• 제목/요약/키워드: $Y_2O_3$ coating

검색결과 1,175건 처리시간 0.031초

가압 졸-겔 코팅법에 의한 세라믹막의 기체투과 특성 (Gas Permaeation Characteristics of Ceramic Membranes by the Pressurized Sol-Gel Coating Techique)

  • 현상훈;강범석
    • 한국막학회:학술대회논문집
    • /
    • 한국막학회 1993년도 춘계 총회 및 학술발표회
    • /
    • pp.35-35
    • /
    • 1993
  • 튜브형 $\alpha-Al_2O_3$ 담체에 졸-겔 침지코팅법과 가압코팅(pressurized coating) 법으로 boehmite 졸과 극미세 입자 SiO$_2$ 및 TiO$_2$ 졸을 코팅한 후 200$\circ$C~500$\circ$C 에서 열처리하여 복합분리막을 제조하였다.

  • PDF

Al2O3 Nano-Coating by Atomic Layer Deposition

  • Min Byung-Don;Lee Jong-Soo;Kim Sang-Sig
    • Transactions on Electrical and Electronic Materials
    • /
    • 제4권3호
    • /
    • pp.15-18
    • /
    • 2003
  • Aluminum oxide ($Al_2O_3$) materials were coated conformally on ZnO nanorods by atomic layer deposition (ALD). The ZnO nanorods were first synthesized on a Si(100) substrate from ball-milled ZnO powders by a thermal evaporation procedure. $Al_2O_3$ films were then deposited on these ZnO nanorods by ALD at a substrate temperature of $300^{\circ}C$ using trimethylaluminum (TMA) and distilled water ($H_2O$). Transmission electron microscopy (TEM) and high-resolution transmission electron microscopy (HRTEM) images of the deposited ZnO nanorods revealed that amorphous $Al_2O_3$ cylindrical shells surround the ZnO nanorods. These TEM images illustrate that ALD has an excellent capability to coat any shape of nanorods conformally.

무전해 Ni-P-X(X : $Al_2O_3$, Diamond) 복합도금층의 내마모성 (A Wear Resistance of Electroless Ni-P-X(X : $Al_2O_3$, Diamond) Composite Coating Layers)

  • 김만;장도연;노병호;한성호;이규환
    • 연구논문집
    • /
    • 통권22호
    • /
    • pp.151-160
    • /
    • 1992
  • The wear resistance of electroless Ni-P-X(X A1203, Diamond) composite coating layers was studied by Taber abrasion test technique. The wear resistance of composite coating layers was particularly relied upon the codeposited content, particle size and distribution of particles, and heat treatment of coating layers, as well as the electroless nickel plating bath employed. In this study, we lay emphasis on the wear resistance of electroless composite coating layers containing A1203 particles(1.2~Im, 6.7hIm, 11.5lIm, 20l1m) or diamond particles (1.5jim, 5gm). From the result of composite coating A1203 and diamond particles, the wear resistance of composite coating layers is as follows.

  • PDF

INTERACTION STUDIES OF CERAMIC VACUUM PLASMA SPRAYING FOR THE MELTING CRUCIBLE MATERIALS

  • Kim, Jong Hwan;Kim, Hyung Tae;Woo, Yoon Myung;Kim, Ki Hwan;Lee, Chan Bock;Fielding, R.S.
    • Nuclear Engineering and Technology
    • /
    • 제45권5호
    • /
    • pp.683-688
    • /
    • 2013
  • Candidate coating materials for re-usable metallic nuclear fuel crucibles, TaC, TiC, ZrC, $ZrO_2$, and $Y_2O_3$, were plasmasprayed onto a niobium substrate. The microstructure of the plasma-sprayed coatings and thermal cycling behavior were characterized, and U-Zr melt interaction studies were carried out. The TaC and $Y_2O_3$ coating layers had a uniform thickness, and high density with only a few small closed pores showing good consolidation, while the ZrC, TiC, and $ZrO_2$ coatings were not well consolidated with a considerable amount of porosity. Thermal cycling tests showed that the adhesion of the TiC, ZrC, and $ZrO_2$ coating layers with niobium was relatively weak compared to the TaC and $Y_2O_3$ coatings. The TaC and $Y_2O_3$ coatings had better cycling characteristics with no interconnected cracks. In the interaction studies, ZrC and $ZrO_2$ coated rods showed significant degradations after exposure to U-10 wt.% Zr melt at $1600^{\circ}C$ for 15 min., but TaC, TiC, and $Y_2O_3$ coatings showed good compatibility with U-Zr melt.

