• Title/Summary/Keyword: $CF_X$

Search Result 211, Processing Time 0.029 seconds

An Investigation on the Surface Reactions after the Etching of $CeO_2$ Thin Films using High Denstity Inductively Coupled $C1_2CF_4Ar$Ar Plasmas (고밀도 유도결합 $C1_2CF_4Ar$ 플라즈마를 이용한 $CeO_2$ 박막 식각후 표면반응에 관한 연구)

  • 장윤성;김남훈;김경섭;이병기;엄준철;김태형;장의구
    • Proceedings of the International Microelectronics And Packaging Society Conference
    • /
    • 2002.05a
    • /
    • pp.255-258
    • /
    • 2002
  • In this study, $CeO_2$thin films were etched with an addition of $Cl_2$gas to $Ar/CF_4$gas mixing in an inductively coupled plasma(ICP) etcher. The surface reactions of the etched $_CeO2$thin films were investigated by X-ray photoelectron spectroscopy(XPS). It was analyzed that Ce peaks were mainly observed in Ce-O bonds formed $CeO_2$or $CeO_3$compounds. Cl peaks were detected by the peaks of Cl $2p_{3/2}$ and Cl $2p_{1/2}$. Almost all of Cl atoms were combined with Ce atoms like $CeCl_{x}$ compounds.

  • PDF

A Study on the Etching Mechanism of (Ba,Sr)$TiO_3$ Thin Films using MEICP (MEICP에 의한 (Ba,Sr)$TiO_3$ 박막의 식각 메커니즘에 관한 연구)

  • Min, Byung-Jun;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.04b
    • /
    • pp.52-55
    • /
    • 2000
  • In this study, (Ba,Sr)$TiO_3$(BST) thin films were etched with a magnetically enhanced inductively coupled plasma(MEICP) as a function Ar/$CF_4$ gas mixing ratio. Experiment was done by varying the etching parameters such as rf power, dc bias voltage and chamber pressure. The maximum etch rate of the BST films was 1700 ${\AA}/min$ under $CF_4/(CF_4+Ar)$ of 0.1, 600 W/350 V and 5 mTorr. The selectivity of BST to Pt and PR was 0.6, 0.7, respectively. X -ray photoelectron spectroscopy(XPS) studies shows that there are surface reaction between Ba, Sr, Ti and C, F radicals during the etching. To analyze the composition of surface residue remaining after the etching, films etched with different $CF_4$/Ar gas mixing ratio were investigated using XPS.

  • PDF

Etching Characteristics BST Thin Film in $CF_4$/Ar Plasma ($CF_4$/Ar 플라즈마에 의한 BST 박막 식각 특성)

  • 김동표;김창일;서용진;이병기;장의구
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.866-869
    • /
    • 2001
  • In this study, (Ba,Sr)TiO$_3$(BST) thin films were etched with a magnetically enhanced inductively coupled plasma(MEICP). Etching characteristics of BST thin films including etch rate and selectivity were evaluated as a function of the etching parameters such as gas mixing ratio, rf power, dc bias voltage and chamber pressure. The maximum etch rate of the BST films was 1700 $\AA$/min at Ar(90)/CF$_4$(10), 600 W/350 V and 5 mTorr. The selectivity of BST to PR was 0.6, 0.7, respectively. To analyze the composition of surface residue remaining after the etching, samples etched with different CF$_4$/Ar gas mixing ratio were investigated with X-ray photoelectron spectroscopy (XPS) and secondary ion mass spectrometry (SIMS). From the results of XPS and SIMS, there are chemical reaction between Ba, Sr, Ti and C, F radicals during the etching and remained on the surface.

  • PDF

Dry etching of ZnO thin film using a $CF_4$ mixed by Ar

  • Kim, Do-Young;Kim, Hyung-Jun
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2009.10a
    • /
    • pp.1504-1507
    • /
    • 2009
  • In this paper, the etching behavior of ZnO in $CF_4$ plasma mixed Ar was investigated. Previously, the etch rate in $CF_4$/Ar plasma was reported that it is slower than that in Cl containing plasma. But, plasma included Cl atom can produce the by-product such as $ZnCl_2$. In order to solve this film contamination, no Cl containing etching gas is required. We controlled the etching parameter such as source power, substrate bias power, and $CF_4$/Ar gas ratio to acquire the fast etch rate using a ICP etcher. We accomplished the etching rate of 144.85 nm/min with the substrate bias power of 200W. As the energetic fluorine atoms were bonded with Zinc atoms, the fluoride zinc crystal ($ZnF_2$) was observed by X-ray photoelectron spectroscopy (XPS).

