• Title/Summary/Keyword: $TiO_2-SiO_2$

Search Result 1,732, Processing Time 0.032 seconds

A New process for the Solid phase Crystallization of a-Si by the thin film heaters (박막히터를 사용한 비정질 실리콘의 고상결정화)

  • 김병동;정인영;송남규;주승기
    • Journal of the Korean Vacuum Society
    • /
    • v.12 no.3
    • /
    • pp.168-173
    • /
    • 2003
  • Recently, according to the rapid progress in Flat-panel-display industry, there has been a growing interest in the poly-Si process. Compared with a-Si, poly-Si offers significantly high carrier mobility, so it has many advantages to high response rate in Thin Film Transistors (TFT's). We have investigated a new process for the high temperature Solid Phase Crystallization (SPC) of a-Si films without any damages on glass substrates using thin film heater. because the thin film heater annealing method is a very rapid thermal process, it has very low thermal budget compared to the conventional furnace annealing. therefore it has some characteristics such as selective area crystallization, high temperature annealing using glass substrates. A 500 $\AA$-thick a-Si film was crystallized by the heat transferred from the resistively heated thin film heaters through $SiO_2$ intermediate layer. a 1000 $\AA$-thick $TiSi_2$ thin film confined to have 15 $\textrm{mm}^{-1}$ length and various line width from 200 to 400 $\mu\textrm{m}$ was used as the thin film heater. By this method, we successfully crystallized 500 $\AA$-thick a-Si thin films at a high temperature estimated above $850^{\circ}C$ in a few seconds without any thermal deformation of g1ass substrates. These surprising results were due to the very small thermal budget of the thin film heaters and rapid thermal behavior such as fast heating and cooling. Moreover, we investigated the time dependency of the SPC of a-Si films by observing the crystallization phenomena at every 20 seconds during annealing process. We suggests the individual managements of nucleation and grain growth steps of poly-Si in SPC of a-Si with the precise control of annealing temperature. In conclusion, we show the SPC of a-Si by the thin film heaters and many advantages of the thin film heater annealing over other processes

Microstructures and Hardness of Al-Si Coated 11%Cr Ferritic Stainless Steel, 409L GTA Welds (Al-Si 용융도금된 11%Cr 페라이트 스테인리스강, STS409L GTA 용접부의 미세조직과 경도)

  • Park, Tae-Jun;Kong, Jong-Pan;Na, Hye-Sung;Kang, Chung-Yun;Uhm, Sang-Ho;Kim, Jeong-Kil;Woo, In-Su;Lee, Jong-Sub
    • Journal of Welding and Joining
    • /
    • v.28 no.3
    • /
    • pp.92-98
    • /
    • 2010
  • Ferritic stainless steels, which have relatively small thermal expansion coefficient and excellent corrosion resistance, are increasingly being used in vehicle manufacturing, in order to increase the lifetime of exhaust manifold parts. But, there are limits on use because of the problem related to cosmetic resistance, corrosions of condensation and high temperature salt etc. So, Aluminum-coated stainless steel instead of ferritic stainless steel are utilized in these parts due to the improved properties. In this investigation, Al-8wt% Si alloy coated 409L ferritic stainless steel was used as the base metal during Gas Tungsten Arc(GTA) welding. The effects of coated layer on the microstructure and hardness were investigated. Full penetration was obtained, when the welding current was higher than 90A and the welding speed was lower than 0.52m/min. Grain size was the largest in fusion zone and decreased from near HAZ to base metal. As welding speed increased, grain size of fusion zone decreased, and there was no big change in HAZ. Hardness had a peak value in the fusion zone and decreased from the bond line to the base metal. The highest hardness in the fusion zone resulted from the fine re-precipitation of the coarse TiN and Ti(C, N) existed in the base metal during melting and solidification process and the presence of fine $Al_2O_3$ and $SiO_2$ formed by the migration of the elements, Al and Si, from the melted coating layer into the fusion zone.

A Study of Pore Formation of AAO Film on Si Substrate with Optimizing Process (Si 기판에 제작된 AAO 박막의 기공 형성 최적화에 관한 연구)

  • Kwon, Soon-Il;Yang, Kea-Joon;Song, Woo-Chang;Lee, Jae-Hyeong;Lim, Dong-Gun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.21 no.5
    • /
    • pp.415-420
    • /
    • 2008
  • AAO films were fabricated on two kinds of substrates such as $Al/SiO_2/Si$ and Al/Ni/Ti/Si. To obtain well-aligned AAO film, we optimized process condition for buffer layer, electrolyte and voltage. In the case of oxalic acid, the AAO film with pore size of approximately 45 nm was obtained at voltage of 40 V, temperature of $10^{\circ}C$, oxalic acid of 0.3 M and widening time of 60 min. Then the thickness of barrier is less than 600 nm. In the case of sulfuric acid, the AAO film has pore size of 40 nm and barrier thickness of 400 nm with optimum conditions such as voltage of 25 V, temperature of $8^{\circ}C$, sulfuric acid of 0.3 M and widening time of 60 min.

