• Title/Summary/Keyword: $CO_2$ welding

Search Result 583, Processing Time 0.023 seconds

A study on the influence of process parameters during laser welding of sheet steels (강판의 레이저 용접시 공정변수의 영향에 관한 연구)

  • Park, Young-Soo;Lee, Yoon-Sik;Kim, Hyung-Sik;Kim, Chan
    • Laser Solutions
    • /
    • v.2 no.3
    • /
    • pp.11-18
    • /
    • 1999
  • This paper describes the weldability of carbon steel and stainless steel using 5㎾ $CO_2$ laser system with nearly multi-mode beam and a parabolic focusing mirror. In the laser welding of steels, major welding parameters are focal point, travel speed, beam power, shield gas and gap tolerance, etc.. Two kinds of gases(Ar, He) were used as a assist gas and supplied through the external nozzle. It is very important for optimum condition to remove plasma plume which absorbs laser beam and to obtain deep penetration and sound weld bead. Bead-on-plate welding tests were carried out for the experiments. Penetration data were obtained with various welding parameters and the effects of welding parameters were discussed. Butt welding tests were performed with various conditions. Only the optimum laser parameters assured good weld quality As a result of this study, We achieve the fundamental weldabilities using a high power $CO_2$ laser for carbon steel and stainless steel.

  • PDF

A Study on the Application of SAW Process for Thin Plate of 3.2 Thickness in Ship Structure (선체외판부 3.2T 박판에 대한 SAW 용접 적용에 관한 연구)

  • Oh, Chong-In;Yun, Jin-Oh;Lim, Dong-Young;Jeong, Sang-Hoon;Lee, Jeong-Soo
    • Proceedings of the KWS Conference
    • /
    • 2010.05a
    • /
    • pp.51-51
    • /
    • 2010
  • Recently just as in the automobile industry, shipbuilders also try to reduce material consumption and weight in order to keep operating costs as low as possible and improve the speed of production. Naturally industry is ever searching for welding techniques offering higher power, higher productivity and a better quality. Therefore it is important to have a details research based on the various welding process applied to steel and other materials, and to have the ability both to counsel interested companies and to evaluate the feasibility of implementation of this process. Submerged-arc welding (SAW) process is usually used about 20% of shipbuilding. Similar to gas metal arc welding(GMAW), SAW involves formation of an arc between a continuously-fed bare wire electrode and the work-piece. The process uses a flux to generate protective gases and slag, and to add alloying elements to the weld pool and a shielding gas is not required. Prior to welding, a thin layer of flux powder is placed on the work-piece surface. The arc moves along the joint line and as it does so, excess flux is recycled via a hopper. Remaining fused slag layers can be easily removed after welding. As the arc is completely covered by the flux layer, heat loss is extremely low. This produces a thermal efficiency as high as 60% (compared with 25% for manual metal arc). SAW process offers many advantages compared to conventional CO2 welding process. The main advantages of SAW are higher welding speed, facility of workers, less deformation and better than bead shape & strength of welded joint because there is no visible arc light, welding is spatter-free, fully-mechanized or automatic process, high travel speed, and depth of penetration and chemical composition of the deposited weld metal. However it is difficult to application of thin plate according to high heat input. So this paper has been focused on application of the field according to SAW process for thin plate in ship-structures. For this purpose, It has been decided to optimized welding condition by experiments, relationship between welding parameters and bead shapes, mechanical test such as tensile and bending. Also finite element(FE) based numerical comparison of thermal history and welding residual stress in A-grade 3.2 thickness steel of SAW been made in this study. From the result of this study, It makes substantial saving of time and manufacturing cost and raises the quality of product.

