Abstract

The corrosion characteristics of Fe-18Cr-10Ni steels were studied between $600^{\circ}C$ and $1000^{\circ}C$ in Ar+(0.2, 1)%$SG_2$ gas for up to 300 hr in order to employ Fe-18Cr-10Ni steels in the coal-fired power plants. The corrosion resistance of Fe-18Cr-10Ni steels was good due mainly to the high amount of Cr, which formed $Cr_2O_3$ from the initial corrosion stage. Fe in the steels corroded to mainly $Fe_2O_3$ and $Fe_3O_4$. Ni was not susceptible to corrosion under the current corrosion condition. Relatively thin, single-layered scales formed.

Keywords

References

  1. K. M. Kim, S. S. Hwang, E. H. Lee, H. P. Kim, U. C. Kim, J. Corros. Sci. of Korea, 27 (1998) 320
  2. J. S. Ha, J. Corros. Sci. of Korea, 27 (1998) 331
  3. A. Fry, S. Osgerby, M. Wright, NPL Report: MATC(A)90, NPL Materials Centre, USA, (2002)
  4. R. L. Klueh, ORNL/TM-2004/176, Oak Ridge National Laboratory, USA, (2004)
  5. S. Mrowec, M. Wedrychowska, Oxid. Met., 13 (1979) 481 https://doi.org/10.1007/BF00812774
  6. Z. Zurek, J. Gilewicz-Wolter, M. Hetmanczyk, J. Dudala, A. Stawiarski, Oxid. Met., 64 (2005) 379 https://doi.org/10.1007/s11085-005-8533-5
  7. I. R. Sohn, T. Narita, Oxid. Met., 65 (2006) 167 https://doi.org/10.1007/s11085-006-9010-5
  8. H. D. Jung, S. G Kang, J. Corros. Sci. of Korea, 18 (1999) 190
  9. N. Birks, G H. Meier, Introduction to High Temperature Oxidation of Metals, Edward Arnold, London (1983) 72
  10. A. Skalli, A. Galerie, M. Caillet, Solid State lonies, 34 (1989) 261 https://doi.org/10.1016/0167-2738(89)90453-0
  11. I. Barin, Thermochemical Data of Pure Substances, VCH, Weinheim, Germany, (1989)