In this study, the mechanical properties, alkali-silica reaction(ASR) expansion and residual mechanical properties after ASR of waste glass fine aggregate(GS) mortar according to mineral mixture were evaluated. As a result, it was found that the mineral mixture reduces the ASR expansion. However, mechanical properties and residual mechanical properties have decreased.