• 제목/요약/키워드: $Ti^+$

검색결과 14,638건 처리시간 0.045초

반응결합 소결에 의한 SiC-TiC계 복합재료 제조 (Manufacture of SiC-TiC System Composite by the Reaction-Bonded Sintering)

  • 한인섭;김홍수;우상국;양준환;정윤중
    • 한국세라믹학회지
    • /
    • 제31권8호
    • /
    • pp.849-860
    • /
    • 1994
  • The microstructural evolution and crystalline phases of this infiltration of Ti+Al liquids in TiC, SiC, TiC+C, and SiC+C preforms have been investigated. As the Ti and Al mixing ratio in Ti+Al infiltrated liquid changes, the newly formed reaction products, which were reacted from the Ti+Al liquid with preforms, consisted of three major phases as Ti3AlC, Al2Ti4C2 or Al4C3. The TiC grain shape was changed to spheroid, when Ti3AlC was formed. In case of Al2Ti4C2 formation, the platelet grain was formed from the original TiC grain. When Al4C3 was formed, nodular or intergranular fine-grained Al4C3 was formed around the TiC grain, while the original TiC grain shape was not changed.

  • PDF

Dissolution and Reprecipitation Behavior of TiC-TiN-Ni Cermets During Liquid-Phase Sintering

  • Yoon, Choul-Soo;Shinhoo Kang;Kim, Doh-Yeon
    • The Korean Journal of Ceramics
    • /
    • 제3권2호
    • /
    • pp.124-128
    • /
    • 1997
  • An attempt was made to understand the dissolution and reprecipitation behavior of the constituent phases such as TiC, TiN, and Ti(CN) in TiC-TiN-Ni system. During the liquid-phase sintering the TiC phase was found to dissolve preferentially in Ni binder. The solid-solution phase, Ti(CN), formed around the TiN phase, resulting in a core/rim structure. This result was reproduced when large TiC particles were used with fine TiN particles. The path for the microstructural change in TiC-TiN-Ni system was largely controlled by the difference in the interfacial energy of each phase with the liquid binder phase. The results were discussed with thermodynamic principles.

  • PDF

아크이온 플레이팅법으로 WC-Co에 증착된 TiN 및 TiAlN박막의 충격특성 비교 (Comparative study on impact behavior of TiN and TiAlN coating layer on WC-Co substrate using Arc ion Plating Technique)

  • 윤순영;류정민;윤석영;김광호
    • 한국표면공학회지
    • /
    • 제35권6호
    • /
    • pp.408-414
    • /
    • 2002
  • TiN and TiAlN coating layer were deposited on WC-Co steel substrates by an arc ion plating(AIP) technique. The crystallinity and morphology for the deposited coating layers were characterized by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The impact behaviors of the deposited TiN and TiAlN coating layer were investigated with a ball-on-plate impact tester. Beyond $10^2$ impact cycle, TiAlN coating layer showed superior impact wear resistance compared to TiN coating layer. On the other hand, both TiN and TiAlN coating layers started to be partially failed between $10^2$ and $10^3$ impact cycle. Above $10^3$ impact cycle, TiN and TiAlN coating layers showed similar impact behavior because of the substrate effect.

Research on Microstructure and Properties of TiN, (Ti, Al)N and TiN/(Ti, Al)N Multilayer Coatings

  • Wang, She Quan;Chen, Li;Yin, Fei;Jia, Li
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part 1
    • /
    • pp.658-659
    • /
    • 2006
  • Magnetron sputtered TiN, (Ti, Al)N and TiN/(Ti, Al)N multilayer coatings grown on cemented carbide substrates have been characterized by using electron probe microanalysis (EPMA), X-ray diffraction (XRD), scanning electron spectroscopy (SEM), nanoindentation, scratcher and cutting tests. Results show that TiN coating is bell mouth columnar structures, (Ti, Al)N coating is straight columnar structures and the modulation structure has been formed in the TiN/(Ti, Al)N multilayer coating. TiN/(Ti, Al)N multilayer coating exhibited higher hardness, better adhesion with substrate and excellent cutting performance compared with TiN and (Ti, Al)N coating.

