• Title/Summary/Keyword: $Cr_3C_2$

Search Result 1,355, Processing Time 0.037 seconds

Surface Acoustic Wave Characteristics of PSS-PZT Cermaics with Cr addition (Cr 첨가에 따른 PSS-PZT 세라믹스의 탄성 표면파 특성)

  • 홍재일;유주현;김준한;강진규;박창엽
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1991.10a
    • /
    • pp.68-72
    • /
    • 1991
  • In this study, to improve temperature stability 0.05 Pb(Sn$\_$$\frac{1}{2}$/Sb$\_$$\frac{1}{2}$/O$_3$ - 0.35PbTiO$_3$ - 0.60PbZrO$_3$ + 0.4[wt%]MnO$_2$ piezoelctric oeramics of low dielectric constant and large mechanical quality factor were manufactured with the addition of Cr$_2$O$_3$by Hot Press method. And the SAW delay line was fabricated and the propagation characteristics of SAW was investigated, and the SAW filter was fabricated on C4 added by 0.2[wt%] Cr$_2$O$_3$and its frequency characteristics was investigated. The specimen, whose propagation characteristics of surface acoustic wave were the best, was C4 added by 0.2[wt%] Cr$_2$O$_3$, and its electromechanical coupling factor(ks$^2$) was 3.11[%] and its temperature coefficient of the center frequency (C$\_$fo/) was -21.27[ppm/$^{\circ}C$]. The 31[MHz] SAW IF filter of C4 scarcely had diffraction phenomena and its group delay time was 1.4673 ${\pm}$40[ns] in the pass band, and the insertion loss was -24.419[dB] on no impedance matching.

The Effects of $MnO_2$ and $Cr_2O_3$ on Piezoelectric Properties of $Pb(Mg_{1/2}W_{1/2})_{0.3} Ti_{0.4} Zr_{0.3}O_3$ Ceramics ($MnO_2$$Cr_2O_3$$Pb(Mg_{1/2}W_{1/2})_{0.3} Ti_{0.4} Zr_{0.3}O_3$ Ceramics의 압전성질에 미치는 영향)

  • 안영필;박종상
    • Journal of the Korean Ceramic Society
    • /
    • v.19 no.4
    • /
    • pp.293-299
    • /
    • 1982
  • The effects of $MnO_2$ and $Cr_2O_3$ on the Piezoelectrictric properties of Pb(Mg1/2W1/2)0.3 Ti0.4 Zr0.3O3 Ceramics. Electromechanical properties in the system in connection with the sintering temperature and the effects of $MnO_2$ and $Cr_2O_3$ addition. The dielectric constant of the ceramics decreased with the additions of $MnO_2$ while the additions of $Cr_2O_3$ increased the value. The Planar coupling factor (Kp) of the ceramics with 0.2wt% $MnO_2$ and with 0.2wt% $Cr_2O_3$ gave the highest value of 0.52 and 0.513 as sintered at 106$0^{\circ}C$, 108$0^{\circ}C$, respectively. The value of mechanical Q-factor were in parallel with the fired density of the ceramics. The optical micrography of the sintered bodies showed that the additions of $MnO_2$ promoted the grain growth, while the additions of $Cr_2O_3$ retarded the grain growth.

  • PDF

Effects of $Cr_2O_3$ Addition in PSS-PZT Piezoelectric Ceramics for Surface Acoustic Wave Filter ($Cr_2O_3$가 탄성 표면파 필터용 PSS-PZT계 압전 세라믹스에 미치는 영향)

  • 홍재일;손은영;박창엽
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.41 no.5
    • /
    • pp.502-507
    • /
    • 1992
  • To improve temperature stability, 0.05Pb(SnS11/2TSbS11/2T)OS13T-0.35PbTiOS13T-0.60PbZrOS13T+0.4[wt%]MnO S12T piezoelectic ceramics were manufactured with the addition of CrS12TOS13T by Hot Press method. And the SAW delay line was fabricated and effects of CrS12TOS13T to the propagation characteristics of SAW was investigated, and the SAW filter was fabricated on C4 specimen added by 0.2[wt%] CrS12TOS13T whose propagation characteriatics of surface acoustic wave were the bast and its frequency characteristics was investigated. Electromechancal coupling factor(kS1sTS02T) was 3.11[%] and its temperature coefficient of the center frequency(CS1foT)was -21.27[ppm/$^{\circ}C$] in C4. The 31[MHz]]SAW IF filter of C4 scarcely had diffraction phenomena and therefore it was proper.

