Dung, Cao Thi My;Thi, Nhu Hoa Tran;Ta, Kieu Hanh Thi;Tran, Vinh Cao;Nguyen, Bao Thu Le;Le, Van Hieu;Do, Phuong Anh;Dang, Anh Tuan;Ju, Heongkyu;Phan, Bach Thang
Journal of Magnetics
/
v.20
no.4
/
pp.353-359
/
2015
Dielectric properties of $xBaTiO_3-(1-x)CoFe_2O_4$ composite materials have been investigated. Dielectric properties of $BaTiO_3$, $CoFe_2O_4$ and $0.5BaTiO_3-0.5CoFe_2O_4$ samples show frequency dependence, which is classified as relaxor behavior with different relaxing degree. The relaxor behaviors were described using the modified Curier-Weiss and Vogel-Fulcher laws. Among three above samples, the $BaTiO_3$ sample has highest relaxing degree. Photoluminescence spectral indicated defects, which might in turn control relaxing degree.
The resonant frequency fo and unloaded quality factor Qu of CoTi-substituted Barium ferrites($\textrm{BaCo}_{x}\textrm{Ti}_{x}\textrm{Fe}_{12-2x}\textrm{O}_{19}$, $1.0\leq\textrm{x}\leq5.0$) were measured at frequencies between 5 to 10GHz using the paralleled copper-plate wave guide method. The measurements showed that the permittivities of CoTi-substituted Barium ferrites(CoTi-BF) increased from 14.7 to 23.4 with the contents of CoTi, x, and the loss tangents had values of $\textrm{10}^{-3}$ order. From these results, CoTi-BF are considered to be very promising materials in microwave devices such as dielctric resonator antennas.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.13
no.6
/
pp.545-550
/
2000
In order to synthesize Ba-ferrite particles by molten salt method KCl and NaCl were added to basic composition to 50% by weight. X was varied from 0.0 to 1.0 to control the magnetic properties in $BaFe_{12-2x}$/ $Co_{x}$ / $Ti_{x}$ / $O_{19}$ and 1 mol% of $SiO_2$was added to control the aspect ratio of hexagonal platelets. And the effects of reaction temperatures were examined by varying the temperature from 85$0^{\circ}C$ to 120$0^{\circ}C$ with 5$0^{\circ}C$ intervals. Eutectic composition of NaCl and KCl lowered the crystallizing temperature of Ba-ferrite in molten salts than using KCl and NaCl separatly. The morphology of resulting Ba-ferrite particles was clearly hexagonal-shaped plates. $H_{c}$ and $M_{r}$ were decreased when F $e^{3+}$ was substitued with $Co^{2+}$ and $Ti^{4+}$ from x=0 to x=1.0 in $BaFe_{12-2x}$/ $Co_{x}$ / $Ti_{x}$ / $O_{19}$ . Adding 1mol% $SiO_2$in molten salt method increased the size but shortened c-axis of the hexagonal ferrites and this result is an opposite phenomenon compared with the result in solid-statge reaction.n.ion.n.
The M-type barium ferrite ($BaFe_{12}O_{19}$) is well known magnetic material to be used as a permanent magnet due to its strong uniaxial anisotropy. The substitution of nonmagnetic $Ti^{+4}$ and magnetically weak $Co+^2ion for Fe^{+3}$ to its strong uniaxial anisotropy. The substitution of nonmagnetic $Ti^{+4}$ and magnetically weak $Co+^2ion for Fe^{+3}$ sublattices reduces the uniaxial anisotropy and those compounds open a new application field of noise suppressor at high frequencies. In this study, the magnetic and microwave absorbing properties are investigated in Ti-and Co-substituted barium ferrites ($BaFe_{12-2X} Ti_XCo_XO_{19}$). The saturated magnetization decreases linearly with the substitution of Ti and Co. The rapid drop in coercive force is observed with Ti and Co substitution upto x=1.2. The magnetic permeability spectrum shows the natural magnetic resonance in the specimens with small coercive force and large attenuation of microwave is predicted in those specimens at high frequencies (above 4 GHz).
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
1996.11a
/
pp.326-329
/
1996
In order to synthesize Ba-ferrite fine particles by molten salt method and inhibit the abnormal grain growth of sintered specimen, KCI anti NaCl were added to basic composition to 50% by weight, and added 1 male% of $SiO_2$ to control the shape of Ba-ferrite particles. $H_{c}$ and $M_{r}$ were decreased when F $e^{3+}$ was substituted with $Co_{2+}$ and $Ti_{4+}$ from x=0 to x=1.0 in $BaFe_{12-2x}$$Ti_{x}$$Co_{x}$$O_{19}$ , and 1 mole% $SiO_2$ increased the size but shortened c-axis of hexagonal ferrite. Seeds added in Ba-ferrite particle effected inhibition of abnormal grain growth during sintering.ing.g.