  • PDF

CaTiO$_3$및 CaTiO$_3$-TiO$_2$세라믹스의 마이크로파 유전특성 (Microwave Dielectric Properties of CaTiO$_3$and CaTiO$_3$-TiO$_2$Ceramics)

  • 홍석경;윤중락;김경용
    • 한국통신학회논문지
    • /
    • 제18권8호
    • /
    • pp.1102-1107
    • /
    • 1993
  • CaO-TiO2 이성분계에서 40~50 mol% CaO 조성범위를 선택하여 CaTiO3과 CaTiO3-TiO2세라믹스의 마이크로파 유전특성을 조사하였다. CaTiO3 단일상 (50 mol% CaO조성)일 때 유전율(er) 178, 공진주파수 (fo)의 온도계수(r,)+1000ppm/C, 픔질계수인 Q값 2760(fo=2.7 GHz)으로 가장 큰 값을 나타내었다. CaTiO3와 TiO2상이 혼합상으로 있는 유전체에서는 CaO 함량이 감소함에 따라서 유전율과 공진주파수의 온도계수는 점차 감소하였으나 Q값과 밀도는 47 mol% CaO조성에서 가장 낮았다. 이것은 이상 혼합 세라믹에서 TiO2상의 감소로 인해 CaTiO3의 결정립 성장이 급속하게 일어남으로써 입계와 입내에 큰 기공이 존재하지 때문으로 생각된다.

  • PDF

$Bi_4Ti_3O_{12}{\cdot}nBaTiO_3(n=1&2)$ 박막에서 $Bi_4Ti_3O_{12}$ 에 대한 $BaTiO_3$의 복합효과 (The Complexing Effect of $BaTiO_3\;for\;Bi_4Ti_3O_{12}$ on Layered Perovskite $Bi_4Ti_3O_{12}{\cdot}nBaTiO_3(n=1&2)$ Thin Films)

  • 신정묵;고태경
    • 한국세라믹학회지
    • /
    • 제35권11호
    • /
    • pp.1130-1140
    • /
    • 1998
  • Thin films of $Bi_4Ti_3O_{12}\;nBaTiO_3(n=1&2)$ were prepared using sols erived Ba-Bi-Ti complex alkoxides. The sols were spin-cast onto $Pt/Ti/SiO_2/Si$ substrates and followed by pyrolysis for 1 hr at $620^{\circ}C,\;700^{\circ}C\;and\;750^{\circ}C$ In the thin films a pyrochlore phase seemed to be formed at a lower temperature and then tran-formed to the layered perovskite phase as the heating temperature increased. In the thin films pyrolyzed at formed to the layered perovskte phase as the heating temperature increased. In the films pyrolyzed at $750^{\circ}C$ the amount of $Bi_4Ti_3O_{12}{\cdot}BaTiO_3$ reached to 94% while $Bi_4Ti_3O_{12}{\cdot}BaTiO_3$ was 77% in composition. This result shows that the formation of the layered pervoskite phase becomes difficult as the amount of complexing $BaTiO_3$ increases. The microstructures and the electrical properties of the thin films were gen-erally improved with the incease of the heating temperature. However the presence of the pyrochlore phase could not be removed effectively. Our study showed that the electrical properties of $Bi_4Ti_3O_{12}{\cdot}BaTiO_3$ were pronouncedly improved with complexing with BaTiO3 when compared to those of $Bi_4Ti_3O_{12}$ while the presence of the pyrochlore phase was detrimental to the those of $Bi_4Ti_3O_{12}{\cdot}2BaTiO_3$.

  • PDF

금속간 화합물 NiTi와 순금속 니켈 및 티타늄의 전기화학적 부식 특성 (Electrochemical Corrosion Characteristics of the Intermetallic Compound NiTi from Pure Metals)

  • 이규환;신명철
    • 분석과학
    • /
    • 제5권1호
    • /
    • pp.97-101
    • /
    • 1992
  • 순수한 니켈과 티타늄이 같은 양 함유되어 있는 NiTi 금속간 화합물의 인공 생리식염수에서의 부식 특성을 순수한 니켈 및 티타늄과 함께 연구하였다. Tafel 외삽법과 선형 분극법 공히 유사한 결과를 보였으며, 부식 전류 Icorr와 부식 속도는 다음과 같은 순서로 증가하였다. NiTi

