• Title/Summary/Keyword: $Al_2O_3-SiC$ composite

Search Result 183, Processing Time 0.025 seconds

Analysis of Temperature dependent Thermal Expansion Behavior in MMCs for Electronic packaging (전자 패키징용 금속복합재료의 온도에 따른 열팽창 특성)

  • 정성욱;남현욱;정창규;한경섭
    • Proceedings of the Korean Society For Composite Materials Conference
    • /
    • 2002.05a
    • /
    • pp.73-76
    • /
    • 2002
  • This study developed SiC/Al composites for electronic packaging to which reinforcements were added with the volume fractions of 49%, 56% and 63% by the squeeze casting method. 0.8 wt.% of the inorganic binder as well as the $Al_2O_3$ fiber and SiC particles with the volume fraction of 1:10 were added to the SiC/Al composites For the produced SiC/Al composites, the CTEs (coefficients of thermal expansion) were measured from 30 to $300^{\circ}C$ and compared with the FEM numerical simulation to analyze the temperature dependent properties. The experiment showed the CTEs of SiC/Al composites that were intermediate values of those of Rule of Mixture and Turner's Model. The CTEs were close to Turner's Model in the room temperature and approached the Rule of Mixture as the temperature increases. These properties analyzed from the difference of the average stress acting between the matrix and the reinforcements proposed in this study

  • PDF

A Study on the Mechanism for the Formation of Partices in electroless Ni Composite Coating(I) (무전해 Ni 복합도금 과정에서 분발의 공석 기구에 대한 연구(I))

  • 이원해;이승평
    • Journal of Surface Science and Engineering
    • /
    • v.22 no.2
    • /
    • pp.69-77
    • /
    • 1989
  • Codeposion of inert particles particles in a metallic mateix by electroless plating process involves two phenomena. Firstly, the adsorption of inercles and secondly, the adsorption of inert particles on the cathode. In the present paper the first adsorption phenomenon and in the next paper the second ane are studied in greaterdetail for the Ni-SiCc, Ni-Al2AO3 and Ni-WC systems. Measurements of the Zeta potentials for the SiC and Al2AO3 particles have been in different electrolyte solutions and the ionic species adsorbed on the Particles studied. The addition of sodium acetate, trisodium citrate and sodium phosphinate to nikel sulface sruomotes the zeta potential of SiC and Al2O3 particles, but zeta phosphinate to nickel is more positive than Al2O3 particles although the amount of nickel ion adsorbrd on the Al2O3 particles become greater than that of SiC particles. It is suggested that this is due to adsortion of Na ion onto the surface SiC particles.

  • PDF

SiC-Whisker Dispersion and Mechanical Properties of $Al_2O_3-SiC Whisker$ Whisker Composite (SiC Whisker의 분산과 $Al_2O_3-SiC Whisker$ 복합재료의 기계적 성질)

  • 정수종;이주완;김득중;신유선;강석중
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.6
    • /
    • pp.492-498
    • /
    • 1993
  • The pretreatment condition for uniform distribution of SiC whisker in A2O3-SiCw composites has been determined and the mechanical properties of the composites with various whisker contents have been measured. Good dispersion of the whisker can be obtained in a solution of pH=10.45 by ball milling and ultrasonic treatment. The relative density of hot pressed composites decreases with the whisker content up to 40vol%, but is found to be satisfactory, over 98% for all samples. The mechanical property of the composites is sensitive to the whisker dispersion. Uniform distributjion of the whisker is critical in order to guarantee good mechanical property.The samples containing 20~30vol% whisker show the best mechanical property within the studied range.

  • PDF

Microstructure and Polytype of in situ-Toughened Silicon Carbide

  • Young Wook Kim;Mamoru Mitomo;Hideki Hirotsuru
    • The Korean Journal of Ceramics
    • /
    • v.2 no.3
    • /
    • pp.152-156
    • /
    • 1996
  • Fine (~0.09 $\mu$m) $\beta$-SiC Powders with 3.3wt% of large (~0.44$\mu$m) $\alpha$-SiC of $\beta$-SiC particles (seeds) added were hotpressed at 175$0^{\circ}C$ using $Y_2O_3$, $Al_2O_3$ and CaO as sintering aids and then annealed at 185$0^{\circ}C$ for 4 h to enhance grain growth. The resultant microstructure and polytypes were analyzed by high resolution electron microscopy (HREM).Growth of $\beta$-SiC with high density of microtwins and formation of ${\alpha}/{\beta}$ composite grains consisting of $\alpha$-SiC domain sandwiched between $\beta$-SiC domains were found in both specimens. When large $\alpha$-SiC (mostly 6H) seeds were added, the $\beta$-SiC transformend preferentially to the 6H polytype. In contrast, when large $\beta$-SiC (3C) seeds were added, the fine $\beta$-SiC transformed preferentially to the 4H polytype. Such results suggested that the polytype formation in SiC was influenced by crystalline form of seeds added as well as the chemistry of sintering aids. The ${\alpha}/{\beta}$ interface played and important role in the formation of elongated grains as evidenced by presence of ${\alpha}/{\beta}$ composite grains with high aspect ratio.

