• 제목/요약/키워드: $TiO_2$ additive

검색결과 159건 처리시간 0.031초

SPRAY DEPOSITION OF MECHANICALLY ALLOYED F/M ODS STEEL POWDER

  • SUK HOON KANG;CHANG-KYU RHEE;SANGHOON NOH;TAE KYU KIM
    • Archives of Metallurgy and Materials
    • /
    • 제64권2호
    • /
    • pp.607-611
    • /
    • 2019
  • Thermal/cold spray deposition were used for additive manufacture of oxide dispersion strengthened (ODS) steel layers. Mechanically alloyed F/M ODS steel powders (Fe(bal.)-10Cr-1Mo-0.25Ti-0.35Y2O3 in wt.%) were sprayed by a high velocity oxygen fuel (HVOF) and cold spray methods. HVOF, as a thermal method, was used for manufacturing a 1 mm-thick ODS steel layer with a ~95% density. The source to objective distance (SOD) and feeding rate were controlled to achieve sound manufacturing. Y2Ti2O7 nano-particles were preserved in the HVOF sprayed layer; however, unexpected Cr2O3 phases were frequently observed at the boundary area of the powders. A cold spray was used for manufacturing the Cr2O3-free layer and showed great feasibility. The density and yield of the cold spray were roughly 80% and 45%, respectively. The softening of ODS powders before the cold spray was conducted using a tube furnace of up to 1200℃. Microstructural characteristics of the cold sprayed layer were investigated by electron back-scattered diffraction (EBSD), the uniformity of deformation amount inside powders was observed.

$Bi_2O_3$ 첨가에 의한 Ca[($Li_{1/3}Nb_{2/3}$)$_{1-x}$$Ti_{x}$$O_{3-{\delta}}$ 세라믹스의 마이크로파 유전 특성 (Microwave Dielectric Properties of Ca[($Li_{1/3}Nb_{2/3}$)$_{1-x}$$Ti_{x}$]$O_{3-{\delta}}$ with $Bi_2O_3$ Additives)

  • 하종윤;최지원;이동윤;윤석진;최두진;김현재
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집
    • /
    • pp.131-134
    • /
    • 2002
  • The effect of the addition on the densification, low temperature sintering, and microwave dielectric properties of the Ca[($Li_{1/3}Nb_{2/3}$)$_{1-x}$$Ti_{x}$]$O_{3-{\delta}}$/(CLNT) was investigated. $Bi_2O_3$ additives improved the dencification and reduced the sintering temperature from $1150^{\circ}C$ to $900^{\circ}C$ of CLNT microwave dielectric ceramics. As increasing $Bi_2O_3$ contents, the dielectric constants and bulk density were increased. The quality factor, however, was decreased slighty. The temperature coefficients of the resonant frequency shifted positive value as increasing $Bi_2O_3$ contents. The dielectric properties of Ca[($Li_{1/3}Nb_{2/3}$)$_{1-x}$$Ti_{x}$]$O_{3-{\delta}}$ and Ca[($Li_{1/3}Nb_{2/3}$)$_{0.8}Ti_{0.2}$]$O_{3-{\delta}}$ with 5wt% $Bi_2O_3$ sintered at $900^{\circ}C$ for 3h were $\varepsilon_{r}$=20, 35 Q.$f_{0}$=6500, 11,000 GHz, $\tau_{f}$=4, 13 ppm/$^{\circ}C$, respectively.

  • PDF

반응표면분석법에 의한 $(Zr_{1-x}Sn_x)TiO_4$계 교주파 유전 특성 (Microwave Dielectric Properties of $(Zr_{1-x}Sn_x)TiO_4$ Ceramics in the Response Surface Methodology)

  • 김왕성;최환;문명립;김경용
    • 한국세라믹학회지
    • /
    • 제32권5호
    • /
    • pp.535-542
    • /
    • 1995
  • The effect of sintering temperature, sintering time and forming pressure on microwave dielectric properties of (Zr1-xSnx)TiO4 ceramics containing 1.0wt% B2O3, 0.3 wt% La2O3 and 1.0wt% NiTa2O6 was investigated using the response surface methodology. The optimum values of processing variables were determined based on the reproducibility. The optimum values of the dielectric constant of >35. Q.f0 of >55000 and $\tau$f=$\pm$5 ppm/$^{\circ}C$ could be obtained when the sample was pressed at 500~600kg/$\textrm{cm}^2$ and sintered at 1500~155$0^{\circ}C$ for 2~3 hrs.

