A Study on the Luminescence Properties of LiGd9(SiO4)6O2:Ce3+ (LiGd9(SiO4)6O2:Ce3+ 형광 특성 연구)

  • Jin, Seongjin
    • Journal of the Korean Society of Radiology
    • /
    • v.9 no.3
    • /
    • pp.169-174
    • /
    • 2015
  • $LiGd_9(SiO_4)_6O_2:Ce^{3+}$ phosphors were synthesized by solid-state reaction method. The structural characteristic was investigated by X-ray powder diffraction analysis. The emission and excitation spectra of the $Ce^{3+}$ ions doped $LiGd_9(SiO_4)_6O_2$ phosphors were obtained under the UV excitation. The emission spectra of $LiGd_9(SiO_4)_6O_2:Ce^{3+}$ shows the band at 410 nm corresponding to the $^2F_{5/2}$ and $^2F_{7/2}$ states of $Ce^{3+}$. The red shift of $Ce^{3+}$ emission is found as the $Ce^{3+}$ concentration increases, which could be explained by the change in crystal-field symmetry and strength with increasing $Ce^{3+}$ concentration. Fluorescence decay time of $Ce^{3+}$ was about 20 ns. When the concentration of $Ce^{3+}$ increases life time was slightly reduced.

Hydrogen Permeation of SrCe0.95Gd0.05O3-α-Ce0.9Gd0.1O2-β Proton-Conducting Ceramic Membranes (프로톤 전도성 SrCe0.95Gd0.05O3-α-Ce0.9Gd0.1O2-β 복합체 멤브레인의 수소투과 특성)

  • Kim, Hwan-Soo;Yu, Ji-Haeng;Shin, Min-Jae
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.22 no.2
    • /
    • pp.161-167
    • /
    • 2011
  • Proton conductors have attracted considerable attention for solid oxide fuel cell (SOFC), hydrogen pump, gas sensor, and membrane separators. Doped $SrCeO_3$ exhibits appreciable proton conductivity in hydrogen-containing atmosphere at high temperature. However commercial realization has been hampered due to the reactivity of $SrCeO_3$ with $CO_2$. The chemical stability and proton conductivity are dependent on dopant type. The purpose of this work is to investigate chemical stability of $SrCe_{0.95}Gd_{0.05}O_{3-\alpha}-Ce_{0.9}Gd_{0.1}O_{2-\beta}$ composites in $CO_2$ and $H_2$ gases. Thermogravimetric analysis (TGA) was performed in gaseous $CO_2$ and electrical conductivity of the composites were also measured between 500 and $900^{\circ}C$ in air and $H_2$ atmosphere. $SrCe_{0.95}Gd_{0.05}O_{3-\alpha}-Ce_{0.9}Gd_{0.1}O_{2-\beta}$ composite membranes showed good chemical stability of in $CO_2$ atmosphere and high conductivity at hydrogen condition. The hydrogen permeation of $SrCe_{0.95}Gd_{0.05}O_{3-\alpha}-Ce_{0.9}Gd_{0.1}O_{2-\beta}$ composite membranes was investigated as a function of volumetric content of $SrCe_{0.95}Gd_{0.05}O_{3-\alpha}$. The $SrCe_{0.95}Gd_{0.05}O_{3-\alpha}-Ce_{0.9}Gd_{0.1}O_{2-\beta}$(6:4) membrane with a thickness of 1.0 mm showed the highest hydrogen permeability with the flux reaching of 0.12 $ml/min{\cdot}cm^2$ at $800^{\circ}C$ in 100%$H_2/N_2$ as feed gas.

