• Title/Summary/Keyword: $(Nb_{1-x}Ta_x)C$

Search Result 43, Processing Time 0.025 seconds

Structure and Elastic Properties of (Nb1-xTax)C, (Nb1-xHfx)C, Ultra-High Temperature Solid Solution Ceramics using the First Principles Calculation (제1원리계산을 이용한 (Nb1-xTax)C, (Nb1-xHfx)C 초고온 세라믹 고용체의 구조 및 탄성특성)

  • Kim, Myungjae;Kim, Jiwoo;Kim, Jiwoong;Kim, Kyung-Nam
    • Korean Journal of Materials Research
    • /
    • v.31 no.12
    • /
    • pp.682-689
    • /
    • 2021
  • NbC, HfC, TaC, and their solid solution ceramics have been identified as the best materials for ultrahigh-temperature ceramics. However, their structural stability and elastic properties are mostly unclear. Thus, we investigated structure and elastic properties of (Nb1-xTax)C and (Nb1-xHfx)C solid solutions via ab initio calculations. Our calculated results show that the stability of (Nb1-xTax)C and (Nb1-xHfx)C increases with the increase of Hf and Ta content, and (Nb1-xHfx)C is more stable than (Nb1-xTax)C at the same content of Hf and Ta. The lattice constants decrease with increasing of Hf and Ta content. (Nb1-xTax)C and (Nb1-xHfx)C carbides are mechanically stable and brittle. Bulk modulus of (Nb1-xTax)C increases with increasing Ta content. In contrast, bulk modulus of (Nb1-xHfx)C decreases with increasing Hf content. Hardness of solid solutions shows the highest values at the (Nb0.25Ta0.75)C and (Nb0.75Hf0.25)C. In particular, (Nb0.75Hf0.25)C shows the highest hardness for the current system. The results indicate that the overall mechanical properties of (Nb1-xHfx)C solid solutions are superior to those of (Nb1-xTax)C solid solutions. Therefore, controlling the Hf and Ta element and content of the (Nb1-xTax)C and (Nb1-xHfx)C Solid solution is crucial for optimizing the material properties.

Low temperature sintering and dielectric properties of $Sr_2(Ta_{1-x}Nb_x)_2O_7$ ceramics by the flux method (용융염합성법에 의한 $Sr_2(Ta_{1-x}Nb_x)_2O_7$ 세라믹스의 저온소성과 유전특성)

  • 남효덕
    • Electrical & Electronic Materials
    • /
    • v.8 no.2
    • /
    • pp.158-164
    • /
    • 1995
  • Solid solutions Sr$_{2}$(Ta$_{1-x}$ Nb$_{x}$)$_{2}$O$_{7}$, (x=0.0-1.0), composed of strontium tantalate(Tc=-107.deg. C) and strontium-niobate(Tc=1342.deg. C) were prepared by the conventional mixed oxide method and the flux method(molten salt synthesis method). Phase relation, sintering temperature, grain-orientation and dielectric properties for sintered ceramic samples were investigated with different compositions. Both Curie temperature and dielectric constant at Curie temperature were increased, and sintering behavior and the degree of grain-orientation were improved with the increase of Nb content. The single phase Sr$_{2}$(Ta/sib 1-x/Nb$_{x}$)$_{2}$O$_{7}$ powder was synthesized by using the flux method at lower temperatures, and sintering temperature was also reduced by using the flux method-derived powder than using the mixed oxide-derived powder. Sintering characteristics and dielectric properties of the specimens prepared by the flux method were better than those derived through the conventional mixed oxide method.thod.hod.

  • PDF

Piezoelectric and Dielectric Characteristics of $((Na_{0.5}K_{0.5})_{1-x}Li_x)(Nb_{0.8}Ta_{0.2})O_3$ Ceramics using Conventional Solid State Sintering method (상용 소결법을 이용한 $((Na_{0.5}K_{0.5})_{1-x}Li_x)(Nb_{0.8}Ta_{0.2})O_3$ 세라믹스의 압전 및 유전 특성)

  • Kim, Min-Soo;Kim, Sin-Woong;Oh, Seok;Jeong, Soon-Jong;Min, Bok-Ki;Song, Jae-Sung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.11a
    • /
    • pp.210-220
    • /
    • 2006
  • Dense $((Na_{0.5}K_{0.5})_{1-x}Li_x)(Nb_{0.8}Ta_{0.2})O_3$ ceramics were developed by conventional sintering process. The electrical properties of $((Na_{0.5}K_{0.5})_{1-x}Li_x)(Nb_{0.8}Ta_{0.2})O_3$ ceramics were investigated as a function of Li substitution. When the sample sintered at $1100^{\circ}C$ for 4 h with the Substitution of 2 mol% Li, electro-mechanical coupling factor ($k_p$) and piezoelectric coefficient ($d_{33}$) were found to reach the highest values of 0.42 and 210 pC/N, respectively.

