• Title/Summary/Keyword: $FeSi_x$

Search Result 485, Processing Time 0.025 seconds

Glass Forming Ability and Mechanical Properties of (Fe79C11B8Si2)100-XCrX (X = 0-8) Amorphous Ribbons ((Fe79C11B8Si2)100-XCrX (X = 0-8) 조성 비정질 리본의 크롬 함량에 따른 비정질 형성능, 기계적 특성 평가)

  • Moon, Jae-Won;Park, Ji-Sung;Yi, Seong-Hoon
    • Journal of Korea Foundry Society
    • /
    • v.36 no.1
    • /
    • pp.18-23
    • /
    • 2016
  • Iron based amorphous ribbons with the nominal compositions of $(Fe_{79}C_{11}B_8Si_2)_{100-X}Cr_X$ (X = 0,2,4,6,8 at%) have been developed as reinforcements that can be applied to the concrete materials. Mechanical properties and glass forming ability of the ribbons can be enhanced by the optimum amounts of Cr additions that can also improve corrosion properties of the ribbons. Vein patterns typical of the fractured surface morphology of amorphous alloys have been observed on the surfaces of ribbons after tensile tests. It is inferred from the EDS analysis results of vein patterns that carbon segregations occur within the narrow shear band regions.

The effect of Mo addion and Magnetic field annealing on the magnetic properties, Magnetostriction and Domain structures of $Fe_{80}B_{12}Si_8$ amorphous alloy. ($Fe_{80}B_{12}Si_8$ 비정질 합금의 자구 및 자왜와 자기적 성질에 미치는 Mo 첨가와 자장 열처리 효과)

  • 고창진;강계명;송진태
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1989.06a
    • /
    • pp.49-51
    • /
    • 1989
  • The effect of Mo elenent and annealing condition on the magnetic properties were investigated in Fe$_{80}$B$_{12}$Si$_{8}$ amorphous alloy. With increasing Mo contents, soft magnetic properties were improved by decreasing coercive force and increasing maximum permeability. These improvements were attributed to the decreasing of magnetostriction by Mo addition. The annealing treatment also improved the soft magnetic properties of (Fe$_{1-x}$ Mo$_{x}$)$_{80}$ B$_{12}$ Si$_{8}$ amorphous alloys. It could be thought that these improvements were ascribed to the relaxation of internal stress.nal stress.ess.

  • PDF

Sintering behavior of Fe-(Mo-Mn-P)-xSi alloys according to the Green Density (Fe-(Mo-Mn-P)-xSi계 합금의 성형밀도에 따른 소결거동)

  • Jung, Woo-Young;Ok, Jin-Uk;Park, Dong-Kyu;Ahn, In-Shup
    • Journal of Powder Materials
    • /
    • v.24 no.5
    • /
    • pp.400-405
    • /
    • 2017
  • The addition of a large amount of alloying elements reduces the compactibility and increases the compacting pressure, thereby shortening the life of the compacting die and increasing the process cost of commercial PM steel. In this study, the characteristic changes of Fe-Mo-P, Fe-Mn-P, and Fe-Mo-Mn-P alloys are investigated according to the Si contents to replace the expensive elements, such as Ni. All compacts with different Si contents are fabricated with the same green densities of 7.0 and $7.2g/cm^3$. The transverse rupture strength (TRS) and sintered density are measured using the specimens obtained through the sintering process. The sintered density tends to decrease, whereas the TRS increases as the Si content increases. The TRS of the sintered specimen compacted with $7.2g/cm^3$ is twice as high as that compacted with $7.0g/cm^3$.

Mechanical and Physical Property Changes of Cu-Ni-Si-Sn-Fe-P Copper Alloy System According to the Heat Treatment Conditions (열처리조건에 따른 Cu-Ni-Si-Sn-Fe-P 석출경화형 동합금계의 물성변화 특성)

  • Kim, Seung-Ho;Yum, Young-Jin
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.26 no.5
    • /
    • pp.225-232
    • /
    • 2013
  • The influence of aging treatment, addition elements and rolling reduction ratio on the microstructure, mechanical, electrical and bendability properties of Cu-Ni-Si-P-x (x = Fe, Sn, Zn) alloys for connector material application was investigated. SEM/EDS analysis exhibited that Ni2-Si precipitates with a size of 20~100 nm were distributed in grains. Fe, Sn, Zn elemnets in Cu-Ni-Si-P alloy imporved the mechanical strength but it was not favor in increasing of electrical conductivity. As higher final rolling reduction ratio, the strength and electrical conductivity is increased after aging treatment, but it indicated excellent bendability. Especially, Cu-2Ni-0.4Si-0.5Sn-0.1Fe-0.03P alloy show the tensile strength value of 700MPa and the electrical conductivity was observed to reach a maximum of 40%IACS. It is optimal for lead frame and connector.

