• Title/Summary/Keyword: ${\beta}$-Ti alloy

검색결과 112건 처리시간 0.031초

산소함량에 따른 Ti-Al-Fe-Si-O 합금의 기계적 특성 및 미세조직 변화 (The Effects of Oxygen Content on Microstructure and Mechanical Properties of Ti-Al-Fe-Si-O alloy)

  • 배진주;염종택;박찬희;홍재근;김성웅;윤석영;이상원
    • 열처리공학회지
    • /
    • 제29권6호
    • /
    • pp.264-271
    • /
    • 2016
  • The effect of the oxygen content and the annealing temperature on the tensile behavior of the Ti-1.5Al-3Fe-0.25Si-(0.1~0.5)O alloy was investigated. The tensile properties were dependent on the volume fraction of the microstructure constituents, i.e. the equixed ${\alpha}$, equixed ${\beta}$ and lamellar ${\alpha}$. The results showed that the O-partitioned equixed ${\alpha}$ had a much higher strength compared to the equixed ${\beta}$. The strength of the lamellar ${\alpha}$ increased with increasing the annealing temperature because the O content of the lamellar ${\alpha}$ increased. Ti-1.5Al-3Fe-0.25Si-0.3O alloy annealed to $900^{\circ}C$ where the volume fraction of lamellar ${\alpha}$ was the highest exhibited an excellent combination of the strength (1198.5 MPa) and ductility (27.5%). The effect of the lamellar ${\alpha}$ on the ductility was discussed.

안경테용 Ti 합금 홈선의 고주파유도가열처리에 따른 특성 변화에 관한 연구 (A Study on the Characteristics for High Frequency Induction Heating of Ti Alloy Groove Wire)

  • 박정식;장우영;이정영
    • 한국안광학회지
    • /
    • 제12권3호
    • /
    • pp.55-58
    • /
    • 2007
  • 티타늄과 그 합금은 경량성, 우수한 기계적 성질 그리고 우수한 내식성 때문에 주요한 안경테 소재로 사용되고 있다. 본 연구에서는 티타늄 합금 홈선에 대하여 안경테 브레이징용으로 사용되고 있는 고주파유도가열 장치를 이용한 열처리 시간의 변화에 따른 경도 및 미세조직의 변화에 대하여 조사하였다. ${\beta}-Ti$ 합금은 고주파유도가열처리 시간의 증가에 따라 경도값의 감소가 나타났으며, 이는 열처리 시간의 증가에 따른 결정립의 조대화 때문인 것으로 생각된다. Ti-325 합금의 고주파유도가열처리에서는 2초까지는 경도값이 감소하였으나, 3초에서는 급격히 증가하였다. 이는 2초까지는 결정립의 조대화에 의한 경도값의 감소가 일어나지만, 3초에서는 미세한 ${\alpha}+{\beta}$ 상의 층상조직이 발달하였기 때문으로 판단된다.

  • PDF

베타 티타늄합금의 준 안정상 TEM 회절도형 분석 (TEM Diffraction Analysis of Metastable Phases in Beta Ti Alloys)

  • 최병학;심종헌;김승언;현용택;박찬희;강주희;이용태;김영욱
    • 한국재료학회지
    • /
    • 제25권8호
    • /
    • pp.403-409
    • /
    • 2015
  • Metastable phase characteristics of beta Ti alloys were investigated to consider the relationship of the microstructure and diffraction pattern in TEM. TEM analysis showed that the microstructure was mottled as a modulated structure, and the diffraction pattern was composed of spot streaks between the main spots of a stable beta phase with a specific lattice relationship. The modulated structure may be induced by short distance slip or atom movement during a very short interval of solution treated and quenched (STQ) materials. The athermal ${\omega}$ phase, which could be precipitated at low temperature aging, is also analysed by the metastable phase. The metastable phases including athermal ${\omega}$ phase had a common characteristic of hardened and brittle behavior because the dislocation slip was restricted by a super lattice effect due to short distance atom movement at the metastable state.

Sn 첨가에 따른 극미세 Ti-Fe-Sn 합금의 미세조직 및 기계적 성질 변화 (Sn Effects on Microstructure and Mechanical Properties of Ultrafine Ti-Fe-Sn Alloys)

  • 한준희;송기안;피동혁;방창욱;김기범
    • 한국주조공학회지
    • /
    • 제28권2호
    • /
    • pp.69-73
    • /
    • 2008
  • In the present study, microstructural evolution and mechanical properties of Ti-Fe-Sn ultrafine eutectic alloys have been investigated. Ultrafine eutectic microstructure consisting of a mixture of ${\beta}$-Ti solid solution and TiFe intermetallic compound homogeneously formed in $(Ti_{70.5}Fe_{29.5})_{100-x}Sn_x$ alloys with x = 0, 1 and 3. Addition of Sn is effective to modify the eutectic colony into the spherical shape with decreasing the lamellar spacing and colony size. This results in enhancing the macroscopic plasticity up to 3.1% of the Ti-Fe-Sn ultrafine eutectic alloys.

