• Title/Summary/Keyword: $Fe^{2+}

Search Result 11,669, Processing Time 0.043 seconds

Selective Oxidation of Cyclohexane at Low Temperature by Fe-Pd Bicatalytic Systems: $FeCl_2$-Pd/alumina System and Pd/$Fe_2O_3$ System

  • 전기원;Lingaiah Nakka;김상범;이규완
    • Bulletin of the Korean Chemical Society
    • /
    • v.18 no.12
    • /
    • pp.1269-1273
    • /
    • 1997
  • The system which employs iron, palladium, molecular oxygen and hydrogen as a model mono-oxygenase, has been investigated to develop a new method for selective cyclohexane oxidation uner mild conditions. This system provides much higher yield and selectivity for the formation of cyclohexanol and cyclohexanone compared to that of the existing industrial method. When the catalytic system, FeCl2-Pd/alumina, was employed, the oxidation system required acetone as a solvent to be efficient and acidifying the solvent by a little addition of acetic acid or HCl made the system more efficient. The Pd catalyst was recyclable without a significant deactivation but the recycling of ferrous chloride showed the decrease in the activity. On the other hand, the heterogeneous catalytic system, Pd/Fe2O3 could be recovered easily and reused after drying treatment.

Tissue Distribution of Divalent Metal Transporter 1 and Regulation by Dietary Iron in Rats (흰쥐에서 Divalent Metal Transporter 1의 조직내 분포와 Iron에 의한 조절)

  • Choi Jae-Hyuck;Park Jung-Duck
    • Environmental Analysis Health and Toxicology
    • /
    • v.19 no.4
    • /
    • pp.359-366
    • /
    • 2004
  • Iron (Fe) is an essential metal in biological processes, which maintains a homeostasis in the human body. Divalent metal transporter 1 (DMT1) has been known as an iron transporting membrane protein, which is involved in the uptake Fe at the apical portion of intestinal epithelium, and may transport Fe across the membrane of acidified endosome in peripheral tissues. In this study, we studied the tissue distribution of DMT1 in the Fe supplemented (FeS) diet fed rats, and the regulation of DMT1 expression by depleting body Fe. Sprague-Dawley rats were divided into two groups, and fed FeS (120 mg Fe/kg) diet or Fe deficient (FeD, 2∼6 mg Fe/kg) diet for 4 weeks. The evaluation of body Fe status was monitored by measuring sFe, UIBC and tissue Fe concentration. Additionally, DMT1 mRNA levels were analyzed in the peripheral tissues by using the quantitative real time RT-PCR method. In the FeS diet fed rats, the tissue Fe was maintained at a relatively high level, and DMT1 was eventually expressed in all tissues studied. DMT1 was highly expressed in the testis, kidney and spleen, while a moderate levels of DMT1 expression was detected in the brain, liver and heart. In the digestive system, the highest level of DMT1 was found in the duodenum. Feeding the FeD diet caused a reduced body weight gain and depletion of body Fe with finding of decreased sFe, increased UIBC and decreased tissue Fe concentration. The depletion of body Fe upregulated DMT1 expression in the peripheral tissue. The expression of DMT1 was very sensitive to the body Fe depletion in the small intestine, especially in the duodenum, showing dramatically higher levels in the FeD rats than those of the FeS group. In the FeD diet fed animals, the expression of DMT1 was low significantly in other tissues compared with the duodenum. The expression of DMT1, however, was 60∼120% higher in the testis, kidney and spleen, and 30∼50% higher in the lung, liver and heart, compared to the FeS diet fed rats. In summary, DMT1 expression was ubiquitous in mammalian tissue, and the level of expression was the organ-dependent. The expression of DMT1 in peripheral tissues was upregulated by depletion of body Fe. Duodenum was the most sensitive tissue among organs studied during Fe depletion, and expressed the greatest level of DMT1, while other tissues were less higher than in duodenum. This study supports that DMT1 plays a role in maintaining the body Fe level through intestinal uptake as well as homeostasis of Fe in the peripheral tissue.