  • PDF

Analysis of Temperature dependent Thermal Expansion Behavior of $\textrm{SiC}_\textrm{p}/\textrm{Al}_2\textrm{O}_{3f}/\textrm{Al}$ Composites ($\textrm{SiC}_\textrm{p}/\textrm{Al}_2\textrm{O}_{3f}/\textrm{Al}$ 복합재료의 온도에 따른 열팽창 특성 해석)

  • 정성욱;남현욱;정창규;한경섭
    • Composites Research
    • /
    • v.16 no.1
    • /
    • pp.1-12
    • /
    • 2003
  • This study developed SiC$_{p}$/A1$_2$O$_3$$_{f}$/Al composites for electronic packaging to which reinforcements were added with the volume fractions of 49%, 56% and 63% by the squeeze casting method. 0.8 wt. % of the inorganic binder as well as the A1$_2$O$_3$ fiber and SiC Particles with the volume fraction of 1:10 were added to the composites, which were produced in the newly designed mold. For the produced SiC/Al composites, the CTEs (coefficients of thermal expansion) were measured from 30 to 300 and compared with the FEM numerical simulation to analyze the temperature dependent properties. The experiment showed the CTEs of SiC$_{p}$/A1$_2$O$_3$$_{f}$/Al composites that were intermediate values of those of Rule of Mixture and Turner's Model. The CTEs were close to Turner's Model in the room temperature and approached the Rule of Mixture as the temperature increases. These properties analyzed from the difference of the average stress acting between the matrix and the reinforcements proposed in this study.

Manufacture and Properties of ${\beta}$-SIC-TiB$_2$ Composites Densified by Pressureless Annealing (無加壓 열처리에 의한 ${\beta}$-SIC-TiB$_2$ 複合體의 製造와 特性)

  • Shin, Yong-Deok;Ju, Jin-Young;Park, Mi-Lim
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.50 no.5
    • /
    • pp.221-225
    • /
    • 2001
  • The effect of $Al_2O_3+Y_2O_3$ additives on fracture toughness of ${\beta}-SiC-TiB_2$ composites by hot-pressed sintering was investigated. The ${\beta}-SiC-TiB_2$ ceramic composites were hot-press sintered and pressureless-annealed by adding 16, 20, 24 wt% ${\beta}-SiC-TiB_2$(6:4 wt%) powder as a liquid forming additives at low temperature(1800 $^{\circ}C$) for 4 h. Phase analysis of composites by XRD revealed mostly of ${\alpha}$-SiC(6H), $TiB_2$, and YAG($Al_5Y_3O_{12}$). The relative density was over 95-88 % of the theoretical density, and the porosity increased with increasing $Al_2O_3+Y_2O_3$ contents because of the increasing tendency of pore formation. The fracture toughness showed the highest value of 5.88 MPa${\cdot}m^{1/2}$ for composites added with 20 wt% $Al_2O_3+Y_2O_3$ additives at room temperature. The electrical resistivity showed the lowest value of $5.22{\times}10^{-4}\;{\Omega}\;{\cdot}\;cm$ for composite added with 20 wt% $Al_2O_3+Y_2O_3$ additives at room temperature, and was all positive temperature coefficeint resistance(PTCR) against temperature up to 900 $^{\circ}C$.

  • PDF

Properties of Electro-Conductive SiC-TiB2 Composites (도전성 ${\beta}-SiC-TiB_2$ 복합체의 특성)

  • Shin, Yong-Deok;Park, Mi-Lim;Song, Joon-Tae;Yim, Seung-Hyuk
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.04b
    • /
    • pp.72-75
    • /
    • 2000
  • The effect of $Al_2O_3+Y_2O_3$ additives on fracture toughness of ${\beta}-SiC-TiB_2$ composites by hot-pressed sintering were investigated, The ${\beta}-SiC-TiB_2$ ceramic composites were hot-presse sintered and annealed by adding 4, 8, 12wt% $Al_2O_3+Y_2O_3$(6 : 4wt%) powder as a liquid forming additives at low temperature($1800^{\circ}C$) for 4h. In this microstructures, the relative density is over 97% of the theoretical density and the porosity increased with increasing $Al_2O_3+Y_2O_3$ contents because of the increasing tendency of pore formation. But the fracture toughness showed the highest of $7.0MPa{\cdot}m^{1/2}$ for composites added with 12wt% $Al_2O_3+Y_2O_3$ additives at room temperature. The electrical resistivity showed the lowest of $1.59\times10^{-3}\Omega{\cdot}cm$ for composite added with 8wt% $Al_2O_3+Y_2O_3$ additives at room temperature and is all positive temperature coefficient resistance(PTCR} against temperature up to $700^{\circ}C$.

