  • Various metal oxides such as Fe2O3, FeO, TiO2, MnO2, MoO3, WO3 and ZnO have been used as a catalyst for Gif-KRICT type cyclohexane oxidation. In this reaction, the conversion of cyclohexane to cyclohexanone and cyclohexanol and the selectivity ratio of cyclohexanone to cyclohexanol were greatly affected by the acidity of metal oxides. When metal oxide has more acidic property, the reactivity on oxidation is increased and the formation of cyclohexanone is more favored. From this result, we proposed a new mechanism for the biomimetic Gif-KRICT oxidation system.

Studies on Spinel Ferrites (I) Effects of Addition of Rare-Earth Oxides on the Magnetic Properties of Mn-Zn Ferrites (Spinel Ferrite에 관한 연구 (I) Mn-Zn계 Ferrite의 자기특성에 대한 희토류산화물의 첨가효과)

  • 김태옥
    • Journal of the Korean Ceramic Society
    • /
    • v.14 no.2
    • /
    • pp.78-81
    • /
    • 1977
  • The effects of variation in composition and the addition of small amount of the rare-earth oxides La2O3, CeO2 and Sm2O3 on the magnetic properties of Mn-Zn system ferrites, 0.5MnO.0.5ZnO.(1+0.1X) Fe2O3(X=-1, 0, 1, 2), were investigated in the range of frequencies of 0.1~100 kHz. It was shown that the magnetic permeability of the specimens with the composition Mn 0.5 Zn 0.5 Fe2O4 was maximum in the Mn-Zn system ferrites, and that the addition of a small amount of the rare-earth oxides to the composition 0.5 MnO.0.5ZnO.0.9 Fe2O3 caused the sharp increase of magnetic permeability and the decrease of the loss factors.

  • PDF

A Study on the Reaction Characteristics of Rare Earth Oxides with Lithium Oxide in LiCl Molten Salt (LiCl 용융염 중에서 희토류 산화물과 산화리튬의 반응특성에 관한 연구)

  • 오승철;박성빈;김상수;도재범;박성원
    • Proceedings of the Korean Radioactive Waste Society Conference
    • /
    • 2003.11a
    • /
    • pp.447-452
    • /
    • 2003
  • We had clarified the reactions of the rare earth oxides($RE_2O_3$) with lithium oxide produced in lithium reduction process of oxide fuels. Oxides of scandium, yttrium, praseodymium, neodymium, samarium, europium, gadolinium, ytterbium and lutetium reacted with lithium oxide in the higher concentration than the respective certain critical concentration of lithium oxide and formed complex oxides($LiREO_2$). The critical lithium oxide concentrations for the formation of complex oxides of scandium, yttrium, praseodymium, neodymium, samarium, europium, gadolinium, ytterbium and lutetium oxide were respectively 0.1 wt%, 1.9 wt%, 5.3 wt%, 5.0 wt%, 3.0 wt%, 3.9 wt% 2.9 wt%, 2.6 wt% and 0.3 wt%. Cerium and lanthanum oxide did not react with lithium oxide. These complex oxides obtained from experiments have limited solubility in lithium chloride at $650^{\circ}C$.

  • PDF

Smart Solid State Syntheses of Well-Crystallized Phase Pure Mixed Oxides for Electroceramics

  • Sennat, Mamoru
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.11 s.294
    • /
    • pp.680-687
    • /
    • 2006
  • An overview is given to optimize the solid state processes toward phase pure and well-crystallized fine particulates of mixed oxides, serving as electroceramic materials in various genres. Elevation of the reactivity and preservation of stoichiometry of the starting mixture are of universal importance. Mechanical activation is versatile for these purposes, particularly when an oxygen atom as a hinge promotes formation of hetero-bridging bonds between dissimilar cationic species prior to calcination. Case studies carried out recently in the author's laboratory are displayed and compared for ferroelectric materials, i.e. $PbMg_{1/3}Nb_{2/3}O_3$ $xPbTiO_3$(PMN-PT), $(1-y)Pb(Zn_xMg{1-x})_{1/3}$ $yNb_{2/3}O_3$ (PZN-PMN), $BaBi_2Ta_2O_9$ (BBT), $Ba(Mg_{1/3}Ta_{2/3})O_3$ (BMT), and ferromagnetics, i.e. M-, Y-, and Z-phases of Ba-hexaferrites.

