Composites of SiC-Si3N4 consisted of uniformly distributed elongated $\beta$-Si3N4 grains and equiaxed $\beta$-SiC grains were fabricated with $\beta$-SiC,. $\alpha$-Si3N4 Al2O3 and Y2O3 powders. By hot-pressing and subsequent annelaing elongated $\beta$-Si3N4 grains were grown via$\alpha$longrightarrow$\beta$ phase transformation and equiaxed $\beta$-Si3N4 composites increased with increasing the Si3N4 content owing to the reduced defect size and enhanced crack deflection by elongated $\beta$-Si3N4 grains and the grain boundary strengthening by nitrogen incorporation. Typical flexural strength and fracture toughness of SiC-40 wt% Si3N4 composites were 783 MPa and 4.2 MPa.m1/2 respectively.
$\beta$-Si$_3$N$_4$종자입자 첨가가 소결조제로 Y-Mg-Si-Al-O-N계 oxynitride glass를 사용하여 일축가압 소결을 행한 SiC-Si$_3$N$_4$복합재료의 미세구조와 기계적 특성에 미치는 영향을 고찰하였다. 길게 자란 $\beta$-Si$_3$N$_4$입자들과 등방성의 $\beta$-SiC 입자들이 균일하게 분포된 미세구조를 얻었다. $\beta$-Si$_3$N$_4$종자입자 함량이 증가함에 따라 SiC-Si$_3$N$_4$복합재료의 강도와 파괴인성이 증가하였고, 이는 복합화에 기인하는 결함크기의 감소와 길게 자란 $\beta$-Si$_3$N$_4$입자에 의한 균열가교 및 균열회절 등에 기인하였다. SiC-70 wt% Si$_3$N$_4$복합재료의 대표적인 강도와 파괴인성은 각각 770 MPa과 6.2 MPa.m$^{1}$2/ 이었다.
SiC and $SiC-Si_3N_4$ powder were synthesized via the carbiding and carbiding-nitriding reaction of Jecheon quartz respectively using graphite as a reducing agent. $\beta$-SiC+($\alpha$+$\beta$)-$Si_3N_4$ composite was obtained by the carbiding-nitriding reaction of Jecheon quartz-graphite mixture at 1, 35$0^{\circ}C$ in $H_2$ atmosphere. $\beta$-SiC+($\alpha$+$\beta$)-$Si_3N_4$ composite was obtained by the carbidint-nitriding reaction of Jecheon quartz-graphite mixture at 1, 35$0^{\circ}C$ in $N_2-H_2$ atmosphere. The ratio of $\beta$-SiC+($\alpha$+$\beta$)-$Si_3N_4$ content in a produced composite could be controlled by adjusting the reaction time and gaseous mixture.
The preparation of $\beta$-SiAlON powder by SHS in the system of $Si-Al-SiO_2-NH_4F(\beta-Si_3N_4)$ was investigated in this study. In the preparation of SiAlON powder, the effect of gas pressure, compositions such as Si, $NH_4F$, \beta-Si_3N_4$ and additive in mixture on the reactivity were investigated. At 50 atm of the initial inert gas pressure in reactor, the optimum composition for the preparation of pure $\beta$-SiAlON was $3Si+Al+2SiO_2+NH_4F$. The $\beta$-SiAlON powder synthesized in this condition was a single phase $\beta$-SiAlON with a rod like morphology.
The $\alpha$ to $\beta$ phase transformation of $\alpha$-Si3N4 whisker and related microstructural changes have been investigated. When only $\alpha$-Si3N4 whisker was heat treated in the range 1650~175$0^{\circ}C$, the $\alpha$ to $\beta$ phase transformation occured. In this case, it eas suggested that the oxygen content in $\alpha$-Si3N4 whisker affected the transformation behavior. Although $\alpha$-Si3N4 whisker with Si was heat treated under the same condition, however, the variation of $\beta$- fraction had a similar tendency with heat treating time. Therfore, it was considered that the oxygen content in $\alpha$-Si3N4 whisker affected the transformation behavior dominently rather than the content of added Si. The added $\beta$ phase did not affect the transformation behaviro of $\alpha$-Si3N4 whisker.
