Research on residual stress in SiCf reinforced titanium matrix composites

  • Qu, Haitao;Hou, Hongliang;Zhao, Bing;Lin, Song
    • Steel and Composite Structures
    • /
    • 제17권2호
    • /
    • pp.173-184
    • /
    • 2014
  • This study aimed to theoretical calculate the thermal residual stress in continuous SiC fiber reinforced titanium matrix composites. The analytical solution of residual stress field distribution was obtained by using coaxial cylinder model, and the numerical solution was obtained by using finite element model (FEM). Both of the above models were compared and the thermal residual stress was analyzed in the axial, hoop, radial direction. The results indicated that both the two models were feasible to theoretical calculate the thermal residual stress in continuous SiC fiber reinforced titanium matrix composites, because the deviations between the theoretical calculation results and the test results were less than 8%. In the titanium matrix composites, along with the increment of the SiC fiber volume fraction, the longitudinal property was improved, while the equivalent residual stress was not significantly changed, keeping the intensity around 600 MPa. There was a pronounced reduction of the radial residual stress in the titanium matrix composites when there was carbon coating on the surface of the SiC fiber, because carbon coating could effectively reduce the coefficient of thermal expansion mismatch between the fiber and the titanium matrix, meanwhile, the consumption of carbon coating could protect SiC fibers effectively, so as to ensure the high-performance of the composites. The support of design and optimization of composites was provided though theoretical calculation and analysis of residual stress.

2.5D Cf/SiCm 복합재의 기계적 물성 시험과 탄소성 모델링을 통한 유한요소해석 (Finite Element Analysis Through Mechanical Property Test and Elasto-plastic Modeling of 2.5D Cf/SiCm Composite Analysis)

  • 이민정;김연태;이연관
    • 한국항공우주학회지
    • /
    • 제48권9호
    • /
    • pp.663-670
    • /
    • 2020
  • 2.5D C/SiC를 적용한 구조물의 거동 특성을 유한요소해석으로 근사하기 위해 기계적 물성 특성화와 모델링 기법에 관한 연구를 수행하였다. 2.5D C/SiC 소재의 거동 특성을 분석하기 위해 인장시험을 수행하였고 수학적 균질화 기법과 수정된 혼합 법칙을 적용하여 2.5D C/SiC를 구성하는 섬유와 기지의 탄성 물성을 정의하였다. 탄소성 거동을 나타내는 기지는 소성 영역의 거동을 bilinear 함수로 근사하고 시험과 해석의 오차를 최소화하여 등가 항복 강도와 등가 소성 강성을 계산하였다. 그리고 2.5D C/SiC의 RVE를 정의하고 수정된 혼합 법칙을 적용하여 유효강성행렬을 계산하는 과정을 ABAQUS의 User-defined subroutine을 통해 구성하였다. 제안된 과정을 바탕으로 정의된 섬유와 기지의 기계적 물성을 적용하여 유한요소해석을 수행한 결과는 시험의 거동을 잘 근사하고 있음을 확인하였다.

반응소결된 다공성 뮬라이트의 미세구조 제어 (Microstructure Control of Reaction-Sintered Porous Mullite)

  • 조범래;윤상렬;강종봉
    • Composites Research
    • /
    • 제13권5호
    • /
    • pp.31-36
    • /
    • 2000
  • 금속/세라믹 복합체의 강화제로 사용가능한 다공성 뮬라이트 제조 시 공정변수 변화가 침상형 미세구조 형성에 미치는 영향에 대해 고찰하였다. 출발물질을 $Al_2O_3+SiO_2$$Al(OH)_3+SiO_2$로 달리하여 미세구조 변화를 고찰한 결과, $Al_2O_3$보다 반응성이 우수한 $Al(OH)_3$를 사용한 시편에서 더욱 발달한 침상형 구조가 나타났으며, 첨가제 $AlF_3$의 함량이 증가할수록, $SiF_4$가 발생하는 온도구간인 $900^{\circ}C$에서 유지하는 시간이 길수록 반응을 잘 일어나 시편 전체에서 침상형 뮬라이트가 형성되었다. 소결 온도의 경우 $1200^{\circ}C$에서부터 뮬라이트가 생성되었고, 소결 온도변화에 따른 미세구조는 큰 변화를 관찰할 수 없었다. 기공률은 첨가제의 양이 증가할수록, $900^{\circ}C$에서의 유지시간이 길수록 증가하였다.

