• 제목/요약/키워드: wool

검색결과 1,111건 처리시간 0.026초

효소가공 양모직물의 표면 성질에 관한 연구 (A Study on the Surface Properties of Wool Fabric Treated with Enzyme)

  • 박미라;김환철;박병기
    • 한국염색가공학회지
    • /
    • 제13권4호
    • /
    • pp.227-233
    • /
    • 2001
  • Wool fabrics were pre-treated with corona prior to treating with enzyme for shrinkage resistance. Commercial protease and cellulase were used for degradation of wool and the treatment conditions such as enzyme amount, treating time, and assistant chemicals. Friction coefficient and zeta-potential were measured to certificate an effect of treatment condition on the handle of wool fabric. Corona pretreatment make the wool fabric soft, which result in the decrease of friction coefficient and zeta-potential. Scale removal of wool surface was observed by scanning electron microscope. Amino acid analysis shows the effectiveness of enzyme, and corona pretreatment does not cause severe internal damage.

  • PDF

tert-Butoxide 처리 양모의 효소처리 및 염색성에 관한 연구 (Dyeability and Enzymetic Treatment of Wool Pretreated with tert-Butoxide)

  • 윤남식;윤성도
    • 한국염색가공학회지
    • /
    • 제9권6호
    • /
    • pp.87-95
    • /
    • 1997
  • Wool samples were treated by potassium tert-Butoxide(t-BuOK) in anhydrous tert-butanol to remove the bound surface lipid-layer, and the weight loss behaviors in protease solution and dyeabilities of the samples were studies. The C/N ratio of the surface of the t-BuOK-treated wool was shown to be 4.3 from XPS analysis. From SEM pictures any remarkable change in the shape of surface curticle during the proteasw treatment was not observed regardless of prior t-BuOK treatment. Dyeing rate and equilibrium adsorption of Orange II, a typical levelling type acid dye, on wool were not changed by protease or t-BuOK treatment, but those of Milling Cyanine 5R, a typical milling type acid dye, on wool were greatly enhanced by t-BuOK treatment in spite that, from alkali and urea-bisulfite solubilities, no damage on the inner part of wool fiber was expected by t-BuOK treatment.

  • PDF

Effect of Feed Protein Source on Digestion and Wool Production in Angora Rabbit

  • Bhatt, R.S.;Sawal, R.K.;Mahajan, A.
    • Asian-Australasian Journal of Animal Sciences
    • /
    • 제12권7호
    • /
    • pp.1075-1079
    • /
    • 1999
  • Adult German cross $(German{\times}British{\times}Russian)$ angora rabbits (one year age), 32 in number were divided randomly into four groups $(T_1-T_4)$ with equal sex ratio and fed diets containing $T_1$ groundnut cake (GNC); $T_3$, soyaflakes (SF); $T_4$, sunflower cake (SFC) and $T_2$, a mixture of all the three cakes along with green forage as roughage for a period of 9 months. Nine per cent protein was added from each protein source. Fibre level was maintained by adjusting the level of rice phak in the diets. The diets were iso-nitrogenous and contained similar level of fibre. DMI through roughage was not affected due to source of protein in the diet, however, DMI through concentrate was higher $(p{\leq}0.05)$ with SFC diet, which resulted in higher total feed intake in the group $(T_4)$. Body weights increased up to second shearing, thereafter it decreased due to summer depression. Diet containing soyaflakes sustained higher wool yield whereas, it was lowest $(p{\leq}0.05)$ on SFC diet. Wool attributes (staple length, medullation, fibre diameter) were not affected due to source of protein in the diet. Digestibility of fibre and its fractions (ADF, cellulose, hemicellulose) decreased $(p{\leq}0.05)$ with incorporation of SFC in the diets. Balance of calcium was lowest whereas, that of nitrogen was highest with SFC diet $(T_4)$. Biological value of N and net protein utilization was better when different protein sources were mixed together $(T_2)$. Protein quality of soyaflakes proved better for wool production followed by groundnut cake and mixture of three protein sources. Sunflower cake alone or in combination decreased wool production which may be checked by supplementation of amino acids and energy.

선인장 열매의 색소 추출물에 의한 양모섬유의 염색 (Dyeing of Wool Fabric by the Pigment Extracted from Opuntia Ficus-indica)

  • 이세희;조용석;최순화
    • 한국염색가공학회지
    • /
    • 제18권2호
    • /
    • pp.8-14
    • /
    • 2006
  • The pigment extraction of Opuntia ficus-indica has been conducted to develop useful natural dyes in place of synthetic dyes which are suspected to bring serious environmental pollutions. The dyeing ability on wool fabric by addition of ascorbic acid and several mordants were investigated by means of color measurement. In addition, the fastness of washing, perspiration, rubbing, light, dry cleaning, effect on bacterial reduction and UV-B protection were also investigated. From these investigation, it is suggested that the pigment extracted from Opuntia ficus-indica can be used as a source of natural dyes and the obtained result are as follows. 1. Maximum absorption band (${\lambda}max$) of Opuntia ficus-indica extract is 533nm. 2. The wool fabric dyed with Opuntia ficus-indica extract has stable color by the addition of ascorbic acid and is achieved with addition of 0.1% ascorbic acid, 0.5% several mordant, and three repeated dying at $50^{\circ}C$ for 1.5hr. 3. The wash fastness of the dyed wool fabric when it is washed with neutral detergent is more effective than alkaline detergent. The dry cleaning fastness of the dyed wool fabric is more excellent. In addition, the perspiration fastness of the dyed wool fabric is increased by mordanting method. And than the rubbing fastness of the dyed wool fabric is showed excellent under dryness and wetness. Light fastness of the dyed wool fabric, however is showed inferiority. 4. The wool fabric dyed with Opuntia ficus-indica extract is showed effective bacterial reduction and UV-B protection is increased remarkably.