  • PDF

The Patterning of Polyimide Thin Films for the Additive $CF_4$ gas ($CF_4$ 첨가에 따른 po1yimide 박막의 패터닝 연구)

  • 강필승;김창일;김상기
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11a
    • /
    • pp.209-212
    • /
    • 2001
  • Polyimide(PI) films have been considered as the interlayer dielectric materials due to low dielectric constant, low water absorption, high gap-fill and planarization capability. The PI film was etched with using inductively coupled plasma (ICP). The etching characteristics such as etch rate and selectivity were evaluated to gas mixing ratio. High etch rate was 8300$\AA$/min and vertical profile was approximately acquired 90$^{\circ}$ at CF$_4$/(CF$_4$+O$_2$) of 0.2. The selectivies of polyimide to PR and SiO$_2$ were 1.2, 5.9, respectively. The etching profiles of PI films with an aluminum pattern were measured by a scanning electron microscope (SEM). The chemical states on the PI film surface were investigated by x-ray photoelectron spectroscopy (XPS). Radical densities of oxygen and fluorine in different gas mixing ratio of 07CF4 were investigated by optical emission spectrometer (OES).

  • PDF

Characteristics of Plasma Damage and Recover in PZT Films by Dry Etching (건식식각에 의한 PZT 박막의 플라즈마 손상 및 회복특성)

  • 강명구;김경태;김동표;김창일
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.07a
    • /
    • pp.375-378
    • /
    • 2002
  • We investigated the reduction of etching damage by additive O$_2$ in etching gas and recovery of etching damage by O$_2$ annealing. The PZT thin films were etched using additive Ar or O$_2$ into Cl$_2$/CF$_4$ gas mixing ratio of 8/2. In order to recover ferroelectric properties of PZT thin films after etching, the etched PZT thin films were annealed at 600 C in O$_2$ atmosphere for 10 min. The remanent polarization is decreased seriously and fatigue is accelerated in the PZT sample etched in Ar/(C1$_2$+CF$_4$) plasma, whereas these characteristics are improved in O$_2$/(Cl$_2$/CF$_4$). From x-ray photoelectron spectroscopy (XPS) analysis, the intensities of Pb-O, Zr-O and Ti-O peaks are changed and the etch byproducts such as metal chloride and metal fluoride are reduced by O$_2$ annealing. From electron probe micro analyzer (EPMA) and auger electron spectroscopy(AES), O$_2$ vacancy is observed after etching. In x-ray diffraction (XRD), the structure damage in the additive O$_2$ into C1$_2$/CF$_4$ is reduced and the improvement of ferroelectric behavioral annealed sample is consistent with the increase of the (100) and (200) PZT peaks.

  • PDF

A Study on Etch Characteristics of CeO2 Thin Film in An Ar/CF4/Cl2 Plasma (Ar/CF4/Cl2 플라즈마에 의한 CeO2 박막의 식각 특성 연구)

  • 장윤성;김동표;김창일;장의구
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.15 no.5
    • /
    • pp.388-392
    • /
    • 2002
  • In this work, the etching of $CeO_2$ thin films has been performed in an inductively coupled $Ar/CF_4/Cl_2$ plasma. The highest etch rate of the $CeO_2$ thin film ws 250 ${\AA}/min$ and the selectivity of CeO$_2$to SBT was 0.4 at a 10% additive $Cl_2$ into Ar/($Ar+CF_4$)gas mixing ratio of 0.8. From result of X-ray photoelectron spectroscopy (XPS) analysis, there are Ce-Cl and Ce-F bonding by chemical reaction between Cl, F and Ce. During the etching of $CeO_2$ thin films in $Ar/CF_4/Cl_2$ plama, Ce-Cl and Ce-F bond is formed, and these prodcuts can be removed by the physical bombardment of Ar ions. The 10% additive $Cl_2$ into the Ar/($Ar+CF_4$)gas mixing ratio of 0.8 could enhance the reaction between Cl, F and Ce.

Etching characteristics of gold thin films using inductively coupled Ar/$CF_4/Cl_2$ plasma (Ar/$CF_4/Cl_2$ 유도 결합 플라즈마에 의한 gold 박막의 식각특성)

  • Kim, Nam-Kyu;Chang, Yun-Seong;Kim, Dong-Pyo;Kim, Chang-Il;Chang, Eui-Goo;Lee, Byeong-Ki
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.11a
    • /
    • pp.190-194
    • /
    • 2002
  • In this study, the etching of Au thin films have been performed in an inductively coupled CF4/Cl2/Ar plasma. The etch properties were measured as the CF4 adds from 0 % to 30 % to the Cl2/(Cl2 + Ar) gas mixing ratio of 0.2. Other parameters were fixed at a rf power of 700 W, a dc bias voltage of 150 V, a chamber pressure of 15 mTorr, and a substrate temperature of $30^{\circ}C$. The highest etch rate of the Au thin film was 370 nm/min at a 10 % additive CF4 into Cl2/(Cl2 + Ar) gas mixing ratio of 0.2. The surface reaction of the etched Au thin films was investigated using x-ray photoelectron spectroscopy (XPS) analysis. From x-ray photoelectron spectroscopy (XPS) analysis, the intensities of Au peaks are changed. There is a chemical reaction between Cl and Au. Au-Cl is hard to remove on the surface because of its high melting point and the etching products can be sputtered by Ar ion bombardment. We obtained the cleaned and steep profile.

