A Study on the Dielectric and Pyroelectric Properties of the PSS-PT-PZ Ceramics Added $MnO_2$

$MnO_2$가 첨가될 PSS-PT-PZ 세라믹의 유전 및 초전특성에 관한 연구

  • 이성갑 (광운대학교 전기재료공학과) ;
  • 류기원 (광운대학교 전기재료공학과) ;
  • 이영희 (광운대학교 전기재료공학과) ;
  • 배선기 (인천대학교 전기공학과) ;
  • 박창엽 (연세대학교 전기공학과)
  • Published : 1991.07.18

Abstract

In this study, $(Pb_{0.99}La_{0.01})[(Sb_{1/2}Sn_{1/2})_{0.10}Ti_{0.25}Zr_{0.65}]O_3$, added $MnO_2$ (0-0.30[mol%]) ceramics were fabricated by the mixed oxide method. The sintering temperature and time were $1250[^{\circ}C]$, 2[hr], respectively. In the $(Pb_{0.99}La_{0.01})[(Sb_{1/2}Sn_{1/2})_{0.10}Ti_{0.25}Zr_{0.65}]O_3$ added $MnO_2$ (0.24[mol%]) specimens, relative dielectric constant and dielectric loss were minimum values 3.52, 0.003, respectively, and Curie temperature were highest values $256[^{\circ}C]$. Pyroelectric coefficient and voltage responsivity of the $(Pb_{0.99}La_{0.01})[(Sb_{1/2}Sn_{1/2})_{0.10}Ti_{0.25}Zr_{0.65}]O_3$, and added $MnO_2$ (0.24[mol%]) specimen were good values, $6.73{\times}10^{-8}[C/cm^2K],\;125[v/W]$, respectively. Figure of merit of pyroelectric current, voltage and detectivity of the specimen, $(Pb_{0.99}La_{0.01})[(Sb_{1/2}Sn_{1/2})_{0.10}Ti_{0.25}Zr_{0.65}]O_3$ added $MnO_2$ (0.24[mol%]) were good values $2.714{\times}10^{-8}[Ccm/J],\;7.706{\times}10^{-11}[Ccm/J],\;2.640{\times}10^{-8}[Ccm/J]$, respectively. Voltage responsivity of the $(Pb_{0.99}La_{0.01})[(Sb_{1/2}Sn_{1/2})_{0.10}Ti_{0.25}Zr_{0.65}]O_3$ added $MnO_2$ (0.24[mol%]) specimens were decreased with increasing the chopper frequency.

Keywords