• Title/Summary/Keyword: $TiO_2-SiO_2$

Search Result 1,741, Processing Time 0.029 seconds

High temperature oxidation of TiAlCrSiN thin films (TiAlCrSiN 박막의 고온산화)

  • Hwang, Yeon-Sang;Kim, Min-Jeong;Kim, Seul-Gi;Bong, Seong-Jun;Won, Seong-Bin;Lee, Dong-Bok
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2012.05a
    • /
    • pp.161-161
    • /
    • 2012
  • 결정질 TiCrN과 AlSiN 나노층이 교대로 구성하는 나노 다층 TiAlCrSiN 박막은 음극 아크 플라즈마 증착법에 의해 증착되었다. 나노 다층 TiAlCrSiN 박막의 산화특성들은 $600{\sim}1000^{\circ}C$사이에서 대기 중 최대 70시간동안 연구 되었다. 형성된 산화물들은 주로 $Cr_2O_3$, ${\alpha}-Al_2O_3$, $SiO_2$ 그리고 rutile-$TiO_2$들로 구성되었다. 나노 다층 TiAlCrSiN 박막이 산화하는 동안, 가장 바깥쪽의 $TiO_2$층은 Ti 이온의 외부확산에 의해, 외부 $Al_2O_3$층은 Al이온의 외부확산에 의해 형성되었다. 동시에, 내부($Al_2O_3$, $Cr_2O_3$) 혼합층과 가장 안쪽의 $TiO_2$층은 산소이온의 내부확산에 의해 형성되었다.

  • PDF

The Application of TiO2 Hollow Spheres on Dye-sensitized Solar Cells

  • Cho, H. J.;Jung, D.
    • Bulletin of the Korean Chemical Society
    • /
    • v.32 no.12
    • /
    • pp.4382-4386
    • /
    • 2011
  • $TiO_2$ hollow spheres were fabricated by using $SiO_2$ as an inorganic template. Spherical $SiO_2$ particles were coated by $TiO_2$ through the nucleation process, and then the core $SiO_2$ part was eliminated by using HF solution. Finally, $TiO_2$ hollow spheres were obtained. The size of the $TiO_2$ hollow spheres was about 300-400 nm and the thickness of the hollow wall was about 20-30 nm. The hollow has several holes whose diameters were within 100-200 nm. Dye-sensitized solar cells fabricated by using the $TiO_2$ hollow spheres were characterized. The solar conversion efficiency of the cell was 8.45% when $TiO_2$ hollow spheres were used as a scattering material, while it was 4.59% when $TiO_2$ hollow spheres were used as a normal electrode material.

Preparation of TiO2-SiO2 Sol and Its Photo-Catalyst Properties for High Temperatures (고온 소성용 TiO2-SiO2계 광촉매의 제조 및 특성)

  • 이명진;전애경;이지영;윤기현
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.6
    • /
    • pp.471-475
    • /
    • 2004
  • TiO$_2$, SiO$_2$, and PBA(Pseudo Boehemite Alumina) sol were prepared by sol-gel process. The particle sizes of these sol exhibited uniform 10∼30 nm. As the amount of SiO$_2$ sol increased, the temperature of phase transition (from anatase phase to rutile phase) was raised temperature than $600^{\circ}C$, which attributed to the enhanced photocatalyst properties. Also, the anatase phase was obtained with very small amount of the rutile phase from the addition of SiO$_2$ (10∼30 wt%) at annealing temperature of 120$0^{\circ}C$. The specimen with 20 wt% SiO$_2$ sol exhibited the maximum photocatalyst properties. But, the specimen with PBA sol did not affect photocatalytic activity due to the presence of rutile phase.

The design of the optical film for absorbent ARAS coating (흡수층을 이용한 무반사, 무정전용 광학박막의 설계)

  • Park, M.C.;Son, Y.B.;Jung, B.Y.;Lee, I.S.;Hwangbo, C.K.
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.5 no.1
    • /
    • pp.7-11
    • /
    • 2000
  • The anti-reflective anti-static (ARAS) optical film is designed using absorbent materials such as ITO, $TiN_xW_y$, Ag by Essential Macleod program. [air ${\mid}TiN_xW_y{\mid}SiO_2{\mid}$ glass] two layer shows wide-band AR coating in the wavelength range of 450~700 nm. The reflectivity, transmittance of this coating are below 0.5%, about 75%, respectively. [air $SiO_2{\mid}TiO_2{\mid}SiO_2{\mid}$, ITO glass] layer can adjust reflectance of below 0.5% with above 97% transmittance. In the [air ${\mid}SiO_2{\mid}TiO_2{\mid}SiO_2{\mid}$ Ag glass] layer, the transmission can be controlled at above 96% with reflectance of 1~2%.