  • PDF

Mechanical Properties of Cf/SiC Composite Using a Combined Process of Chemical Vapor Infiltration and Precursor Infiltration Pyrolysis

  • Kim, Kyung-Mi;Hahn, Yoonsoo;Lee, Sung-Min;Choi, Kyoon;Lee, Jong-Heun
    • 한국세라믹학회지
    • /
    • 제55권4호
    • /
    • pp.392-399
    • /
    • 2018
  • $C_f/SiC$ composites were prepared via a process combining chemical vapor infiltration (CVI) and precursor infiltration pyrolysis (PIP), wherein silicon carbide matrices were infiltrated into 2.5D carbon preforms. The obtained composites exhibited porosities of 20 vol % and achieved strengths of 244 MPa in air at room temperature and 423 MPa at $1300^{\circ}C$ under an Ar atmosphere. Carbon fiber pull-out was rarely observed in the fractured surfaces, although intermediate layers of pyrolytic carbon of 150 nm thickness were deposited between the fiber and matrix. Fatigue fracture was observed after 1380 cycles under 45 MPa stress at $1000^{\circ}C$. The fractured samples were analyzed by transmission electron microscopy to observe the distributed phases.

탄소-탄소 복합재료의 하프늄 탄화물 코팅재의 열적/기계적 특성 (Thermal/Mechanical Properties of Hafnium Carbide Coatings on Carbon-Carbon Composites)

  • 최소담;서형일;임병주;신인철;이정민;박종규;이기성
    • Composites Research
    • /
    • 제31권5호
    • /
    • pp.260-266
    • /
    • 2018
  • 본 논문에서는 C/C-SiC 복합재료의 하프늄 탄화물 코팅재에 대한 열적, 기계적 특성을 평가하였으며 특히 코팅에 의한 내산화성과 내마모성의 향상여부를 평가하였다. 하프늄 탄화물(HfC)을 용사시켜 코팅한 샘플들을 가공한 후, 공기 중에서 열적 특성평가 및 마모, 압입시험 평가에 대한 연구를 수행하였다. 공기 중에서 $1200^{\circ}C$의 온도까지 승온시킨 후 1시간 유지하는 싸이클을 10싸이클 진행하여 각 싸이클마다의 무게변화를 통해 탄소의 산화저항성을 평가하였고, 초경 구(tungsten carbide)를 사용하여 마모시험과 압입시험을 수행하여 그 결과를 비교하였다. 열피로 시험 수행 결과 하프늄 탄화물 코팅재가 상대적으로 무게감소가 적어 상대적으로 내산화성이 높은 것으로 평가되었다. 코팅된 하프늄 탄화물에 의해 탄성계수가 상대적으로 증가하였으며, 또한 C/C-SiC 복합재료는 하프늄 탄화물의 코팅에 의하여 내마모성이 향상되어 동일조건에서 마모량이 상대적으로 적었고 낮고 안정된 마찰계수가 유지되었다.

