• Title/Summary/Keyword: $TiO_2$thin film

Search Result 1,091, Processing Time 0.026 seconds

Photocatalytic Properties of TiO2 Thin Films Prepared by RF Sputtering (RF Sputtering법으로 제조된 TiO2 박막의 광촉매 특성)

  • Jeong, Min-ho;Jin, Duk-yong;Hayashi, Y.;Choi, Dae-kue
    • Korean Journal of Materials Research
    • /
    • v.13 no.3
    • /
    • pp.185-190
    • /
    • 2003
  • Titanium dioxide films were prepared by RF sputtering method on glass for various oxygen partial pressures at power 270 W. The crystal structure, photocatalytic property and the hydrophilicity of $TiO_2$thin film the deposition conditions were investigated. Crystallized anatase phase was observed in $TiO_2$film deposited at the ratio of oxygen partial pressure 10% and 20% for 2 hrs. As the increase of deposition time, the grain size and void size of $TiO_2$film have increased and also $V_2$films have been good crystallinity. The ultraviolet-visible light absorption of $TiO_2$films was increased with increasing of deposition time and occured chiefly at the wavelength between 280 and 340 nm. The absorption band was shifted to a longer wave length as deposition time increased. Water contact angle on the X$TiO_2$film of anatase structure was decreased with increasing ultraviolet illumination time and became lower than $11^{\circ}$ from $83^{\circ}$. When hydrophilic $TiO_2$film changed by enough ultraviolet illumination was stored in the dark, the film surface gradually turned to hydrophobic state.

Optical and Electrical Properties of $Ti_xSi_{1-x}O_y$ Films

  • Lim, Jung-Wook;Yun, Sun-Jin;Kim, Je-Ha
    • ETRI Journal
    • /
    • v.31 no.6
    • /
    • pp.675-679
    • /
    • 2009
  • $Ti_xSi_{1-x}O_y$ (TSO) thin films are fabricated using plasma-enhanced atomic layer deposition. The Ti content in the TSO films is controlled by adjusting the sub-cycle ratio of $TiO_2$ and $SiO_2$. The refractive indices of $SiO_2$ and $TiO_2$ are 1.4 and 2.4, respectively. Hence, tailoring of the refractivity indices from 1.4 to 2.4 is feasible. The controllability of the refractive index and film thickness enables application of an antireflection coating layer to TSO films for use as a thin film solar cell. The TSO coating layer on an Si wafer dramatically reduces reflectivity compared to a bare Si wafer. In the measurement of the current-voltage characteristics, a nonlinear coefficient of 13.6 is obtained in the TSO films.

Preparation of $\textrm{BaTiO}_3$ Thin Films by Electrochemical Method (전기화학법을 이용한 $\textrm{BaTiO}_3$박막의 제조)

  • Gong, Pil-Gu;Yoo, Young-Sung;Lee, Jong-Kook;Kim, Hwan;Park, Soon-Ja
    • Korean Journal of Materials Research
    • /
    • v.7 no.2
    • /
    • pp.114-120
    • /
    • 1997
  • Perovskite $BaTiO_3$ thin films on stainless steel substrate were prepared by using electrochemical reduction method in solution of $TiCl_4\;and\;Ba(N0_3)_2$. According to current density and electrolysis time. the morphology and thickness of film were varied. Ra/'Ti atomic ratio in $BaTiO_3$ film was controlled by Ha/Ti atomic ratio in solution. Although the excess $TiO_2{\cdot}nH_2O$ film was coated in initial stage of electrolysis. UiilTi atomic ratio in film was nearly constant in later stage. $BaTiO_3$ film precursor was obtained under the condition of $1OmA/cm^2$ current density and Smin electrolysis time. $BaTiO_2$ thin films with perovskite phase were formed 11,. the heat treatment above $500^{\circ}$.

  • PDF

Electrical Properties of $TiO_2$ and $Al_2O_3/TiO_2$ Thin Films Deposited by E-beam Evapration (전자빔 증착법에 의한 $TiO_2$ 박막 및 $Al_2O_3/TiO_2$ 박막의 전기적 특성)

