Automatic Ultrasonic Inspection on Heater Sleeves and J-Groove Welds of Pressurizer

가압기 전열기 슬리브 및 J-Groove 용접부의 자동 초음파검사

  • 류승우 (두산중공업(주) 비파괴검사부) ;
  • 장희준 (두산중공업(주) 비파괴검사부) ;
  • 김선제 (두산중공업(주) 비파괴검사부) ;
  • 이상덕 (두산중공업(주) 비파괴검사부) ;
  • 성종환 (두산중공업(주) 비파괴검사부)
  • Published : 2010.12.01

Abstract

In order to prevent the corrosion of component contacted primary water designed alloy 600 material in the nuclear power plant. But the primary water stress corrosion cracking(PWSCC) of alloy 600 and weld area occurs continuously due to the residual stress. The leakage accident resulted from PWSCC in the drain nozzle of the steam generator of domestic power plants. Heater sleeves of the pressurizer are welded with alloy 600 weld material and therefore exposed to the primary water environment. PWSCC occurred in heater sleeve material and weld area of many foreign power plants. The current issue of domestic nuclear power plants are consequently concentrated to PWSCC of similar material. In order to improve the detection and the sizing of the PWSCC in the welding sleeve of the pressurizer, the automatic UT system and multi-directions probe sets have been developed. The experimental studies have been performed using the mock-up block containing artificial reflectors(ID connected EDM notch) and semi-artificial cracks made from thermal fatigue. The automatic UT System is applied in the detection and the length sizing of the ID/OD on the tube and the J-groove weld area of the artificial reflectors and results of the detection and the sizing are compared respectively. Also, the developed automatic UT system is successfully accomplished to inspect the heater sleeve and the J-groove weld area on the pressurizer for the detection of PWSCC.

Keywords