  • PDF

The study on the dry etching characteristics of $CeO_2$ thin films ($CeO_2$ 박막의 건식 식각 특성 연구)

  • Oh, Chang-Seck;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.05b
    • /
    • pp.84-87
    • /
    • 2001
  • In this study, $CeO_2$ thin films were etched with a $CF_4/Ar$ gas combination in inductively coupled plasma (ICP), The maximum etch rate of $CeO_2$ thin films is $270{\AA}/min$under $CF_4/(CF_4+Ar)$ of 0.2, 600 W/-200 V, 15 mTorr, and $25^{\circ}C$. The selectivities of $CeO_2$ to PR and SBT are 0.21, 0.25. respectively. The surface reaction of the etched $CeO_2$ thin films was investigated with x-ray photoelectron spectroscopy (XPS). There is a chemical reaction between Ce and F, Compounds such as $Ce-F_x$ are remains on the surface of $CeO_2$ thin films. Those products can be removed by Ar ion bombardment effect, The results of secondary ion mass spectrometer (SIMS) were equal to these of XPS. Scanning electron microscopy (SEM) was used to examine etched profiles of $Ce-F_x$ thin films. The etch profile of over-etched $CeO_2$ films with the $0.5 {\mu}m$ line was approximately $65^{\circ}$.

  • PDF

The effects of Hemistepta lyrata Bunge (Bunge) fractionated extract on liver X receptor α-dependent lipogenic genes in hepatocyte-derived cells (간 실질세포주에서 니호채(泥胡菜) 분획물이 liver X receptor α 의존적 지방 생성 유전자의 발현에 미치는 효과)

  • Kim, Jae Kwang;Cho, Il Je;Kim, Eun Ok;Jung, Dae Hwa;Ku, Sae Kwang;Kim, Sang Chan
    • Herbal Formula Science
    • /
    • v.28 no.3
    • /
    • pp.255-269
    • /
    • 2020
  • Objectives : Hemistepta lyrata Bunge (Bunge) is a wild herb that has been used for managing fever and wound in Korean Traditional Medicine. The present study explored the effects of H. lyrata extract on liver X receptor (LXR) α-dependent lipogenic genes in hepatocyte-derived cells. Methods : After HepG2 cells or Huh7 cells were pre-treated with 1-10 ㎍/mL of H. lyrata extract or its fractionated extract for 0.5 h, the cells were subsequently exposed to LXR ligand for 6-24 h. Cell viability, LXR response element (LXRE)-driven luciferase activity, sterol regulatory element binding protein-response element (SREBP-RE)-driven luciferase activity, SREBP-1c expression, and mRNA levels of LXRα and its-dependent target genes were determined. In addition, LC-MS/MS analysis was conducted to explore major compounds in H. lyrata-chloroform fractionated extract #4 (HL-CF4). Results : Of various H. lyrata extracts tested, chloroform extract and its fractionated extract #4, HL-CF4, significantly decreased T0901317-mediated SREBP-1c expression. In addition, HL-CF4 significantly reduced LXRE atransactivation and LXRα mRNA expression without any cytotoxicity. Moreover, HL-CF4 prevented the SREBP-RE-driven luciferase activity and mRNA levels of fatty acid synthase and stearoyl-CoA desaturase-1 induced by T0901317. Results from LC-MS/MS analysis at positive/negative mode indicated that HL-CF4 contained several compounds showing m/z 197.1176 (C11H17O3), 693.2913/227.1069 (C38H45O12/C15H15O2), 203.1797 (C15H23), 181.1225 (C11H17O2), 591.2957 (C35H43O8), 379.1040 (C18H19O9), 409.1509 (C20H25O9), 309.1348 (C16H21O6), 391.1404 (C20H23O8), and 669.2924/389.1248 (C36H45O12/C20H21O8). Conclusion : Based on its inhibition of the LXRα-dependent signaling pathway, H. lyrata chloroform extract and HL-CF4 have prophylactic potentials for managing non-alcoholic fatty liver.