  • Ryu, Hyun-Wook;Park, Jin-Seong
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.04b
    • /
    • pp.5-8
    • /
    • 2004
  • 전자빔 증착법 (e-beam evaporation)를 이용하여 $TiO_2$ 박막과 $Al_2O_3/TiO_2$ 이중박막을 제조한 후, $800^{\circ}C$ 공기 중에서 열처리하여, 알루미나 층의 유무에 따른 두 박막의 전기전도 특성과 100 ppm CO 가스에 대한 반응 특성을 고찰하였다. 알루미나 층이 증착되지 않은 순수한 $TiO_2$ 박막의 전기 전도도 (in dry air)는 $100^{\circ}C-500^{\circ}C$ 온도범위에서 온도가 증가함에 따라 증가하였으며 알루미나 층이 증착된 $Al_2O_3/TiO_2$ 이중막보다 높은 전도도를 나타내고 있으나, 약 $300^{\circ}C$이상의 온도에서는 $Al_2O_3/TiO_2$ 이중막의 전기 전도도가 급격히 증가하여 $TiO_2$ 박막의 전기전도도 보다 더 높은 값을 나타내었다. 또한 온도에 따른 CO 가스 감도(sensitivity)는 $TiO_2$ 박막의 경우 $400^{\circ}C$까지는 서서히 증가하여 그 이상의 온도에서 급격히 감소하였으나, $Al_2O_3/TiO_2$ 이중막은 $250^{\circ}C$에서 감도가 급격히 증가하여 최대값을 나타내었으며, $350^{\circ}C$에서 감도가 급격히 감소하는 특성을 나타내었다.

  • PDF

Preparation and Electric Properties of PbTiO$_3$Thin Films by Low-pressure Thermal Plasma Deposition

  • Nagata, Shingo;Wakiya, Naoki;Shinozaki, Kazuo;Mizutani, Nobuyasu
    • The Korean Journal of Ceramics
    • /
    • v.7 no.1
    • /
    • pp.20-25
    • /
    • 2001
  • PbTiO$_3$ thin films were prepared by low-pressure thermal plasma deposition on (100)Pt/(100)MgO substrates. Mist of source material in which metal alkoxides are dissolved in 2-methoxyethanol was introduced into plasma through heating furnace and deposited onto substrates at $600^{\circ}C$. As-deposited PbTiO$_3$/Pt/MgO thin film prepared at 1.33$\times$10$^4$ Pa was grown epitaxially, but was consisted of many rectangular shaped grains, with many grain boundaries and it was impossible to measure electric properties. As-deposited film prepared at 1.00$\times$10$^4$ Pa showed weak peaks of X-ray diffraction and the film was not grown epitaxially. On the other hand, the film after annealed at $700^{\circ}C$ showed strong diffraction peaks and epitaxial growth was also observed. For annealed film, moreover, no clear grain boundaries were observed. The value of ${\varepsilon}_r$, tan${\delta}$, Pr and Ec of annealed film were 160, 3.2%, 10.4${\mu}$C.cm$^-2$ and 51.2kV.cm$^-1$, respectively. Since the composition, Pb/Ti, measured by EDS attaching to SEM changed point by point, the distribution of composition in annealed film was investigated and found out several relations between composition and electric properties. At stoichiometric composition, Pr and Ec showed the lowest value and they gradually became large as composition deviated from stoichiometric one. Moreover, the value of ${\varepsilon}_r$ became gradually large as the ratio of Ti became high.

  • PDF

Phenomenological Analysis of Piezoelectric Properties in 0.88Pb(Zn1/3Nb2/3)O3−0.12PbTiO3 Single Crystals with an Engineering Domain Configuration

  • Ha, Jong-Yoon;Kim, Jin-Sang;Jeong, Dae-Yong;Kim, Hyun-Jai;Yoon, Seok-Jin
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.3
    • /
    • pp.139-141
    • /
    • 2008
  • The piezoelectric properties of tetragonal 0.88Pb$(Zn_{1/3}Nb_{2/3)O_3-0.12PbTiO_3$ single crystals are characterized along the <111> direction, which composed the engineering domain configuration in the tetragonal phase. The <111>-oriented crystal possessed smaller $d_{33}$ values compared to the crystal along the <001> spontaneous polarization direction. Based on phenomenological theory, it is shown that the engineering domain configuration does not enhance the piezoelectric constant in tetragonal 0.88Pb$(Zn_{1/3}Nb_{2/3)O_3-0.12PbTiO_3$ single crystals. In addition, the electrostrictive coefficients of $Q_{12}=-0.03706m^4/C^2,\;Q_{11}=0.10765m^4/C^2,\;and\;Q_{44}=0.02020m^4/C^2$ of tetragonal 0.88PZN-0.12PT single crystals were calculated.

Electrochemical Behavior of TiO2 Nanotube/Ti Prepared by Anodizing for Micro-Lithium Ion Batteries

  • Park, Soo-Gil;Yang, Jeong-Jin;Rho, Jin-Woo;Kim, Hong-Il;Habazaki, Hiroki
    • Journal of the Korean Electrochemical Society
    • /
    • v.17 no.1
    • /
    • pp.13-17
    • /
    • 2014
  • The $TiO_2$ nanotube/Ti electrode are used as an anode in thin-film lithium microbatteries is known to have high oxidation-reduction potential of 1.8 V (vs. $Li/Li^+$). It can prevent from dendrite growth of lithium during charging. The $TiO_2$ nanotube/Ti electrode was prepared by anodizing at constant voltages for thin-film lithium microbatteries. The capacities of $TiO_2$ nanotube/Ti anode prepared by anodizing at 10 V, 20 V and 30 V were observed to be $23.9{\mu}Ah\;cm^{-2}$, $43.1{\mu}Ah\;cm^{-2}$ and $74.0{\mu}Ah\;cm^{-2}$. We identified it was found that the capacity of $TiO_2$ nanotube/Ti increases with increasing anodizing voltage and the anatase structure of $TiO_2$ nanotube/Ti compared with amorphous structure has batter cycle performance than amorphous $TiO_2$ nanotube/Ti.