A Study of Neolithic era Plain Coarse Pottery of Cheju Island by Mossbauer Spectroscopy (제주도 신석기 토기에 대한 Mossbauer 연구)

  • 윤태건;최원준;고정대;홍성락
    • Journal of the Korean Magnetics Society
    • /
    • v.10 no.4
    • /
    • pp.183-190
    • /
    • 2000
  • This study aims at making a research into the physical and chemical properties of the neolithic era potterys, which are unearthed from Gosanli, Sagaeli, Bukchonli, Samyangdong and Gonaili districts in Cheju Island, by using X-ray diffraction, X-ray fluorescence spectrometer and Mossbauer spectroscopy. This results are as follows. The principal component of five plain coarse pottery sherds by X-ray fluorescence spectrometer and X-ray diffraction spectrum at the room temperature is silicate mineral which is equal to SiO$_2$, and they also have a little magetite, hematite and goethite. The most existent Fe is Fe$\^$+3/ through Mossbauer spectroscopy analysis of plain coarse pottery sherds and it is presumed that the magnetic hyperfine splitting caused this result. The ratio of Fe$\^$2+//(Fe$\^$2+/+Fe$\^$3+/) is mostly zero by Mossbauer spectrum at the room temperature of plain coarse pottery sherds and it is thought because they were fired in the atmosphere.

  • PDF

A Study on Iron Compounds of Volcanic Rock in the Seaside Area of Ulleung Island (울릉도 해안지역 화산암의 철 화합물에 관한 연구)

  • Yoon, In-Seop;Kim, Sun-Bae;Kim, Hyung-Sang
    • Journal of the Korean Magnetics Society
    • /
    • v.20 no.3
    • /
    • pp.114-119
    • /
    • 2010
  • Fe compounds of volcanic rock samples distributed in the seaside area of Ulleung island were investigated by means of X-ray diffractometry (XRD), X-ray fluorescence spectroscopy (XRF) and M$\ddot{o}$ssbauer spectroscopy. We found that samples were typical basic rock which had the total amount of iron compounds including hematite ($\alpha-Fe_2O_3$) varies from 10.6 w% to 14.5 w% depending on the different regions by XRF. The M$\ddot{o}$ssbauer spectra of the samples were consisted of one sextet due to hemitite and doublets due to $Fe^{3+}$ in various clay mineral and $Fe^{2+}$ in pyroxene $(Ca,Fe,Mg)_2(SiO_4)_2$, ilmenite ($FeTiO_3$) and olivine $(Mg,Fe)_2SiO_4$. The balance state of Fe ions of all samples was chiefly $Fe^{3+}$, so we could find that the volcanic rocks distributed in the seaside area of Ulleung island were made in inland.

Synthesis of iron disilicide single crystal by chemical vapour transport (기상성장법(CVT)에 의한 Iron disilicide단결정의 합성)

  • 이충효;홍대석;이상진;최종건;김판채
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.12 no.2
    • /
    • pp.68-72
    • /
    • 2002
  • The $\beta$-$FeSi_2$ and $\alpha$-$FeSi_2$ single crystals were synthesized by chemical vapour transport (CVT) using iodine as a transporting agent from the commercially available $FeSi_2$ powder. The $FeSi_2$ powder together with iodine were sealed in an evacuated quartz ampoule and the ampoule then being placed in two-zone electrical furnace for growing crystal. The CVT of $FeSi_2$ with iodine yielded $\beta$-$FeSi_2$ and $\alpha$-FeSi$_2$ single crystals at deposition temperature of 750 and $950^{\circ}C$ respectively. The source temperature was $1050^{\circ}C$ in both cases. The crystals of the $\alpha$-FeSi$_2$ phase were typically plate shaped with dimensions of about $10\times 10 \textrm{mm}^2$, whereas the crystals of orthorhombic $\beta$-$FeSi_2$ phase grew predominantly in the fonts of thin needle of about 10 mm in length. The composition of$\alpha$-FeSicrystal determined by electron probe microanalysis (EPMA) resulted in Si-rich $FeSi_{2.58}$ . 57. Furthermore, the CVT $\beta$-$FeSi_2$ crystal was found to be transformed to the high temperature $\alpha$-$FeSi_2$phase above $930^{\circ}C$.

