Properties Analysis of Environment Friendly Coating Films Formed by Using Electrodeposition Principle on Seawater (해수환경중 전착원리에 의해 형성시킨 환경친화적인 코팅막의 특성 분석)

  • Baek, S.M.;Lee, C.S.;Kim, K.J.;Moon, K.M.;Lee, M.H.
    • Proceedings of the Korean Society of Marine Engineers Conference
    • /
    • 2005.11a
    • /
    • pp.196-197
    • /
    • 2005
  • Cathodic protection is one of the successful ways to prevent corrosion of steel structures in marine environments. The unique feature of cathodic protection in seawater is the formation of calcareous deposits on cathodic metal surface. The formation principles of calcareous deposit seawater had been known for a long time. That is, cathodic reduction reactions associated with cathodic protection in seawater generate $OH^-$ at the metal surface in accordance with the formular ; 1/2 $O_2$ + $H_2O$ + $2e^-$ $2OH^-$ and $2H_2O$ + $2e^-$ ${\rightarrow}$ $H_2$ + $2OH^-$. These reactions increase the pH at the metal / seawater interface. The high pH causes precipitation of $Mg(OH)_2$ and $CaCO_3$ in accordance with the formular ; $Mg^{2+}$ + $2(OH)^-$ ${\rightarrow}$ $Mg(OH)_2$ and $Ca^{2+}$ + $HCO_3^-$ + $OH^-$ ${\rightarrow}$ $H_2O$ + $CaCO_3$. These are typically the main compounds in calcareous deposits. It obviously has several advantages compared to the conventional coatings, since the environment-friendly calcareous deposit coating is formed by the elements($Mg^{2+}$, $Ca^{2+}$) naturally present in seawater. In this study, environmental friendly calcareous deposit films were prepared on steel plates by electro plating technic in natural seawater. The influence of current density on composition ratio, structure and morphology of the coated films were investigated by scanning electron microscopy formation process of calcareous deposits films in natural seawater. And we confirmed the properties of all the films can be improved greatly by controlling the material structure and morphology with effective use of the electroplating method in natural seawater.

  • PDF

An experimental study on preparation of precipitated calcium carbonate using Ca component dissolution characteristics and liquid carbonation by the Industrial byproducts (산업부산물의 Ca 성분 용출 특성 및 액상탄산화 반응을 이용한 침강성 탄산칼슘 제조에 관한 실험적 연구)

  • Lim, Yun-Hui;Lee, Ju-Yeol;Shin, Jae-Ran;Choi, Chang-Sik;Hong, Bum-Ui;Kang, Ho Jong;Park, Byung Hyun
    • Journal of the Korean Applied Science and Technology
    • /
    • v.32 no.1
    • /
    • pp.116-126
    • /
    • 2015
  • The present study utilized a shuttle mechanism of wet chemical absorption using MEA. In addition, industrial by-products containing a large amount of inorganic alkali substances were utilized for wet carbonization process. Chemical pretreatment of industrial by-products extracted calcium ions. ICP result of calcium ion was obtained up to 17,900 ppm(17.9%) by acidic substance. And also, In this work, 94% of recovery rate was obtained using wet MEA absorption process from $CO_2$ flow at the ambient condition. Through the liquid carbonation process, a sludge was fixed with rate of 0.175 mg of $CO_2$ per mg of sludge. It was found from XRD results that the structure of final product was composed of a calcite structure which is general structure of $CaCO_3$.

Formation Characteristics of Environment Friendly Electrodeposit Films Formed in Natural and Synthetic Seawater Conditions (천연 및 인공해수를 이용하여 제작한 환경친화적인 전착코팅막의 형성 특성)

  • 이명훈;이찬식
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.28 no.6
    • /
    • pp.1000-1009
    • /
    • 2004
  • The environment friendly calcareous deposit films were formed on steel plates by electrodeposition technique in natural seawater and synthetic solutions such as dissolved $\textrm{Mg}^{2+}$ and $\textrm{Ca}^{2+}$ ions at various potential conditions. The influence of potential conditions on composition ratio, structure and morphology of the electrodeposited films were investigated by scanning electron microscopy(SEM), energy dispersive spectroscopy(EDS) and X-ray diffractor (XRD). Accordingly, this study was provided a better understanding of the composition between the growth of $\textrm{Mg(OH)}_2$ and that of $\textrm{CaCO}_3$ during the formation of calcareous deposit films on steel substrate under cathodically electrodeposition in synthetic and natural seawater. The results showed that the formation of good overall calcareous deposited film in seawater can be achieved by controlling the Ca/Mg ratio according to interfacial pH with the effective use of the electro deposition technique.