  • PDF

The Preparation and Characterization of Bismuth Layered Ferroelectric Thin Films by Sol-Gel Process (II. Dielectric Properties of Ferroelectric $Sr_{0.7}/B_{2.3}(Ta_{1-x}Nb_x)_2O_9$ Thin Films Prepared by MOD Process) (솔 - 젤법을 이용한 Bismuth Layered Structure를 가진 강유진성 박막의 제조 및 특성평가에 관한 연구 (II. MOD법으로 제조한 강유전성 $Sr_{0.7}/B_{2.3}(Ta_{1-x}Nb_x)_2O_9$ 박막의 유전특성))

  • 최무용;송석표;정병직;김병호
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.12 no.1
    • /
    • pp.62-68
    • /
    • 1999
  • Ferroelectric $Sr_{0.7}/B_{2.3}(Ta_{1-x}Nb_x)_2O_9$(x=0, 0.1, 0.2, 0.3) thin films were deposited on $Pt/SiO_2/Si$ substrate by MOD(Metalorganic Decomposition) process. Metal carboxylate and metal alkoxide were used as precursors, and 2-methoxyethanol, xylene as solvents. After spin coating, thin films were pre-annealed at $400^{\circ}C$, followed by RTA(Rapid Thermal Annealing) and final annealing at $800^{\circ}C$ in oxygen atmosphere. These procedures were repeated three times to obtain thin films with the thickness of $2000{\AA}$. To enhance the nucleation and growth of layered-perovskite phase, thin films were rapid-thermally annealed above $720^{\circ}C$ in oxygen atmosphere. As RTA temperature increased, fluorite phase was transformed to layered-perovskite phase. And the change of Nb contents affected dielectric / electrical properties and microstructure. The ferroelectric characteristics of $Sr_{0.7}/B_{2.3}(Ta_{1-x}Nb_x)_2O_9$ thin film were Pr=8.67 $\mu{C}/cm^2$, Ec=62.4kV/cm and $I_{L}=1.4\times10^{-7}A/cm^2$ at the applied voltage of 5V, respectively.

  • PDF

Surface Characteristics of Anodized Ti-30Nb-xTa Alloys with Ta Content

  • Kim, Eun-Sil;Ko, Yeong-Mu;Choe, Han-Cheol
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2012.05a
    • /
    • pp.254-254
    • /
    • 2012
  • The purposed of this work was to determine surface charateristics of anodized Ti-30Nb-xTa alloys with Ta content. Samples were prepared by arc melting, followed by followed by homogenization for 12 hr at $1000^{\circ}C$ in argon atmosphere. The electrolyte for anodization treatment was prepared by mixing 465ml $H_2O$ with 35M $H_3PO_4$ and anodized at 180V to 220V. The microstructures of the alloys were examined by X-ray diffractometer (XRD) and optical microscopy (OM). Surface characteristics of anodized Ti-30Nb-xTa alloys was investigated by potentiodynamic test and potentiostatic in 0.9% Nacl solution at $36.5{\pm}1^{\circ}C$. It was observed that the changed ${\alpha}$ phase to ${\beta}$ phase with Ta content.

  • PDF

Effect of Ta Substitution on the Dielectric and Piezoelectric Properties of (Li0.04(Na0.54K0.46)0.96(Nb0.96-xTaxSb0.04)O3Ceramics (Ta 치환이 (Li0.04(Na0.54K0.46)0.96(Nb0.96-xTaxSb0.04)O3 세라믹스의 유전 및 압전 특성에 미치는 영향)

  • Noh, Jung-Rae;Yoo, Ju-Hyun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.24 no.8
    • /
    • pp.627-631
    • /
    • 2011
  • [ $[Li_{0.04}(Na_{0.54}K_{0.46})_{0.96}](Nb_{1-0.04-X}TaxSb_{0.04})O_3$ ]lead-free piezoelectric ceramics have been prepared by normal sintering at $1,100^{\circ}C$ for 5 h. X-ray diffraction analysis indicated that specimens demonstrate orthorhombic symmetry when $Ta\leq5$ mol%. While transforming into tetragonal symmetry when $x\geq20$ mol%. These suggest that the orthorhombic and tetragonal phases co-exist in the ceramics with 5 mol% $cm^3$. As the result of SEM images, the grain growth was decreased with the increase of Ta substitution. The ceramics become 'softening', leading to improvements in $k_p$, $\varepsilon_r$ and $d_{33}$, but a decrease in $Q_m$. Excellent properties of $k_p$= 0.46, $d_{33}$= 293 pC/N, ${\varepsilon}_r$= 1,583 and Tc= $340^{\circ}C$ were obtained when Ta= 15 mol%.

