The Mixing Control Range Selection of Concrete according to High Volume Mineral Admixture Replacement

광물질 혼화재 다량 치환에 따른 콘크리트의 배합 조정 범위 선정

  • Received : 2013.01.25
  • Accepted : 2013.04.19
  • Published : 2013.06.20

Abstract

In this study, the adjustment range of mixture factor with replacement mineral admixture was reviewed to secure the mixture change data of high volume concrete compared to general concrete. When changing the concrete mix to high volume concrete within the universal concrete mixing, the adjustment range of mixture to ensure optimum quality is as follows. Unit-water content is $20{\sim}30kg/m^3$ downward. Fine aggregate ratio dropped by approximately 1% when W/B was reduced by 5%, and it is reduced by approximately 0.12% when there is a 5% increase in the total replacement rate. When the FA replacement rate was increased by 5%, the AE agent was approximately 20% to 30% higher compared with the conventional one. When the FA and BS replacement rate rose by 5%, W/B was reduced by about 1 to 4%.

본 연구는 혼화재의 다량 치환 시 배합 요인의 조정 범위를 검토하기 위한 목적으로 일반 콘크리트에서 혼화재 다량 치환 콘크리트로의 배합변경 데이터를 확보하고자 하였다. 실험결과를 요약하면, 일반 범용적 배합내에서 혼화재 다량 치환 콘크리트로 배합을 변경 시 적정 품질을 확보하기 위한 단위수량의 경우 $20{\sim}30kg/m^3$ 하향 조정, 잔골재율은 W/B 5 % 하향조정 시 약 1 %, 총 치환율 5 % 증가 시약 0.12 %로 중복 하향 조정, AE제는 FA 치환율 5 % 증가 시 컨벤셔널 대비 약 20~30 % 정도 상향 조정, W/B는 FA 및 BS의 치환율이 5 % 상향 시 W/B를 약 1~4 % 정도 하향 조정함으로써 콘크리트의 기본 물성을 확보할 수 있는 것으로 나타났다.

Keywords

References

  1. The Korea Concrete Institute. Concrete & Environment. 1st ed. Seoul (Korea): The Korea Concrete Institute; 2010. 298 p.
  2. Cho YJ. Concrete Technology at an the Era of Green Growth. Journal of the Korea Concrete Institute. 2009 Sep;21(5): 22-7.
  3. Park CJ, Song RF, Ryu GS, Koh KT, Han MC, Han CG. Strength Development of High Volume Fly-Ash Concrete Using High Early Strength Type Admixture, Proceedings of fall Conference of Korea Concrete Institute; 2009 Nov 7; Dankook University. Seou l(Korea): Proceedings of the Korea Concrete Institute; 2009. p. 273-4.
  4. Kim KH, Hwang IS, Kwon OB, Kim KM, Park HC. A Study on the Improvement of Early Strength of Low Carbon Concrete. Proceedings of spring Conference of Korea Concrete Institute; 2011 May 11-13; R Renaissance hotel(Jeju). Seoul (Korea): Proceedings of the Korea Concrete Institute; 2011. p. 687-8.
  5. Park SW, Cho HD, Janug JD. The Experimental Study on the Compressive Strength of the High Strength Concrete with the Fly Ash and Blast Furnace Slag. Proceedings of fall Conference of Korea Concrete Institute; 2010 Nov 5-6; Chun-cheon. Seoul (Korea): Proceedings of the Korea Concrete Institute; 2010. p. 175-6.
  6. Paik MS, Lee YD, Jung SJ. A Study on Hydration Heat Properties and Strength Properties of High Volume Fly-Ash Concrete. Journal of the Korea Institute of Building Construction. 2003 Sep;3(3):135-42.
  7. Lee BK, Kim GY, Lee SB, Lee BC, Shin KS, Kim HS. Evaluation of Compressive Strength of Mortar Replaced to High Volume Blast Furnace Slag. Proceedings of the Korea Institute of Building Construction; 2012 Nov 16; Hanyang University. Seoul (Korea): The Korea Institute of Building Construction; 2012. p. 103-5.
  8. Park CK, Lee SH, Kim HJ, The Characteristic of Strength Development of High Volume Fly-Ash Concrete. Proceedings of the Korea Institute of Building Construction; 2007 Nov; Hannam University. Seoul(Korea): The Korea Institute of Building Construction; 2007. p. 67-70.
  9. Kim YR, Kim OJ, Kim DS, Khil BS, Kim SS, Choi SJ, Investigation on the Fundamental Properties of Low Heat Concrete using High Volume Mineral Admixture, Proceedings of the Korea Institute of Building Construction; 2010 Nov 12; Chung-nam University. Seoul (Korea): The Korea Institute of Building Construction; 2010. p. 65-8.
  10. Han CG. Character and Mix design of Concrete Chapter 4, Mix design of Concrete. Seoul (Korea): Kimoondang; 2011. p. 101-66.