A Study on the Electromagnetic Wave Absorption Properties and Microstructure for the Composition Ratio of Ni-Zn-Fe$_2$O$_4$ (Ni-Zn-Fe$_2$O$_4$의 조성비에 따른 전파흡수 특성과 미세구조에 관한 연구)

  • 조재원;문치현;문현욱;신용진
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1993.11a
    • /
    • pp.144-148
    • /
    • 1993
  • This paper is a study on electromagnetic wave absorption properties for the composition ratio of Ni-Zn-Fe$_2$O$_4$. Li-Zn-Fe$_2$O$_4$was composed of Fe$_2$O$_3$ 48∼51mo1%, LiO 18 ∼22mo1%, ZnO 34∼27mo1%. and sintering was carried out at 1200$^{\circ}C$. Through the experiments, the resonance phenomenon occured at low frequence range for high permeability, and vice versa. Specialy, In the case of Fe$_2$O$_3$49mol%, NiO 20mo1%, ZnO 3lmol% ,and the matching thickness was 10mm , the absorbing bandwith was 0.35 ∼0.95GHz. Also, In the case of Fe$_2$O$_3$51mo1%. NiO 22mo1%, ZnO 27mol%, we could get the absorbing bandwith of 0.45∼1.2GHz when the matching thickness was 6mm. Therefore. it is proved that electromagnetic wave absorbers with the above bandwidth range can be fabricated successful1y.

  • PDF

Sintering Characteristics of ZnO Fabricated by Spark Plasma Sintering Process for High Temperature Thermoelectric Materials Application (고온용 ZnO계 열전 재료의 방전플라즈마 소결 특성 및 미세구조)

  • 심광보;김경훈;홍영호;채재홍
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.6
    • /
    • pp.560-565
    • /
    • 2003
  • M-doped (M=Al, Ni) ZnO thermoelectric materials were fully densified at low temperatures of 800∼1,000$^{\circ}C$ and their sintering characteristics and microstructural features were investigated. Electron microscopic analysis showed that the addition of NiO promoted tile formation of solid solution and caused actively grain growth. The addition of A1$_2$O$_3$ prevented the evaporation of pure ZnO at grain boundaries and suppressed the grain growth by the formation of secondary phase. In case of the addition of A1$_2$O$_3$ together with NiO, the specimen showed an excellent microstructure and also the SEM-EBSP (Electron Back-scattered Diffraction Pattern) analysis confirmed that it shows a superior grain boundary distribution to the others specimens. These microstructural characteristics induced by the addition of A1$_2$O$_3$ together with NiO may increase the electrical conductivity by the increase in carrier concentration and decrease the thermal conductivity by the phonon scattering effect and, consequently, improve the thermoelectric property.

Electrical Properties as the ratio of ZnO/$Mn_3$$O_4$ of NTC Thermistor with $Mn_3$$O_4$-NiO-CuO-$Co_3$$O_4$-ZnO system for Inrush Current Limited (돌입전류 제한용 $Mn_3$$O_4$-NiO-CuO-$Co_3$$O_4$-ZnO계 NTC 써미스터에서 ZnO/$Mn_3$$O_4$비에 따른 전기적 특성)

  • 윤중락;김지균;권정렬;이현용;이석원
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.13 no.6
    • /
    • pp.472-477
    • /
    • 2000
  • Oxides of the form Mn$_{4}$/O$_{4}$-CuO-Co$_{3}$/O$_{4}$-NiO-ZnO present properties that make them useful as power NTC thermistor for current limited. Electrical properties of Mn$_{3}$/O$_{4}$-CuO-Co$_{3}$/O$_{4}$-CuO-Co$_{3}$/O$_{4}$-NiO-ZnO power NTC thermistor such as I-V characteristics tim constant activation energy and heat dissipation coefficient measured as a function of temperature and composition. In Mn$_{4}$/O$_{4}$-CuO-Co$_{3}$/O$_{4}$-NiO-ZnO system with the 5wt% addition of Co$_{3}$/O$_{4}$ it can be seen that resistivity and B-constant were increased as the ratio of ZnO/Mn$_{3}$/O$_{4}$ was increased. Heat dissipation constant, I-V characteristics and time constant showed similar behaviour compared with those of conventional thermistors. In particular resistance change ratio ($\Delta$R) the important factor for reliability varied within $\pm$5% indicating the compositions of these products could be available for power thermistor.