The structural and Microwave Dielectric Properties of (1-x)Ba($Mg_{1/3}Ta_{2/3})O_3$-xBa($Co_{1/3}Nb_{2/3})O_3$(x=0.25~0.5) Ceramics ((1-x)Ba($Mg_{1/3}Ta_{2/3})O_3$-xBa($Co_{1/3}Nb_{2/3})O_3$(x=0.25~0.5) 세라믹스의 구조 및 마이크로파 유전특성)

  • 황태광;최의선;임인호;이영희
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.14 no.3
    • /
    • pp.197-201
    • /
    • 2001
  • The microwave dielectric properties of (1-x)Ba(Mg$_{1}$3/Ta$_{2}$3/)O$_3$-xBa(Co$_{1}$3/Nb$_{2}$3)O$_3$(x=0.25~0.5) ceramics depending on the Ba(Co$_{1}$3/Nb$_{2}$3/)O$_3$[BCN] contents and the possibility of application as a microwave dielectric resonator were investigated. The specimens were prepared by he conventional mixed oxide method using there sintering temperature of 1575$^{\circ}C$. It was found that Ba(Mg$_{1}$3/Ta$_{2}$3/)O$_3$[BMT] and BCN formed a solid solution with complex perovskite structure. As the mole fraction of BCN increased, dielectric constant increased while temperature coefficient of resonant frequency decreased. The highest value of quality factor, Qxf$_{0}$=138,205GHz, obtained in the sample of 0.9BMT-0.1BCN ceramics. In the range of x$\geq$0.4, the dielectric constant was about 30. The 0.55BMT-0.45BCN ceramics showed excellent microwave dielectric properties with $\varepsilon$$_{r}$=30.84, Qxf$_{0}$=75,325GHz and $\tau$$_{f}$=2.9015ppm/$^{\circ}C$.EX>.EX>.

  • PDF

Structural Characterization of the (TEX)$Sr_2Co_0.5Nb(Ta)_0.5O_4$(/TEX) and (TEX)$Sr_3CoNb(Ta)O_7$(/TEX)

  • Jo, Han Sang;Ri-Zhu Yin;Ryu, Gwang Hyeon;Yu, Cheol Hyeon
    • Bulletin of the Korean Chemical Society
    • /
    • v.21 no.7
    • /
    • pp.679-684
    • /
    • 2000
  • The Sr2Co0.5Nb(Ta)0.5O4 and Sr3CoNb(Ta)O7 compounds, both with Ruddlesden-Popper structures, have been synthesized by the ceramic method at $1150^{\circ}C$ under atmospheric pressure. The crystallographic structure of the compounds was assigned to the tetr agonal system with space group 14/mmm by X-ray diffraction(XRD) Rietveld refinement. The reduced lattice volume and lattice parameters increased as the Ta with 5d substitutes for the Nb with 4d in the compounds. The Co/Nb(Ta)O bond length has been determined by X-ray absorption spectroscopic(EXAFS/XANES) analysis and the XRD refinement. The CoO6,octahedra were tetragonally distorted by elongation of Co-O bond along the c-axis. The magnetic measurement shows the compounds Sr2Co0.5Nb(Ta)0.5O4 and Sr3CoNb(Ta)O7 have paramagnetic properties and the Co ions with intermediate spin sates between high and low spins in D4h symmetry. All the compounds showed semiconducting behavior whose electrical conductivity increased with temperature up to 1000 K. The electrical conductiviy increased and the activation energy for the conduction decreased as the number of perovskite layers increased in the compounds with chemical formula An+1BnO3n+1.

A study on the Microwave Dielectric Properties of Ba(Mg,Co)(Ta,Nb)$O_3$ Ceramics (Ba(Mg,Co)(Ta,Nb)$O_3$ 세라믹의 마이크로파 유전특성에 관한 연구)

  • Lee, Moon-Kee;Chung, Jang-Ho;Bae, Seon-Gi;Lee, Young-Hi
    • Proceedings of the KIEE Conference
    • /
    • 1998.11c
    • /
    • pp.752-754
    • /
    • 1998
  • $Ba(Mg_{(1-x)}Co_x)_{1/3}(Ta_{(1-x)}Nb_x)_{2/3}O_3$ ($x=0.3{\sim}0.6$) ceramics were prepared by the conventional mixed oxide method. The sintering temperature and time were of $1400{\sim}1575[^{\circ}C]$,5[hr.] respectively. The structural and microwave dielectric Properties were investigated with composition ratio and sintering temperature. And then the application for the microwave dielectric resonator was investigated.

  • PDF

Characterization of Ag doped 0.9(Na0.52K0.48)NbO3-0.1LiTaO3 Ceramics (Ag가 첨가된 0.9(Na0.52K0.48)NbO3-0.1LiTaO3 세라믹스)

  • Lee, Kyoung-Soo;Koh, Jung-Hyuk
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.23 no.7
    • /
    • pp.517-520
    • /
    • 2010
  • Lead-free $0.9(Na_{0.52}K_{0.48})NbO_3$ - $0.1LiTaO_3$ piezoelectric ceramics doped with $Ag_2O$ (0-4 mol%) have been prepared by the conventional mixed oxide method. The structural and electrical properties were analyzed in order to find its potential applications. The crystal structure of 1-4 mol% Ag doped $0.9(Na_{0.52}K_{0.48})NbO_3$-$0.1LiTaO_3$ lead free piezoelectric ceramics were investigated for several sintering temperatures ($1100^{\circ}C$) by the use of X-ray diffraction analysis. In order to analyze the effect of Ag dopants on the $0.9(Na_{0.52}K_{0.48})NbO_3$-$0.1LiTaO_3$ ceramic, the diffraction intensity ratio of the (002) to (200) planes were calculated from the X-ray diffraction patterns of the ceramic samples.