Dielectric and Electric Properties of Nb Doped PZT Thin Films by Sol-gel Technique (솔-젤법으로 제조한 PZT 박막의 Nb 첨가에 따른 유전 및 전기적 특성)

  • 김창욱;김병호
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.10
    • /
    • pp.1101-1108
    • /
    • 1996
  • No-doped PZT thin films have been fabricated on Pt/Ti/SiO2/Si substrate using Sol-Gel technique. A fast annealing metho (three times of intermediate and final annealing) was used for the preparation of multi-coated 1800$\AA$ thick Nb-doped PZT thin films. As Nb doping percent was increased leakage current was lowered approximately 2 order but dielectic properties were degraded due to the appearance of pyrochlore phase and domain pinning. Futhermore the increase of the final annealing temperature up to 74$0^{\circ}C$lowered the pyrochlore phase content resulting in enhancing the dielectric properties of the Nb doped films. The 3%-Nb doped PZT thin films with 5% excess Pb showed a capacitance density of 24.04 fF/${\mu}{\textrm}{m}$2 a dielectric loss of 0.13 a switchable polarization of 15.84 $\mu$C/cm2 and a coercive field of 32.7 kV/cm respectively. The leakage current density of the film was as low as 1.47$\times$10-7 A/cm2 at the applied voltage of 1.5 V.

  • PDF

Soft Lithographic Patterning Method for Flexible Graphene-based Chemical Sensors with Heaters

  • Kang, Min-a;Jung, Min Wook;Myung, Sung;Song, Wooseok;Lee, Sun Suk;Lim, Jongsun;Park, Chong-Yun;An, Ki-Seok
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2014.02a
    • /
    • pp.176.2-176.2
    • /
    • 2014
  • In this work, we demonstrated that the fabrication of flexible graphene-based chemical sensor with heaters by soft lithographic patterning method [1]. First, monolayer and multilayer graphene were prepared by thermal chemical vapor deposition transferred onto SiO2 / Si substrate in order to fabrication of patterned-sensor and -heater. Second, patterned-monolayer and multilayer graphene were detached through soft lithography process, which was transferred on top and bottom sides of PET film. Third, Au / Ti (Thickness : 100/30 nm) electrodes were deposited end of the patterned-graphene line by sputtering system. Finally, we measured sensor properties through injection of NO2 and CO2 gas on different temperature with voltage change of graphene heater.

  • PDF

Fracture Toughness and Slinding Wear Properties of ABOw/AC4CH by Binder Additives (ABOw/AC4CH의 바인더 종류에 따른 파괴인성 및 미끄럼마모 특성)

  • Park, Won-Jo;Jung, Jae-Wook;Choi, Yong-Bum;Lee, Kwung-Young
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2002.10a
    • /
    • pp.373-378
    • /
    • 2002
  • Metal matrix composites have a great interest in recent years because high specific strength, high specific stiffness characteristics, and application ranges of the composites are extend to variety industry. In this paper, an investigation was performed on the plane strain fracture toughness and slinding wear properties of AC4CH alloy(Al-Si-Mg line) reinforced with 20wt% aluminum borate whisker expect one, which contained a inorganic binder($TiO_2$). the binder led to the formation of strengthen the whisker each other. The test of fracture toughness was using CT(half size) specimen of thickness 12.5mm, width 25mm. and test of slinding wear of using tribo a pin-on-disk machine and lubricant is used without paraffine 8.2CST at room temperature. As results, Fracture toughness $K_{IC}$ is $8.7MPa-m^{05}$ for ABOw/AC4CH, $9.28MPa-m^{05}$ for ABOw/AC4CH added $TiO_2$. but AC4CH alloy was violated the critical stipulated by ASTM standard for valid measurement of $K_{IC}$. In case of, it was performed $J_{IC}$ test instead of $K_{IC}$ based on ASTM E 1820.

  • PDF

Fabrication of Butt-Coupled SGDBR Laser Integrated with Semiconductor Optical Amplifier Having a Lateral Tapered Waveguide

  • Oh, Su-Hwan;Ko, Hyun-Sung;Kim, Ki-Soo;Lee, Ji-Myon;Lee, Chul-Wook;Kwon, Oh-Kee;Park, Sahng-Gii;Park, Moon-Ho
    • ETRI Journal
    • /
    • v.27 no.5
    • /
    • pp.551-556
    • /
    • 2005
  • We have demonstrated a high-power widely tunable sampled grating distributed Bragg reflector (SGDBR) laser integrated monolithically with a semiconductor optical amplifier (SOA) having a lateral tapered waveguide, which is the first to emit a fiber-coupled output power of more than 10 dBm using a planar buried heterostructure (PBH). The output facet reflectivity of the integrated SOA using a lateral tapered waveguide and two-layer AR coating of $TiO_2\;and\;SiO_2$ was lower than $3\;{\times}\;10^{-4}\;over$ a wide bandwidth of 85 nm. The spectra of 40 channels spaced by 50 GHz within the tuning range of 33 nm were obtained by a precise control of SG and phase control currents. A side-mode suppression ratio of more than 35 dB was obtained in the whole tuning range. Fiber-coupled output power of more than 11 dBm and an output power variation of less than 1 dB were obtained for the whole tuning range.