  • PDF

The effect of $Co_3O_4$ substitution on properties of Ni-Zn Ferrite (Ni-Zn 페라이트 물성의 $Co_3O_4$ 치환효과)

  • An, Yong-Woon;Kim, Jong-Ryung;Oh, Young-Woo;Kim, Hyun-Sik;Lee, Hae-Yon
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.07a
    • /
    • pp.569-572
    • /
    • 2003
  • 전력선 통신용 LC 공진필터에 사용되는 Ni-Zn 페라이트를 제조하기 위해 Ni0.8Zn0.2Fe2O4를 기본조성으로 선택하고 x (Co mol 비)를 변화시켜 전자기적 특성을 조사하였다. $Bi_2O_3$ CaO가 첨가됨으로써 균일한 입자성장과 입계에 고저항층이 형성되어 주파수 손실이 감소하였으며, $Ni_{0.8-x}Zn_{0.2}Co_xFe_2O_{\delta}$의 기본조성에 Co의 함량을 증가시키면 x = 0.05에서 투자율 75, 공진주파수 20 MHz의 특성을 나타내고 결정 입자 크기와 같은 구조적 특성에는 영향을 거의 미치지 않지만 자기이방성 변화에 따라 전자기적 특성에는 영향을 미친다. 또한, $Ni_{0.75}Zn_{0.2}Co_{0.05}Fe_2O_{4.017}$ 조성의 페라이트 코어의 발열량은 큐리온도 이하에서 일어난다.

  • PDF

A Study on the Electromagnetic Wave Absorption Properties by the Composition Ratio and Sintering Condition of NiCuZn Ferrite (NiCuZn 페라이트의 조성 및 소결조건에 따른 전자파흡수 특성에 관한 연구)

  • 이영구;박찬규;이문수
    • Journal of the Korea Institute of Information and Communication Engineering
    • /
    • v.5 no.5
    • /
    • pp.994-1000
    • /
    • 2001
  • With the development of electromagnetic communication technology and increased use of electromagnetic wave, the countermeasure of EMI(Electromagnetic Interference) becomes more important socially, and interest for the electromagnetic wave absorber has also increased. In this paper, we have studied characteristics of frequency dependency on complex permittivity and complex permeability according to the changes of composition rate and sintering temperature of NiCuZn ferrite also known as electromagnetic wave absorber and further looked into effect of electromagnetic wave absorption properties. From the measurement where the composition of $Fe_2O_3$ and ZnO of NiCuZn ferrite was fixed at 49 and 34 mol% respectively while composition of NiO and CuO has been varied at each test, we found out that Initial permeability and permittivity were high and the absorbing ability of electromagnetic wave recorded best with $loss tangent(=\mur"/\mur')$ displays more than 1 within the frequency band of 2MHz~9.5MHz when the composition ratio of NiO was ranged around 8.5~9.5 mol% and the sintering temperature was $1080^{\circ}C$.TEX>.

  • PDF

ZnNiO thin films deposited by r.f. magnetron sputtering method (RF Magnetron Sputtering법으로 증착된 ZnNiO박막의 특성)

  • 오형택;이태경;김동우;박용주;박일우;김은규
    • Journal of the Korean Vacuum Society
    • /
    • v.12 no.4
    • /
    • pp.269-274
    • /
    • 2003
  • The electrical, optical and structural properties of ZnNiO thin _ films deposited on Si substrates using rf-magnetron sputtering method have been investigated before and after the thermal annealing processes. The crystallinity of the ZnNiO thin film become degraded with increasing the Ni contents. This is mainly because the lattice of the thin film was expanded due to the oxygen-deficient conditions. Concerning the electrical properties of the thin film, the carrier concentration increases ($6.81\times10^{14}\textrm{cm}^{-2}$) and Hall mobility decreases (36.3 $\textrm{cm}^2$/Vㆍs) with higher doping concentration of Ni. However, the carrier concentration and Hall mobility became low ($1.10\times10^{14}\textrm{cm}^2$ and high (209.6 $\textrm{cm}^2$/Vㆍs), respectively, after the thermal annealing process at $1000 ^{\circ}C$. We also observed a strong luminescene center peaking at 546 nm in photoluminescence spectra, which was caused by a deep level center in the ZnO band gap with oxygen deficient ZnNiO structure.

Impurity Pick-Up for the Preparation of NiCuZn Ferrite Powder Using Ball Milling Process (NiCuZn Ferrite 분말제조에 있어서 Ball Mill 분쇄 공정 중에 혼입되는 불순물의 함량)

  • 고재천;류병환
    • Journal of the Korean Magnetics Society
    • /
    • v.9 no.4
    • /
    • pp.217-222
    • /
    • 1999
  • The pick up impurity was studied for preparing the NiCuZn ferrite powder by a ball milling method that usually uses in the industrial ceramic process. The raw materials of NiO, CuO, ZnO, and $Fe_2O_3$ powder were weighted according to various spinel composition and mixed for 18 hrs by a wet ball milling method after that the slurry was followed by spray dried and calcined at $700^{\circ}C$ 3 hrs. The calcined NCZF powder was finally ball milled during 65 hrs as same method. The stainless steel ball and jar are used as mixing and milling equipment and the solid concentration of the slurry was 25 vol%. The impurities, stainless steel pickup, were effected by the composition of raw materials especially iron oxide, nickel oxide in the mixing process and by the rate of calcine of NiCuZn ferrite in final milling process. The empirical equation of stainless steel pickup was driven in the wet ball milling system. Finally, the composition of NiCuZn ferrite could be controlled by the empirical equation.