다공성 실리카 지지체 제조 및 Sol-Gel법에 의한 TiO2코팅 (Preparation of Porous Silica Support and TiO2 Coating by Sol-Gel Method)

  • 한요섭;박재구
    • 한국세라믹학회지
    • /
    • 제41권7호
    • /
    • pp.548-554
    • /
    • 2004
  • 슬러리 발포법을 이용하여 다공성 실리카 지지체를 제조하였으며, 지지체 표면에 졸-겔법을 이용하여 TiO$_2$을 코팅하였다. TiO$_2$ 코팅층에 대한 XRD, SEM 및 BET 측정 결과, 열처리 온도가 50$0^{\circ}C$에서 TiO$_2$의 anatase 결정상이 나타나기 시작하여, $700^{\circ}C$에서 그 피크가 최대가 되었다. 이 때 결정 성장한 TiO$_2$ 입자의 크기는 약 1$mu extrm{m}$ 정도로 판명되었다. 또한, 촉매지지체로 활용성을 검토하기 위해 TiO$_2$코팅 전후로 지지체의 굽힘 강도와 기체 투과율을 측정하였다. 강도의 경우, 코팅 전 2.4 MPa에서 이후 3.9∼4.3MPa로 증가하였으나 열처리 온도의 영향에 의한 변화는 나타나지 않았다. 한편, 투과율은 코팅 전 770${\times}$$10^{-13}$ $m^2$에서 코팅 후 363${\times}$$10^{-13}$ $m^2$로 감소하였고 열처리 온도의 증가와 함께 감소하는 것으로 나타났다.

플라즈마 용사법에 의한 Hydroxyapatite코팅층의 제조와 미세구조 (Fabrication and Microstructure of Hydroxyapatite Coating Layer by Plasma Spraying)

  • 이치우;오익현;이형근;이병택
    • 한국세라믹학회지
    • /
    • 제41권3호
    • /
    • pp.259-265
    • /
    • 2004
  • 플라즈마 용사법에 의해 나노크기의 하이드록시 아파타이트 분말을 지르코니아 소결체 기판에 용사한 후 코팅층의 미세조직에 대해 조사하였다. 나노크기의 하이드록시 아파타이트 분말은 Ca(NO$_3$)$_2$$.$4$H_2O$과 (NH$_4$)$_2$HPO$_4$ 용액을 이용한 침전법에 의해 성공적으로 합성되었다. 코팅 후 지르코니아 기판과 코팅층 계면에서 균열은 발생하지 않았으며 코팅층의 두께는 150-250 $\mu\textrm{m}$였다. 나노크기의 하이드록시아파타이트 분말과 용사된 HAp코팅층에서는 비이상적인 상들의 출현이 발견되지 않았다. 80$0^{\circ}C$에서 열처리된 코팅층의 경우 하이드록시 아파타이트 이외에 TTCP와 $\beta$-TCP같은 상이 관찰되었지만 열처리온도 90$0^{\circ}C$에서 TTCP와 $\beta$-TCP상은 소멸되었다. XRD 분석결과, 열처리온도 110$0^{\circ}C$에서 HAp코팅층은 높은 결정화도를 나타내었다.

SnO2-CoO/carbon-coated CoO core/shell 나노선 복합체의 합성 및 구조분석 (Synthesis and Characterization of SnO2-CoO/carbon-coated CoO Core/shell Nanowire Composites)

  • 이유진;구본율;안효진
    • 한국분말재료학회지
    • /
    • 제21권5호
    • /
    • pp.360-365
    • /
    • 2014
  • $SnO_2-CoO$/carbon-coated CoO core/shell nanowire composites were synthesized by using electrospinning and hydrothermal methods. In order to obtain $SnO_2-CoO$/carbon-coated CoO core/shell nanowire composites, $SnO_2-Co_3O_4$ nanowire composites and $SnO_2-Co_3O_4$/polygonal $Co_3O_4$ core/shell nanowire composites are also synthesized. To demonstrate their structural, chemical bonding, and morphological properties, field-emission scanning electron microscopy, transmission electron microscopy, X-ray diffraction, and X-ray photoelectron spectroscopy were carried out. These results indicated that the morphologies and structures of the samples were changed from $SnO_2-Co_3O_4$ nanowires having cylindrical structures to $SnO_2-Co_3O_4/Co_3O_4$ core/shell nanowires having polygonal structures after a hydrothermal process. At last, $SnO_2-CoO$/carbon-coated CoO core/shell nanowire composites having irregular and high surface area are formed after carbon coating using a polypyrrole (PPy). Also, there occur phases transformation of cobalt phases from $Co_3O_4$ to CoO during carbon coating using a PPy under a argon atmosphere.