Electrical Properties of Ultrafine $(CeO_2)_{0.9}(Gd_2O_3)_{0.1}$ Powders Prepared by Glycine Nitrate Process for the High Efficient Solid Oxide Fuel Cell Applications

  • Lee, Kang-Ryeol;Park, Sung
    • The Korean Journal of Ceramics
    • /
    • v.7 no.1
    • /
    • pp.6-10
    • /
    • 2001
  • Ultrafine $(CeO_2)_{0.9}(Gd_2O_3)_{0.1}$ solid solution powders synthesized by the glycine-nitrate process, with specific surface areas of $19-23\;\textrm{m}^2$/g were sintered at $1500^{\circ}C$ for various sintering times and then their electrical characteristics were investigated using AC impedance and four-point probe measurements. The electrical resistivity of the sintered $(CeO_2)_{0.9}(Gd_2O_3)_{0.1}$ bodies showed the minimum value at the sintering time of 10 hrs. The minimum total resistivity of the $(CeO_2)_{0.9}(Gd_2O_3)_{0.1}$ bodies sintered at $1500^{\circ}C$ for 10 hrs seems to result from the lowest activation energy for the electrical resistivity by the combination between the activation energies for the resistivities at the grain interior and grain boundary.

  • PDF

Preparations of (Yl-xGdx)2O3:Eu3+ Phosphors Particles by. Solvothermal Synthesis Using the 2-Methoxy Ethanol (2-메톡시에탄올을 사용한 용매열 합성법에 의해 합성되어진 (Yl-xGdx)2O3:Eu3+ 형광체입자)

  • Shin, Su-Cheol;Cho, Tae-Hwan
    • Korean Journal of Materials Research
    • /
    • v.13 no.8
    • /
    • pp.537-542
    • /
    • 2003
  • ($Y_{l-x}$ $Gd_{x}$ )$O_2$$_3$: $Eu^{ 3+}$ red phosphors were prepared with the solvothermal synthesis using the 2-methoxy-ethanol solvents and the emission intensity was investigated that applied with the 254 nm wavelength and the maximum excitation wavelength for energy source. The used solvents for the solvothermal synthesis were made of nitrate salt solutions of Y, Gd and Eu. These solutions dropped in autoclave have be reacted with the solvothermal synthesis at $200^{\circ}C$ for 5hrs and the red phosphors prepared here in were showed the pure cubic phase after annealing at $1000∼1200^{\circ}C$. The brightness of ($Y_{l-x}$ $Gd_{x}$)$_2$$O_3$: $Eu^{3+}$ phosphors particles was increased as an increase of Gd ratio. The maximum excitation wavelengths of ($Y_{l-x}$ $Gd_{x}$ )$_2$$O_3$: $Eu^{3+}$ / phosphors particles were increased according to increasing Gd ratio from 253 nm to 259 nm wavelength. The maximum emission intensity of $Gd_2$$O_3$: $Eu^{3+}$ (Y/Gd = 1/0) phosphors particles under UV 259 nm was found to be higher than the commercial product of $Y_2$$O_3$: $Eu^{3+}$ phosphors.

Phase Separation of Gd-doped UO2 and Measurement of Gd Content Dissolved in Uranium Oxide (Gd-doped UO2의 상분리 및 UO2에 고용된 Gd 함량 측정)

  • 김건식;양재호;송근우;김길무
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.9
    • /
    • pp.916-920
    • /
    • 2003
  • The change of structure and morphology in ( $U_{0.913}$G $d_{0.087}$) $O_2$ during oxidation at 475$^{\circ}C$ and heat treatment at 130$0^{\circ}C$ in air were investigated using XRD, SEM, and EPMA. The ( $U_{0.913}$G $d_{0.087}$) $O_2$ cubic phase converted to ( $U_{0.913}$G $d_{0.087}$)$_3$ $O_{8}$ orthorhombic phase by oxidation at 475$^{\circ}C$ in air. The XRD and EPMA result of the 130$0^{\circ}C$ heat treated powder revealed that ( $U_{0.913}$G $d_{0.087}$)$_3$ $O_{8}$ orthorhombic phase was separated into $U_3$ $O_{8}$ and ( $U_{0.67}$G $d_{0.33}$) $O_{2+}$x/ cubic phase. The weight variations of (U,Gd) $O_2$ with various Gd contents were measured using TGA at the same heat treated condition. The weight variation during the heat treatment of Gd dissolve (U,Gd) $O_2$ in air can be expressed in terms of phase reaction equations related with oxidation and phase separation. Based on these phase reaction, a initial content of Gd dissolved in (U,Gd) $O_2$ can be exactly calculated by measuring the weight change during the heat treatment.