  • PDF

An Analysis of Structural Characteristics in Amorphous Vanadium Oxide ($V_2$$O_5$) Cathode Film for Thin Film Batteries after Cycling by High-resolution Electron Microscopy (HREM) (고분해능 투과전자 현미경을 이용한 박막 전지용 비정질 산화 바나듐 양극 박막의 충-방전에 따른 구조변화 분석)

  • 김한기;성태연;전은정;옥영우;조원일;윤영수
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.3
    • /
    • pp.274-279
    • /
    • 2001
  • Pt/Ti/Si 기판 위에 성장시킨 박막 전지용 비정질 산화 바나듐 박막에 고상 전해질 박막 LiPON을 이용하여 전고상형 박막전지를 제작하여 충-방전 시험을 시행하였다. 이렇게 제작된 전고상형 박막전지는 500 사이클 이상까지 평균 15$\mu$Ah의 방전용량을 나타내었으나 초기 사이클 영역부터 방전 용량의 감소가 일어나기 시작했다. 박막 전지의 방전 용량 감소에 따른 비정질 산화 바나듐 박막의 구조적 특성 변화를 관찰하기 위하여 고분해능 현미경 분석을 시행하였다. 충-방전을 하지 않은 초기의 산화 바나듐 박막은 입계를 갖지 않고 다결정 특성을 보이지 않는 완전한 비정질 특성을 보였고 이는 TED 결과와 일치하였다. 그러나 450번의 반복적인 충-방전을 시행한 후의 비정질 산화 바나듐 박막 내에는 microcrystalline 형태의 산화 바나듐의 형성됨을 고분해능 전자 현미경 분석을 통해 발견할 수 있었다. 비정질 산화바나듐 박막의 방전 용량 감소의 원인인 Li의 비가역적 탈-삽입은 비정질 내에 형성된 microcrystalline에 의해 유발된다고 사료된다. 또한 LiPON 전해질 박막과 산화 바나듐 박막사이의 계면에 Li 이온과 산화바나듐과의 반응에 의해 형성된 계면 층에 발견할 수 있었는데 이러한 계면 층 역시 Li 확산과 계면 저항에 영향을 주어 방전 용량 감소에 원인으로 작용한다.

  • PDF

Anti-Reflection Thin Film For Photoelectric Conversion Efficiency Enhanced of Dye-Sensitized Solar Cells (염료감응형 태양전지의 광전변환효율 향상을 위한 무반사 박막)

  • Jung, Haeng-Yun;Ki, Hyun-Chul;Hong, Kyung-Jin
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.29 no.12
    • /
    • pp.814-818
    • /
    • 2016
  • DSSCs (dye-sensitized solar cells) based on $TiO_2/SiO_2$ multi layer AR (anti-reflection) coating on the outer glass FTO (fluorine-doped tin oxide) substrate are investigated. We have coated an AR layer on the surface of a DSSCs device by using an IAD (ion beam-assisted deposition) system and investigated the effects of the AR layer by measuring photovoltaic performance. Compared to the pure FTO substrate, the multi layer AR coating increased the total transmittance from 67.4 to 72.9% at 530 nm of wavelength. The main enhancement of solar conversion efficiency is attributed to the reduction of light reflection at the FTO substrate surface. This leads to the increase of Jsc and the efficiency improvement of DSSCs.

Color Adjustment Study by Micro-Pattern Embedding in Optical Multilayer Thin Film (다층광학필름에서 마이크로패턴 삽입을 통한 색 조정 연구)

  • Kim, Min;Woo, Ju Yeon;Yoon, Junho;Hwangbo, Chang Kwon;Han, Chang-Soo
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.33 no.5
    • /
    • pp.409-417
    • /
    • 2016
  • It is well known that Morpho butterflies show distinctive, brilliant and iridescent colors and have micro-nano scale structures, instead of dyes and pigments, on their wings. This structural coloration is regarded as a novel technique to express color with a long lifetime, ease and precise tenability. Here, we studied optical multilayer thin films with thickness of several tens of nm ($TiO_2$ and $SiO_2$) and lens-shape micro-patterns. Fabrication and characterization of the multilayer stacking structure and the micro-pattern structure were performed and the films were analyzed via several optical measuring techniques. Finally, we discussed how the micro-pattern structure could enhance independence with color changes according to the viewing angle.