN). The PESN creates only $NH_3$ and non-toxic salts without harmful $CN^{-}$ or toxic gas such as that found in previous salt bath nitriding. In general, ion nitriding and gas nitriding create high hardness and a strong brittle white layer on the surface. However, the PESN shows a thin white and gray layer. The PESN was applied to the defense material, 3%Cr-Mo-V steel, to study the surface characteristics at $480^{\circ}C$, $530^{\circ}C$, and $580^{\circ}C$ for 4 hrs, 20 hrs, 40 hrs, and 60 hrs of nitriding time condition. As a result, the best nitriding layer was found at $530^{\circ}C$ for 40 hrs. If we improve corrosion resistance and nitriding layer depth, the PESN will be able to be applied to the defense industry parts.

The Crystal Structure of One Natural Compound Cyclo-(1,10-Docandiamino-11,20-Docanedioic) Amide (1,12-Diazacyclodocosane-2,11-Dione)

  • Wei, Wan-Xing;Pan, Yuan-Jiang
    • Bulletin of the Korean Chemical Society
    • /
    • v.23 no.11
    • /
    • pp.1527-1530
    • /
    • 2002
  • 1,12-diazacyclodocosane-2,11-dione was first isolated from a plant Phyllanthus niruri Linn. Its structure has been determined by means of spectroscopy methods and X-ray crystallography. Two peptide groups in the big ring (lactam) are the main factors influencing intermolecular contacts. The hydrogen-bond interaction of these hydrophilic groups is observed in the crystal structure. Meanwhile, C-H···O hydrogen bonds in molecules contribute to the formation of the whole crystal. These two kinds of hydrogen-bond form six- member rings among molecules. This compound crystallizes in the triclinic space group P-1 with a= 9.588(1) $\AA$, b= $9.850(1)\AA$, c = $11.810(1)\AA$, $\alpha=$ 68.18(1)$^{\circ}C$ , $\beta=$ 84.98(1), $\gamma$ = 86.03(1)$^{\circ}C$ , V = $1030.66(17)\AA3$ , Z = 2. A disorder of five-member carbon chain in the whole ring is observed in the title compound. The bond angle 105.8(4) is determined for a extreme configuration C(14)-C(15)-C(16), and 117.7(10) for another extreme configuration C(14')-C(15')-C(16'). In this crystal, two molecules are tied each other by short intermolecular hydrogen bonds, the oxygen atom being tied by hydrogen bond to nitrogen atom of another two molecules. The NMR and IR spectral data coincides to the structure of the compound.

Low-temperature Oxidation of Odor Compounds over La-based Perovskite Catalyst (란탄 기반 페롭스카이트 촉매를 이용한 악취 유발 물질의 저온 산화 반응)

  • Bang, Yong-Ju;Seo, Jeong-Gil;Lee, Gi-Chun;Park, Chan-Jung;Kim, Hyung-Tae;Song, In-Kyu
    • Korean Chemical Engineering Research
    • /
    • v.49 no.2
    • /
    • pp.168-174
    • /
    • 2011
  • Various La-based perovskite catalysts were prepared by a Pechini method, and they were applied to the low-temperature oxidation of odor compounds exhausted from waste food treatment process for effective deodorization. Quantitative and qualitative analyses of exhausted gas were conducted to measure the amount of major odor compounds with respect to operation time. A standard odor sample composed of major odor compounds was then prepared for use as a feed for oxidation reaction system. Various transition metal(M)-substituted La-based perovskite catalysts ($LaMO_{3}$: M=Cr, Mn, Fe, Co, and Ni) were prepared and applied to the oxidation of odor compounds in order to investigate the $LaNiO_3$ catalyst showed the best catalytic performance. Pt-substituted perovskite catalysts ($LaNi_{1-x}Pt_{x}O_{3}$: x=0, 0.03, 0.1, and 0.3) were then prepared for enhancing the catalytic performance. It was found that $LaNi_{0.9}Pt_{0.1}O_{3}$ catalyst served as the most efficient catalyst. Supported perovskite catalysts ($XLaNi_{0.9}Pt_{0.1}O_{3}/Al_{2}O_{3}$: X=perovskite content(wt%), 0, 10, 20, 30, 40, 50, and 100) were finally applied for the purpose of maximizing the catalytic performance of perovskite catalyst in the low-temperature oxidation reaction. Catalytic performance of $XLaNi_{0.9}Pt_{0.1}O_{3}/Al_{2}O_{3}$ catalysts showed a volcano-shaped curve with respect to perovskite content. Among the catalysts tested, $20LaNi_{0.9}Pt_{0.1}O_{3}$/$Al_{2}O_{3}$ catalyst exhibited the highest conversion of odor compounds of 88.7% at $180^{\circ}C$.