Study on the reducibility of substituted $LaMnO_3$ (치환된 $LaMnO_3$의 환원반응성에 대한 연구)

  • Lee, Sang-Beom;Jeon, Hyun-Pyo
    • The Journal of Natural Sciences
    • /
    • v.14 no.2
    • /
    • pp.41-54
    • /
    • 2004
  • $LaMnO_3$ and A site substituted $La_{0.9}Sr_{0.1}MnO_3$(a=$5.33\AA$, c=$13.27\AA$), B site substituted $LaMn_{0.9}Cu_{0.1}O_3$(a=$5.52\AA$, c=$13.31\AA$) mixed oxides were prepared by Citrate sol-gel method. The powder X-ray diffraction patterns of these oxides were indexed with single phase hexagonal perovskite structures. According to the TRR result, oxygen stoichiometry of these oxides were oxidative nonstoichiometry as like $LaMnO_{3.16}$, $La_{0.9}Sr_{0.1}MnO_{3.10}$ and $LaMn_{0.9}Cu_{0.1}O_{3.14}$ Reduction reactions of un-substituted $LaMnO_3$ was two steps, but specific site(A site of B site) partially substituted $LaMnO_3$ oxides were procees to three reactions.

  • PDF

A Study on Catalysts for Simultaneous Removal of 1,2-Dichlorobenzene and NOx (1,2-Dichlorobenzene 및 질소산화물 동시제거를 위한 촉매연구)

  • Park, Kwang Hee;Hong, Sung Chang
    • Applied Chemistry for Engineering
    • /
    • v.20 no.5
    • /
    • pp.522-526
    • /
    • 2009
  • The catalytic oxidation of 1,2-dichloribenzene (1,2-DCB) and simultaneous catalytic reduction of nitrogen oxides over the single catalyst has been investigated over various metals (Ru, Mn, Co and Fe) supported on $Al_2O_3$ and $CeO_{2}$. The activity of the different catalysts for catalytic oxidation of 1,2-dichloribenzene depended on the used metal, Ru/Co/$Al_2O_3$, Mn-Fe/CeO2 and Cr/$Al_2O_3$ (commercial catalysts) being the most actives ones. In the catalytic oxidation of chlorobenzene (CB), Ru/Co/$Al_2O_3$ is better than Pt-Pd/$Al_2O_3$, which is the well-known catalyst good for VOC oxidation. Furthermore, it has a good durability on the deactivation by $Cl_2$ and sulfur. For nitrogen oxides (NOx) removal, NOx conversion was 70% at $260^{\circ}C$.

Effect of Additives on the Refractive Index of B2O3-SiO2-Al2O3 Glasses for Photolithographic Process in Electronic Micro Devices

  • Won, Ju-Yeon;Hwang, Seong-Jin;Lee, Jung-Ki;Kim, Hyung-Sun
    • Korean Journal of Materials Research
    • /
    • v.20 no.7
    • /
    • pp.370-373
    • /
    • 2010
  • In fabricating plasma display panels, the photolithographic process is used to form patterns of barrier ribs with high accuracy and high aspect ratio. It is important in the photolithographic process to control the refractive index of the photosensitive paste. The composition of this paste for photolithography is based on the $B_2O_3-SiO_2-Al_2O_3$ glass system, including additives of alkali oxides and rare earth oxides. In this work, we investigated the density, structure and refractive index of glasses based on the $B_2O_3-SiO_2-Al_2O_3$ system with the addition of $Li_2O$, $K_2O$, $Na_2O$, CaO, SrO, and MgO. The refractive index of the glasses containing K2O, Na2O and CaO was similar to that of the [BO3] fraction while that of the SrO, MgO and Li2O containing glasses were not correlated with the coordination fraction. The coordination number of the boron atoms was measured by MAS NMR. The refractive index increased with a decrease of molar volume due to the increase in the number of non-bridging oxygen atoms and the polarizability. The lowest refractive index (1.485) in this study was that of the $B_2O_3-SiO_2-Al_2O_3-K_2O$ glass system due to the larger ionic radius of $K^+$. Based on our results, it has been determined that the refractive index of the $B_2O_3-SiO_2-Al_2O_3$ system should be controlled by the addition of alkali oxides and alkali earth oxides for proper formation of the photosensitive paste.