Magnetic Properties of RF Diode Sputtered $Ni_{80}Fe_{20}/SiO_2$ Multilayers (모양으로 유도된 자기 이방성을 가진 $Ni_{80}Fe_{20}/SiO_2$ 다층막의 자기적 성질)

  • Yun, Eui-Jung;Jung, Myung-Hee
    • Journal of the Institute of Electronics Engineers of Korea SD
    • /
    • v.44 no.2
    • /
    • pp.1-6
    • /
    • 2007
  • This study investigated the magnetic properties of $Ni_{80}Fe_{20}/SiO_2$ laminates with shape-induced magnetic anisotropy. The multilayer films were deposited on Si or upilex substrates, from separate $Ni_{80}Fe_{20}$ and $SiO_2$ (at %) alloy targets using a rf diode sputtering system. $Ni_{80}Fe_{20}/SiO_2$ laminates with a various number of bilayers (N) were prepared. The laminates with ellipse array patterns were prepared using photolithographic technique. The magnetic properties were measured at room temperature using a B-H hysteresisgraph and a high frequency permeameter. The several steps during domain wall reversal were observed in multilayer films, attributing to inter-magnetic layer coupling. Intrinsic uniaxial anisotropy field increases with N. The experimental values of the total anisotropy field are found to be in good agreement with the calculated values. This study utilized the shape anisotropy of the laminated film objects with small ellipse array patterns to induce a larger uniaxial anisotropy so as to maximize their operating frequency.

Pre-Irradiation Grafting of Acrylic Acid onto Polyethylene Film (전조사법에 의한 아크릴산의 폴리에틸렌 필름에 대한 그라프트 반응)

  • Nho, Young Chang;Jin, Joon-Ha;Lee, Myun Zu
    • Applied Chemistry for Engineering
    • /
    • v.7 no.1
    • /
    • pp.75-82
    • /
    • 1996
  • Acrylic acid was graft-copolymerized on polyethylene film in the presence of additives such as acid and $FeSO_4(NH_4)_2SO_4{\cdot}6H_2O$ using peroxide grafting technique by ${\gamma}$-ray and electron beam, and the effect of $FeSO_4(NH_4)_2SO_4{\cdot}6H_2O$ and acid on the grafting yield was evaluated. The grafting mechanism and the physical property of grafted films were also examined. The results showed that the inclusion of $FeSO_4(NH_4)_2SO_4{\cdot}6H_2O$ in acidified acrylic acid grafting solution was extremely beneficial and led to a most unusual enhancement effect in the radiation grafting. In the other hand, inclusion of mineral acid in the grafting solution in the absence of $FeSO_4(NH_4)_2SO_4{\cdot}6H_2O$ could not lead to he suitable grafting reaction by the severe homopolymerization of acrylic acid. The addition of $H_2SO_4$, and HCl led to much higher grafting yield than $HNO_3$and $CH_3COOH$. It was shown that grafting yield of ${\gamma}$-ray irradiated-polyethylene was higher than that of electron beam irradiated polyethylene.

  • PDF

Detection of Iron Phases Presents in Archaeological Artifacts by Raman Spectroscopy

  • Barbosa, A.L.;Jimenez, C.;Mosquera, J.A.
    • Corrosion Science and Technology
    • /
    • v.17 no.2
    • /
    • pp.60-67
    • /
    • 2018
  • The compounds associated with corrosion, in metallic archaeological samples of carbon steel of insular origin were evaluated to establish their degree of deterioration and structural damage against air pollution. The iron phases present in samples of archaeological artifacts were detected by Raman spectroscopy and confocal Raman microcopy. These samples mainly exhibited ing mainly ${\beta}$-FeO(OH) type goethite oxyhydroxides and small amounts of akaganeite ${\alpha}$-FeO(OH) lepidocrocite ${\gamma}$-FeO(OH) due to dominant chloride in a marine environment and non-stoichiometric oxyhydroxides Fe (II + / III +) as indicators of early corrosion. Some parts showed the presence of magnetic maghemite indicating high corrosion. ${\gamma}$-FeO(OH) is a precursor of phases associated with advanced marine corrosion. By studying its decomposition by Raman spectroscopy, it was synthesized with the following sequence: ${\gamma}-FeO(OH){\rightarrow}{\alpha}-FeO(OH)+{\gamma}-FeO(OH)$, ${\rightarrow}{\gamma}-Fe_2O_3+Fe_3O_4$. Ferric compounds provided evidence for the effect of intensity of laser on them, constituting a very useful input for the characterization of oxidation of iron in this type of artifacts. Thus, destructive analysis techniques should be avoided in addition to the use of small amounts of specimen.