Advanced Powder Processing Techniques of Ti Alloy Powders for Medical and Aerospace Applications

  • Miura, Hideshi
    • 한국분말재료학회지
    • /
    • 제20권5호
    • /
    • pp.323-331
    • /
    • 2013
  • In this paper, two kinds of advanced powder processing techniques Metal Injection Molding (MIM) and Direct Laser Forming (DLF) are introduced to fabricate complex shaped Ti alloy parts which are widely used for medical and aerospace applications. The MIM process is used to strengthen Ti-6Al-4V alloy compacts by addition of fine Mo, Fe or Cr powders. Enhanced tensile strength of 1030 MPa with 15.1% elongation was obtained by an addition of 4 mass%Cr because of the microstructural modification and also the solution strengthening in beta phase. However, their fatigue strength was lower compared to wrought materials, but was improved by HIP. Subsequently, the effect of feeding layer height (FLH) on the characteristics of the DLF compacts was investigated. In the case of 100 ${\mu}m$ FLH, surface roughness was improved and nearly full density (99.8%) was obtained. Also, tensile strength of 1080 MPa was obtained, which is higher than the ASTM value.

Ti-Mo-Fe 합금의 Fe 함량에 따른 기계적 특성과 전기화학적 특성 비교·분석 (Effect of Fe Content on Mechanical and Electrochemical Properties of Ti-Mo-Fe Alloys)

  • 김지원;박정연;강민;박지환;이동근
    • 열처리공학회지
    • /
    • 제36권3호
    • /
    • pp.145-152
    • /
    • 2023
  • β titanium alloys containing β stabilizing elements such as V, Nb, Ta, Mo and Fe are widely used etc, due to their excellent specific strength, corrosion resistance, fatigue strength and easy formability. New metastable β titanium alloys are developed containing low-cost elements (Mo and Fe) in this study. Fe element is a strong β-stabilizer which can affect the mechanical and electrochemical properties of Ti-5Mo-xFe (x = 1, 4 wt%) alloys. These properties were analyzed in connection with microstructure and phase distribution. Ti-5Mo-4Fe alloy showed higher compression yield stress and maximum stress than Ti-5Mo-1Fe alloy due to solid-solution hardening and grain refinement hardening effect. As Fe element increased, Fe oxide formation and reduction of ${\bar{Bo}}$ (bond order) value affect the decrease of corrosion resistance. Ti-5Mo-xFe alloys were more excellent than Ti-6Al-4V ELI alloy.

Ti-6Al-4V합금의 비틀림 및 압축변형에 따른 고온변형거동 고찰 (Investigation of High Temperature Deformation Behavior in Compression and Torsion of Ti-6Al-4V Alloy)

  • 염종택;정은정;김정한;홍재근;박노광;이종수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2008년도 춘계학술대회 논문집
    • /
    • pp.435-438
    • /
    • 2008
  • High temperature deformation of Ti-6Al-4V alloy with a lamellar colony microstructure was investigated by hot compression and torsion tests. The torsion and compression tests were carried out under a wide range of temperatures and strain rates with true strain up to 2 and 0.7, respectively. The processing maps were generated on the basis of compression and torsion test data and using the principles of dynamic materials modeling (DMM). The shapes of the strain-stress curves in alpha-beta region and processing maps obtained on the two different tests have been compared with a view to evaluate the effect of the microstructure evolution on the flow softening behavior of Ti-6Al-4V alloy with a lamellar colony microstructure.

  • PDF

Ti-Al-Fe계 합금의 고온산화거동에 미치는 Fe의 영향 (Effect of Fe on the High Temperature Oxidation of Ti-Al-Fe Alloys)

  • 윤장원;현용택;김정한;염종택;윤석영
    • 한국재료학회지
    • /
    • 제21권7호
    • /
    • pp.357-363
    • /
    • 2011
  • In this paper, high temperature oxidation behavior of newly developed alloys, Ti-6Al-4Fe and Ti-6Al-1Fe, is examined. To understand the effect of Fe on the air oxidation behavior of the Ti-Al-Fe alloy system, thermal oxidation tests are carried out at $700^{\circ}C$ and $800^{\circ}C$ for 96 hours. Ti-6Al-4V alloy is also prepared and tested under the same conditions for comparison with the developed alloys. The oxidation resistance of the Ti-Al-Fe alloy system is superior to that of Ti-6Al-4V alloy. Ti-6Al-4V shows the worst oxidation resistance for all test conditions. This is not a result of the addition of Fe, but rather it is due to the elimination of V, which has deleterious effects on high temperature oxidation. The oxidation of the Ti-Al-Fe alloy system follows the parabolic rate law. At $700^{\circ}C$, Fe addition does not have a noticeable influence on the amount of weight gain of all specimens. However, at $800^{\circ}C$, Ti-6Al-4Fe alloy shows remarkable degradation compared to Ti-6Al-1Fe and Ti-6Al. It is discovered that the formation of $Al_2O_3$, a diffusion resistance layer, is remarkably hindered by a relative decrease of the ${\alpha}$ volume fraction. This is because Fe addition increases the volume fraction of ${\beta}$ phase within the Ti-6Al-xFe alloy system. Activities of Al, Ti, and Fe with respect to the formation of oxide layers are calculated and analyzed to explore the oxidation mechanism.

