• 제목/요약/키워드: $\beta$ phase

검색결과 1,327건 처리시간 0.027초

AM50-0.3 wt%CaO 합금의 미세조직과 상·고온 기계적 특성 (Microstructure and Mechanical Properties at Room and Elevated Temperatures in AM50-0.3 wt%CaO Alloy)

  • 조은호;전중환;김영직
    • 한국재료학회지
    • /
    • 제22권10호
    • /
    • pp.499-503
    • /
    • 2012
  • The present study is intended to comparatively investigate the changes in microstructure and tensile properties at room and elevated temperatures in commercial AM50(Mg-5%Al-0.3%Mn) and 0.3 wt%CaO added ECO-AM50 alloys produced by permanent mould casting. The typical microstructure of AM50 alloy was distinctively characterized using two intermetallic compounds, ${\beta}(Mg_{17}Al_{12})$ and $Al_8Mn_5$, along with ${\alpha}$-(Mg) matrix in an as-cast state. The addition of a small amount of CaO played a role in reducing dendrite cell size and quantity of the ${\beta}$ phase in the AM50 alloy. It is interesting to note that the added CaO introduced a small amount of $Al_2Ca$ adjacent to the ${\beta}$ compounds, and that inhomogeneous enrichment of elemental Ca was observed within the ${\beta}$ phase. The ECO-AM50 alloy showed higher hardness and better YS and UTS at room temperature than did the AM50 alloy, which characteristics can be mainly ascribed to the finer-grained microstructure that originated from the CaO addition. At $175^{\circ}C$, higher levels of YS and UTS and higher elongation were obtained for the ECO-AM50 alloy, demonstrating that even 0.3 wt%CaO addition can be beneficial in promoting the heat resistance of the AM50 alloy. The combinational contributions of enhanced thermal stability of the Ca-containing ${\beta}$ phase and the introduction of a stable $Al_2Ca$ phase with high melting point are thought to be responsible for the improvement of the high temperature tensile properties in the ECO-AM50 alloy.

Intra-articular Injection of $IL-1{\beta}$ Facilitated Formalin-induced Temporomandibular Joint Pain in Freely Moving Rats

  • Choi, Hyo-Soon;Jung, Sung-Chul;Choi, Byung-Ju;Ahn, Dong-Kuk
    • The Korean Journal of Physiology and Pharmacology
    • /
    • 제9권1호
    • /
    • pp.23-27
    • /
    • 2005
  • The present study was performed to investigate the effects of intra-articular injection of interleukin-1${\beta}$ (IL-1${\beta}$) on the formalin-induced temporomandibular joint (TMJ) pain. Under anesthesia, a 30-gauge needle was introduced into the right TMJ region for injection of formalin. Microinjection of 50 ${\mu}l$ of 5% formalin significantly produced noxious scratching behavioral response, and the scratching behavior lasted for 40 min. Although the responses produced by formalin injection were divided into two phases, the response of 1st phase did not significantly differ from the scratching behavior response in the saline-treated group. We examined the effects of intra-articular injection of IL-1${\beta}$ on the number of noxious behavioral responses produced by 50${\mu}l$ of 5% formalin injection. Intra-articular injection of 100 pg and 1 ng of IL-1${\beta}$ significantly increased the number of behavioral responses of the 2nd phase, while 10 pg of IL-1${\beta}$ did not change the formalin-induced behavioral responses. To investigate whether IL-1 receptor was involved in the intra-articular administration of IL-1${\beta}$-induced hyperalgesic response, IL-1 receptor antagonist (IL- ra, 50 ng) was administrated together with IL-1${\beta}$ injection. IL-1${\beta}$ receptor antagonist blocked IL-1${\beta}$- induced hyperalgesic response in the TMJ formalin test. These results suggest that intra-articular injection of IL-1${\beta}$ facilitated the transmission of nociceptive information in the TMJ area.