Structureal and dielectric properties of $(Pb_{x},Sr_{x-1})TiO_{3}$ thin film for tunable device application (Tunable 소자 응용을 위한 $(Pb_{x},Sr_{x-1})TiO_{3}$ 박막의 구조 및 유전특성)

  • Kim, Kyoung-Tae;Kim, Chang-Il;Lee, Sung-Gap
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.05b
    • /
    • pp.78-81
    • /
    • 2002
  • Ferroelectric thin film is a very attractive material for the tunable microwave device applications such as electronically tunable mixers, delay lines, filters and phase shifters. Thin films of $Pb_{x}Sr_{1-x}TiO3(PST)$ were fabricated onto Pt/Ti/SiO2/Si substrate by the sol-gel method. We have investigated the structural and dielectric properties of PST(50/50) thin films for tunable microwave device applications. The PST thin films show typical polycrystalline structure with a dense microstructure without secondary phase formation. Dielectric properties of PST films are strongly dependent on annealing temperature. The dielectric constants, loss and tunability of the PST (50/50) thin films were 404, 0.023 and 51.73 %, respectively.

  • PDF

Microstructure and Properties of $(Sr_{1-x}Ca_x)TiO_3$Ceramic Thin film ($(Sr_{1-x}Ca_x)TiO_3$세라믹 박막의 미세구조 및 특성)

  • Kim, Jin-Sa;Lee, Jun-Ung
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.50 no.10
    • /
    • pp.504-508
    • /
    • 2001
  • The$(Sr_{1-x}Ca_x)TiO_3$(SCT) thin films are deposited on Pt-coated electrode $(Pt-TiN /SiO_2Si)$ using RF sputtering method at various deposition temperature. The crystallinity of thin films was increased with increased of deposition temperature n the temperature range of 200~500 $[^{\circ}C]$. The capacitance changes almost linearly in temperature ranges of -80~+90$[^{\circ}C]$. All SCT thin films used in the study the phenomena of dielectric relaxation with the increase of frequency, and the relaxation frequency is observed above 200[kHz]. V-I characteristics of SCT thin films show the increasing leakage current with the increases of deposition temperature.

  • PDF

The Complexing Effect of $BaTiO_3\;for\;Bi_4Ti_3O_{12}$ on Layered Perovskite $Bi_4Ti_3O_{12}{\cdot}nBaTiO_3(n=1&2)$ Thin Films ($Bi_4Ti_3O_{12}{\cdot}nBaTiO_3(n=1&2)$ 박막에서 $Bi_4Ti_3O_{12}$ 에 대한 $BaTiO_3$의 복합효과)

  • 신정묵;고태경
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.11
    • /
    • pp.1130-1140
    • /
    • 1998
  • Thin films of $Bi_4Ti_3O_{12}\;nBaTiO_3(n=1&2)$ were prepared using sols erived Ba-Bi-Ti complex alkoxides. The sols were spin-cast onto $Pt/Ti/SiO_2/Si$ substrates and followed by pyrolysis for 1 hr at $620^{\circ}C,\;700^{\circ}C\;and\;750^{\circ}C$ In the thin films a pyrochlore phase seemed to be formed at a lower temperature and then tran-formed to the layered perovskite phase as the heating temperature increased. In the thin films pyrolyzed at formed to the layered perovskte phase as the heating temperature increased. In the films pyrolyzed at $750^{\circ}C$ the amount of $Bi_4Ti_3O_{12}{\cdot}BaTiO_3$ reached to 94% while $Bi_4Ti_3O_{12}{\cdot}BaTiO_3$ was 77% in composition. This result shows that the formation of the layered pervoskite phase becomes difficult as the amount of complexing $BaTiO_3$ increases. The microstructures and the electrical properties of the thin films were gen-erally improved with the incease of the heating temperature. However the presence of the pyrochlore phase could not be removed effectively. Our study showed that the electrical properties of $Bi_4Ti_3O_{12}{\cdot}BaTiO_3$ were pronouncedly improved with complexing with BaTiO3 when compared to those of $Bi_4Ti_3O_{12}$ while the presence of the pyrochlore phase was detrimental to the those of $Bi_4Ti_3O_{12}{\cdot}2BaTiO_3$.