Durability Characteristics of Concrete Containing Lightly Burnt MgO Powder

저온 소성한 MgO 분말을 혼입한 콘크리트의 내구 특성

  • Choi, Seul-Woo (Dept. of Civil, Architectural and Environmental System Engineering, Sungkyunkwan University) ;
  • Kim, Joo-Hyung (Dept. of Civil, Architectural and Environmental System Engineering, Sungkyunkwan University) ;
  • Lee, Kwang-Myong (Dept. of Civil, Architectural and Environmental System Engineering, Sungkyunkwan University) ;
  • Kwon, Yong-Gil (K-water Institute, Korea Water Resources Corporation) ;
  • Jang, Bong-Seok (K-water Institute, Korea Water Resources Corporation)
  • 최슬우 (성균관대학교 건설환경시스템공학과) ;
  • 김주형 (성균관대학교 건설환경시스템공학과) ;
  • 이광명 (성균관대학교 건설환경시스템공학과) ;
  • 권용길 (한국수자원공사 K-water 연구원) ;
  • 장봉석 (한국수자원공사 K-water 연구원)
  • Received : 2011.04.06
  • Accepted : 2011.07.08
  • Published : 2011.10.31

Abstract

MgO concrete containing lightly burnt MgO powder at $850{\sim}1,000^{\circ}C$ may have a long-term expansibility characteristic. Such expansibility of MgO concrete can compensate the shrinkage at later ages since the hydration of the MgO is very slow. However, the addition of MgO delays the initial hydration of cement and increases the setting time of cement. Also, the porosity and pore-size distribution of the MgO concrete are different from OPC concrete. Therefore, in order to use MgO in practice, both mechanical and durability properties of MgO concrete should be carefully examined. In this study, durability tests on carbonation, freezing-thawing, and diffusion of chloride were carried out after 56 days of underwater curing at $20^{\circ}C$ to compare durability characteristics of 5% MgO-mixed concrete with those of OPC concrete. The results showed that MgO concrete shows a greater durability than the concrete with no MgO, because the micro structure in the MgO concrete is much denser due to its expansibility characteristic.

$850{\sim}1,000^{\circ}C$ 정도의 저온에서 소성된 MgO 분말을 혼입한 MgO 콘크리트는 장기적인 팽창성을 보인다. 이러한 팽창성은 MgO 분말의 느린 수화 반응을 통해 이루어지기 때문에 늦은 재령에서의 수축을 보상하는 특성을 가진다. 하지만 MgO 분말의 혼입은 시멘트의 초결을 지연시키며 응결 시간을 증가시키고, MgO 콘크리트의 공극률과 공극의 크기 분포가 일반 콘크리트와 다르기 때문에 현장 적용을 위해서는 MgO 콘크리트의 역학적 특성뿐만 아니라 다양한 내구 성능에 대한 검토가 필요하다. 이 연구에서는 MgO 콘크리트의 내구 특성을 평가하기 위하여 5% 수준으로 MgO 분말을 혼입한 콘크리트를 재령 56일까지 $20^{\circ}C$에서 수중 양생한 후 탄산화, 동결융해 및 염화물 확산에 대한 실험을 수행하여 MgO 분말을 혼입하지 않은 콘크리트의 내구 특성과 비교하였다. 그 결과 MgO 분말을 혼입한 콘크리트에서 콘크리트의 내구 성능이 다소 향상되는 것을 확인할 수 있었으며, 이는 MgO 분말의 수화 반응에 따른 팽창 효과로 콘크리트의 미세 구조가 치밀해지기 때문으로 사료된다.

Keywords

References

  1. Du, C., "A Review of Magnesium Oxide in Concrete," Concrete International, Vol. 27, No. 12, 2005, pp. 45-50.
  2. Gao, P., Lu, X., Geng, F., Li, X., Hou, J., Lin, H., and Shi, N., "Production of MgO-Type Expansive Agent in Dam Concrete by Use of Industrial by-Products," Building and Environment, Vol. 43, No. 4, 2008, pp. 453-457. https://doi.org/10.1016/j.buildenv.2007.01.037
  3. Gao, P., Wu, S., Lu, X., Deng, M., Lin, P., Wu, Z., and Tang, M., "Soundness Evaluation of Concrete with MgO," Construction and Building Materials, Vol. 21, No. 1, 2007, pp. 132-138. https://doi.org/10.1016/j.conbuildmat.2005.06.033
  4. Lingling, X. and Deng, M., "Dolomite Used as Raw Material to Produce MgO-Based Expansive Agent," Cement and Concrete Research, Vol. 35, No. 8, 2005, pp. 1480-1485. https://doi.org/10.1016/j.cemconres.2004.09.026
  5. 장봉석, 권용길, 최슬우, 이광명, "저온 소성한 MgO 분말을 혼입한 시멘트 복합체의 기초 물성," 콘크리트학회 논문집, 23권, 2호, 2011, pp. 225-233. https://doi.org/10.4334/JKCI.2011.23.2.225
  6. Li, Z., Cui, X., and Tang, M., "MgO-Type Delayed Expansive Cement," Cement and Concrete Research, Vol. 21, No. 6, 1991, pp. 1049-1057. https://doi.org/10.1016/0008-8846(91)90065-P
  7. Liu, Z., Cui, X., and Tang, M., "Hydration and Setting Time of MgO-Type Expansive Cement," Cement and Concrete Research, Vol. 22, No. 1, 1992, pp. 1-5. https://doi.org/10.1016/0008-8846(92)90129-J
  8. Li, C. M., "Mechanical Properties and Durability of MgO Concrete," Advanced in Science and Technology of Water Resources, Vol. 20, No. 5, 2000, pp. 30-35 (in Chinese).
  9. Chen, L. D., Xie, L. G., Li, H. Y., and Li, C. M., "Further Study of Mechanical Properties of MgO Concrete under Different Curing Temperatures," Guangdong Water Resources and Hydropower, No. 2, 2003, pp. 11-13 (in Chinese).
  10. 김태상, 장봉석, 정상화, 김주형, "MgO를 혼합한 콘크리트의 내구 특성 평가에 관한 실험적 연구," 한국콘크리트 학회 가을 학술대회 논문집, 20권, 2호, 2008, pp. 397-400.
  11. 최성, 이광명, 정상화, 김주형, "급속 촉진 탄산화 시험을 통한 플라이애쉬 콘크리트의 탄산화특성 연구," 콘크리트학회 논문집, 21권, 4호, 2009, pp. 449-455.
  12. 김생빈, 문제길, 김동신, "고강도 콘크리트에서 기포조직 및 강도특성이 동결융해저항에 미치는 영향," 대한토목학회 논문집, 13권, 3호, 1993, pp. 13-24.
  13. 김생빈, "고강도 콘크리트의 동결융해저항에 미치는 기포조직의 영향," 콘크리트학회 논문집, 4권, 1호, 1992, pp. 89-96.

Cited by

  1. Long-term Durability Characteristics of Fly ash Concrete Containing Lightly Burnt MgO Powder vol.33, pp.3, 2013, https://doi.org/10.12652/Ksce.2013.33.3.909
  2. Characteristics of Bond Strength as Types of Primer for the Facilities of Anti-corrosion Waterproofing Materials by the Reversed Pressure and Concrete Surface Condition vol.18, pp.1, 2014, https://doi.org/10.11112/jksmi.2014.18.1.068