Sasa borealis의 Diastereomeric 성분들의 역상 고속액체크로마토그래프 분석방법 (Reverse-Phase HPLC Method for Identification of Diastereomeric Constituents from Sasa borealis)

  • 정연희;이준;권영주;서은경
    • 약학회지
    • /
    • 제50권1호
    • /
    • pp.21-25
    • /
    • 2006
  • Reiterated normal-phase column chromatography lead to the isolation and purification of six known compounds but for the first time from the whole plant of Sasa borealis (Hack.) Makino (Gramineae): tricin 4'-O-(erythro-${\beta}$-guaia-cylglyceryl) ether (1), tricin 4'-O-(threo-${\beta}$-guaiacylglyceryl) ether (2), tricin 4'-O-[erythro-${\beta}$-guaiacyl-(9'-O-acetyl)-glyceryl] ether (3), tricin 4'-O-[threo-${\beta}$-guaiacyl-(9'-O-acetyl)-glyceryl] ether (4), (-)-pinoresinol (5), and vanillin (6). The structures of the compounds (1-6) were established based on interpretation of high resolution NMR (COSY, HSQC, HMBC, and NOESY) spectral data. In particular, compounds 1 and 3 were diastereomers of compounds 2 and 4, respectively. These two sets of diastereomers were able to be simultaneously identified and quantified by a gradient reversed-phase HPLC method with UV photodiode array, This sensitive HPLC method is noteworthy as a simultaneous separation and identification method to test the extract of the family Gramineae which contains these compounds.

경피제제로서 수종의 플루비프로펜 Vehicle과 O/W 마이크로에멀젼의 평가 (Evaluation or various vehicles and O/W Microemulsions of Flurbiprofen as Transdermal Delivery System)

  • 이계원;지웅길
    • Journal of Pharmaceutical Investigation
    • /
    • 제28권3호
    • /
    • pp.141-149
    • /
    • 1998
  • In order to reduce systemic side effects following administration, flurbiprofen was formulated as O/W microemulsion consisting of the surfactant, oil phase and aqueous phase. Particle size distribution, apparent viscosity, solubility and skin permeation of flurbiprofen in various vehicles and microemulsion were evaluated. The domain of O/W microemulsion s phase diagram had difference between oil types and the area of O/W microemulsion was wide distributed by adding to PG and cosurfactant than that of water alone. As increasing 10, 15 and 20% of Brij 97 content and 1, 2.5, 5% of oil content, the solubility of flurbiprofen in O/W microemulsions and various vehicles was $400{\sim}1,000$ and $10{\sim}500$ times higher than that of control. Also, apparent viscosity of soybean oil microemulsions was higher than that of IPM microemulsions and that of vehicle were increased as increasing vehicle content. Since skin permeation of flurbiprofen decreased as increasing viscosity, in each vehicle, it was not affected 2% ${\beta}-CD$ and decreased as increasing PG content and to 2, 5 and 10% of $HP-{\beta}-CD$. In O/W microemulsion, 5% soybean oil. 20% Brij 97 and 75% water(A-1) with high viscosity showed low skin penetration.

  • PDF

SiO2 첨가량에 따른 Hydroxyapatite β-TCP 복합체의 기계적 특성 (Mechanical Properties of Hydroxyapatite β-TCP Composite with Changing SiO2 Contents)

  • 류수착;민상호;박영민
    • 한국재료학회지
    • /
    • 제17권9호
    • /
    • pp.480-483
    • /
    • 2007
  • Hydroxyapatites were prepared by the different $SiO_2$ addition at $1450^{\circ}C$ for 2h. With the increase of $SiO_2$ addition, microstructure, bulk density, porosity, mechanical strength of $hydroxyapatite/{\beta}-TCP$ composite were investigated. When the sintered HAp contained 1 wt% $SiO_2$, the each properties of the HAp were increased. But the excess addition of $SiO_2$ content above 1wt% the each property were decreased. This results were due to the ${\beta}-TCP$ phase. The ${\beta}-TCP$ phase appeared at 3 wt% $SiO_2$ addition and the ${\beta}-TCP$ phase was enhanced by the $SiO_2$ increasing.