Sr substituted materials for some barium in M-type barium ferrite powder and Co-Ti substituted Sr-Ba hexagonal ferrite powder were prepared by citrate sol-gel method and 2 MOE sol-gel method these hexaferrite particles were reduced for 1hr in the hydrogen gas. The reduction temperatures were varied in the range of 250 $^{\circ}C$ to 500 $^{\circ}C$. X-ray diffraction patterns were measured using diffractometer with Cu $K_{\Alhpa}$ radiation. Mossbauer absorption spectra were measured with a constant acceleration spectrometer. We have focused on studying the origin of increasing $M_s$ by M$\"{o}$ssbauer spectroscopy. Ferrite particles which were sintered at 105$0^{\circ}C$ were found to be typical magnetoplumbite structure and single phase. XRD patterns with varying the reduction temperatures in $Sr_{0.5}Ba_{0.5}Fe_{10}O_{19}$ indicates ferrites particles become composite hexaferrites containing $\alpha$-Fe at T_{red}=350 \;$^{\circ}C$$. On the otherhand, it was found that $Co^{2+}$ ions and $Ti^{4+}$ ions in $Sr_{0.7}Ba_{0.3}Fe_{10}CoTiO_{19}$ prevent from changing $Fe^{3+}$ ions to $\alpha$-Fe during the $H_2$ reduction. Comparing Mossbauer results with XRD results, we have determined most of $\alpha$-Fe are reduced from $4f_{vi}$ sites and 12k sites of $Fe^{3+}$ ions. These $\alpha$-Fe phase bring the induced anisotropy and increase saturation magnetization $M_s$.TEX>.
The purpose of this experimenL is to investigate the magnetic anisotropy and microwave absorbing properties in M-type Bat territe (${BaFe}_{12-2X}{A}_{X}{Me}_{X}{O}_{19}$), where $Fe_{3+}$ is substituted by $Ti_{4+}$ in A site and $Co_{2+}$ in Me site. The saturation magnetization (Ms) is linearly decreased with the substitution rate(x) and the coerciviLy (He) is rapidly decreased in accordance with the reduction in t the magnetocrystalline anisotropy For the specimen with x=0.8 and thickness of 2 mm, the reflection loss calculated from the n material constants is less than -10 dB (90% absorption) in the frequency range of 10~16 GHz. The absorption loss is pre이.ctcd t to be more than 20 dElern in the frequency range of 12-16 GHz. The results demonstrate that the Ti-Co substituted M-type Ba-ferrite can be effectively used as a microwave absorber at high frequency range.
Kim, Jong-Pyo;Pyo, Dae-Woong;Park, Jung-Hoon;Lee, Yong-Taek
Membrane Journal
/
v.22
no.1
/
pp.8-15
/
2012
Tubular $Ba_{0.5}Sr_{0.5}Co_{0.8}Fe_{0.2}O_{3-{\delta}}$ membranes with $La_{0.6}Sr_{0.4}Ti_{0.3}Fe_{0.7}O_{3-{\delta}}$ porous coating layer were prepared by extrusion and dip coating technique. XRD and SEM result showed the tubular membrane possessed the perovskite structure and porouscoating layer (thickness= about $2{\mu}m$) in surface. The oxygen permeation test was measured at condition of ambient air (feed side) and vacuum (permeate side) in the temperature range from 750 to $950^{\circ}C$. The oxygen permeation flux of $Ba_{0.5}Sr_{0.5}Co_{0.8}Fe_{0.2}O_{3-{\delta}}$ tubular membrane with $La_{0.6}Sr_{0.4}Ti_{0.3}Fe_{0.7}O_{3-{\delta}}$ porous coating layer reached maximum $3.2mL/min{\cdot}cm^2$ at $950^{\circ}C$ and was higher than non-coated $Ba_{0.5}Sr_{0.5}Co_{0.8}Fe_{0.2}O_{3-{\delta}}$ tubular membrane. Long-term stability test result indicated that the oxygen permeation flux was quite stable during the 11 day.
Physical and magnetic behaviors of reduced Co-Zn-Ti-Sn substituted Ba-ferrite particles with hydrogen are different from those of reduced-pure Ba-ferrite particles. The coercivity of substituted Ba-feffite particles shows a peaking effect with the reduction temperature ranging from 250 to 520 $^{\circ}C$, while the coercivity of pure Ba-ferrite decreases monotonically. The reduction process of substituted Ba-ferrite has been found to be devided into three steps. At the first and second steps, the magneto-plumbite structure maintained. When the reduced-substituted Ba-ferrite particles are reoxidized, the coercivity is reversible at the first step but irreversible at the second step. During the third step of reduction process above 410 $^{\circ}C$. The magneto plumbite structure was collapsed with formation of $\alpha$-Fe and $BaFeO_{3-x}$ phases and consequently the coercivity distribution is broaden and the coercivity irreversible. The coercivity and saturation magnetization decreases and increases up to 130 emu/g respectively. In this study, it is found that the substituted elements prevent the magneto-plumbite structure from collapse during the reduction process and furthermore migrate from the magnetic sites of $2a+4f_{IV}$, 2b, and 12k to $4f_{VI}$ and 12k'. An increase in the coercivity before the collapse of magneto-plumbite structure is attributed to the migration of cations in hexagonal Ba-ferrite structure.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.