Size Control of Nd-Fe-B Precursor Particles Prepared by Spray Drying and Its Effect on the Magnetic Properties of Nd-Fe-B Alloy Powders after Reduction-Diffusion (분무건조된 Nd-Fe-B 전구체 입자의 크기조절 및 환원-확산 후 자기 특성에 미치는 영향)

  • Baek, Youn-Kyoung;Seo, Young-Taek;Lee, Jung-Goo;Kim, Dong Su;Bae, Dong Sik;Choi, Chul-Jin
    • Journal of Powder Materials
    • /
    • v.20 no.5
    • /
    • pp.359-365
    • /
    • 2013
  • In this study, we fabricated $Nd_2Fe_{14}B$ hard magnetic powders with various sizes via spray drying combined with reduction-diffusion process. Spray drying is widely used to produce nearly spherical particles that are relatively homogeneous. Thus, the precursor particles were prepared by spray drying using the aqueous solution containing Nd salts, Fe salts and boric acid with the target stoichiometric composition of $Nd_2Fe_{14}B$. The mean particle sizes of the spray-dried powders are in the range from one to seven micrometer, which are adjusted by controlling the concentrations of precursor solutions. After debinding the as-prepared precursor particles, ball milling was also conducted to control the particle sizes of Nd-Fe-B oxide powders. The resulting particles with different sizes were subjected to subsequent treatments including hydrogen reduction, Ca reduction and washing for CaO removal. The size effect of Nd-Fe-B oxide particles on the formation of $Nd_2Fe_{14}B$ phase and magnetic properties was investigated.

Synthesis and Characterization of Polyphase Waste Form to Immobilize High Level Radioactive Wastes (고준위 방사성 폐기물의 고정화를 위한 다상 고화체 합성)

  • Chae Soo-Chun;Jang Young-Nam;Bae In-Kook;Ryu Kyung-Won
    • Economic and Environmental Geology
    • /
    • v.39 no.2 s.177
    • /
    • pp.173-180
    • /
    • 2006
  • The synthesis of polyphase waste form, which is an immobilization matrix fur the high level radioactive wastes, was performed with the mixed composition of garnet and spinel $(Gd_3Fe_5O_{12}+(Ni_xMn_{1-x})(Fe_yCr_{1-y})_2O_4)$ in the range of 1200 to $1400^{\circ}C$. The phases synthesized from all stoichiometric compositions were garnet, perovskite, and spinel. Especially, garnet was synthesized only in the composition of the highest content of Fe(y=0.9), whereas it was not synthesized in other compositions. This result indicated that the content of Fe was closely related to the formation of garnet. The composition of garnet revealed that the content of Gd was exceeded and that of Fe was depleted. Preferential distribution of elements in the phases can be attributed to the nonstoichiometric composition of garnet.

Effects of Alloying Elements on the Properties of High Strength and High Thermal Conductivity Al-Zn-Mg-Fe Alloy for Die Casting (다이캐스팅용 Al-Zn-Mg-Fe 합금의 특성에 미치는 Zn 및 Mg 첨가의 영향)

  • Kim, Ki-Tae;Lim, Young-Suk;Shin, Je-Sik;Ko, Se-Hyun;Kim, Jeong-Min
    • Journal of Korea Foundry Society
    • /
    • v.33 no.4
    • /
    • pp.171-180
    • /
    • 2013
  • The effects of alloying elements on the solidification characteristics, microstructure, thermal conductivity, and tensile strength of Al-Zn-Mg-Fe alloys were investigated for the development of high strength and high thermal conductivity aluminium alloy for die casting. The amounts of Zn and Mg in Al-Zn-Mg-Fe alloys had little effect on the liquidus/solidus temperature, the latent heat for solidification, the energy release for solidification and the fluidity of Al-Zn-Mg-Fe alloys. Thermo-physical modelling of Al-Zn-Mg-Fe alloys by the JMatPro program showed $MgZn_2$, AlCuMgZn and $Al_3Fe$ phases in the microstructure of the alloys. Increased amounts of Mg in Al-Zn-Mg-Fe alloys resulted in phase transformation, such as $MgZn_2{\Rightarrow}MgZn_2+AlCuMgZn{\Rightarrow}AlCuMgZn$ in the microstructure of the alloys. Increased amounts of Zn and Mg in Al-Zn-Mg-Fe alloys resulted in a gradual reduction of the thermal conductivity of the alloys. Increased amounts of Zn and Mg in Al-Zn-Mg-Fe alloys had little effect on the tensile strength of the alloys.