습식법으로 제조된 BN 중간층을 가진 Cf/SiC 복합재의 제조 및 물성 평가 (Fabrication and Characterization of Cf/SiC Composite with BN Interphase Coated by Wet Chemical Process)

  • 구준모;김경호;한윤수
    • 한국표면공학회지
    • /
    • 제50권6호
    • /
    • pp.523-530
    • /
    • 2017
  • In this study, we developed the h-BN interphase for ceramic matrix composites (CMCs) through a wet chemical coating method, which has excellent price competitiveness and is a simple process as a departure from the existing high cost chemical vapor deposition method. The optimum condition for nitriding an h-BN interphase using boric acid and urea as precursors were derived, and the h-BN interphase coating through a wet method on a carbon preform of 2.5 D was conducted to apply the optimum conditions to the CMCs. In order to control the coating property via the wet coating method, four parameters were investigated such as dipping time of the specimen in the precursor solution, the ratio of boric acid and urea in the precursor, the concentration of solution where the precursor was dissolved, and the cycle of dipping and dry process. The CMCs was fabricated through polymer impregnation and pyrolysis (PIP) processes and a three-point flexural strength test was conducted to verify the role of the coated h-BN interphase.

$CaF_2$가 Filler로 첨가된 유리복합체의 고주파 유전특성 (High Frequency Dielectric Properties of $CaF_2$ filled Glass-Composites)

  • 김선영;이경호;김성원
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 춘계학술대회 논문집 센서 박막재료 반도체 세라믹
    • /
    • pp.277-281
    • /
    • 2003
  • Effects of $CaF_2$ addition as a filler on the high frequency dielectric properties and sintering of CaO-$Al_2O_3-SiO_2-B_2O_3$(CASB) and ZnO-MgO-$B_2O_3-SiO_2$(ZMBS) glass composites were investigated. The optimal glass composition in the CASB system was 33.0CaO-$17.0Al_2O_3-35.0SiO_2-15.0B_O_3$(in wt%). The corresponding dielectric properties were k=8.1 and $Q{\times}fo$=1,200GHz. The sintering temperature was $800{\mu}m$. In case of 2MBS system, 25.0ZnO-25.0MgO-20.0$B_2O_3-30.0SiO_2$(in wt%) glass showed k=6.8 and $Q{\times}fo$=5,200GHz when it was sintered at $750^{\circ}C$. The maximum amount of $CaF_2$ in the CASB and 2MBS glass system without any detrimental effect on the sintering was 25.0 v/o and 15.0 v/o, respectively. The addition of $CaF_2$ in the glass systems improved the high frequency dielectric properties. In case of CASB+$CaF_2$ composite, k was 7.1 and $Q{\times}fo$ was 2,300GHz. And in case of 2MBS+$CaF_2$ composite, k was 5.9 and $Q{\times}fo$ was 8,100GHz. $CaF_2$ addition also reduced sintering temperature. Effects of $CaF_2$ on the dielectric and sintering properties was analyzed in terms of viscosity and crystallization behavior changes due to the interaction between $CaF_2$ and the glass systems.

  • PDF

저온 소결 세라믹스용 SiO2-B2O3-R(CaO, BaO, ZnO, Bi2O3 붕규산염계 세라믹/유리 복합체의 특성 (The Properties on Ceramic/glass Composites of SiO2-B2O3-R(CaO, BaO, ZnO, Bi2O3 Borosilicate Glass System for Low Temperature Ceramics)

  • 김관수;윤상옥;심상흥;박종국
    • 한국전기전자재료학회논문지
    • /
    • 제20권1호
    • /
    • pp.19-24
    • /
    • 2007
  • The effects of $B_2O_3-SiO_2-R(R;CaO,\;BaO,\;ZnO,\;Bi_2O_3)$ borosilicate glass system on the sintering behavior and microwave dielectric properties of ceramic/glass composites were investigated as functions of modifier, glass addition ($30{\sim}50\;vol%$) and sintering temperature ($500{\sim}900^{\circ}C$ for 2 hrs). The addition of 50 and 45 vol% glass ensured successful sintering below $900^{\circ}C$. Sintering characteristics of the composites were well described in terms of modifier. Borosilicate glass enhanced the reaction with $Al_{2}O_{3}$ to form pores, second phases and liquid phases, which was responsible to component of modifier. Dielectric constant (${\varepsilon}_{r},\;Q{\times}f_{o}$) and temperature coefficient of resonant frequency (${\tau}_{f}$) of the composite with 50 and 45 vol% glass contents($B_{2}O_{3}:SiO_{2}:R=25:10:65$) demonstrated A-CaBS(7.8, 2,560 GHz, -81ppm/$^{\circ}C$), A-BaBs(5.8, 3.130 GHz, -64 ppm/$^{\circ}C$), A-ZnBS(5.7, 17,800 GHz, -21 ppm/$^{\circ}C$), A-BiBs(45 vol% glass in total)(8.3, 2,700 GHz, -45 ppm/$^{\circ}C$) which is applicable to substrate requiring an low dielectric properties.