A Study on the Mechanical and Thermal Properties of Spray-cast Hypereutectic Al-Si-Fe Alloys (분사주조한 과공정 Al-Si-Fe 합금의 기계적 및 열적 특성에 관한 고찰)

  • Park, Jae-Sung;Ryou, Min;Yoon, Eui-Pak;Yoon, Woo-Young;Kim, Kwon-Hee;Kim, Myung-Ho
    • Journal of Korea Foundry Society
    • /
    • v.26 no.3
    • /
    • pp.123-128
    • /
    • 2006
  • Mechanical and thermal properties of spray-cast hypereutectic Al-20wt.%Si-xwt.%Fe alloys (x=0, 1, 3, 5) were investigated. After the spray-casting, hot extrusion was performed at $400^{\circ}C$. Intermetallic compound (${\beta}-Al_5FeSi$) and primary Si are observed in the spray-cast aluminum alloys. The size of primary Si and intermetallic compound of the spray-aluminum alloys became finer and more uniformly distributed than that of the permanent mold cast ones. Ultimate tensile strength of the spray-cast aluminum alloys increased by increasing Fe contents, but that of the permanent mold cast aluminum alloys decreased by increasing Fe contents possibly due to increased amount of coarse intermatallic compound. The coefficient of thermal expansion (CTEs) of the aluminum alloys became lower with finer primary Si and intermetallic compound, and this is attributed to the increased amount of interfacial area between the aluminum matrix and the phases of finer Si and intermetallic compound.

A Study on the Properties of Substituted Ferrite (Fe-Al-Ga-Si) (치환형 Ferrite (Fe-Al-Ga-Si)의 특성 연구)

  • Choi, Seung-Han
    • Korean Journal of Materials Research
    • /
    • v.21 no.8
    • /
    • pp.439-443
    • /
    • 2011
  • The crystal structure and magnetic properties of a new solid solution type ferrite $(Fe_2O_3)_5-(Al_2O_3)_{3.4}-(Ga_2O_3)_{0.6}-SiO$ were investigated using X-ray diffraction and M$\"{o}$ssbauer spectroscopy. The results of the X-ray diffraction pattern indicated that the crystal structure of the sample appears to be a cubic spinel type structure. The lattice constant (a = 8.317 ${\AA}$) decreases slightly with the substitution of $Ga_2O_3$ even though the ionic radii of the Ga ions are larger than that of the Al ions. The results can be attributed to a higher degree of covalency in the Ga-O bonds than in the Al-O and Fe-O bonds, which can also be explained using the observed M$\"{o}$ssbauer parameters, which are the magnetic hyperfine field, isomer shift, and quadrupole splitting. The drastic change in the magnetic structure according to the Ga ion substitution in the $ (Fe_2O_3)_5(Al_2O_3)_{4-x}(Ga_2O_3)_xSiO$ system and the low temperature variation have been studied through a M$\"{o}$ssbauer spectroscopy. The M$\"{o}$ssbauer spectrum at room temperature shows the superpositions of two Zeeman patterns and a strong doublet. It shows significant departures from the prototypical ferrite and is comparable with the diluted ferrite. The doublet of spectrum at room temperature appears to originate from superparamagnetic clusters and also the asymmetry of the doublet appears to be caused by the preferred orientation of the crystallites. The M$\"{o}$ssbauer spectra below room temperature show various complicated patterns, which can be explained by the freezing of the superparamagnetic clusters. On cooling, the magnetic states of the sample were various and multi critical.

Effect of Mn-Addition on the Cavitation Erosion Resistance of Surface-hardened Fe-20Cr-1Si-1C Aolly (Fe-20Cr-1Si-1C계 경면처리 합금의 cavitation erosion 저항성에 미치는 Mn 첨가의 영향)

  • 김수철;박인호;장세기;김선진;강성군
    • Journal of the Korean institute of surface engineering
    • /
    • v.33 no.1
    • /
    • pp.10-16
    • /
    • 2000
  • Characteristics of cavitation erosion resistance of Fe-20Cr-1Si-1C-xMn(x=0, 5, 15) alloys were investigated by SEM and XRD analysis. The effects on strain-induced transformations were considerably reduced with increasing the amounts of Mn due to twining that occurred at 5, 15Mn alloys, activating cavitation erosion rates(mg/$\textrm{cm}^2$) which varied as 0.055, 0.114 and 0.160mg/$\textrm{cm}^2$ for 0, 5, 15Mn. From the results, it was found that the addition of Mn element in Fe-base alloy provides more cracking sites at twins rather than absorbing strain energies, so accelerates cavitation erosion rates.

  • PDF