Simultaneously Enhanced Magnetic and Ferroelectric Properties of $Bi_{0.9}Dy_{0.1}Fe_{0.97}Co_{0.03}O_3 $ compound

  • Yu, Yeong-Jun;Hwang, Ji-Seop;Park, Jeong-Su;Lee, Ju-Yeol;Gang, Ji-Hun;Lee, Gwang-Hun;Lee, Bo-Hwa;Kim, Gi-Won;Lee, Yeong-Baek
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.08a
    • /
    • pp.147-147
    • /
    • 2013
  • Multiferroic material $BiFeO_3$ (BFO) is a typical multiferroic material with a room-temperature magnetoelectric coupling in view of high magnetic- and ferroelectric-ordering temperatures (Neel temperature $T_N$ ~ 647 K and Curie temperature TC ~1,103 K). Rare-earth ion substitution at the Bi sites is very interesting, which induces suppressed volatility of the Bi ion and improved ferroelectric properties. At the same time, the Fe-site substitution with magnetic ions is also attracting, since the enhanced ferromagnetism was reported. In this study, BFO, $Bi_{0.9}Dy_{0.1}FeO_3$ (BDFO), $BiFe_{0.97}Co_{0.03}O_3$ (BFCO) and $Bi_{0.9}Dy_{0.1}Fe_{0.97}Co_{0.03}O_3 $ (BDFCO) compounds were prepared by conventional solid-state reaction and wet-mixing method. High-purity $Bi_2O_3$, $Dy_2O_3$, $Fe_2O_3$ and $Co_3O_4$ powders with the stoichiometric proportions were mixed, and calcined at $500^{\circ}C$ for 24 h. The samples were immediately put into an oven, which was heated up to 800oC and sintered in air for 1 h. The crystalline structure of samples was investigated at room temperature by using a Rigaku Miniflex powder diffractometer. The field-dependent magnetization measurements were performed with a vibrating-sample magnetometer. The electric polarization was measured at room temperature by using a standard ferroelectric tester (RT66B, Radiant Technologies). Dy and Co co-doping at the Bi and the Fe sites induce the enhancement of both magnetic and ferroelectric properties of $BiFeO_3$.

  • PDF

Improved Photolysis of Water from Ti Incorporated Double Perovskite Sr2FeNbO6 Lattice

  • Borse, P.H.;Cho, C.R.;Yu, S.M.;Yoon, J.H.;Hong, T.E.;Bae, J.S.;Jeong, E.D.;Kim, H.G.
    • Bulletin of the Korean Chemical Society
    • /
    • v.33 no.10
    • /
    • pp.3407-3412
    • /
    • 2012
  • The Ti incorporation at Fe-site in the double perovskite lattice of $Sr_2FeNbO_6$ (SFNO) system is studied. The Ti concentration optimization yielded an efficient photocatalyst. At an optimum composition of Ti as x = 0.07 in $Sr_2Fe_{1-x}Ti_xNbO_6$, the photocatalyst exhibited 2 times the quantum yield for photolysis of $H_2O$ in presence of $CH_3OH$, than its undoped counterpart under visible light (${\lambda}{\geq}420nm$). Heavily Ti-doped $Sr_2Fe_{1-x}Ti_xNbO_6$ lattice exhibited poor photochemical properties due to the existence of constituent impurity phases as observed in the structural characterization, as well as deteriorated optical absorption. The higher electron-density acquired by n-type doping seem to be responsible for the more efficient charge separation in $Sr_2Fe_{1-x}Ti_xNbO_6$ (0.05 < x < 0.4) and thus consequently displays higher photocatalytic activity. The Ti incorporated structure also found to yield stable photocatalyst.