  • PDF

Wear and Friction characteristics of $Cr_2$$O_2$ coating included $SiO_2$ and $TiO_2$ ($SiO_2$$TiO_2$가 첨가된 $Cr_2$$O_3$용사코팅의 마찰 .마멸 특성)

  • 서보현;김태형;김석삼
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2001.11a
    • /
    • pp.69-77
    • /
    • 2001
  • Wear and Friction characteristics of plasma-sprayed Cr$_2$O$_3$ coating and Cr$_2$O$_3$ coating included SiO$_2$ and TiO$_2$ against SiC ball have been investigated under different loads. Worn surfaces were observed by SEM and worn surfaces were analyzed by EDS. The Friction coefficient and the Wear resistance of Cr$_2$O$_3$-5SiO$_2$-3TiO$_2$coating was less than that of Cr$_2$O$_3$ coating. The main mechanisms were plastic deformation and brittle fracture. The film on surface were made by plastic deformation and compacted wear debris. This film protect wear of coating

  • PDF

Studied on the Crystallization of $Li_2O-Al_2O_3-SiO_2$ Glass by Adding $TiO_2$ and $ZrO_2$ ($TiO_2$$ZrO_2$의 첨가에 따르는 $Li_2O-Al_2O_3-SiO_2$ 계 유리의 결정화에 관한 연구)

  • 박용완;전문덕
    • Journal of the Korean Ceramic Society
    • /
    • v.18 no.3
    • /
    • pp.187-191
    • /
    • 1981
  • The effect of additions, $TiO_2$ and $ZrO_2$ as nucleant on the base glass which composition was determined to 0.97 $Li_2O-Al_2O_3-SiO_2$ has been investigated by means of D.T.A., X-ray diffraction and dilatation. $TiO_2$ and $ZrO_2$ as nucleant were added 0.06mole, in which ratios of $TiO_2$/$ZrO_2$ were varied 1/0, 2/1, 1/1, 1/2 and 0/1. The crystalline phases were appeared to $\beta$-spodumene as principal, $\beta$-eucryptite and $ZrO_2$ as secondary, regardless of nucleant variations. The crystallinity of the crystallized glass added $TiO_2$, $ZrO_2$ mixture as nucleant was higher than that of the glass added $TiO_2$ or $ZrO_2$ only. The crystallinity of the glass added $TiO_2$/$ZrO_2$ =1/1 was highest. Increasing the addition of $ZrO_2$, it has been observed that the crystal growing temperature became higher.

  • PDF

Electric Field-activated Self-propagating Synthesis of ${Ti}_{5}{Si}_{3}$ and ${Ti}_{5}{Si}_{3}-{ZrO}_{2}$ Composites (통전 활성 연소에 의한 ${Ti}_{5}{Si}_{3}$${Ti}_{5}{Si}_{3}-{ZrO}_{2}$복합재료 합성)

  • Son, In-Jin;Go, In-Yong
    • Korean Journal of Materials Research
    • /
    • v.6 no.7
    • /
    • pp.709-715
    • /
    • 1996
  • The influence of an electric field on the combustion synthesis of ${Ti}_{5}{Si}_{3}$-x ${ZrO}_{2)$(0 $\leq$ x $\leq$0.6)was investigated. Composite of X $\geq$0.45 can only be synthesized in the presence of an electric field. Although in the absence of an electri field the system with x = 0.45 and x=0.6 can sustain a nonsteady combustion wave, the reaction is not complete. That is, an unstable wave propagates to the middle of the sample and them becomes extinguished. Wave velocity o the ${Ti}_{5}{Si}_{3}-{ZrO}_{2}$ Composites slightly increases with the imposition of external field across the sample.

  • PDF

Synthesis and Hardness of Glass Ceramics for Dental Crown Prosthetic Application in the system CaO-MgO-SiO2-P2O5-TiO2 (치관 보철용 CaO-MgO-$SiO_2-P_2O_5-TiO_2$계 글라스 세라믹의 합성과 경도)

  • Chung, In-Sung;Kim, Kap-Jin;Cheong, HO-Keun;Lee, Jong-Il
    • Journal of Technologic Dentistry
    • /
    • v.21 no.1
    • /
    • pp.5-14
    • /
    • 1999
  • Glass ceramics for dental crown prosthesis were prepared by crystallization of CaO-MgO-SiO2-$P_2O_5-TiO_2$ glasses. Their crystallization behaviors have been investigated as a function of heattreatment temperature, holding time and chemical composition in relation to mechinical properties. Crystallization peak temperatures were determined by differential thermal analysis(DTA). Crystalline phases and mircostructures of heat-treated sample were determined by the means of powder X-ray diffraction(XRD) and scanning electron microscopy(SEM). The final crystalline phase assemblages and the microstructures of the samples were found to be dependent on glass compositions, heattreatment temperature, and holding time. 1st crystallization peak temperature(TP), affected strongly by apatite, was found to be increased or decreased. From the experiment, the following results were obtained : 1. The crystallization peak temperature($T_P$) formed by apatite increased until adding up to 9wt% $TiO_2$ to base glass composition, then decreased above that. 2. Apatite($Ca_{10}P_6O_{25}$), whitlockite(${\beta}-3CaO-P_2O_5$), $\beta$-wollastonite($CaSiO_3$), magnesium tianate($MaTiO_3$) and diopside(CaO-MgO-$2SiO_2$) crystal phase were precipitated in MgO-CaO-$SiO_2-TiO_2-P_2O_5$ glass system containing 9wt% and 11wt% of $TiO_2$ 3. Vickers hardness of samples increased with increasing heat-treatment temperature and Vickers hardness of S415T9 samples heat-treated at 1075 was approxi-mately 813Kg $mm^{-2}$ as maximum value. 4. Vickers hardness of samples increased due to precipitation of apatite, whitlockite, $\beta$-wollastonite, magnesium titanate, and diopside crystal phases within glass matrix.

  • PDF