  • PDF

High-temperature Oxidation of the TiAlCrSiN Film (TiAlCrSiN 박막의 고온 산화 부식)

  • Lee, Dong-Bok;Kim, Min-Jeong;Abro, M.A.;Yadav, P.;Shi, Y.
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2016.11a
    • /
    • pp.107-107
    • /
    • 2016
  • TiCrAlSiN films were developed in order to improve the high-temperature oxidation resistance, corrosion resistance, and mechanical properties of conventional TiN films that are widely used as hard films to protect and increase the lifetime and performance of cutting tools or die molds. In this study, a nano-multilayered TiAlCrSiN film was deposited by cathodic arc plasma deposition. It displayed relatively good oxidation resistance at $700-900^{\circ}C$, owing to the formation protective oxides of $Al_2O_3$, $Cr_2O_3$, and $SiO_2$, and semiprotective $TiO_2$. At $1000^{\circ}C$, the increased temperature led to the formation of the imperfect oxide scale that consisted primarily of the outer ($TiO_2$,$Al_2O_3$)-mixed scale and inner ($TiO_2$, $Al_2O_3$, $Cr_2O_3$)-mixed scale.

  • PDF

A Study on the Physical Properties of Compound of Pyrazine with Cromium Trioxide (Pyrazine의 Cr$O_3$ 화합물의 물성에 관한 연구)

  • Jung Sung Yang
    • Journal of the Korean Chemical Society
    • /
    • v.33 no.1
    • /
    • pp.11-17
    • /
    • 1989
  • Pyrazinium chlorochromate and dipyrazinium trichromate which are pyrazinium salts were prepared by the each reaction of pyrazine with chromium trioxide under the presence of HCl and $CH_2Cl_2$. These compounds wese nonhygroscopic and were solved in water very well. Physical properties such as solubility, pH, electrical conductivity, and melting point were measured. These compounds were considered to be ionic ; $C_4H_4N_2H^+$, $CrO_3Cl^-$, $Cr_3O^{2-}_{10}$ by the measurement of electrical conductivity. It was found that CrO$_3$ was formed in the first decomposition process of salts and it was changed into $Cr_2O_3$ in the second process as its weight is decreased. It was also found that especially under the same condition dipyrazinium salt was in the form of isopoly ($Cr_2O^{2-}_{10}$)anion which has been thought to be in the form of $Cr_2O^{2-}_{7}$ obtained from pyridine.

  • PDF

As-Cast and Solidification Structures of Fe-3%C-x%Cr-y%V-w%Mo-z%W Multi- Component White Cast Irons (Fe-3%C-x%Cr-y%V-w%Mo-z%W 다합금계백주철의 주방상태 및 급냉조직)

  • Yu, sung-Kon;Shin, Sang-Woo
    • Korean Journal of Materials Research
    • /
    • v.12 no.5
    • /
    • pp.414-422
    • /
    • 2002
  • Three different multi-component white cast irons alloyed with Cr, V, Mo and W were prepared in order to study their as-cast and solidification structures. Three combinations of the alloying elements were selected so as to obtain the different types of carbides and matrix structures : 3%C-10%Cr-5%Mo-5%W(alloy No.1), 3%C-10%V-5% Mo-5%W(alloy No. 2) and 3%C-17%Cr-3% V(alloy No.3). The as-cast microstructures were investigated with optical and scanning electron microscopes. There existed two different types of carbides, $M_7C_3$ carbide with rod-like morphology and $M_6C$ carbide with fishbone-like one, and matrix in the alloy No. 1. The alloy No. 2 consisted of MC carbide with chunky and flaky type and needle-like $M_2C$ carbide, and matrix. The chunky type referred to primary MC carbide and the flaky one to eutectic MC carbide. The morphology of the alloy No. 3 represented a typical hypo-eutectic high chromium white cast iron composed of rod-like $M_7C_3$ carbide which is very sensitive to heat flow direction and matrix. To clarify the solidification sequence, each iron(50g) was remelted at 1723K in an alumina crucible using a silicon carbide resistance furnace under argon atmosphere. The molten iron was cooled at the rate of 10K/min and quenched into water at several temperatures during thermal analysis. The solidification structures of the specimen were found to consist of austenite dendrite(${\gamma}$), $ ({\gamma}+ M_7C_3)$ eutectic and $({\gamma}+ M_6C)$ eutectic in the alloy No. 1, proeutectic MC, austenite dendrite(${\gamma}$), (${\gamma}$+MC) eutectic and $({\gamma}+ M_2C)$ eutectic in the alloy No. 2, and proeutectic $M_7C_3$ and $ ({\gamma}+ M_7C_3)$ eutectic in the alloy No 3. respectively.

High Temperature SO2-gas Corrosion of Fe-18%Cr-10%Ni Steels for Coal-fired Power Plant (화력발전소용 Fe-18%Cr-10%Ni 강의 고온 SO2 가스 부식)

  • Lee, Dong-Bok
    • Journal of the Korean institute of surface engineering
    • /
    • v.40 no.5
    • /
    • pp.219-224
    • /
    • 2007
  • The corrosion characteristics of Fe-18Cr-10Ni steels were studied between $600^{\circ}C$ and $1000^{\circ}C$ in Ar+(0.2, 1)%$SG_2$ gas for up to 300 hr in order to employ Fe-18Cr-10Ni steels in the coal-fired power plants. The corrosion resistance of Fe-18Cr-10Ni steels was good due mainly to the high amount of Cr, which formed $Cr_2O_3$ from the initial corrosion stage. Fe in the steels corroded to mainly $Fe_2O_3$ and $Fe_3O_4$. Ni was not susceptible to corrosion under the current corrosion condition. Relatively thin, single-layered scales formed.