  • PDF

($Ba_{1-x}Sr_{x}$)O-$Sm_2O_3$-$TiO_2$세라믹스의 마이크로파 유전특성 (Microwave Dielectric Properties of the ($Ba_{1-x}Sr_{x}$)O-$Sm_2O_3$-$TiO_2$ Ceramics.)

  • 박인길;류기원;배선기;이영희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1995년도 추계학술대회 논문집
    • /
    • pp.5.2-8
    • /
    • 1995
  • 0.15($Ba_{1-x}Sr_{x}$)O-$0.15Sm_2O_3$-$0.7TiO_2$(x=0∼9[m/o]ceramics were fabricated by mixed-oxide method. Microwave dielectric properties were investigated with sintering conditions aid Sr addictive. In the specimen with x=0[m/o] sintered at 1350∼1470[$^{\circ}C$], dielectric constant, quality factor and temperature coefficient of resonant frequency were 70∼74, 2800∼3300(at 3[GHz]), -1.33∼+l.66[ppm/$^{\circ}C$, respectively. Increasing the Sr additive from 0 to 5[m/o], dielectric constant and temperature coefficient of resonant frequency were increased and quality factor was decreased. In the specimen with x=r[m/o] sintered at 1375[$^{\circ}C$], 6[hr], dielectric constant, quality factor and temperature coefficient resonant frequency were 75.62, 2785(at 3[GHz]), +8.39[ppm/$^{\circ}C$], respectively.

pH, duty cycle, 교반, 첨가제가 Ni-TiO2 전기도금 복합체의 TiO2 공석특성과 열적안정성에 미치는 영향 연구 (A Study of pH, Duty Cycle, Agitation on the Property of Co-deposited TiO2 and Thermal Stability in the Electrodeposited Ni-TiO2 Composite)

  • 김명진;김정수;김동진;김홍표;황성식
    • 한국표면공학회지
    • /
    • 제45권3호
    • /
    • pp.97-105
    • /
    • 2012
  • The effects of pH, types of applied current, agitation method and time, additive on the amount of co-deposited $TiO_2$ particles in the matrix were investigated. The deposition rates increased with increasing pH values, while the volume fraction of $TiO_2$ particles and the size of agglomerated $TiO_2$ particles in the composite decreased. The volume fraction of $TiO_2$ particles in the composite decreased when pulsed current of 50% duty cycle was used. And the size of agglomerated $TiO_2$ particles in the nickel matrix of pulsed current was smaller than that of DC current specimen. The volume fraction of $TiO_2$ particles in the matrix decreased with longer time by air agitation, but in case of using magnetic bar, volume fraction in the same range of time was relatively constant. The volume fraction of the electrodeposited Ni-$TiO_2$ composite in the solution containing 0.01 M Dimethylamine borane (DMAB) increased slightly with increasing agitation time regardless of agitation methods. Thermal stability of the electrodeposited Ni-$TiO_2$ composite increased with lower pH at the temperature range of $200{\sim}800^{\circ}C$, and the results showed that the amount of co-deposited $TiO_2$ relies more on the deposition rate than zetapotential of $TiO_2$ particles.

$BaTiO_3$의 유전성에 미치는 $Dy_2O_3$의 영향 (Effect of $Dy_2O_3$ on Dielectric Properties of Barium Titanate)

  • 윤기현;송효일
    • 한국세라믹학회지
    • /
    • 제19권4호
    • /
    • pp.316-320
    • /
    • 1982
  • The effect of the additive on dielectric properties of $BaTiO_3$ containing 0.030 mol% $Dy_2O_3$ was investigated function of frequency from 5$\times$104 to 0.3$\times$107cps and temperature from 25 to 1$25^{\circ}C$. The dielectric constant increased with increasing $Dy_2O_3$ concentration from 0 to 0.05mol% due to space charge polarization. However, the dielectric constant decreased for further increase of $Dy_2O_3$ concentration due to density increase. The dielectric constant exhibits rapid change at the Curie temperature and the Curie temperature drops from 122 to 116$^{\circ}C$ with increasing amount of $Dy_2O_3$ concentration.