Stbilization of Perovskite Phase and Enhanced DPT Characteristics of $Pb(Zn, Mg)_{1/3}Nb_{2/3}O_3-PbTiO_3$ Ceramics by the Additionof Excess Constituent Oxides ($Pb(Zn, Mg)_{1/3}Nb_{2/3}O_3-PbTiO_3$계에서 구성 산화물 첨가에 따른 Perovskite상 안정화 및 DPT성 증대 효과)

  • 이규만;장현명;유병두
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.11
    • /
    • pp.925-932
    • /
    • 1993
  • The perovskite phase in PZN-PMN-PT (Pb(Zn, Mg)1/3Nb2/3O3-PbTiO3) pseudoternary ceramics was stabilized by the addition of excess constituent divalent oxides (PbO, MgO and ZnO). The excess addition of 5mol% MgO or 7.5mol% PbO fully stabilized the perovskite phase. The enhanced diffuse phase transition (DPT) and the decrease in the electrical resistivity observed in the presence of excess ZnO or MgO were interpreted in terms of the additional formation of negatively charged, short-range ordered 1:1 domains with a concomitant generation of charge carriers, holes.

  • PDF

The Effect of $Y_2O_3$ Dispersoids on the High Temperature Oxidation of Ti-34wt%Al-1.5wt%Mn Alloys (Ti-34wt%Al-1.5wt%Mn 합금의 고온산화에 미치는 $Y_2O_3$ 분산입자 첨가효과)

  • Lee, Dong-Bok
    • Journal of the Korean institute of surface engineering
    • /
    • v.39 no.6
    • /
    • pp.288-294
    • /
    • 2006
  • Alloys of TiAl-Mn-(0, 5, 10)wt.% $Y_2O_3$ were prepared by a powder metallurgical route, and their oxidation behavior was studied at 800, 900 and $1000^{\circ}C$ in 1 atm of air. The scale formed on the alloys consisted of $TiO_2$ and $Al_2O_3$ oxides. During oxidation, Mn tended to diffuse outward, whereas oxygen diffused inward. The dispersoids of $T_2O_3$, which segregated at the matrix grain boundaries, acted as a diffusion channel for cations and oxygen ions, nucleation sites for oxides, and vacancy annihilation sites. $T_2O_3$ increased the scale thickness, but improved the scale adherence.

Characterization of Oxide Scales Formed on Ni3Al-7.8%Cr-1.3%Zr-0.8%Mo-0.025%B (Ni3Al-7.8%Cr-1.3%Zr-0.8%Mo-0.025%B 합금의 고온산화막분석)

  • Kim, Gi-Yeong;Lee, Dong-Bok
    • Korean Journal of Materials Research
    • /
    • v.12 no.3
    • /
    • pp.220-224
    • /
    • 2002
  • The oxide scales formed on $Ni_3Al$-7.8%Cr-1.3%Zr-0.8%Mo-0.025%B after oxidation at 900, 1000 and 110$0^{\circ}C$ in air were studied using XRD, SEM, EPMA and TEM. The oxide scales consisted primarily of $NiO,\; NiAl_2O_4,\;{\alpha}-Al_2O_3,\; monoclinic-ZrO_2,\; and \;tetragonal-ZrO_2$. The outer layer of the oxide scale was rich in Ni-oxides, whereas the internal oxide stringers were rich in Al-oxides and $ZrO_2$. Within the above oxide scales, Cr and Mo tended to exist as dissolved ions.