Glass Wool Filtration을 이용한 개 희석정액의 운동성과 생존률의 검정 (Evaluation of Extended Canine Semen by Glass Wool filtration)

  • 윤재원;이영준;김수희;지동범;김용준
    • 한국임상수의학회지
    • /
    • 제22권3호
    • /
    • pp.228-232
    • /
    • 2005
  • Damaged spermatozoa are supposed to be trapped in glass wool. In the respect of this, two glass wool filtration spermatozoa groups (0.5 cm, 1 cm depth) were compared with control group to assay sperm motility, HOS values, and vital rate by CFDA/PI staining method following glass wool filtration. The motility of canine sperm extended with PBS+PVP after glass wool filtration was lower in both filtrated groups than that of the control group (p<0.01) and the same significant difference was also shown in canine semen extended with Tris buffer (p<0.01). The motility of canine sperm diluted with PBS+PVP was higher than that diluted with Tris buffer in the same experimental groups (p<0.05). The motility of control group was not significantly decreased until 2 hours immediately after extending, however, the motility of both glass wool filtrated spermatozoa were significantly decreased as time passed until 2 hours after filtration (p<0.01). At each time for assay (immediately, 30 min, 2 hours after filtration), the motility of canine sperm of control group was higher than the filtrated groups (p<0.05), whereas the motility of 0.5 cm depth group was higher than 1 cm depth group at the immediate time after filtration (p<0.05), 30 minutes later (p<0.05) with no difference at 2 hours. No difference was shown among the experimental groups in HOS values of canine sperm after glass wool filtration. The vital rate assayed by CFDA/PI staining of both filter groups was higher than the control group (p<0.05).

한랭환경하에서 운동발한시 인체의 체온조절반응에 대한 내의소재의 생리학적 의의 (Physiological Effects of Different Underwear Materials Thermoregulatory Response during Exercise with Sweating at Cold Environments)

  • 권오경;김태규;손부헌;박승한
    • 한국의류산업학회지
    • /
    • 제1권1호
    • /
    • pp.43-49
    • /
    • 1999
  • This study conducted 4 different kinds of underwear materials, which were A (Cotton 100%), B (Wool 100%), C (Cotton/Wool, 50/50%) and D (Acrylic/Cotton, 50/50%) and were done in a climate chamber under cold ambient $10{\pm}1^{\circ}C$, $40{\pm}5%RH$ by 6 male subjects who were in good health. Physiological parameters such as rectal and local skin temperature(forehead, forearm, hand, trunk, thigh, leg, foot, back and chest), heart rate, body weight loss, clothing microclimate, blood lactic acid concentration, and wearing sensation were measured. Started with a 15-min rest period, 15-min of exercise 1 (the condition of 4.5 mile/hr walking speed equivalent to with 8.5 Kcal energy consumption on the treadmill) period, 15-min rest period, exercise 2 (after 3minutes warming-up at 3.0. 3.7, 4.5. 5.2. 6.0, 6.7 mile/hr) until exhaustion period, and final 15-min of recovery period were performed. The results were as follows: The lowest mean skin temperature was acrylic/cotton in order of wool > cotton/wool > cotton > acrylic/cotton (F=13. 79. p<0.00l). Most of all skin temperature by parts of body had turned out in sequence of temperature wool > cotton/wool > acrylic/cotton > cotton. Fore arm part showed highest temperature about $32.43^{\circ}C$ on wool and had a tendency approximately $1.8^{\circ}C$ higher than cotton which had the lowest temperature, and had the biggest difference among garments in terms of skin temperature. The back temperature within clothing showed about $2^{\circ}C$ higher than the chest temperature within clothing. but the back humidity within clothing showed about 4~12% higher than the chest humidity within clothing. Body weight loss by each garment was this sequence; cotton > acrylic/cotton > wool > cotton/wool.

