Evolution of surface morphology of ${\alpha}-Al_2O_3$ substrate was investigated as a function of annealing temperature and time. Commercial (0001) ${\alpha}-Al_2O_3$ single crystal substrates were annealed in the range of $600-1000^{\circ}C$ in air. At $600^{\circ}C$, step-terrace structure started to be formed on the substrate. However, the surface roughness on the terrace was still considerable and a number of islands were observed on the step edges as well as the terraces. As the annealing temperature increased, the islands were absorbed into the step edges. Thus the terraces were smoother and the step edges were more straightened. Well-defined surface with a step height of 0.2 nm was formed above $900^{\circ}C$. On the other hand, when the substrate was annealed at a fixed temperature of $1000^{\circ}C$, the change of surface morphology was observed for the substrate annealed for 10 min. After the annealing for 30 min, the surface on which any islands could not survive was observed.
In this study, the Al-rich AlTiSiN thin films that consisted of TiN/AlSiN nano-multilayers were deposited on the steel substrate by magnetron sputtering, and their high-temperature oxidation behavior was investigated, which has not yet been adequately studied to date. Since the oxidation behavior of the films depends sensitively on the deposition method and deposition parameters which affect their crystallinity, composition, stoichiometry, thickness, surface roughness, grain size and orientation, the oxidation studies under various conditions are imperative. AlTiSiN nano-multilayer thin films were deposited on a tool steel substrate, and their oxidation behavior of was investigated between 600 and $1000^{\circ}C$ in air. Since the amount of Al which had a high affinity for oxygen was the largest in the film, an ${\alpha}-Al_2O_3-rich$ scale formed, which provided good oxidation resistance. The outer surface scale consisted of ${\alpha}-Al_2O_3$ incoporated with a small amount of Ti, Si, and Fe. Below this outer surface scale, a thin ($Al_2O_3$, $TiO_2$, $SiO_2$)-intermixed scale formed by the inwardly diffusing oxygen. The film oxidized slower than the $TiO_2-forming$ kinetics and TiN films, but faster than ${\alpha}-Al_2O_3-forming$ kinetics. During oxidation, oxygen from the atmosphere diffused inwardly toward the reaction front, whereas nitrogen and the substrate element of iron diffused outwardly to a certain extent.
Continuous and dense ZIF-7 membranes were successfully synthesized on ${\alpha}-Al_2O_3$ porous substrate via two-step crystallization technique. ZIF-7 seeding layer was first deposited on porous ${\alpha}-Al_2O_3$ substrate by in-situ low temperature crystallization, and then ZIF-7 membrane layer can be grown through the secondary high-temperature crystallization. Two synthesis solutions with different concentration were used to prepare ZIF-7 seeding layer and membrane layer on porous ${\alpha}-Al_2O_3$ substrate, respectively. As a result, a continuous and defect-free ZIF-7 membrane layer can be prepared on porous ${\alpha}-Al_2O_3$ substrate, as confirmed by scanning electron microscope. XRD characterization shows that the resulting membrane layer is composed of pure ZIF-7 phase without any impurity. A single gas permeation test of $H_2$, $O_2$, $CH_4$ or $CO_2$ was conducted based on our prepared ZIF-7 membrane. The ZIF-7 membrane exhibited excellent H2 molecular sieving properties due to its suitable pore aperture and defect-free membrane layer.
[ ${\alpha}-Al_2O_3$ ] precursor was synthesised by sol-gel method using aluminum sulfate, sodium sulfate and sodium carbonate as law materials. The flaky ${\alpha}-Al_2O_3$ crystals were prepared by heating using precursor about $1,050^{\circ}C$. In this study, the effect of some transition-metal sulfate ($FeSO_4,\;SnSO_4,\;ZnSO_4$) addition have been investigated. When iron sulfate was added, it could see that act on impurities in crystal growth process. In case of tin sulfate, distribution of Platelets was very broad. When flaky ${\alpha}-Al_2O_3$ crystals were prepared zinc sulfate addition, thickness, size, and distribution of platelets was suited to industrial application. The average diameter of flaky ${\alpha}-Al_2O_3$ crystals was about 20 $\mu$m, and its thickness was about 0.3 $\mu$m. Increasing addition of zinc sulfate, thickness of ${\alpha}-Al_2O_3$ platelet was decreased.
Lee, Dong Bok;Xiao, Xiao;Hahn, Junhee;Son, Sewon;Yuke, Shi
한국표면공학회지
/
제52권5호
/
pp.246-250
/
2019
Nano-multilayered $Cr_{25.2}Al_{19.5}Si_{4.7}N_{50.5}$ films were deposited on the steel substrate by cathodic arc plasma deposition. They were corroded at $900^{\circ}C$ in $Ar/1%SO_2$ gas in order to study their corrosion behavior in sulfidizing/oxidizing environments. Despite the presence of sulfur in the gaseous environment, the corrosion was governed by oxidation, leading to formation of protective oxides such as $Cr_2O_3$ and ${\alpha}-Al_2O_3$, where Si was dissolved. Iron diffused outward from the substrate to the film surface, and oxidized to $Fe_2O_3$ and $Fe_3O_4$. The films were corrosion-resistant up to 150 h owing to the formation of thin ($Cr_2O_3$ and/or ${\alpha}-Al_2O_3$)-rich oxide layers. However, they failed when corroded at $900^{\circ}C$ for 300 h, resulting in the formation of layered oxide scales due to not only outward diffusion of Cr, Al, Si, Fe and N, but also inward movement of sulfur and oxygen.