Physical Properties of Pyrolized Oyster Shell Consisting of Porous CaO/CaCO3 and Phosphorus Removal Efficiency (CaO/CaCO3 다공체로 이루어진 활성 굴 패각의 물성 및 인 제거 효능에 관한 연구)

  • Lee, Chan-Won;Jeon, Hong-Pyo;Kwon, Hyok-Bo
    • Journal of the Korean Ceramic Society
    • /
    • v.47 no.6
    • /
    • pp.524-528
    • /
    • 2010
  • In this study, the structure and properties of waste oyster shell and its phosphorus removal efficiency were investigated. Waste oyster shells are troublesome environmental waste in the coastal region where the oysters are produced. Waste oyster shells were pyrolyzed by bench-scale rotary kiln for its activation. It shows maximum 76% of phosphorus removal efficiency for the municipal wastewater and livestock wastewater. We found that the activated oyster shells can be used as a phosphorus removal agent with the consideration of high efficiency, easy processing, and cost effectiveness.

Properties of Cement Paste Containing High Volume γ-C2S and MgO Subjected to CO2 Curing (γ-C2S 및 MgO를 다량 혼입한 시멘트 페이스트의 CO2 양생유무에 따른 특성변화)

  • Sung, Myung-Jin;Cho, Hyeong-Kyu;Lee, Han-Seung
    • Journal of the Korea Institute of Building Construction
    • /
    • v.15 no.3
    • /
    • pp.281-289
    • /
    • 2015
  • Carbonation of concrete causes reduction of pH and subsequently causes steel corrosion for reinforced concrete structure. However, for plain concrete structure or PC product, it can lead to a decrease in porosity, high density, improvement of concrete, shrinkage-compensation. Recently, based on this theory, research of $CO_2$ curing effect has been performed, but it was mainly focused on its effects on compressive strength using only ordinary portland cement. Researches on $CO_2$ curing effect for concrete containing $CO_2$ reactive materials such as ${\gamma}-C_2S$, MgO haven't been investigated. Therefore, this study has performed experiments under water-binder ratio 40%, and the replacement ratios of ${\gamma}-C_2S$ and MgO were 90%. Micro-chemical analysis, measurement of compressive strength according to admixtures and $CO_2$ curing were investigated. Results from this study revealed that higher strength was measured in case of $CO_2$ curing compared with none $CO_2$ curing for plain specimen indicating difference between 1.08 and 1.26 times, in case of ${\gamma}-C_2S$ 90, MgO 90 specimen, incorporating high volume replaced as much as 90%, it was proven that when applying $CO_2$ curing, higher strength which has difference between 14.56 and 45.7 times, and between 6.5 and 10.37 times was measured for each specimen compared to none $CO_2$ curing. Through micro-chemical analysis, massive amount of $CaCO_3$, $MgCO_3$ and decrease of porosity were appeared.

Zeolitification Characteristics of Coal Fly Ash by Amount of Na2CO3 Using the Fusion/Hydrothermal Method (용융/수열합성법으로부터 Na2CO3 첨가량에 따른 석탄비산재의 제올라이트화 특성)

  • Lee, Chang-Han
    • Journal of Environmental Science International
    • /
    • v.28 no.6
    • /
    • pp.553-559
    • /
    • 2019
  • In this study, zeolitic materials at $Na_2CO_3/CFA$ ratio of 0.6 - 1.8 were synthesized from coal fly ash from a thermal power plant using a fusion/hydrothermal method. The zeolitic materials were found to have cubic crystals structure and X-ray diffraction (XRD) peaks of Na-A zeolite by XRD and SEM analysis. When the zeolitic materials were synthesized from the coal fly ash, the XRD peaks of the zeolitic materials at $Na_2CO_3/CFA$ ratios of 0.9-1.8 had the same location as the XRD peaks of commercial Na-A zeolite. The XRD peaks of the Na-A zeolite ($Na_{12}Al_{12}Si_{12}O_{48}27.4H_2O$) were confirmed in the $2{\theta}$ in the range of 7.18-34.18. However, it was also confirmed that peaks of $CaCO_3$, an impurity inhibiting synthesis of Na-A zeolite from CaO and $Na_2CO_3$ in the coal fly ash, occurred in the XRD peaks of the zeolitic materials at $Na_2CO_3/CFA$ ratio of 1.5-1.8. The crystallinities of the zeolitic materials tended to increase gradually within the $Na_2CO_3/CFA$ ratio range of 0.6-1.8.

Sorption-enhanced reforming of tar: Influence of the preparation method of CO2 absorbent

  • Xie, Huaqing;Zhang, Weidong;Zhao, Xiangnan;Chen, Hao;Yu, Qingbo;Qin, Qin
    • Korean Journal of Chemical Engineering
    • /
    • v.35 no.11
    • /
    • pp.2191-2197
    • /
    • 2018
  • To remove tar and produce environment-friendly $H_2$, one of the promising routes is the sorption-enhanced steam reforming (SESR) process, in which the $CO_2$ sorbent is a key element. We prepared the $CO_2$ sorbents with $Ca_{12}Al_{14}O_{33}$ as carrier with various methods. Their characterizations were examined, and the sample prepared by solgel (SG) method showed the strongest CaO and $Ca_{12}Al_{14}O_{33}$ phases and the most excellent pore structure among all the samples. Then, a thermogravimetric experiment was conducted, and the results showed that the sample prepared by sol-gel (SG) method had the best $CO_2$ adsorption capacity and excellent long-term cyclic stability. Finally, the sorbent was used into the steam reforming experiments of tar. Under the action of the sorbent, the reforming reaction was enhanced in-situ, with the $H_2$ yield and concentration improved obviously, and especially, $H_2$ concentration can reach over 98.85%.