  • PDF

EB-PVD법에 의한 Ti/TiN film 코팅된 스테인리스강 소결체의 표면특성 (The Surface Characteristics of Ti/TiN Film Coated Sintered Stainless Steels by EB-PVD Method)

  • 최한철
    • 한국표면공학회지
    • /
    • 제34권3호
    • /
    • pp.195-205
    • /
    • 2001
  • The surface characteristics of Ti/TiN films coated on sintered stainless steels (SSS) by electron beam physical vapour deposition (EB-PVD) were investigated. Stainless steel compacts containing 2, 4, and 10wt%Cu were prepared by the electroless Cu-plating method, which results in increased homogenization in the alloying powder. The specimens were coated with Ti and TiN with a 1.0$\mu\textrm{m}$ thickness respectively by EB-PVD. The microstructures were investigated using scanning electron microscopy (SEM). The corrosion behaviors were investigated using a potentiosat in 0.1 M $H_2$$SO_4$, and 0.1M HCl solutions and the corrosion surface was observed using SEM and XPS. The Ti coated specimens showed rough surface compared to Ti/TiN coated specimens. Ti and Ti/TiN coated SSS revealed a higher corrosion and pitting potential from anodic polarization curves than that of Ti and Ti/TiN uncoated SSS. In addition, Ti/TiN coated SSS containing 10wt% Cu exhibited good resistance to pitting corrosion due to the formation of a dense film on the surface and the decrease in interconnected porosity by electroless coated Cu.

  • PDF

치과주조용 Ti-Zr-(Cu)계 합금의 경도 및 미세조직 (Hardness and Microstructures of Ti-Zr-(Cu) based Alloys for Dental Castings)

  • 주규지
    • 대한치과기공학회지
    • /
    • 제27권1호
    • /
    • pp.65-71
    • /
    • 2005
  • Experimental Ti-13%Zr and Ti-13%Zr-5%Cu alloys were made in an argon-arc melting furnace. The grade 2 CP Ti was used to control. The alloys were cast into phosphate bonded $SiO_2$ investment molds using an argon-arc casting machine, and The hardness and microstructures of the castings were investigated in order to reveal their possible use for new dental casting materials and to collect useful data for alloy design. The hardness of the Ti-13%Zr-5%Cu alloy(379Hv) became higher than that of Ti-13%Zr(317Hv) alloy, and the hardness of this alloys became higher than that of CP Ti(247Hv). Increasing in the hardness of the Ti-13%Zr-5%Cu alloy was considered to be solid solution hardening as the Ti-Zr system shows a completely solid solution for both high temperature $\beta$phase and low temperature $\alpha$ phase and also the inclusion of the eutectoid structure($\alpha Ti+Ti_{2}Cu$). No martensitic structures are observed in the specimen made of CP Ti, but Ti-13%Zr and Ti-13%Zr-5%Cu alloys show a kind of martensitic structure. Ti-13%Zr-5%Cu shows the finest microstructure. From these results, it was concluded that new alloys for dental casting materials should be designed as Ti-Zr-Cu based alloys.

  • PDF

ALD법으로 증착한 TiN막의 특성 (Physical Properties of TiN films grown by ALD)

  • 김재범;홍현석;오기영;이종무
    • 한국진공학회지
    • /
    • 제11권3호
    • /
    • pp.159-165
    • /
    • 2002
  • 본 연구에서는 $TiCl_4$$NH_3$을 이용하여 atomic layer deposition(ALD)법으로 TiN막을 증착한 후, 그 막의 특성에 관하여 조사하였다. 최적 공정조건에서 TiN막의 성장률은 cycle당 두께가 약 0.6 $\AA$인 것으로 나타났고, 비저항은 반응온도 구간에서 200~350 $\mu\Omega$cm 수준으로 낮게 얻어졌다. XRD분석결과 TiN-ALD온도구간에서 TiN막이 결정화되었음을 알 수 있었다. AES 분석결과 Cl불순물의 함량이 거의 없는 상태(<1 at%)로 나타났고, TiN막에서의 Ti:N비가 1:1인 것으로 보아 거의 균일하게 형성되었음을 알 수 있었다. 또한 SEM관찰로 Aspect ratio 10:1의 trench 내에 형성된 TiN막의 스텝.커버리지는 극히 우수함을 알 수 있었다.