Initial Growth Mode and Epitaxial Growth of AIN Thin Films on $Al_2O_3(0001)$ Substrate by DC Faced Target Sputtering

  • Kim, Jin-Woo;Kang, Kwang-Yong;Lee, Su-Jae
    • The Korean Journal of Ceramics
    • /
    • v.5 no.4
    • /
    • pp.368-370
    • /
    • 1999
  • Using DC faced target sputtering method we grow AIN the films on the $Al_2O_3$(0001) substrate with varying thickness(17$\AA$-1000$\AA$). We measured x-ray diffraction(XRD) profiles by synchrotron radiation($\lambda$=1.12839 $\AA$) with four circle diffractometer. The full width half maximum(FWHM) of rocking curve for the AIN (0002) diffraction of the film grown at $500^{\circ}C$ was $0.029^{\circ}$. Also, we confirmed that the stress between AIN thin film and $Al_2O_3$(0001) substrate was reduced as increasing AIN film thickness, and the critical thickness of 400~500 $\AA$, defined as a lattice constant in the film agrees with that in a bulk without stress, was obtained.

  • PDF

A Study on Rolling Contact Behaviors of a Flat Rough Surface with a Smooth Ball (구와 평면간의 구름접촉거동에 관한 연구)

  • 김경모;정인성
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.14 no.3
    • /
    • pp.554-570
    • /
    • 1990
  • he rolling contact behaviors between a smooth ball and a flat rough surface under dynamic load are intricately affected by many factors, such as the diameter of a ball, normal load and the roughness of a flat surface etc. Accordingly, the experimental study is done to find them on the base of elastic hysteresis loss as theoretical approach is very difficult. The experimental apparatus composed of damped-free vibration system is used. This paper investigates the damping characteristics on the rolling contact area through rolling friction force and logarithmic decrement versus displacement obtained in accordance with the variations of those factors, and presents a new experimental method to find out contact width using the relations of logarithmic decrement and rolling friction force with displacement.

Fabrication and Device Characteristics of Infrared Photodetector Based on InAs/GaSb Strained-Layer Superlattice (InAs/GaSb 응력초격자를 이용한 적외선검출소자의 제작 및 특성 연구)

  • Kim, J.O.;Shin, H.W.;Choe, J.W.;Lee, S.J.;Kim, C.S.;Noh, S.K.
    • Journal of the Korean Vacuum Society
    • /
    • v.18 no.2
    • /
    • pp.108-115
    • /
    • 2009
  • The superlattice infrared photodetector (SLIP) with an active layer of 8/8-ML InAs/GaSb type-II strained-layer superlattice (SLS) of 150 periods was grown by MBE technique, and the proto-type discrete device was defined with an aperture of $200-{\mu}m$ diameter. The contrast profile of the transmission electron microscope (TEM) image and the satellite peak in the x-ray diffraction (XRD) rocking curve show that the SLS active layer keeps abrupt interfaces with a uniform thickness and a periodic strain. The wavelength and the bias-voltage dependences of responsivity (R) and detectivity ($D^*$) measured by a blackbody radiation source give that the cutoff wavelength is ${\sim}5{\mu}m$, and the maximum Rand $D^*$ ($\lambda=3.25{\mu}m$) are ${\sim}10^3mA/W$ (-0.6 V/13 K) and ${\sim}10^9cm.Hz^{1/2}/W$ (0 V/13 K), respectively. The activation energy of 275 meV analyzed from the temperature dependent responsivity is in good agreement with the energy difference between two SLS subblevels of conduction and valence bands (HH1-C) involving in the photoresponse process.