• Title/Summary/Keyword: $\beta$-$Si_3$$N_4$

Search Result 142, Processing Time 0.021 seconds

Mechanical Properties of Silicon Carbide-Silicon Nitride Composites Sintered with Yttrium Aluminum Garnet (YAG상 첨가 탄화규소-질화규소 복합재료의 기계적 특성)

  • 이영일;김영욱;최헌진;이준근
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.8
    • /
    • pp.799-804
    • /
    • 1999
  • Composites of SiC-Si3N4 consisted of uniformly distributed elongated $\beta$-Si3N4 grains and equiaxed $\beta$-SiC grains were fabricated with $\beta$-SiC,. $\alpha$-Si3N4 Al2O3 and Y2O3 powders. By hot-pressing and subsequent annelaing elongated $\beta$-Si3N4 grains were grown via$\alpha$longrightarrow$\beta$ phase transformation and equiaxed $\beta$-Si3N4 composites increased with increasing the Si3N4 content owing to the reduced defect size and enhanced crack deflection by elongated $\beta$-Si3N4 grains and the grain boundary strengthening by nitrogen incorporation. Typical flexural strength and fracture toughness of SiC-40 wt% Si3N4 composites were 783 MPa and 4.2 MPa.m1/2 respectively.

  • PDF

Mechanical Properties of SiC-$Si_3$$N_4$Composites Containing $\beta$-$Si_3$$N_4$Seeds ($\beta$-$Si_3$$N_4$종자입자 첨가 SiC-$Si_3$$N_4$복합재료의 기계적 특성)

  • 이영일;김영욱;최헌진;이준근
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.1
    • /
    • pp.22-27
    • /
    • 2001
  • $\beta$-Si$_3$N$_4$종자입자 첨가가 소결조제로 Y-Mg-Si-Al-O-N계 oxynitride glass를 사용하여 일축가압 소결을 행한 SiC-Si$_3$N$_4$복합재료의 미세구조와 기계적 특성에 미치는 영향을 고찰하였다. 길게 자란 $\beta$-Si$_3$N$_4$입자들과 등방성의 $\beta$-SiC 입자들이 균일하게 분포된 미세구조를 얻었다. $\beta$-Si$_3$N$_4$종자입자 함량이 증가함에 따라 SiC-Si$_3$N$_4$복합재료의 강도와 파괴인성이 증가하였고, 이는 복합화에 기인하는 결함크기의 감소와 길게 자란 $\beta$-Si$_3$N$_4$입자에 의한 균열가교 및 균열회절 등에 기인하였다. SiC-70 wt% Si$_3$N$_4$복합재료의 대표적인 강도와 파괴인성은 각각 770 MPa과 6.2 MPa.m$^{1}$2/ 이었다.

  • PDF

Syntheses of SiC and $SiC-Si_3N_4$ Powder from Jecheon Quartz (제천규석으로부터 SiC 및 $SiC-Si_3N_4$계 분말 합성)

  • 이홍림;배철훈;문준화
    • Journal of the Korean Ceramic Society
    • /
    • v.23 no.1
    • /
    • pp.67-73
    • /
    • 1986
  • SiC and $SiC-Si_3N_4$ powder were synthesized via the carbiding and carbiding-nitriding reaction of Jecheon quartz respectively using graphite as a reducing agent. $\beta$-SiC+($\alpha$+$\beta$)-$Si_3N_4$ composite was obtained by the carbiding-nitriding reaction of Jecheon quartz-graphite mixture at 1, 35$0^{\circ}C$ in $H_2$ atmosphere. $\beta$-SiC+($\alpha$+$\beta$)-$Si_3N_4$ composite was obtained by the carbidint-nitriding reaction of Jecheon quartz-graphite mixture at 1, 35$0^{\circ}C$ in $N_2-H_2$ atmosphere. The ratio of $\beta$-SiC+($\alpha$+$\beta$)-$Si_3N_4$ content in a produced composite could be controlled by adjusting the reaction time and gaseous mixture.