Cathodic Polarization of $La_{0.5}Sr_{0.5}MnO_{3-\delta}$ on $Ce_{0.8}Gd_{0.2}O_{1.9}$ Electrolyte ($Ce_{0.8}Gd_{0.2}O_{1.9}$ 전해질에서 $La_{0.5}Sr_{0.5}MnO_{3-\delta}$ 양극의 과전압특성)

  • 윤희성;노의범;김병호
    • Journal of the Korean Ceramic Society
    • /
    • v.35 no.9
    • /
    • pp.981-987
    • /
    • 1998
  • $La_{0.5}Sr_{0.5}MnO_{3-\delta}$ as air electrode for soild oxide fuel cell was synthesized by a citrate process and its cathodic polarization was determinated by the current interruption method on the Gd-doped ceria as electrolyte. The addition of citric acid increased the exothermic heat for the formation of $La_{0.5}Sr_{0.5}MnO_{3-\delta}$ perovskite oxide. The degree of the initial particle agglomeration was affected by the exothermic heat. Also the increase of cal-cination temperature enlarged the particle size and the higher sintering temperature accelerated the den-sification of $La_{0.5}Sr_{0.5}MnO_{3-\delta}$ layer after its being painted on $Ce_{0.8}Gd_{0.2}O_{1.9}$ electrolyte. In this study $La_{0.5}Sr_{0.5}MnO_{3-\delta}$ synthesized by citrate process of which the molar ratio of citric acid to metal nitrate was 2 calcined at $650^{\circ}C$ for 2hr and sintered at 1100 at $1200^{\circ}C$ for 4 hrs after slurry coating on Ce0.8Gd0.2O1.9 electrlyte showed the lowest cathodic polarization.

  • PDF

Upconversion luminescence from poly-crystalline Yb3+, Er3+ co-doped NaGd(MoO4)2 by simple solid state method (Er3+, Yb3+ 이온이 동시 도핑된 NaGd(MoO4)2의 업컨버젼 분석)

  • Kang, Suk Hyun;Kang, Hyo Sang;Lee, Hee Ae;Shim, Kwang Bo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.26 no.4
    • /
    • pp.159-163
    • /
    • 2016
  • Up-conversion (UC) luminescence properties of polycrystalline $Er^{3+}/Yb^{3+}$ doped $NaGd(MoO_4)_2$ phosphors synthesized by a simple solid-state reaction method were investigated in detail. Used to 980 nm excitation (InfraRed area), $Er^{3+}/Yb^{3+}$ co-doped $NaGd(MoO_4)_2$ exhibited very weak red emissions near 650 and 670 nm, and very strong green UC emissions at 540 and 550 nm corresponding to the infra 4f transitions of $Er^{3+}(^4F_{9/2},\;^2H_{11/2},\;^4S_{3/2}){\rightarrow}Er^{3+}(^4I_{15/2})$. The optimum doping concentration of $Er^{3+}$, $Yb^{3+}$ for highest emission intensity was determined by XRD and PL analysis. The $Er^{3+}/Yb^{3+}$ (10.0/10.0 mol%) co-doped $NaGd(MoO_4)_2$ phosphor sample exhibited very strong shiny green emission. A possible UC mechanism for $Er^{3+}/Yb^{3+}$ co-doped $NaGd(MoO_4)_2$ depending on the pump power dependence was discussed.

Spherical-shaped Zn2SiO4:Mn Phosphor Particles with Gd3+/Li+ Codopant (Gd3+/Li+ 부활성제가 첨가된 구형의 Zn2SiO4:Mn 형광체 입자)