  • PDF

EFFECT OF WELDING SEQUENCE ON THE RESIDUAL STRESSES OF PLATE WITH LONGITUDINAL STIFFENERS

  • Kim, Namin;Lee, Jeongsoo;Woohyeon Choe
    • Proceedings of the KWS Conference
    • /
    • 2002.10a
    • /
    • pp.657-660
    • /
    • 2002
  • In this paper, a study on the residual stress of plate with longitudinal stiffeners is explained in terms of the welding sequences. In order to verify the results of numerical analysis, the hole drilling method (HDM) is performed, to measuring the residual stresses of the test plates in $CO_2$ Flux Cored Arc Welding (FCAW) under various welding conditions. The non-linear transient analysis technique for the numerical analysis in a large and complicate structure is considered. The residual stress of plate in consideration of the welding sequences and directions is evaluated by some numerical simulations and also by experiments. Comparison of numerical analysis results with experimental data shows the accuracy and validity of the proposed method.

  • PDF

$CO_2$ Laser Beam Welding and Formability of Steel Plates with Different Thicknesses (이종두께 강판의 $CO_2$ 레이저 용접 및 성형성)

  • Suh, J.;Han, Y.H.;Kim, J.O.;Lee, Y.S.
    • Journal of Welding and Joining
    • /
    • v.14 no.1
    • /
    • pp.82-91
    • /
    • 1996
  • The maximum butt-joint gap size in $CO_2$ laser beam welding of SAPH steel plates with different thicknesses and its bending formability were studied. In the range of the gap size$\geq$0.1mm, the optimal butt welding speed was faster than that of no gap (air gap) condition. This behaviour was independent on the difference of thickness at any combination. Also, the allowable gap size in steel plates with different thicknesses was larger than with same thicknesses. In the range of $T/T_0$(bead shape) $\geq$ 0.8, good bending formability was obtained at any combination of thickness. The formability was improved by reducing the hardness in weld bead using pre-heating process. Finally, FEM result of the laser beam welded underframe with different thicknesses was compared to that of the conventional spot welded underframe.

  • PDF

A Study of Rotating Arc Sensor Using Fuzzy Controller for$CO_2$ Arc Welding ($CO_2$ 아크 용접에서 퍼지 제어기를 이용한 회전 아크센서에 관한 연구)

  • Choi Youngsoo;Park Hyunsung
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • v.13 no.5
    • /
    • pp.110-117
    • /
    • 2004
  • In automatic welding process using a robot, seam tracking is one of the important parts. Sensor for seam tracking is divided broadly into two categories as non contact sensor and contact sensor. The arc sensor is one of the non contact sensors, and it can be applied in weaving arc and rotating arc welding process. In such the arc sensors, rotating arc sensor can be applied to high speed welding over tens of Hz. The decrease of self regulation by high rotating speed causes to improve accuracy and response of sensor. In this study, fuzzy controller was used to track the seam for the $CO_2$ arc welding which had unstable arc. It could be shown that the rotating arc sensor was better than the weaving arc sensor.

A Study on Locally Drying Underwater Welding (국부건식(물커튼식)수중용접법에 관한 연구)

  • 이규복;황선효;박영조;김종열
    • Journal of Welding and Joining
    • /
    • v.10 no.2
    • /
    • pp.51-62
    • /
    • 1992
  • A torch was designed and fabricated in order to develope the technology of "locally drying underwater welding" by water curtain method. The condition for the formation of the possible local cavity, the mechanical properties and the thermal cycle of welds were investigated in the developed welding equipment compared with in-air welding. The possibility of highly reliable and practical underwater welding was found. The proper local cavity was formed above the water flowrate of 30l/min and CO$_{2}$ gas flowrate of 100l/min. The bead width and penetration depth were increased with increasing welding current. The hardness of weldments is about 160Hv in air welding, but about 210Hv in underwater welding. The elongation and the impact value of underwater weldments are 15% and 6Kg/cm$^{2}$ respectively, which are only half as much as the values of in-air welding. The cooling time in the temperature range from 800.deg.C to 500.deg.C affecting the structure and the hardness of weldments is about 22sec. in air welding while about 10sec. in underwater welding.r welding.