To precipitate the complex gel of flux and aluminum hydroxides gel, aqueous solution of the mixture of $Na_2CO_3\;and\;Na_2PO_4{\cdot}12H_2O$ was added with stirring in aqueous solution of the mixture of $Al_2(SO_4)_3{\cdot}14{\sim}18H_2O,\;Na_2SO_4$, and then the complex gel was aged in $0{\sim}30h\;at\;90^{\circ}C$. As aging time passed, the aluminum hydroxides was grown into the acicular AlO(OH) gel. Also, aging time had an effect on physical properties of the AlO(OH) gel and on crystal growth of the flaky ${\alpha}-Al_2O_3$ prepared by molten-salt precipitation. In this study, the complex gel was crystallized in temperature range of $400{\sim}1,200^{\circ}C$ after drying at $110^{\circ}C$, and then it was investigated to effect of aging time on precipitation temperature, size, thickness, morphology and particle size distribution of the flaky ${\alpha}-Al_2O_3$ crystal. As aging time passed, the flaky a${\alpha}-Al_2O_3$ crystal showed a tendency toward an increase in size and thickness as result from an increase in BET surface area and pore volume of the acicular AlO(OH) gel.
Dense glass-ceramics for low firing temperature substrate were prepared by addition of CeO2 flux to the glass of MgO-Al2O3-SiO2 system. Glass powders were fabricated by melting at 150$0^{\circ}C$ and ball milling. Glass powder compacts were sintered at 800~100$0^{\circ}C$ for 3h. The crystallization and the shrinkage behaviors of glass powder compacts were analyzed by XRD, DTA and TMA. The shrinkage of glass powder compact increased with increasing the amount of CeO2. Because the softening temperature decreased and the crystallization temperature increased with increasing the amount of CeO2. Apparently, addition of CeO2 prevented formation of $\mu$-cordierite phase from the glass-ceramics and improved formation of $\alpha$-cordierite phase. Therefore crystallization properties were enhanced.
Al$_2$O$_3$-TiO$_2$powders of six different compositions were plasma-sprayed on Ti substrate. The spray powders and the spray coated layers were analysed and compared using SEM and X-RD. The elastic properties (specific elastic constant and damping coefficient) of the coated specimens were measured in order to select the optimum composition range of ceramics for use in a speaker diaphragm. A correlation between the microstructure and elastic properties was also investigated. When $Al_2$O$_3$powders with 0- 13% TiO$_2$were plasma sprayed, the coated layers were composed of metastable y-Al$_2$O$_3$with small amount of $\alpha$-Al$_2$O$_3$and the content of $\alpha$-Al$_2$O$_3$was increased with TiO$_2$content. Specific elastic constant was rapidly increased with 2 and 13% TiO$_2$addition to $Al_2$O$_3$. The internal damping was nearly unchanged with TiO$_2$content The specific elastic constant seemed to be dependent on the content of $\alpha$-Al$_2$O$_3$in the coated layer.
Fe-28%Al($Fe_3Al$)과 Fe-28%Al-4%Cr($Fe_3Al-4Cr$) 금속간화합물을 대기중 1073, 1273, 1473k의 온도에서 최고 17일까지 장시간 산화시켰다. $Fe_3Al-4Cr$의 산화저항은 근본적으로 $Fe_3Al$과 거의 비슷하거나, 약간 우수하였다. $Fe_3Al$ 위에 형성된 산화물은 거의 순수한 ${\alpha}-AL_2O_3$로만 구성되어 있었으며, $Fe_3Al-4Cr$ 위에 형성된 산화물은 약간의 Fe와 Cr 이온이 고용된 ${\alpha}-AL_2O_3$로 구성되어 있었다. 외부산화막을 형성하기 위해 모재원소의 외부확산에 의해 산화물-모재 계면에는 Kirkendall 기공이 존재하였다. $Fe_3Al(-4Cr)$ 표면에 형성된 산화막은 1273k가지는 비교적 얇고 치밀하였으나, 1473k에서 산화막의 박리와 함께 상대적으로 큰 무게증가가 발생하였다.
Kim, Bum-Jin;Lee, Eun-Tae;Jang, Gun-Eik;Chung, Yong-Sun
한국결정성장학회:학술대회논문집
/
한국결정성장학회 1997년도 Proceedings of the 12th KACG Technical Meeting and the 4th Korea-Japan EMGS (Electronic Materials Growth Symposium)
/
pp.79-85
/
1997
Fe$_2$O$_3$ thin films were prepared on $Al_2$O$_3$ substrate by PECVD(Plasma-Enhanced Chemical Vapor Deposition) process. The phase transformation of iron oxide film was determined as the substrate temperature and reduction-oxidation process. $\alpha$-Fe$_2$O$_3$ was stable in deposition temperature ranges of 80~15$0^{\circ}C$. Fe$_3$O$_4$ phase was obtained by the reduction process of $\alpha$-Fe$_2$O$_3$ phase in H$_2$ ambient. Fe$_3$O$_4$ phase was transformed into a ${\gamma}$-Fe$_2$O$_3$ thin film under controlled oxidation conditions at 280~30$0^{\circ}C$.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.