Discovery of Cyclin-dependent Kinase Inhibitor, CR229, Using Structure-based Drug Screening

  • Kim, Min-Kyoung;Min, Jae-Ki;Choi, Bu-Young;Lim, Hae-Young;Cho, Youl-Hee;Lee, Chul-Hoon
    • Journal of Microbiology and Biotechnology
    • /
    • v.17 no.10
    • /
    • pp.1712-1716
    • /
    • 2007
  • To generate new scaffold candidates as highly selective and potent cyelin-dependent kinase (CDK) inhibitors, structure-based drug screening was performed utilizing 3D pharmacophore conformations of known potent inhibitors. As a result, CR229 (6-bromo-2,3,4,9-tetrahydro-carbolin-1-one) was generated as the hit-compound. A computational docking study using the X-ray crystallographic structure of CDK2 in complex with CR229 was evaluated. This predicted binding mode study of CR229 with CDK2 demonstrated that CR229 interacted effectively with the Leu83 and Glu81 residues in the ATP-binding pocket of CDK2 for the possible hydrogen bond formation. Furthermore, biochemical studies on inhibitory effects of CR229 on various kinases in the human cervical cancer HeLa cells demonstrated that CR229 was a potent inhibitor of CDK2 ($IC_{50}:\;3\;{\mu}M$), CDKI ($IC_{50}:\;4.9\;{\mu}M$), and CDK4 ($IC_{50}:\;3\;{\mu}M$), yet had much less inhibitory effect ($IC_{50}:>20\;{\mu}M$) on other kinases, such as casein kinase 2-${\alpha}1$ (CK2-${\alpha}1$), protein kinase A (PKA), and protein kinase C (PKC). Accordingly, these data demonstrate that CR229 is a potent CDK inhibitor with anticancer efficacy.

Tribological Behavior Analysis of WC-Ni-Cr + Cr3C2 and WC-Ni-Cr + YSZ Coatings Sprayed by HVOF (고속 화염 용사법으로 제조된 WC계 Cr3C2 코팅과 WC계 YSZ 코팅의 마찰 및 마모 거동 연구)

  • Tae-Jun Park;Gye-Won Lee ;Yoon-Suk Oh
    • Journal of Powder Materials
    • /
    • v.30 no.5
    • /
    • pp.415-423
    • /
    • 2023
  • With the increasing attention to environmental pollution caused by particulate matter globally, the automotive industry has also become increasingly interested in particulate matter, especially particulate matter generated by automobile brake systems. Here, we designed a coating composition and analyzed its mechanical properties to reduce particulate matter generated by brake systems during braking of vehicles. We designed a composition to check the mechanical properties change by adding Cr3C2 and YSZ to the WC-Ni-Cr composite composition. Based on the designed composition, coating samples were manufactured, and the coating properties were analyzed by Vickers hardness and ball-on-disk tests. As a result of the experiments, we found that the hardness and friction coefficient of the coating increased as the amount of Cr3C2 added decreased. Furthermore, we found that the hardness of the coating layer decreased when YSZ was added at 20vol%, but the friction coefficient was higher than the composition with Cr3C2 addition.

Effects of Carbide and Matrix Structures on Abrasion Wear Resistance of Multi-Component White Cast Iron (다합금계 백주철의 탄화물 및 기지조직이 내마모성에 미치는 영향)

  • Ryu, Seong-Geun
    • Korean Journal of Materials Research
    • /
    • v.7 no.4
    • /
    • pp.310-316
    • /
    • 1997
  • The effects of carbide and matrix structures on the abrasion wear resistance of multi-component white cast irons with 3.0 mass%C have been studied in this paper. Four different heats were poured in order to obtain the specimens with different combinations of the carbide structures: a basic iron(3.0 mass%C-5.0 mass%Cr-5.0 mass%V-5.0 mass% Mo-12.5mass%W)for M$_{6}$C and M$_{7}$C$_{3}$ carbides, and a Cr free iron(3.0 mass%C-5.0 mass%V-2.5mass%Mo-12.5 mass%W) for MC and M6C carbides. A conventional high Cr free free iron(3.0 mass%C-5.0 mass%V-2.5 mass%Mo-12.5 mass%W) for MC and M6C carbides. A conventional high Cr white cast iron was also poured to compare its wear resistance with those of the multi-component white cast irons. In the as-cast condition, the range of abrasive wear rate(Rw=mg/min) was from 4.15 to 5.98 . The lowest Rw, which means the highest wear resistance, was obtained in the basic iron with nodular MC, lamellar M$_{2}$C and cellular M$_{7}$C$_{3}$ carbides. On the other hand, the Rw of the high Cr white cast iron ranked between the basic iron and the Mo and W free iron. In each alloy, the Rw of air hardened or tempered specimen was lower than that of the as-cast one because of the change of matrix structures by the heat treatments. The Rw of the hear treated speci-mens increased in the order Mo and W free iron, basic iron, Cr free iron, high Cr iron, and V free iron.n.n.n.

  • PDF