  • PDF

$Cr_2$$O_3$가 첨가된 $CaMnO_3$-$CaTiO_3$계 페로브스카이트 써미스터의 전기적 특성 (Electrical Properlies of $Cr_2$$O_3$ Added $CaMnO_3$-$CaTiO_3$ Perovskite Thermistor)

  • 양기호;윤상옥;윤종훈;장성식
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 하계학술대회 논문집
    • /
    • pp.399-402
    • /
    • 2000
  • For improvement of B constant in $CaMnO_3$-$CaTiO_3$ perovskite type thermistors, effect of $Cr_2$$O_3$ addition ranged from 0.0wt% to 5.0wt% on electrical properties were investigated with contents and sintering temperatures in the view of crystal and microstructures. The solubility limit of Cr$_2$O$_3$was up to 0.5wt% judging from the result of lattice parameter. The grain size was decreased and the resistance at room temperature and B constant were increased with the addition of $Cr_2$$O_3$.On particular, B constant of$CaMnO_{3-x}$$Cr_2$$O_3$ system was increased greatly from 1574k to 2598k at 0.5wt% $Cr_2$$O_3$addition. Further addition of $Cr_2$$O_3$, however, resulted in the decrease of the resistance and B constant due to the $Cr_2$$O_3$ precipitation on the grain boundary. As the$CaTiO_3$contents increased in the $CaMnO_3$-$CaTiO_3$ system, the resistance at room temperature and B constant were highly changed.

  • PDF

Ni가 첨가된 $(Zr_{0.8}Sn_{0.2})$TiO$_4$세라믹스의 미세구조와 고주파유전성질 (Microstructure and Microwave Dielectric Properties of Ni-doped $(Zr_{0.8}Sn_{0.2})$TiO$_4$ Ceramics)

  • 이달원;남산;변재동;김명호
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1996년도 추계학술대회 논문집
    • /
    • pp.59-62
    • /
    • 1996
  • The effect of NiO addition on the microstructure and microwave dielectric properties of (Zr$_{0.8}$Sn$_{0.2}$)TiO$_4$(ZST) was investigated. With the NiO addition, a dense ZST body of density higher than 95% has been achieved in the sintering temperature range of 1400 to 150$0^{\circ}C$. Energy dispersive X-ray spectrometry (EDS) analysis of sintered specimen shows the presence of second phase at grain boundaries, which is considered to be NiTiO$_3$. Dielectric constant of the specimen is found to increase linearly with density. Q-values and TC$_{f}$decrease with increasing NiO content. The variation of dielectric properties with NiO content is discussed in term of the second phase. The ZST ceramics with small amount of additive gave $\varepsilon$$_{r}$=38, Q=7000 at 7 GHz and TC$_{f}$=-0.5 ppm/$^{\circ}C$, comparable with the values obtained by previous investigation.stigation.

  • PDF

첨가제에 의한 PWM-PSN-PZT계 세라믹의 유전특성에 관한 연구 (A study on the dielectric characteristics of PWM-PSN-PZT ceramics with additive)

  • 신혜경;송현재;김유신;배선기
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2003년도 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.107-109
    • /
    • 2003
  • This paper was to measure the structure, piezoelectric properties of $0.03Pb(Mg_{0.5}W_{0.5})O_3$ - $0.12Pb(Sb_{0.5}Nb_{0.5})O_3$ - $0.85Pb(Zr_{0.52}Ti_{0.48})O_3$ + $0.5[wt%]MnO_2$ ceramics dropped with additive CuO after manufacturing the specimens with a general method. It is shown that X-ray diffraction pattern variation of lines (211) have tendency to move minutely by addition of additive CuO. According to dropping with Cu, the dielectric constant at 20[$^{\circ}C$] reduced to CuO 3.0[wt%]. In case of sintering at 1050[$^{\circ}C$], dielectric constant was maximum value 623.59 at CuO 1.0[wt%]. Dielectric loss was maximum value 2.7[%] at Cu 2.0[wt%] in case of sintering at 1050[$^{\circ}C$].

  • PDF

포스테라이트계 유전체의 마이크로파 유전특성 (Microwave dielectric properties of Forsterite based Ceramics)

  • 김동영;이홍열;전동석;이상석
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 추계학술대회 논문집 Vol.16
    • /
    • pp.279-282
    • /
    • 2003
  • For the millimeter-wave dielectrics, Forsterite-based ceramics were produced. Pure forsterite ceramics($Mg_2SiO_4$) shows porous micro-structure and very low Q*f values, which is not suitable for the dielectrics for the millimeter-wave band. Several sintering aids including $Al_2O_3$, $Li_2CO_3$, $Li_2SiO_4$, were added to the forsterite ceramics in order to produce dense low-loss dielectrics. Among these additives, $Li_2CO_3$ is the most effective sintering aids. Several sub-components including NiO, ZnO, $SnO_2$, $TiO_2$, were added to enhance the microwave dielectric properties. $TiO_2$ is the most effective additive to enhance the dielectric properties at microwave bands. The simultaneous addition of $TiO_2$ and $Li_2CO_3$ increases Q*f value over 170,000, which can be used as dielectrics in millimeter-wave bands.

  • PDF