뼈 대체용 생체활성 다공질 세라믹스의 제조 및 특성 (Fabrication and Properties of Bioactive Porous Ceramics for Bone Substitution)

  • 이락형;하정수
    • 한국세라믹학회지
    • /
    • 제45권10호
    • /
    • pp.584-588
    • /
    • 2008
  • Porous hydroxyapatite(HA) and HA-coated porous $Al_2O_3$ possessing pore characteristics required for bone substitutes were prepared by a slurry foaming method combined with gelcasting. The HA coating was deposited by heating porous $Al_2O_3$ substrates in an aqueous solution containing $Ca^{2+}$ and ${PO_4}^{3-}$ ions at $65{\sim}95^{\circ}C$ under ambient pressure. The pore characteristic, microstructure, and compressive strength were investigated and compared for the two kinds of samples. The porosity of the samples was about 81% and 80% for HA and $Al_2O_3$, respectively with a highly interconnected network of spherical pores with size ranging from 50 to $250{\mu}m$. The porous $Al_2O_3$ sample showed much higher compressive strength(25 MPa) than the porous HA sample(10 MPa). Fairly dense and uniform HA coating(about $2{\mu}m$ thick) was deposited on the porous $Al_2O_3$ sample. Since the compressive strength of cancellous bone is $2{\sim}12$ MPa, both the porous HA and HA-coated porous $Al_2O_3$ samples could be successfully utilized as scaffolds for bone repair. Especially the latter is expected suitable for load bearing bone substitutes due to its excellent strength.

Laser Diode의 무반사코팅 설계 및 특성에 관한 연구 (Study about Anti-Reflection Coating Design and Characteristic of Laser Diode)

  • 기현철;김효진;김희종;한정희;구할본
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 하계학술대회 논문집 Vol.8
    • /
    • pp.424-425
    • /
    • 2007
  • Anti-Reflection and High-reflection coating on the facet of semiconductor laser diode. To prevent internal feedback from both facets for realizing super luminescent diode and reducing the reflection-induced intensity noise of laser diode. Anti-Reflection coating Film was designed by Macleod Simulator. Coating Materials were decided $Ti_3O_5$ and $SiO_2$. Thickness of Coating layer $Ti_3O_5/SiO_2$ were 105[nm], 165[nm]. In the study Anti-Reflection coating Film was design for Laser diode and deposited by Ion-Assisted Deposition system. Then manufactured thin film measured electrical properties(L-I-V, Se, Resistor) and Optical properties(wavelength FFP). Slop-efficiency and FFP characteristic is 0.302[W/A], $22.3^{\circ}$(Horizontal), $24.4^{\circ}$(Vertical).

  • PDF

플라즈마 용사용 $Al_2O_3/SS316$ 복합 분말 제조 및 경사 코팅충의 제조에 관한 연구 (Properties of Plasma Sprayed $Al_2O_3/SS316$ Graded Coatings)

  • 민재웅;송병길;김삼중;노재승;서동수
    • Journal of Welding and Joining
    • /
    • 제20권2호
    • /
    • pp.109-115
    • /
    • 2002
  • In the case of using high temperature by coating ceramic/metal, large stress was produced due to difference of thermal expansion coefficient between those. And then lead to delamination. In order to relaxation of the stress A1$_2$O$_3$/SS316 composite powders with $10wt.%Al_2O_3$ compositional gradient and $10wt.%Al_2O_3$ agglomerated powder were made by spray drying method. These powders were sintered to improve the strength and to be plasma sprayed in order to fabricate the FGC(functionally graded coating). The influence of gun power, working distance and Ar pressure on the microstructure of the coating layer was studied in order to optimize the plasma spray conditions. It was proven that the optimum conditions were 40kw gun power, 5cm working distance and $100ft^3/h$ Ar flow for both powders. FGC with 10 compositional steps was fabricated and the total thickness was 1.3mm. FGC was heat treated at $1100^{\circ}C$for 10hours to evaluate the heat resisting characteristics.