  • PDF

Cracked-Healing and Elevated Temperature Bending Strength of Al2O3 Composite Ceramics by an Amount of Y2O3 (Y2O3 첨가량에 의한 Al2O3 복합재 세라믹스의 균열 치유와 고온 굴힘강도 특성)

  • Nam, K.W.;Kim, H.S.;Son, C.S.;Kim, S.K.;Ahn, S.H.
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.31 no.11
    • /
    • pp.1108-1114
    • /
    • 2007
  • The low kinds of $Al_2O_3$ composite ceramics were prepared using a mixture of 85 wt.% $Al_2O_3$ (mean size $0.5\;{\mu}m$), 15 wt.% SiC Powder with $Y_2O_3$, as an additive powder (0, 1, 3 and 5 wt.%). The crack-healing strengths were studied as functions of crack-healing temperature and amount of $Y_2O_3$. The in-situ crack-healing behavior was observed at 1,573 K for 1 h in the air. The heat treated specimen with 3 wt.% of $Y_2O_3$ showed better crack-healing ability than specimen with 1 or 5 wt.% of $Y_2O_3$. In case of specimen with 3 wt.% of $Y_2O_3$, the bending strength of the crack-healed specimen at 1,473 K was recovered to the bending strength of smooth specimen treated at 1573 K. The heat-resistance limit temperature of $Al_2O_3$ composite ceramics was 1,073 K, 1,373 K, 873 K for the specimen with 1, 3, 5 wt.% of $Y_2O_3$.

Manufacture of $\beta-SiC-TiB_2$ Composites Densified by Liquid-Phase Sintering (액상소결에 의한 $\beta-SiC-TiB_2$ 복합체의 제조와 특성)

  • Shin, Yong-Deok;Ju, Jin-Young;Park, Mi-Lim;So, Byung-Moon;Lim, Seung-Hyuk;Song, Joon-Tae
    • Proceedings of the KIEE Conference
    • /
    • 2000.11c
    • /
    • pp.479-481
    • /
    • 2000
  • The effect of $Al_{2}O_{3}+Y_{2}O_{3}$ additives on fracture toughness of $\beta-SiC-TiB_2$ composites by hot-pressed sintering were investigated. The f$\beta-SiC-TiB_2$ ceramic composites were hot-presse sintered and annealed by adding 16, 20, 24wt% $Al_{2}O_{3}+Y_{2}O_{3}$(6 : 4wt%) powder as a liquid forming additives at low temperature($1800^{\circ}C$) for 4h. In this microstructures, the relative density is over 95.88% of the theoretical density and the porosity increased with increasing $Al_{2}O_{3}+Y_{2}O_{3}$ contents because of the increasing tendency of pore formation. The fracture toughness showed the highest of $5.88MPa{\cdot}m^{1/2}$ for composites added with 20wt% $Al_{2}O_{3}+Y_{2}O_{3}$ additives at room temperature. The electrical resistivity showed the lowest of $5.22{\times}10^{-4}\Omega{\cdot}cm$ for composite added with 20wt% $Al_{2}O_{3}+Y_{2}O_{3}$ additives at room temperature and is all positive temperature coefficient resistance (PTCR) against temperature up to $700^{\circ}C$.

  • PDF

A Study on Sintering and mechanical Properties of Sinter/HIPed SiC Whisker/$Al_2O_3$ Composite (Sinter/HIP 공정으로 제조한 SiC whisker/$Al_2O_3$ 복합재료의 소결 및 기계적 물성에 관한 연구)

  • Lee, Chae-Hyun;Kim, Jong-Ock;Kim, Chong-Hee
    • The Journal of Natural Sciences
    • /
    • v.8 no.1
    • /
    • pp.53-59
    • /
    • 1995
  • Effects of sintering additives and sintering temperatures on the sintering behavior and mechanical properties of SiC whisker reinforced alumina composites have been investigated in this study. Dense (>95% TD) composites were obtained by using 2 wt% $Y_2O_3$ as liquid phase sintering additive. But only porous composite could be obtained when the sintering additives were MgO and $TiO_2$, which were known as the sintering additives for solid state sintering of alumina. Bending strength and fracture toughness were enhanced by reinforcement of SiC whisker. It is belived from the microstructure investigation that the enhanced by strength and toughness could be attribute to the reinforcing and grain growth inhibition effects of SiC whisker. After HIP treatment, fully dense composites were obtained and further enhanced mechanical properties achieved.

  • PDF