알콕사이드로부터 Si-Al-O-N계 분말합성 I. 알콕사이드로부터 Si3N4와 $\beta$-Sialon 초미분말 합성 (Synthesis of Powder of the System Si-Al-O-N from Alkoxides I. Synthesis of Si3N4 and $\beta$-Sialon Ultrafine Powders from Alkoxides)

  • 이홍림;유영창
    • 한국세라믹학회지
    • /
    • 제24권1호
    • /
    • pp.23-32
    • /
    • 1987
  • Synthesis of high purity ultrafine Si3N4 and ${\beta}$-Sialon powders was investigated via the simultaneous reduction and nitriding of amorphous SiO2, SiO2-Al2O3 system prepaerd by hydrolysis of alkoxides, using carbonablack as a reducing agent. In Si(OC2H5)4-C2H5 OH-H2 O-NH4OH system, hydrolysis rate increased with increasing reaction temperature and pH. Pure ${\alpha}$-Si3N4 was formed at 1350$^{\circ}C$ for 5 hrs in N2 atmosphere. In Si(OC2H5)4-Al(OC3H7)3-C6H6-H2 O-NH4OH system, weight loss increased as Si/Al ratio decreased. Single phase ${\beta}$-Sialon consisted of Si/Al=2 was formed at 1350$^{\circ}C$ in N2 and minor phases of ${\alpha}$-Si3N4, AIN, and X-phase were existed besides theSialon phase at other Si/Al ratios. The Si3N4 and Sialon powders synthesized from alkoxides consisted of uniform find particles of 0.05-0.2$\mu\textrm{m}$ in diameter, respectively.

  • PDF

Chiral Separation of $\beta$-Blockers after Derivatization with (-)-Menthyl chloroformate by Reversed-Phase High Performance Liquid Chromatography

  • Kim, Kyeong-Ho;Choi, Pok-Wha;Hong, Seon-Pyo;Kim, Hyun-Ju
    • Archives of Pharmacal Research
    • /
    • 제22권6호
    • /
    • pp.608-613
    • /
    • 1999
  • Optimum conditions of chiral derivatization reaction of $\beta$-blockers (acebutolol, arotinolol, betaxolol, bisoprolol, celiprolol, metoprolol and pindolol) with (-)-menthyl chloroformate were investigated for the resolution by HPLC. With more than 30 times molar excess of (-)-methyl chloroformate chiral derivatization reactions were completed within one hour at room temperature except arotinolol and celiprolol. Diastereomeric derivatives of $\beta$-blockers were well resolved on the ODS column using acetonitrile-methanol-water as a mobile phase.

  • PDF

침전법으로 제조된 전구체 성질에 의한 LiCoO2의 특성에 관한 연구 (Characterization of LiCoO2 Synthesized via Structural and Compositional Variations of Precursors Prepared by Precipitation)

  • 정명국;황치석;최청송
    • 청정기술
    • /
    • 제12권2호
    • /
    • pp.101-106
    • /
    • 2006
  • 본 연구에서는 수산화물 전구체로부터 HT-$LiCoO_2$ 분말을 제조하였다. 사용된 $Co(OH)_2$${\alpha}$상 및, 또는 ${\beta}$ 상의 수산화물이며 여러 조건에서 침전법으로 제조되었다. 제조시에 $[OH^-]/[CO^{2+}]$ 농도 비와 숙성시간을 조절함으로써 원하는 특성을 지닌 $Co(OH)_2$ 제조가 가능하였다. 침전법으로 합성한 $Co(OH)_2$와 LiOH를 메탄올 수용액을 이용하여 혼합한 후 이어서 증발, 건조 그리고 숙성 조작에 의하여 HT-$LiCoO_2$의 전구체를 합성하였다. 숙성기간에 tailor-made ${\beta}$-phase $Co(OH)_2$는 CoOOH로 변환되면서 고용체를 형성한다. 이 같은 결과로 HT-$LiCoO_2$가 낮은 온도($600^{\circ}C$), 짧은 시간(10분)에 합성이 가능하게 된다.