  • PDF

High Power $CO_2$ Laser Beam Welding of AISI 316 Stainless Steel (AISI 316 스테인레스강의 $CO_2$ 레이저 용접)

  • 김재도
    • Journal of Welding and Joining
    • /
    • v.9 no.2
    • /
    • pp.29-36
    • /
    • 1991
  • 6mm 두께의 AISI 316 스테인레스강의 레이저 용접 특성에 대해서 고찰하였다. 3kW C $O_{2}$레이저를 사용하였으며, 레이저 빔은 TE $M_{00}$모우드였고 연속파이었다. 용입 깊이, 비드 폭, 고온 크랙, 가공등의 특성을 고찰하는데 있어서, 레이저 출력은 1kW에서 2.5kW까지, 용접 속도는 5.1m/min까지 적용하였다. 3차원 열전달 방정식에 의한 용입 깊이와 비드 폭에 대한 예측치와 실험 결과를 비교하였는데, 서로 잘 일치하였다.다.

  • PDF

$CO_2$ Weldability of Zn Coated Steel Sheet(2) -Mechanism of Weld Defect Formation- (아연도금강판의 $CO_2$ 용접특성(2) - 용접결함의 형성기구 -)

  • 이종봉;안영호;박화순
    • Journal of Welding and Joining
    • /
    • v.18 no.2
    • /
    • pp.64-68
    • /
    • 2000
  • The mechanism of the blowhole and the pit formation in lap-jointed fillet Co₂arc welds of Zn-coated steel sheet was established by the direct observation of the gas behavior in the molten pool with the high speed camera system. Main conclusions obtained are as follows: 1) Some blowholes were formed by incomplete back-filling to the pits at the last stage of the solidification. This type of blowhole was formed through four stages of gas in the molten pool, incubation, explosion, back-filling and completion of back-filling stage. 2) Most of the pits was back-filled at the last stage of their formation.

  • PDF

A Study on the Feasibility of Partial Penetration Laser Welding for the Lap Joint of 390MPa High Strength Steel Sheets (390MPa급 고장력강판의 경치기 레이저 용접에서 부분용입 용접의 적용 가능성에 대한 연구)

  • 이경돈;박기영;김주관
    • Journal of Welding and Joining
    • /
    • v.20 no.2
    • /
    • pp.95-101
    • /
    • 2002
  • After high power lasers are avaliable in the commercial market, the number of applications of the laser welding has been increased in manufacturing industries. Although the tailored blank laser welding of butt jointed steel sheets is well known recently in the automotive industries, the lap joint laser welding is a new technology to the automotive manufacturing people as well as the design people. But the deep penetration laser welding seems to be preferred to the partial penetration welding for the lap joint welding in the automotive manufacturers because the partial penetration is a serious deflect for the butt joint. In this study, the feasibility of partial penetration welding fur the lap joint $CO_2$ laser welding was studied fur the 1mm thick 390MPa high strength steel sheets for automotive bodies. The process window of the lap joint partial penetration welding was obtained from experiments with the gap size and the welding speed as process parameters. The partial penetration welding was found excellent on the basis of the tensile shear strength and sectional geometry. The bead width, input energy Per volume, tensile-shear strength, deformation energy and the sectional geometries after tensile-shear tests of partial penetration welded specimens are compared with those of full penetration welded specimens with a series of gaps and welding speeds.

Effect of base metal and welding heat input on the properties of low temperature steel welds made by Electro Gas Welding (저온용 강재 Electro Gas 용접부 물성에 미치는 모재와 용접 입열의 영향)

  • Sung, Hee-Joon;Goo, Yeon-Baeg;Kim, Kyeong-Ju
    • Proceedings of the KWS Conference
    • /
    • 2009.11a
    • /
    • pp.51-51
    • /
    • 2009
  • In order to understand the properties of high heat input welds made by electro gas welding, two kinds of low temperature steel were welded. Welding heat inputs were controlled by width of root gap and ranged from 118 to 143kJ/cm. Chemical composition and micro-structural analysis were performed. To understand low temperature impact properties, Charpy impact test was conducted at several temperatures. The results were summarized as follows; 1) Grain size of weld metal and heat affected zone was increased with an increase in welding heat input. 2) Impact test values at fusion line were severely fluctuated regardless of base metals, showing enormous difference among the values at the same test temperature.

  • PDF