The Evaluation of Flexural Performance in UHPC(Ultra High Performance Concrete) according to Placement Methods

타설방법에 따른 초고성능 콘크리트의 휨성능 평가

  • 류금성 (한국건설기술연구원 구조재료연구실) ;
  • 강수태 (한국건설기술연구원 구조재료연구실) ;
  • 박정준 (한국건설기술연구원 구조재료연구실) ;
  • 안기홍 (한국건설기술연구원 구조재료연구실) ;
  • 고경택 (한국건설기술연구원 구조재료연구실) ;
  • 김성욱 (한국건설기술연구원 구조재료연구실)
  • Published : 2008.11.07

Abstract

UHPC which was a structural material exhibiting very remarkable mechanical performances with compressive strength, tensile strength and flexural strength rising up to 200MPa, 15MPa and 35MPa, respectively. In addition, this material presents exceptional durability regard to the very low diffusion and penetration speeds of noxious substances like chloride ions This study was carry out to evaluate the effect of flexural behavior according to placement method in UHPC. The results is showing that the placement methods have remarkable influence flexural strength Addition to it is showing that the placement methods made little difference in the first cracking strength but considerable gap up to 2 or 3 times in the ultimate flexural strength.

초고성능 콘크리트(Ultra High Performance Concrete)는 압축강도 200MPa, 인장강도 15MPa 및 휨강도 35MPa 정도의 높은 강도 특성과 열화인자의 침투 및 확산 속도가 보통콘크리트에 비해 1/20에서 최대 1/10,000까지 낮은 고내구성을 나타내면서 동시에 슬럼프 플로우가 약 220mm정도의 자기충전성 특성을 갖는 콘크리트이다. 또한 초고성능 콘크리트의 가장 큰 특징으로는 강섬유의 혼입함으로써 휨강도와 인성의 향상이다. 따라서 본 연구에서는 초고성능 콘크리트의 타설 방법에 따라 휨거동특성에 미치는 효과를 평가하였다. 그 결과 타설 방법에 따라 휨강도에 큰 영향을 미치는 것으로 나타났다. 또한 초기균열강도에는 큰 영향을 미치지 않고 최대휨강도에는 2$\sim$3배 정도까지 차이를 발생시키는 것으로 나타났다.

Keywords