백서 태자 두개관세포에서 Ti-8Ta-3Nb 합금의 생체적합성 (Biocompatibility of Ti-8Ta-3Nb alloy with fetal rat calvarial cells)

  • 조인구;최득철;김영준;이경구;이도재
    • Journal of Periodontal and Implant Science
    • /
    • 제36권4호
    • /
    • pp.849-861
    • /
    • 2006
  • 타이타늄은 기계적 특성이 우수하고 생체적합성이 뛰어나 의료용 장비의 주 재료로 사용되고 있으며 타이타늄 보다 기계적 특성이 더 우수한 타이타늄 합금들(주로 Ti-6Al-4V와 Ti-6Al-7Nb 합금)도 개발되어 치과와 의료용 임플란트로 사용되고 있다. 그러나 타이타늄 합금 성분들 중 알루미늄 (aluminum)과 바나디움(vanadium)은 인체에 노출되면 세포손상과 신경계에 문제를 일으킬 수 있다. 따라서 인체에 독성이 없으면서 기계적 성질과 생체적합성이 우수한 타이타늄 합금의 개발이 필요하다. 최근 인체에 독성이 없는 성분들이 함유된 새로운 ${\beta}$ - 형태의 타이타늄 합금들이 개발되고 있는데, ${\beta}$ - 타이타늄 합금은 그 기계적 성질이 기존의 ${\alpha}+{\beta}$ 타이타늄 합금에 비해 우수하다고 알려져 있다. 최근 새로운 ${\beta}$ - 타이타늄 합금이 전남대학교 부설 타이타늄 연구소에서 개발되었다. 이 연구는 새로 개발된 ${\beta}$ - 타이타늄 합금의 생채 적합성을 세포 증식도, 알카리 인산 분해 효소 활성과 유전자 증폭을 통해 알아보고자 하였다. 그 결과는 다음과 같다; 1. Titanium-6aluminum-4vanadium (Ti-6Al-4V) 합금 표면애서의 세포 증식율은 Titanium-Titanium8Tantalum-3Niobium (Ti-8Ta-3Nb) 합금과 순수 타이타늄 표면에 비해 유의하게 낮았다(p<0.00l). Ti-8Ta-3Nb 합금 표면에서의 증식도는 순수 타이타늄 표면과 유사하였다. 2. Ti-8Ta-3Nb 합금과 순수 타이타늄에서 배양된 세포이 알카리 인산 분해 효소의 활성도는 Ti-6Al-4V 합금에서의 것보다 유의하게 높았다 (p<0.001). 3. 유전자 증폭 분석 결과, Ti-8Ta-3Nb 합금과 순수 타이타늄에서 collagen type I과 bone sialoprotein mRNA 가 유사한 수준으로 발현되었다. 이상의 결과는 생체 적합성 측면에서 Ti-8Ta-3Nb 합금과 순수 타이타늄의 차이가 없음을 보여주며 따라서 Ti-8Ta-3Nb 합금이 의학 및 치의학 영역에서 새로운 임프란트 재료로 사용될 수 있음을 의미한다.

Ti-2Al-9.2Mo-2Fe 합금의 후공정 특성에 미치는 보론의 영향 (Effect of Boron on the Manufacturing Properties of Ti-2Al-9.2Mo-2Fe Alloy)

  • 김태용;임가람;이용태;조경목;이동근
    • 한국재료학회지
    • /
    • 제25권11호
    • /
    • pp.636-641
    • /
    • 2015
  • Titanium has many special characteristics such as specific high strength, low elastic modulus, excellent corrosion and oxidation resistance, etc. Beta titanium alloys, because of their good formability and strength, are used for jet engines, and as turbine blades in the automobile and aerospace industries. Low cost beta titanium alloys were developed to take economic advantage of the use of low-cost beta stabilizers such as Mo, Fe, and Cr. Generally, adding a trace of boron leads to grain refinement in casted titanium alloys due to the pinning effect of the TiB phases. This study analyzed and evaluated the microstructural and mechanical properties after plastic deformation and heat treatment in boron-modified Ti-2Al-9.2Mo-2Fe alloy. The results indicate that a trace of boron addition made grains finer; this refinement effect was found to be maintained after subsequent processes such as hot forging and solution treatment. This can effectively reduce the number of required manufacturing process steps and lead to savings in the overall cost as well as low-cost beta elements.