  • PDF

Preparation of β-SiAlON Powder by Combustion Reaction in the System of Si-Al-SiO2-NH4F(β-Si3N4) (Si-Al-SiO2-NH4F(β-Si3N4)계에서 연소반응에 의한 β-SiAlON분말의 제조)

  • Min, Hyun-Hong;Shin, Chang-Yun;Won, Chang-Whan
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.10 s.293
    • /
    • pp.595-600
    • /
    • 2006
  • The preparation of $\beta$-SiAlON powder by SHS in the system of $Si-Al-SiO_2-NH_4F(\beta-Si_3N_4)$ was investigated in this study. In the preparation of SiAlON powder, the effect of gas pressure, compositions such as Si, $NH_4F$, \beta-Si_3N_4$ and additive in mixture on the reactivity were investigated. At 50 atm of the initial inert gas pressure in reactor, the optimum composition for the preparation of pure $\beta$-SiAlON was $3Si+Al+2SiO_2+NH_4F$. The $\beta$-SiAlON powder synthesized in this condition was a single phase $\beta$-SiAlON with a rod like morphology.

$\alpha$ to $\beta$ Phase Transformation of $\alpha$-Si3N4 Whisker ($\alpha$-질화규소 Whisker의 $\alpha$/$\beta$ 상변태)

  • 박지연;김종희
    • Journal of the Korean Ceramic Society
    • /
    • v.25 no.5
    • /
    • pp.502-508
    • /
    • 1988
  • The $\alpha$ to $\beta$ phase transformation of $\alpha$-Si3N4 whisker and related microstructural changes have been investigated. When only $\alpha$-Si3N4 whisker was heat treated in the range 1650~175$0^{\circ}C$, the $\alpha$ to $\beta$ phase transformation occured. In this case, it eas suggested that the oxygen content in $\alpha$-Si3N4 whisker affected the transformation behavior. Although $\alpha$-Si3N4 whisker with Si was heat treated under the same condition, however, the variation of $\beta$- fraction had a similar tendency with heat treating time. Therfore, it was considered that the oxygen content in $\alpha$-Si3N4 whisker affected the transformation behavior dominently rather than the content of added Si. The added $\beta$ phase did not affect the transformation behaviro of $\alpha$-Si3N4 whisker.

  • PDF

Fabrication and Properties of $SiC/Si_3N_4$ Hybrid Composite Materials ($SiC/Si_3N_4$ 하이브리드 복합체이 제조 및 특성)

  • Gang, Jong-Bong;Jo, Beom-Rae;Lee, Su-Yeong
    • Korean Journal of Materials Research
    • /
    • v.6 no.4
    • /
    • pp.428-435
    • /
    • 1996
  • 초미립 SiC분말과 SiC platelet을 2차성으로 Si3N4에 첨가하여 SiC/Si3N4 하이브리드 복합체를 가압소결로 제조한 후 2차상의 영향을 조사한 결과핫프레스법을 이용한 경우 SiC platelet은 Si3N4 기지 복합채의 치밀화를 저해하지 않고 초미립의 SiC 첨가는 Si3N4의 입성장을 효과적으로 억제하여 미세한 $\beta$-Si3N4의 grain을 형성함을 관찰하였다. 초미립 SiC첨가를 통한 복합체의 강도 증진은 상대적으로 $\beta$-Si3N4입자의 미세화에 의한 인성의 저하를 유도하나 SiC platelet을 첨가하여 급격한 강도 저하 없이 높은 인성을 갖는 하이브리드 복합체를 제조할 수 있었으며 SiC/Si3N4 하이브리드 복합체의 인성증진은 elongated $\beta$-Si3N4와 platelet SiC의 debonding에 의한 grain pull-out 영향임을 알 수 있었다.

  • PDF

Microstructure and Mechanical Properties of Self-Reinforced Si3N4 Ceramic Prepared by Pressureless-Sintering (상압소결에 의해 제조한 자체 강인화 질화규소 세리믹의 미세조직과 기계적 성질)

  • 김완중;이영규;조원승;최상욱
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.5
    • /
    • pp.547-554
    • /
    • 1999
  • The self-reinforced Si3N4 ceramics were prepared by pressureless-sintering using ${\beta}$-Si3N4 whiskers as a seed. Effects of ${\beta}$-Si3N4 whiskers on microstructure and mechanical properties and the ${\alpha}$ to ${\beta}$ phase transition of Si3N4 were investigated. The self-reinforced Si3N4 ceramics were densified(relative density$\geq$98%) by pressureless-sintering (1800$^{\circ}C$ 2h) using 8mol% Y2O3 and 6mol% Al2O3 as sintering aids and 5 vol% ${\beta}$-Si3N4 whiskers within self-reinforced Si3N4 ceramic seemed to hinder the densification owing to their acicular shapes but accelerated the ${\alpha}$ to ${\beta}$ phase transition because they acted as pre-existing nuclei. It was found that the more ${\beta}$-Si3N4 nucei the faster ${\alpha}$ to ${\beta}$ phase transition.