  • PDF

2염기산 무수물에 의한 양모섬유의 아실화(II) -아실화된 양모섬유의 성질을 중심으로- (Acylation of Wool Keratin with Dibasic Acid Anhydrides(II) ―on properties of acylated wool―)

  • Shin, Eun Joo;Park, Chan Hun;Choi, Suk Chul
    • 한국염색가공학회지
    • /
    • 제8권2호
    • /
    • pp.64-70
    • /
    • 1996
  • Wool yarns were treated in dimethylformamide solutions containing various concntrations of three dibasic acid anhydrides: succinic, itaconic, and phthalic arthydrides in various conditions. The structurl aspects of these dibasic acid anhydries are different: succinic, itaconic, and phthalic acid arthydrides have saturated aliphatic ethylene, unsaturated aliphatic vinyl and aromatic phenyl one groups, respectively. The properties of acylated wool keratin are as follows: Decreasing amino group and increasing carboxyl group by acylation lowered the hydrophilic property, and then moisture regain, and decreased acid dye uptake and enhanced cationic dye uptake of wool keratin. In the case of phthalic acid anhydries, in spite of lowest acyl content, the minimum of moisture regain was resulted from the bulk benzen ring, occuping much more voids on wool keratin molecules than other reagents. Acid solubility was increased by the decrease of amino group and hydrogen bonding by acylation. Alkali solubility was also increased formation of new amide group on the side chain of keratin, which can be degraded easily by alkali. In the case of phthalic acid anhydride, the relative high solubility was resulted from the much higher molecular weight of dissolved fractions. The surface of wool keratin was not damaged by treatment with any acylating agent.

  • PDF

양모 복지의 초기열류속최대치($q_{max}$)에 관한 연구( I ) -열전도도, 열통과성, 표면기공도와의 상관성을 중심으로- (A Study on the Initial Maximum Value of Heat Flux, $q_{max}$ of Wool Fabrics (Part I) - The correlation between $q_{max}$ and thermal conductivity, thermal transmittance, surface air cavity of wool fabrics -)

  • 최석철;정진순;천태일
    • 한국의류학회지
    • /
    • 제15권4호
    • /
    • pp.367-372
    • /
    • 1991
  • In this study, we discussed about the factors effected upon the initial maximum value of heat flux ($q_{max}$). Thermal conductivity, thermal transmittance and surface air cavity of wool fabrics were examind and their correlation to the $q_{max}$ was studied. The factors were examined which had an effect upon the $q_{max}$ of an objective measure of warm/cool feeling. It was simulated by Thermo-Labo apparatures. We selected twenty sorts of pure wool woven fabrics for men's fall -winter cloth (all Wool). The conclusions are as follows; 1. There was not a certain correlation between the $q_{max}$ and the thermal conductivity of wool fabric. 2. When the fabrics touched on the copper plates, the thickness of wool fabric had a negative correlation to the $q_{max}$. The thermal transmittance had a positive correlation. Both of them had a good correlation to the $q_{max}$. 3. As a major factor, the thickness of fabric effected on the $q_{max}$.

  • PDF

랫드에 주입된 국내산 암면의 호흡기 독성 및 생체내구성 평가 (Domestic Rock Wool Toxicity Study on Respiratory System and Biopersistence Evaluation in Sprague-Dawely Rats)

  • 정용현;한정희;강민구;이성배;김현영
    • 한국산업보건학회지
    • /
    • 제19권2호
    • /
    • pp.127-138
    • /
    • 2009
  • Rock wool, a kind of asbestos substitutes, was analyzed for its physicochemical properties. After fivers of rock wool were instilled into rat lungs, These pathological changes were evaluated. In addition, the fibers in the lungs were counted and characterized after the lungs were treated for electron microscopical analysis. The lungs of rats showed pathological lesions such as granulomatous changes, but these lesions disappeared at 28 days groups after instilled rats. The rock wool fibers in the lungs decreased more 50 % after 28 days instilled into rat lungs. And rock wool showed early change in fiber compositions after 3 days compare with chrysotile showed after 7 days instilled into rat lungs. This study showed that the durability of rock wool in the lungs is more milder than chrysotile.

줄풀염색에 의한 모직물의 염색성과 기능성 (Dyeability and Functionality of Wool Fabrics Dyed with Zizania latifolia Turcz. extract)

  • 고은숙;이혜선
    • 한국의류산업학회지
    • /
    • 제21권2호
    • /
    • pp.231-236
    • /
    • 2019
  • This study investigated the proper dyeing conditions, color fastness and functionality of wool fabrics dyed with Zizania latifolia Turcz. We also tried to improve light fastness through treatment with benzophenone ultraviolet absorber. The dyeing of wool fabrics using Zizania latifolia Turcz was good even without pretreatment or mordanting treatment. Optimal wool fabric dyeing conditions were colorant concentration of 200% (o.w.f.), dyeing temperature of $100^{\circ}C$, dyeing time of 80 minutes and a dye bath pH of 3. Color fastness of dyed wool fabrics to washing, rubbing, perspiration and light was 4-5, 5, 4-4-5 (acidic), 4-5 (alkaline) and 2 respectively. The results after treatment with ultraviolet absorber for improving the fastness of daylight were improved to 3-4 grade. The UV protection rate were increased after dyeing and the deodorization of ammonia gas improved to 98%. Bacterial reduction rate (Staphylococcus aureus) of wool fabrics was excellent at 99.9%. All dye fastness (except for light fastness) was excellent; in addition, the functionality of wool fabrics dyed with Zizania latifolia Turcz also improved. The results are expected to be applied to various fields because they indicate excellent results after treatment with ultraviolet absorber for improving the fastness of daylight.