Pt/Ti/Si 기판위에 형성시킨 PZT박막의 특성 (Characterizations of Sputtered PZT Films on Pt/Ti/Si Substrates.)

  • 황유상;백수현;백상훈;박치선;마재평;최진석;정재경;김영남;조현춘
    • 한국재료학회지
    • /
    • 제4권2호
    • /
    • pp.143-151
    • /
    • 1994
  • $(PbZr_{52},Ti_{48})O_{3}$인 composite ceramic target을 사용하여 R. F. 마그네트론 스퍼터링 방법으로 기판온도 $300^{\circ}C$에서 Pt/Ti/Si 기판위에 PZT 박막을 증착하였다. 페롭스 카이트 PZT박막을 얻기 위하여 PbO분위기에서 로열처리를 행하였다. 하부전극으로 Pt를 사용하였으며 Pt(205$\AA$)/Ti(500 $\AA$)/Si 및 Pt(1000$\AA$)/Ti(500$\AA$)/Si기판을 준비하여 Pt두께화 Ti층이 산소의sink로 작용함으로서 이를 가속화하였다. Ti층의 상부는 산소의 확산으로 인하여 TiOx층으로 변태하였고 하부는 in diffused Pt와 함께 실리사이드층을 형성하였다. TiOx 층의 형성은PZT층의 방향성에 영향을 주었다. 유전상수 (10kHz), 누설전류, 파괴전압, 잔류분극 및 항전계는 각각 571, 32,65$\mu A /\textrm{cm}^2$, 0.40MV/cm, 3.3$\mu C /\textrm{cm}^2$, 0.15MV/cm이었다.

  • PDF

$Al_2O_{3f}/SiC_p$ 금속복합재료의 섬유방향과 혼합비가 윤활마모특성에 미치는 영향 (Effects of Fiber Orientations and Hybrid Ratios on Lubricant Tribological Characteristics of $Al_2O_{3f}/SiC_p$ Reinforced MMCs)

  • 왕일기;송정일
    • Composites Research
    • /
    • 제22권5호
    • /
    • pp.15-23
    • /
    • 2009
  • 가압주조법으로 제조한 $Al_2O_3$ 섬유와 SiC 입자 혼합 보강 금속복합재료(MMCs)의 상온과 고온에서 윤활마모특성을 조사하였다. 마모시험은 거리와 온도의 변화에 따라 속도를 고정시켜 25Kgf의 하중하에서 수행하였으며 MMCs의 시험편은 가압의 수평(PR)방향과 수직(N)방향에서 채취하였다. 혼합비의 영향을 관찰한 결과 상온에서는 20%섬유만 보강한 PR방향 MMCs의 마모거동은 N방향 보다 우수한 결과를 보였으나, 혼합보강 MMCs는 반대로 나타내었다. 고온($100^{\circ}C$)에는 모든 MMCs에서 PR방향의 마모거동이 N 방향보다 우수한 결과를 보인 것은 보강재와 마찰면간 윤활필름이 강호작용에 기인한 것으로 밝혀졌다. $150^{\circ}C$에서는 혼합 MMCs의 마모거동은 온도영향으로 PR이 N 보다 우수한 결과를 보였다.