  • PDF

2상 Ti-6Al-4V 합금, 준단상 Ti-6.85Al-1.6V 및 단상 Ti-7.0Al-1.5V 합금의 고온 변형거동에 관한 연구 (Constitutive Analysis of the High-temperature Deformation Behavior of Two Phase Ti-6Al-4V Near-α Ti-6.85Al-1.6V and Single Phase-α Ti-7.0Al-1.5V Alloy)

  • 김정한;염종택;박노광;이종수
    • 소성∙가공
    • /
    • 제14권8호통권80호
    • /
    • pp.681-688
    • /
    • 2005
  • The high-temperature deformation mechanisms of a ${\alpha}+{\beta}$ titanium alloy (Ti-6Al-4V), near-a titanium alloy (Ti-6.85Al-1.6V) and a single-phase a titanium alloy (Ti-7.0Al-1.5V) were deduced within the framework of inelastic-deformation theory. For this purpose, load relaxation tests were conducted on three alloys at temperatures ranging from 750 to $950^{\circ}C$. The stress-versus-strain rate curves of both alloys were well fitted with inelastic-deformation equations based on grain matrix deformation and grain-boundary sliding. The constitutive analysis revealed that the grain-boundary sliding resistance is higher in the near-${\alpha}$ alloy than in the two-phase ${\alpha}+{\beta}$ alloy due to the difficulties in relaxing stress concentrations at the triple-junction region in the near-${\alpha}$ alloy. In addition, the internal-strength parameter (${\sigma}^*$) of the near-${\alpha}$ alloy was much higher than that of the ${\alpha}+{\beta}$ alloy, thus implying that dislocation emission/ slip transfer at ${\alpha}/{\alpha}$ boundaries is more difficult than at ${\alpha}/{\beta}$ boundaries.

가공 열처리에 따른 Ti-10Ta-10Nb합금의 미세조직 및 기계적 특성 변화 (Effects of Thermomechanical Processing on Changes of Microstructure and Mechanical Properties in Ti-10Ta-10Nb Alloy)

  • 이도재;황주영;이경구;윤계림;전충극
    • 열처리공학회지
    • /
    • 제18권2호
    • /
    • pp.91-98
    • /
    • 2005
  • Both commercially pure titanium and Ti-6Al-4V alloy have been widely used as biomaterials because of their excellent biocompatibility, corrosion resistance and mechanical properties. However, in recent years, vanadium has been found to cause cytotoxic effects and adverse tissue reactions, while aluminium has been associated with potential neurological disorders. A newly designed ${\alpha}+{\beta}$ type Ti alloy, Ti-10Ta-10Nb alloy showed superior properties to CP Ti and Ti-6Al-4V alloy in the point of biomaterial, and elucidated the future uses as a biomaterial. Microstructural changes of Ti-10Ta-10Nb alloy after hot-rolling, warm-rolling, solution and aging treatment were investigated. According to TEM results, the microstructures after solution treatment were composed of mostly ${\alpha}$ phase with a trace of ${\beta}$ phase due to adding ${\beta}$-phase stabilizer tantalum and niobium. The microstructures after warm-rolling is coarse and elongated ${\alpha}$ phase and hot rolling resulted in very fine ${\alpha}$ widmanst$\ddot{a}$tten. The highest value of hardness was obtained by aging treatment at $400^{\circ}C$ for 20hr in which microstructure consisted of very fine ${\alpha}$ phase in ${\beta}$ matrix.