초미립 SiC분말과 SiC platelet을 2차성으로 Si3N4에 첨가하여 SiC/Si3N4 하이브리드 복합체를 가압소결로 제조한 후 2차상의 영향을 조사한 결과핫프레스법을 이용한 경우 SiC platelet은 Si3N4 기지 복합채의 치밀화를 저해하지 않고 초미립의 SiC 첨가는 Si3N4의 입성장을 효과적으로 억제하여 미세한 $\beta$-Si3N4의 grain을 형성함을 관찰하였다. 초미립 SiC첨가를 통한 복합체의 강도 증진은 상대적으로 $\beta$-Si3N4입자의 미세화에 의한 인성의 저하를 유도하나 SiC platelet을 첨가하여 급격한 강도 저하 없이 높은 인성을 갖는 하이브리드 복합체를 제조할 수 있었으며 SiC/Si3N4 하이브리드 복합체의 인성증진은 elongated $\beta$-Si3N4와 platelet SiC의 debonding에 의한 grain pull-out 영향임을 알 수 있었다.
The self-reinforced Si3N4 ceramics were prepared by pressureless-sintering using ${\beta}$-Si3N4 whiskers as a seed. Effects of ${\beta}$-Si3N4 whiskers on microstructure and mechanical properties and the ${\alpha}$ to ${\beta}$ phase transition of Si3N4 were investigated. The self-reinforced Si3N4 ceramics were densified(relative density$\geq$98%) by pressureless-sintering (1800$^{\circ}C$ 2h) using 8mol% Y2O3 and 6mol% Al2O3 as sintering aids and 5 vol% ${\beta}$-Si3N4 whiskers within self-reinforced Si3N4 ceramic seemed to hinder the densification owing to their acicular shapes but accelerated the ${\alpha}$ to ${\beta}$ phase transition because they acted as pre-existing nuclei. It was found that the more ${\beta}$-Si3N4 nucei the faster ${\alpha}$ to ${\beta}$ phase transition.
The self-toughened Si3N4 ceramics where needle-like coarse ${\beta}$-Si3N4 grains were dispersed within fine-grain-ed matrix were prepared via hot-prssing at 1730$^{\circ}C$ for 2 h using 5 vol% ${\beta}$-Si3N4 whiskers as a seed. In this study the microstructures and mechanical properties of self-toughened Si3N4 ceramics were investigated. The flexural strength of self-toughened Si3N4 ceramics was increased from 600-800 MPa of the Si3N4 monolith to 830-1025 MPa. The KIC was also increased from 4.0-5.0MPa$.$m1/2 of the Si3N4 monolith to 5.8-6.5MPa$.$m1/2$.$The needle-like coarse Si3N4 grains in self-toughened ceramics were considered to induce various toughening mechanisms including the crack deflection pull-out and bridging and to contribute to KIC improvement. In ad-dition to toughening mechanisms the KIC improvement was considered to be partially indebted also to the orien-tation of large ${\beta}$-Si3N4 grains and to the promoting effect of ${\beta}$-Si3N4 whiskers on the ${\alpha}$ to ${\beta}$ transtion.
Synthesis of high purity ultrafine Si3N4 and ${\beta}$-Sialon powders was investigated via the simultaneous reduction and nitriding of amorphous SiO2, SiO2-Al2O3 system prepaerd by hydrolysis of alkoxides, using carbonablack as a reducing agent. In Si(OC2H5)4-C2H5 OH-H2 O-NH4OH system, hydrolysis rate increased with increasing reaction temperature and pH. Pure ${\alpha}$-Si3N4 was formed at 1350$^{\circ}C$ for 5 hrs in N2 atmosphere. In Si(OC2H5)4-Al(OC3H7)3-C6H6-H2 O-NH4OH system, weight loss increased as Si/Al ratio decreased. Single phase ${\beta}$-Sialon consisted of Si/Al=2 was formed at 1350$^{\circ}C$ in N2 and minor phases of ${\alpha}$-Si3N4, AIN, and X-phase were existed besides theSialon phase at other Si/Al ratios. The Si3N4 and Sialon powders synthesized from alkoxides consisted of uniform find particles of 0.05-0.2$\mu\textrm{m}$ in diameter, respectively.
Journal of the Korean Crystal Growth and Crystal Technology
/
v.6
no.3
/
pp.386-391
/
1996
SiC particles (average size is 270 nm) of 0, 10, 20, 30, 40 vol% were dispersed in $Si_{3}N_{4}$, and $Si_{3}N_{4}/SiC$ nanocomposites were fabricated by hot press. After sintering, matrix phase, ${\alpha}-Si_{3}N_{4}$ was transformed to ${\beta}-Si_{3}N_{4}$, and second phase, ${\beta}-SiC$ was not changed. No grain boundary crystalline phase by adding of sintering additives was detected. Grain growth of $Si_{3}N_{4}$ was supressed with increasing of SiC contents, and then fine grain was occurred. The highest fracture strength was obtained at 10 vol% SiC, and fracture toughness was decreased, but hardness was linearly increased with SiC content.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.