  • Roh, Hyun Sook;Lee, Chang Hee;Yoon, Ho Shin;Kang, Yun Chan;Park, Hee Dong;Park, Seung Bin
    • Korean Chemical Engineering Research
    • /
    • v.40 no.6
    • /
    • pp.752-756
    • /
    • 2002
  • Green-emitting $Zn_2SiO_4:Mn$ phosphors for PDP(Plasma Display Panel) application were synthesized by colloidal seed-assisted spray pyrolysis process. The codoping with $Gd^{3+}/Li^+$, which replaces $Si^{4+}$ site in the willemite structure, was performed to improve the luminous properties of the $Zn_2SiO_4:Mn$ phosphors. The particles prepared by spray pyrolysis process using fumed silica colloidal solution had a spherical shape, small particle size, narrow size distribution, and non-aggregation characteristics. The $Gd^{3+}/Li^+$ codoping amount affected the luminous characteristics of $Zn_2SiO_4:Mn$ phosphors. The codoping with proper amounts of $Gd^{3+}/Li^+$ improved both the photoluminescence efficiency and decay time of $Zn_2SiO_4:Mn$ phosphor particles. In spray pyrolysis, the post-treatment temperature is another factor controlling the luminous performance of $Zn_2SiO_4:Mn$ phosphors. The $Zn_{1.9}SiO_4:Mn_{0.1}$ phosphor particles containing 0.1 mol% $Gd^{3+}/Li^+$ co-dopant had a 5% higher PL intensity than the commercial product and 5.7 ms decay time after post-treatment at $1,145^{\circ}C$.

Luminescence properties of Eu3+ : RE2O3 [RE = Gd, Y, La] nanocrystallines prepared by solvothermal reaction method

  • Chung, Jong Won;Yang, Hyun Kyoung;Moon, Byung Kee;Choi, Byung Chun;Jeong, Jung Hyun;Kim, Kwang Ho
    • Journal of Ceramic Processing Research
    • /
    • v.13 no.spc1
    • /
    • pp.6-9
    • /
    • 2012
  • Eu3+-doped RE2O3 (RE = Gd, Y and La) phosphors were prepared by solvothermal reaction method and their crystalline structure, phase transformation and surface morphologies were investigated by using X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM). The obtained RE2O3:Eu3+ phosphors are nanocrystalline-sized. The luminescence properties of Eu3+ ions in different host materials, namely, Gd2O3, Y2O3 and La2O3 have been investigated. PACS number: 32.50.+d, 78.55.-m, 81.40.Tv.

Pharmacokinetics and Bio-distribution of New Gd-complexes of DTPA-bis (amide) (L3) in a Rat Model (쥐를 이용한 새로운 가돌리늄 조영제 Gd-DTPA-bis(amide)(L3)의 약동학 및 생체내 분포 특성에 대한 연구)

  • Yan, Gen;Wu, Renhua;Chang, Yongmin;Kang, Duksik
    • Investigative Magnetic Resonance Imaging
    • /
    • v.17 no.4
    • /
    • pp.259-266
    • /
    • 2013
  • Purpose : To investigate the blood pharmacokinetics and bio-distribution of DTPA-bis-amide (L3) Gd(III) complexes. Materials and Methods: The pharmacokinetics and bio-distribution of Gd $(L3)(H_2O){\cdot}nH_2O$ were investigated in Sprague-Dawley rats after intravenous administration at a dose of 0.1 mmol Gd/kg. The Gd content in the blood, various tissues, and organs was determined by ICP-AES. Blood pharmacokinetic parameters were calculated using a two-compartment model. Results: The half-lives of ${\alpha}$ phase and ${\beta}$ phase Gd $(L3)(H_2O){\cdot}nH_2O$ were $2.286{\pm}0.11$ min and $146.1{\pm}7.5$ min, respectively. The bio-distribution properties reveal that the complex is mainly excreted by the renal pathway, and possibly excreted by the hepatobiliary route. The concentration ratio of Gd (III) was significantly higher in the liver and spleen than in other organs, and small amounts of Gd (III) ion were detected in the blood or other tissues of rats only after 7 days of intravenous administration. Conclusion: The MRI contrast agent Gd $(L3)(H_2O){\cdot}nH_2O$ provides prolonged blood pool retention in the circulation and then clears rapidly with minimal accumulation of Gd(III) ions. The synthesis of gadolinium complexes with well-balanced lipophilicity and hydrophilicity shows promise for their further development as blood pool MRI contrast agents.