Crystal Structure and Piezoelectric Properties of Four Component Langasite A3B Ga3Si2O14 (A = Ca or Sr, B = Ta or Nb)

  • Ohsato, Hitoshi;Iwataki, Tsuyoshi;Morikoshi, Hiroki
    • Transactions on Electrical and Electronic Materials
    • /
    • v.13 no.4
    • /
    • pp.171-176
    • /
    • 2012
  • As langasite $A_3BC_3D_2O_{14}$ compounds with piezoelectric properties exhibit no phase transition up to the melting point of 1,400-$1,500^{\circ}C$, many high temperature applications are expected for the SAW filter, temperature sensor, pressure sensor, and so on, based on the digital transformation of wider bandwidth and higher-bit rates. It has a larger electromechanical coupling factor compared to quartz and also nearly the same temperature stability as quartz. The $La_3Ga_5SiO_{14}$ (LGS) crystal with the $Ca_3Ga_2Ge_4O_{14}$-type crystal structure was synthesized and the crystal structure was analyzed by Mill et al. It is also an important feature that the growth of the single crystal is easy. In the case of three-element compounds such as $[R_3]_A[Ga]_B[Ga_3]_C[GaSi]_DO_{14}$ (R=La, Pr and Nd), the piezoelectric constant increases with the ionic radius of R. In this study, crystal structures of four-element compounds such as $[A_3]_A[B]_B[Ga_3]_C[Si_2]_DO_{14}$ (A = Ca or Sr, B = Ta or Nb) are analyzed by a single crystal X-ray diffraction, and the mechanism and properties of the piezoelectricity depending on the species of cation was clarified based on the crystal structure.

The Study of $Eu^{2+}$-activated Calcium Aluminium Silicate Phosphors for White UV-LED (백색 UV-LED를 위한 $Eu^{2+}$-활성화 칼슘 알루미늄 실리케이트 형광체 연구)

  • Hwang, Jung-Ha;Jang, Bo-Yun;Park, Joo-Seok
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.06a
    • /
    • pp.32-35
    • /
    • 2006
  • For the white UV-LED applications, $Eu^{2+}$-activated calcium aluminium silicate phosphors were synthesized for the first time and the structures and luminescence characteristics of these phosphors were investigated. The phosphors in this study emitted blue. green or blue-green light depending on the starting materials for synthesis. In addition, the structure was also changed when the different starting materials were used. When CaO and $CaCO_3$ was used as a starting material. tetragonal $Ca_2Al_2SiO_7$ was formed and blue-green and pure green light was emitted. respectively. However. in the case of $CaSiO_3$, triclinic $CaAl_2Si2O_8$ was formed and only pure blue emission was detected. The maximum emission intensity was obtained from $CaAl_2Si_2O_8:Eu^{2+}$ phosphors, which intensity was about 1.4 times higher than that of YAG:$Ce^{3+}$ phosphor used for blue LED.

  • PDF

A Study on Effect of Inorganic Fillers to Rubber Properties (고무물성(物性)에 미치는 국산(國産) 무기충전제(無機充塡劑)의 효과(效果)에 관(關)한 연구(硏究))

  • Kim, Ki-Joo;Kim, Jong-Seok;Ahn, Byung-Kook;Suh, Soo-Kyo;Chang, Young-Jae;Kang, Kyoung-Ho
    • Elastomers and Composites
    • /
    • v.24 no.4
    • /
    • pp.276-289
    • /
    • 1989
  • This study deals with both effects of inorganic fillers to vulcanized rubbers such as NR, CR, EPDM, NBR & SBR and inorganic characteristics of domestic fillers in comparision with hard clay produced in the USA. The results were as follows. 1. Main ingredient of domestic clay "Ha-dong clay" was Halloysite, "No-ha Island" was Pyrophyllite with $\alpha$-Quartz, and both of "Hard clay" & "Hwa-soon clay" were proved to be Kaolinite by XRD, DT-TGA and chemical analysis by XRF. 2. Tensile strength value of SBR compounded with these fillers, was Hard clay $146kg\;f/cm^2$, Kaolinite $123kg\;f/cm^2$, Pyrophyllite $82kg\;f/cm^2$, Halloysite $80kg\;f/cm^2$, precipitated $CaCO_3\;27kg\;f/cm^2$, and ground $CaCO_3$ was $21kg\;f/cm^2$. These results showed the increase of seven times according to filler species. 3. The physical properties of non-crystalline rubbers, such as SBR, NBR & EPDM, compared with NR & CR, have been considerably changed according to crystalline phase, particle size, shape and surface structure of fillers. Especially, tensile strength value in case of SBR & EPDM, was differentiated about 1.5 times by the particle size of fillers. 4. In SBR, physical properties of rubber compounded with Kaolinite which was surface treated with fatty acid and silane, almost approach to the value of hard clay. 5. Delayed cure time of Kaolinite and decrease of rubber properties by $CaCO_3$ can be improved by blending kaolinite & $CaCO_3$ in the ratio of 2:1.