  • PDF

Mechanical Properties and Microstructures of Self-toughened Silicon Nitride Cermic Prepared by Microstructural Control (미세구조 제어에 의해 제조한 자체 강인화 질화규소 세라믹의 기계적 성질과 미세조직)

  • 김완중;이영규;조원승;최상욱
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.4
    • /
    • pp.432-443
    • /
    • 1999
  • The self-toughened Si3N4 ceramics where needle-like coarse ${\beta}$-Si3N4 grains were dispersed within fine-grain-ed matrix were prepared via hot-prssing at 1730$^{\circ}C$ for 2 h using 5 vol% ${\beta}$-Si3N4 whiskers as a seed. In this study the microstructures and mechanical properties of self-toughened Si3N4 ceramics were investigated. The flexural strength of self-toughened Si3N4 ceramics was increased from 600-800 MPa of the Si3N4 monolith to 830-1025 MPa. The KIC was also increased from 4.0-5.0MPa$.$m1/2 of the Si3N4 monolith to 5.8-6.5MPa$.$m1/2$.$The needle-like coarse Si3N4 grains in self-toughened ceramics were considered to induce various toughening mechanisms including the crack deflection pull-out and bridging and to contribute to KIC improvement. In ad-dition to toughening mechanisms the KIC improvement was considered to be partially indebted also to the orien-tation of large ${\beta}$-Si3N4 grains and to the promoting effect of ${\beta}$-Si3N4 whiskers on the ${\alpha}$ to ${\beta}$ transtion.

  • PDF

Synthesis of Powder of the System Si-Al-O-N from Alkoxides I. Synthesis of Si3N4 and $\beta$-Sialon Ultrafine Powders from Alkoxides (알콕사이드로부터 Si-Al-O-N계 분말합성 I. 알콕사이드로부터 Si3N4와 $\beta$-Sialon 초미분말 합성)

  • 이홍림;유영창
    • Journal of the Korean Ceramic Society
    • /
    • v.24 no.1
    • /
    • pp.23-32
    • /
    • 1987
  • Synthesis of high purity ultrafine Si3N4 and ${\beta}$-Sialon powders was investigated via the simultaneous reduction and nitriding of amorphous SiO2, SiO2-Al2O3 system prepaerd by hydrolysis of alkoxides, using carbonablack as a reducing agent. In Si(OC2H5)4-C2H5 OH-H2 O-NH4OH system, hydrolysis rate increased with increasing reaction temperature and pH. Pure ${\alpha}$-Si3N4 was formed at 1350$^{\circ}C$ for 5 hrs in N2 atmosphere. In Si(OC2H5)4-Al(OC3H7)3-C6H6-H2 O-NH4OH system, weight loss increased as Si/Al ratio decreased. Single phase ${\beta}$-Sialon consisted of Si/Al=2 was formed at 1350$^{\circ}C$ in N2 and minor phases of ${\alpha}$-Si3N4, AIN, and X-phase were existed besides theSialon phase at other Si/Al ratios. The Si3N4 and Sialon powders synthesized from alkoxides consisted of uniform find particles of 0.05-0.2$\mu\textrm{m}$ in diameter, respectively.

  • PDF

Effect of SiC volume fraction on mechanical properties and microstructure of $Si_{3}N_{4}/SiC$ nanocomposites (SiC 부피분율이 $Si_{3}N_{4}/SiC$ 초미립복합재료의 기계적 특성과 미세구조에 미치는 영향)

  • 황광택;김창삼;오근호
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.6 no.3
    • /
    • pp.386-391
    • /
    • 1996
  • SiC particles (average size is 270 nm) of 0, 10, 20, 30, 40 vol% were dispersed in $Si_{3}N_{4}$, and $Si_{3}N_{4}/SiC$ nanocomposites were fabricated by hot press. After sintering, matrix phase, ${\alpha}-Si_{3}N_{4}$ was transformed to ${\beta}-Si_{3}N_{4}$, and second phase, ${\beta}-SiC$ was not changed. No grain boundary crystalline phase by adding of sintering additives was detected. Grain growth of $Si_{3}N_{4}$ was supressed with increasing of SiC contents, and then fine grain was occurred. The highest fracture strength was obtained at 10 vol% SiC, and fracture toughness was decreased, but hardness was linearly increased with SiC content.