  • PDF

Electrochemical Properties of LiNi1-yMyO2(M=Zn2+, Al3+, and Ti4+ Synthesized by Combustion Method (연소법으로 합성한 LiNi1-yMyO2(M=Zn2+, Al3+, and Ti4+ 전기화학적 특성)

  • Kwon, Ikhyun;Song, Myoungyoup
    • Journal of the Korean Ceramic Society
    • /
    • v.42 no.4
    • /
    • pp.276-281
    • /
    • 2005
  • $LiNi_{1-y}M_{y}O_{2}(M=Zn^{2+},\;Al^{3+},\;and\;Ti^{4+},\;0.000\{\le}y{\le}0.100)$ were synthesized by the combustion method by calcining in $O_{2}$ stream at $750^{\circ}C$ for 36 h. XRD analyses, observation by FE-SEM and measurement of the variation of discharge capacity with the number of cycles were carried out. The composition $LiNi_{0.99}M_{0.01}O_{2}(M=Zn^{2+},\;Al^{3+},\;and\;Ti^{4+})$ of all the compositions showed relatively good electrochemical properties. $LiNi_{0.99}M_{0.01}O_{2}$ exhibited poor crystallinity and $LiNi_{0.99}M_{0.01}O_{2}$ showed the cation mixing of large fraction. $LiNi_{0.99}M_{0.01}O_{2}$ with improved cycling performance showed good crystallinity and the cation mixing of small fraction.

Sintering and Electrical Properties of Ni-doped ZnO-Bi2O3-Sb2O3 (Ni를 첨가한 ZnO-Bi2O3-Sb2O3계의 소결과 전기적 특성)

  • Hong, Youn-Woo;Shin, Hyo-Soon;Yeo, Dong-Hun;Kim, Jong-Hee;Kim, Jin-Ho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.22 no.11
    • /
    • pp.941-948
    • /
    • 2009
  • The present study aims at the examination of the effects of 1 mol% NiO addition on the reaction, microstructure development, resultant electrical properties, and especially the bulk trap and interface state levels of $ZnO-Bi_2O_3-Sb_2O_3$ (Sb/Bi=0.5, 1.0, and 2.0) systems (ZBS). The samples were prepared by conventional ceramic process, and characterized by density, XRD, SEM, I-V, impedance and modulus spectroscopy (IS & MS) measurement. The sintering and electrical properties of Ni-doped ZBS (ZBSN) systems were controlled by Sb/Bi ratio. Pyrochlore ($Zn_2Bi_3Sb_3O_{14}$) was decomposed more than $100^{\circ}C$ lowered in ZBS (Sb/Bi=1.0) by Ni doping. The reproduction of pyrochlore was suppressed by the addition of Ni in ZBS. Between two polymorphs of $Zn_7Sb_2O_{12}$ spinel ($\alpha$ and $\beta$), microstructure of ZBSN (Sb/Bi=0.5) composed of a-spinel was more homogeneous than $Sb/Bi{\geq}1.0$ composed of $\beta$-spinel phase. In ZBSN, the varistor characteristics were not improved drastically (non-linear coefficient $\alpha\;=\;6{\sim}11$) and independent on microstructure according to Sb/Bi ratio. Doping of Ni to ZBS seemed to form ${V_0}^{\cdot}$ (0.33 eV) as dominant bulk defect. From IS & MS, especially the grain boundaries of Sb/Bi=0.5 systems were divided into two types, i.e. sensitive to oxygen and thus electrically active one and electrically inactive intergranular one with temperature.

Electrical and Dielectric Characteristics of Zn-Pr-Co-Er-M(M=Ni, Mg, Cr) Oxides-Based Varistors (Zn-Pr-Co-Er-M(M=Ni, Mg, Cr)산화물계 바리스터의 전기적, 유전적 특성)

  • 남춘우;김명준
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.8
    • /
    • pp.605-609
    • /
    • 2004
  • The microstructure, electrical and dielectric characteristics of ZnO varistors were investigated at various metal oxide (NiO, MgO, and Cr$_2$O$_3$) additives. The average grain size was increased with addition of NiO while that was decreased with addition of Cr$_2$O$_3$-Thereby, the varistor voltage was higher in Cr$_2$O$_3$-added composition. Among varistors, the varistor added with Cr$_2$O$_3$ exhibited the highest nonlinearity, with 40.5 in the nonlinear exponent and 2.7 ${\mu}$A in the leakage current and its dielectric dissipation factor was relatively low value of 0.0589.